CN103044940A - 一种环保型木塑料铅笔笔杆及其生产方法 - Google Patents

一种环保型木塑料铅笔笔杆及其生产方法 Download PDF

Info

Publication number
CN103044940A
CN103044940A CN2011103076329A CN201110307632A CN103044940A CN 103044940 A CN103044940 A CN 103044940A CN 2011103076329 A CN2011103076329 A CN 2011103076329A CN 201110307632 A CN201110307632 A CN 201110307632A CN 103044940 A CN103044940 A CN 103044940A
Authority
CN
China
Prior art keywords
powder
lubricant
wood
environment
pencil
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2011103076329A
Other languages
English (en)
Inventor
傅文进
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
YIWU SHUNYI STATIONERY CO Ltd
Original Assignee
YIWU SHUNYI STATIONERY CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by YIWU SHUNYI STATIONERY CO Ltd filed Critical YIWU SHUNYI STATIONERY CO Ltd
Priority to CN2011103076329A priority Critical patent/CN103044940A/zh
Publication of CN103044940A publication Critical patent/CN103044940A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种塑料铅笔笔杆,其中笔杆料包括:复合稳定剂、PVC树脂、植物粉(如木粉、竹粉、玉米杆粉、麦杆粉等)、润滑剂(外)、润滑剂(内)、环保增塑剂、腊、硬脂酸、橡胶、ACR、工程塑料(ABS)、AC发刨剂、成型调节剂、石墨。其重量配比为:复合稳定剂0.5%-10%、PVC树脂10%-50%、植物粉(如木粉、竹粉、玉米杆粉、麦杆粉等)10%-80%、润滑剂(外)1%-10%、润滑剂(内)1%-10%、环保增塑剂1%-10%、腊1%-10%、硬脂酸1%-10%、橡胶1%-10%、ACR1%-10%、工程塑料(ABS)1%-15%、AC发刨剂1%-10%、成型调节剂5%-15%、石墨5%-25%。本发明外形与木制铅笔相同,书写流利、光滑,切削、卷削容易,字迹易擦,价格低于木制铅笔,可节约大量木材。

Description

一种环保型木塑料铅笔笔杆及其生产方法
本发明涉及一种文具的制造方法,一种特别的环保、节能型塑料铅笔笔杆及其生产方法。
目前,公知的铅笔笔杆多采用木制,需要消耗大量的木材,且因有些树种的材质问题,木材利用率相对低下。加工过程较复杂,成本高,与目前所倡导的绿色环保精神相悖。
本发明的目的是提供一种新型环保节能型塑料铅笔笔杆及其生产方法,它不仅具有与木杆铅笔一样的粗细度和密度适中、均匀性好不亚于木杆铅笔的塑杆铅笔,且减少了木材的使用,保护了生态环境,减少环境污染。符合绿色环保要求。
本发明的技术方案是铅笔笔杆料为木塑,笔杆料包括:复合稳定剂、PVC树脂、植物粉(如木粉、竹粉、玉米杆粉、麦杆粉等)、润滑剂(外)、润滑剂(内)、环保增塑剂、腊、硬脂酸、橡胶、ACR、工程塑料(ABS)、AC发刨剂、成型调节剂、石墨。其重量配比为:复合稳定剂0.5%-10%、PVC树脂10%-50%、植物粉(如木粉、竹粉、玉米杆粉、麦杆粉等)10%-80%、润滑剂(外)1%-10%、润滑剂(内)1%-10%、环保增塑剂1%-10%、腊1%-10%、硬脂酸1%-10%、橡胶1%-10%、ACR1%-10%、工程塑料(ABS)1%-15%、AC发刨剂1%-10%、成型调节剂5%-15%、石墨5%-25%。
本发明制作工艺包括以下步骤:
(1)配料:按上述配比将笔杆料配制好,对其进行混合。
(2)造粒:采用小于12mm的粒度。
(3)挤出:将有粒度的笔杆料投入挤出机,挤出时的温度控制在100-220℃之间,挤出机的可控螺杆转速为10-100转。
(4)复合:经挤出机的笔杆料进入模具,进入模具的温度控制在220℃以下。
(5)定型冷却:笔杆料成型后进入定型模定型,再进入循环冷却槽冷却。
(6)切断整理:冷却后进入切断机,按照尺寸要求进行切断,最后进行表面的磨光,打字整理得到成品。
本发明外形与木制铅笔相同,切削、卷削容易,满足铅笔国家标准的要求,价格低于木制铅笔,有利于保护林木资源和改善生态环境。
具体实施方式
实施例1:笔杆料以100公斤计算,取植物粉48公斤、PVC粉16公斤、复合稳定剂3公斤、工程塑料(ABS)10公斤、共聚物(SBS)8公斤、内外滑剂10公斤、环保增塑剂2公斤、AC发泡剂、硬脂酸锌3公斤。
按上述配比将笔杆料配制好,对其进行2次混合,采用小于12mm的粒度,将有粒度的笔杆料投出挤出机,挤出时的温度控制在180℃,挤出机的可控螺杆转速为60转,经挤出机的笔杆料进入复合模,进入模具的温度控制在160℃,复合成型后进入定型模定型,再进入循环冷却槽冷却,冷却后进入切割机,按尺寸要求进行切断,最后进行表面的磨光、打字整理得到成品。
实施例2:笔杆料以100公斤计算。
取聚乙烯35公斤、植物粉35公斤、复合稳定剂6公斤、工程塑料(ABS)5公斤、共聚物(SBS)5公斤、内外滑剂8公斤、环保增塑剂2公斤、AC发泡剂、硬脂酸4公斤。
按上述配比将笔杆料配制好,对其进行2次混合,采用小于12mm的粒度,将有粒度的笔杆料投出挤出机,挤出时的温度控制在175℃,挤出机的可控螺杆转速为70转,经挤出机的笔杆料进入复合模,进入模具的温度控制在165℃,复合成型后进入定型模定型,再进入循环冷却槽冷却,冷却后进入切割机,按尺寸要求进行切断,最后进行表面的磨光、打字整理得到成品。

Claims (2)

1.一种塑料铅笔的制造方法,其特征在于铅笔笔杆是有塑料注塑成型,塑料的成分包括主料有复合稳定剂、PVC树脂、植物粉(如木粉、竹粉、玉米杆粉、麦杆粉等)、润滑剂(外)、润滑剂(内)、环保增塑剂、腊、硬脂酸、橡胶、ACR、工程塑料(ABS)、AC发刨剂、成型调节剂、石墨。
2.根据权利要求1所述的方法,其特征在于塑料各成分的百分组成是主料:复合稳定剂0.5%-10%、PVC树脂10%-50%、植物粉(如木粉、竹粉、玉米杆粉、麦杆粉等)10%-80%、润滑剂(外)1%-10%、润滑剂(内)1%-10%、环保增塑剂1%-10%、腊1%-10%、硬脂酸1%-10%、橡胶1%-10%、ACR1%-10%、工程塑料(ABS)1%-15%、AC发刨剂1%-10%、成型调节剂5%-15%、石墨5%-25%。
CN2011103076329A 2011-10-12 2011-10-12 一种环保型木塑料铅笔笔杆及其生产方法 Pending CN103044940A (zh)