CN102992679A - 一种石油沥青抗剥剂、制备方法及使用方法 - Google Patents

一种石油沥青抗剥剂、制备方法及使用方法 Download PDF

Info

Publication number
CN102992679A
CN102992679A CN2012105120320A CN201210512032A CN102992679A CN 102992679 A CN102992679 A CN 102992679A CN 2012105120320 A CN2012105120320 A CN 2012105120320A CN 201210512032 A CN201210512032 A CN 201210512032A CN 102992679 A CN102992679 A CN 102992679A
Authority
CN
China
Prior art keywords
parts
stripping agent
gasoline
petroleum pitch
pitch
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2012105120320A
Other languages
English (en)
Other versions
CN102992679B (zh
Inventor
车春玲
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANDONG XINGHUO INTELLECTUAL PROPERTY SERVICE Co.,Ltd.
Original Assignee
SHANDONG TAIDE NEW ENERGY CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANDONG TAIDE NEW ENERGY CO Ltd filed Critical SHANDONG TAIDE NEW ENERGY CO Ltd
Priority to CN201210512032.0A priority Critical patent/CN102992679B/zh
Publication of CN102992679A publication Critical patent/CN102992679A/zh
Application granted granted Critical
Publication of CN102992679B publication Critical patent/CN102992679B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明属于建设材料的技术领域,涉及一种石油沥青抗剥剂、制备方法及使用方法,该石油沥青抗剥剂由按重量计的下述的组分组成:脂肪酸铁盐20-35份,羟基磷酸钙5-10份,季铵盐5-10份,汽油40-80份。此抗剥剂可提高沥青与酸性石料的粘附性,提高沥青混合料的抗水损害能力,改善沥青的抗老性,延长路面使用寿命。

Description

一种石油沥青抗剥剂、制备方法及使用方法
技术领域
本发明属于建设材料的技术领域,涉及一种石油沥青抗剥剂、制备方法及使用方法。
背景技术
剥落是沥青路面最普遍的破坏。沥青膜与集料之间丧失粘结力,并从集料颗粒表面脱落下来,导致路面使用寿命缩短,养护路费增高,而且严重影响沥青路面的使用性能。因此,提高沥青与集料之间的抗剥落性能,是长期以来道路部门和沥青研究领域共同面临的一项重大课题。
抗剥落措施主要有:用干燥的磨细消石灰粉或生石灰粉、水泥作为填料的一部分,其用量宜为矿料总量的1-2%;将粗集料用石灰浆处理后使用;在沥青中掺加抗剥落剂等,目前普遍采用第三种方法。但一般的抗剥落剂在沥青加热过程达到150℃时,容易分解,影响抗剥落效果,而且对于酸性较强的石料吸附能力有限。
针对该难题,本发明提供了一种耐高温、可持续性强、吸附能力强的高效抗剥落剂。将其添加于石油沥青中,可提高道路的抗水损害能力,延长路面使用寿命。
发明内容
本发明的目的就是针对上述存在的缺陷而提供一种石油沥青抗剥剂、制备方法及使用方法,此抗剥剂可提高沥青与酸性石料的粘附性,提高沥青混合料的抗水损害能力吗,改善沥青的抗老性,延长路面使用寿命。
本发明的一种石油沥青抗剥剂技术方案为,是由按重量计的下述的组分组成:脂肪酸铁盐20-35份,羟基磷酸钙5-10份,季铵盐5-10份,汽油40-80份。
优选配方是由按重量计的下述的组分组成:25份脂肪酸铁盐、5份羟基磷酸钙、10份季铵盐和60份汽油。
另一优选配方是由按重量计的下述的组分组成:30份脂肪酸铁盐、10份羟基磷酸钙、6份季铵盐和54份汽油。
该石油沥青抗剥剂制备方法是,称取配方比例的各组分溶于汽油中,加热溶化即可得到。
该石油沥青抗剥剂的使用方法为,将基质沥青加热到170~180℃,边搅拌边加入相当于沥青质量0.5%的按照配方比例配好的抗剥剂,初步混合后用高剪切乳化机以7000 r/min速率剪切搅拌30min,可制得抗剥石油沥青。
本发明的有益效果为:本发明的石油沥青抗剥剂是由按重量计的下述的组分组成:脂肪酸铁盐20-35份,羟基磷酸钙5-10份,季铵盐5-10份,汽油40-80份。脂肪酸铁盐和季铵盐可以与沥青互溶,其对石料的结合力大于水与石料的结合力,使沥青与石料紧密结合,有效抵制水的进入;羟基磷酸钙起巩固结合的作用,并可隔离水分;汽油具有氧化安定性,可防止氧气对沥青的损害。
利用本发明的抗剥剂可提高沥青与酸性石料的粘附性,提高沥青混合料的抗水损害能力吗,改善沥青的抗老性,延长路面使用寿命。另外,本发明提供的方法具有工艺流程简单、操作方便、成本低等优点。
具体实施方式:
为了更好地理解本发明的技术方案,以下通过具体的实施例进一步作详细描述。
实施例1
按20份脂肪酸铁盐、10份羟基磷酸钙、5份季铵盐和65份汽油的比例加热融化制得抗剥剂A,将基质沥青加热到170~180℃,边搅拌边加入相当于沥青质量0.5%的按照配方比例配好的抗剥剂,初步混合后用高剪切乳化机以7000 r/min速率剪切搅拌30min,可制得抗剥石油沥青A。
实施例2
按30份脂肪酸铁盐、8份羟基磷酸钙、6份季铵盐和56份汽油的比例加热融化制得抗剥剂A,将基质沥青加热到170~180℃,边搅拌边加入相当于沥青质量0.5%的按照配方比例配好的抗剥剂,初步混合后用高剪切乳化机以7000 r/min速率剪切搅拌30min,可制得抗剥石油沥青B。
实施例3
按25份脂肪酸铁盐、5份羟基磷酸钙、10份季铵盐和60份汽油的比例加热融化制得抗剥剂A,将基质沥青加热到170~180℃,边搅拌边加入相当于沥青质量0.5%的按照配方比例配好的抗剥剂,初步混合后用高剪切乳化机以7000 r/min速率剪切搅拌30min,可制得抗剥石油沥青C。
实施例4
按35份脂肪酸铁盐、6份羟基磷酸钙、8份季铵盐和51份汽油的比例加热融化制得抗剥剂A,将基质沥青加热到170~180℃,边搅拌边加入相当于沥青质量0.5%的按照配方比例配好的抗剥剂,初步混合后用高剪切乳化机以7000 r/min速率剪切搅拌30min,可制得抗剥石油沥青D。
实施例5
按30份脂肪酸铁盐、10份羟基磷酸钙、6份季铵盐和54份汽油的比例加热融化制得抗剥剂A,将基质沥青加热到170~180℃,边搅拌边加入相当于沥青质量0.5%的按照配方比例配好的抗剥剂,初步混合后用高剪切乳化机以7000 r/min速率剪切搅拌30min,可制得抗剥石油沥青E。
测试实施例:
将10kg基质沥青加热到170~180℃, 边搅拌边加入50g抗剥剂A、B、C、D、E,初步混合后用高剪切乳化机以7000 r/min速率剪切搅拌30min,可制得抗剥沥青样品A、B、C、D、E。分别对沥青A、B、C、D、E水煮粘附度指标进行了测试,结果见表1。结果显示:添加了本发明提供的抗剥剂后,沥青水煮粘附度有大幅改善。
表 1
Figure 2012105120320100002DEST_PATH_IMAGE001

Claims (5)

1. 一种石油沥青抗剥剂,其特征在于,是由按重量计的下述的组分组成:脂肪酸铁盐20-35份,羟基磷酸钙5-10份,季铵盐5-10份,汽油40-80份。
2. 根据权利要求1所述的一种石油沥青抗剥剂,其特征在于,是由按重量计的下述的组分组成:25份脂肪酸铁盐、5份羟基磷酸钙、10份季铵盐和60份汽油。
3. 根据权利要求1所述的一种石油沥青抗剥剂,其特征在于,是由按重量计的下述的组分组成:30份脂肪酸铁盐、10份羟基磷酸钙、6份季铵盐和54份汽油。
4. 一种如权利要求1-3任一所述的石油沥青抗剥剂制备方法,其特征在于,称取配方比例的各组分溶于汽油中,加热溶化即可得到。
5. 如权利要求4所述的制备方法制取的石油沥青抗剥剂的使用方法,其特征在于,将基质沥青加热到170~180℃,边搅拌边加入相当于沥青质量0.5%的按照配方比例配好的抗剥剂,初步混合后用高剪切乳化机以7000 r/min速率剪切搅拌30min,可制得抗剥石油沥青。
CN201210512032.0A 2012-12-04 2012-12-04 一种石油沥青抗剥剂、制备方法及使用方法 Active CN102992679B (zh)