CN102977871A - 环空保护液 - Google Patents
环空保护液 Download PDFInfo
- Publication number
- CN102977871A CN102977871A CN2012105066400A CN201210506640A CN102977871A CN 102977871 A CN102977871 A CN 102977871A CN 2012105066400 A CN2012105066400 A CN 2012105066400A CN 201210506640 A CN201210506640 A CN 201210506640A CN 102977871 A CN102977871 A CN 102977871A
- Authority
- CN
- China
- Prior art keywords
- protection fluid
- casings
- underground
- annulus protection
- oil pipes
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种抑制井下油管和套管腐蚀的环空保护液,它的组成成分及各成分质量百分比为:三乙醇胺20%~30%,钼酸钠30~45%,水25~40%。这种环空保护液主要用于保护油管和套管不受腐蚀以及井下注水封隔器能够安全起出,根据油管和套管的井下腐蚀状况,优选出环空保护液的使用浓度。该保护液稳定性好,对钢片的腐蚀性低,腐蚀速率低于0.075mm/a,在井下对油管和套管能起到很好的保护作用。
Description
技术领域:
本发明涉及防腐试剂,具体地说是一种抑制井下油管和套管腐蚀的环空保护液。
背景技术:
油田开始采用无套压力注水工艺,为保护套管不受腐蚀以及井下注水封隔器能够安全起出,需要在套管环空中注入保护液。在静置阶段,处于油管和套管间的环空水,实质上是具有一定矿化度的电解质溶液,除配液水本身固有的离子外,还有添加的可溶性加重剂、防腐剂和缓蚀剂等。油管和套管大部分浸泡在这种电解质溶液中,会产生相应的电化学反应,加之溶解氧、二氧化碳和氯离子引起的腐蚀,而氯离子引起的腐蚀尤为严重,因此在设计环空保护液时要考虑多方面因素。
发明内容:
为解决以上所述油管和套管的腐蚀问题,本发明提供一种环空保护液,采用以下技术方案实现:它的组成分及各成分质量百分比为:三乙醇胺20%~30%,钼酸钠30~45%,水25~40%,将其各成分按其质量百分比混合搅拌均即可。
本发明环空保护液主要用于保护油管和套管不受腐蚀以及井下注水封隔器能够安全起出,需要在套管环空中注入。该保护液具有良好的稳定性和防腐性,在修井或投产时既保护油管和套管不受腐蚀又不伤害油气层。
具体实施方式
下面结合实施例对本发明作进一步说明。
实施例一:
名称 | 三乙醇胺 | 钼酸钠 | 水 |
配比 | 25 | 40 | 35 |
将该表格中的各组成成分按照其配比中的质量百分比混合均匀即可使用。
实施例二:
名称 | 三乙醇胺 | 钼酸钠 | 水 |
配比 | 30 | 40 | 30 |
将该表格中的各组成成分按照其配比中的质量百分比混合均匀即可使用。
根据套管和油管的井下腐蚀状况,优选出环空保护液的使用浓度。该保护液稳定性好,对钢片的腐蚀性低,腐蚀速率低于0.075mm/a,在井下对油管和套管能起到很好的保护作用。
Claims (1)
1.一种用于抑制井下油管和套管腐蚀的环空保护液,其特征是,它的组成成分及各成分质量百分比为:三乙醇胺20%~30%,钼酸钠30~45%,水25~40%。