- CN102837421A CN102837421A CN2011101695555A CN201110169555A CN102837421A CN 102837421 A CN102837421 A CN 102837421A CN 2011101695555 A CN2011101695555 A CN 2011101695555A CN 201110169555 A CN201110169555 A CN 201110169555A CN 102837421 A CN102837421 A CN 102837421A
- Authority
- CN
- China
- Prior art keywords
- structural member
- inner casing
- composite material
- thermosetting compound
- same
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Moulding By Coating Moulds (AREA)
- Laminated Bodies (AREA)
Abstract
本发明提供一种复合材料结构件制程及其结构,其利用一预先成型的塑胶内壳,再覆上预定的热固型复材结构,置入模具中,再予以充压加热成型,借由上述制造方法,内壳除提供加热成型的充压使用,加热成型后,使内壳与复材结构件结合,可以提升复材结构件整体强度及韧性,并减少习用制程中充气的预备流程,可有效降低生产成本,降低工时,提高产品良率,使整体极具创新及产业实用性。
Description
技术领域
本发明涉及一种复合材料,尤其是一种复合材料结构件制程及其结构。
背景技术
本发明提供一种复合材料结构件制程及其结构,其利用一预先成型的塑胶内壳,再覆上预定的热固型复材结构,置入模具中,再予以充压加热成型,借由上述制造方法,内壳除提供加热成型的充压使用,加热成型后,使内壳与复材结构件结合,可以提升复材结构件整体强度及韧性,并减少习用制程中充气的预备流程,可有效降低生产成本,降低工时,提高产品良率,使整体极具创新及产业实用性。
一种复合材料结构件制程,其包括:A、以塑胶材料预先成形一与结构件造型相仿的内壳,内壳并连接一充气口;B、包覆预定的热固性复合材料于内壳外;C、将上述已包覆热固性复合材料的预成形结构件置入模具中,并将模具夹合于加热油压台平台中;D、由充气口加入预先设定的气压,撑起内壳,使热固性复合材料贴附模具;E、模具受热传导至热固性复合材料,使其固化成型,完成热固性复合材料结构件,其特征二在于:该内壳可选用HDPE、NYLON、PE、PVC、PET、PEEK、PC、ABS等塑胶材料制作,其特征三在于:该热固性复合材料可为预浸树脂之碳纤维或玻璃纤维等预浸纤维布或预浸编织纤维布,其特征四在于:该内壳仅有一充气口,其特征五在于:以塑胶内壳,该内壳稍小于结构件,形状与轮廓与结构件相仿,再包覆热固型复合材料,加热固化成型的热固型复合材料结构件,其不仅可以提高整体结构的强度及韧性,其制作程序可以简化,也可以节省生产成本,降低不良率。
发明内容
针对上述问题,本发明提供一种复合材料结构件制程及其结构。
本发明提供一种复合材料结构件制程及其结构,其利用一预先成型的塑胶内壳,再覆上预定的热固型复材结构,置入模具中,再予以充压加热成型,借由上述制造方法,内壳除提供加热成型的充压使用,加热成型后,使内壳与复材结构件结合,可以提升复材结构件整体强度及韧性,并减少习用制程中充气的预备流程,可有效降低生产成本,降低工时,提高产品良率,使整体极具创新及产业实用性。
一种复合材料结构件制程,其包括:A、以塑胶材料预先成形一与结构件造型相仿的内壳,内壳并连接一充气口;B、包覆预定的热固性复合材料于内壳外;C、将上述已包覆热固性复合材料的预成形结构件置入模具中,并将模具夹合于加热油压台平台中;D、由充气口加入预先设定的气压,撑起内壳,使热固性复合材料贴附模具;E、模具受热传导至热固性复合材料,使其固化成型,完成热固性复合材料结构件,其特征二在于:该内壳可选用HDPE、NYLON、PE、PVC、PET、PEEK、PC、ABS等塑胶材料制作,其特征三在于:该热固性复合材料可为预浸树脂之碳纤维或玻璃纤维等预浸纤维布或预浸编织纤维布,其特征四在于:该内壳仅有一充气口,其特征五在于:以塑胶内壳,该内壳稍小于结构件,形状与轮廓与结构件相仿,再包覆热固型复合材料,加热固化成型的热固型复合材料结构件,其不仅可以提高整体结构的强度及韧性,其制作程序可以简化,也可以节省生产成本,降低不良率。
具体实施方式
本发明提供一种复合材料结构件制程及其结构,其利用一预先成型的塑胶内壳,再覆上预定的热固型复材结构,置入模具中,再予以充压加热成型,借由上述制造方法,内壳除提供加热成型的充压使用,加热成型后,使内壳与复材结构件结合,可以提升复材结构件整体强度及韧性,并减少习用制程中充气的预备流程,可有效降低生产成本,降低工时,提高产品良率,使整体极具创新及产业实用性。
一种复合材料结构件制程,其包括:A、以塑胶材料预先成形一与结构件造型相仿的内壳,内壳并连接一充气口;B、包覆预定的热固性复合材料于内壳外;C、将上述已包覆热固性复合材料的预成形结构件置入模具中,并将模具夹合于加热油压台平台中;D、由充气口加入预先设定的气压,撑起内壳,使热固性复合材料贴附模具;E、模具受热传导至热固性复合材料,使其固化成型,完成热固性复合材料结构件,其特征二在于:该内壳可选用HDPE、NYLON、PE、PVC、PET、PEEK、PC、ABS等塑胶材料制作,其特征三在于:该热固性复合材料可为预浸树脂之碳纤维或玻璃纤维等预浸纤维布或预浸编织纤维布,其特征四在于:该内壳仅有一充气口,其特征五在于:以塑胶内壳,该内壳稍小于结构件,形状与轮廓与结构件相仿,再包覆热固型复合材料,加热固化成型的热固型复合材料结构件,其不仅可以提高整体结构的强度及韧性,其制作程序可以简化,也可以节省生产成本,降低不良率。
Claims (5)
1.一种复合材料结构件制程,其包括:A、以塑胶材料预先成形一与结构件造型相仿的内壳,内壳并连接一充气口;B、包覆预定的热固性复合材料于内壳外;C、将上述已包覆热固性复合材料的预成形结构件置入模具中,并将模具夹合于加热油压台平台中;D、由充气口加入预先设定的气压,撑起内壳,使热固性复合材料贴附模具;E、模具受热传导至热固性复合材料,使其固化成型,完成热固性复合材料结构件。
2.如权利要求1所述的复合材料结构件制程,其特征在于:该内壳可选用HDPE、NYLON、PE、PVC、PET、PEEK、PC、ABS等塑胶材料制作。
3.如权利要求1所述的复合材料结构件制程,其特征在于:该热固性复合材料可为预浸树脂之碳纤维或玻璃纤维等预浸纤维布或预浸编织纤维布。
4.如权利要求1所述的复合材料结构件制程,其特征在于:该内壳仅有一充气口。
5.一种复合材料结构件制程所制成的结构件,其特征在于:以塑胶内壳,该内壳稍小于结构件,形状与轮廓与结构件相仿,再包覆热固型复合材料,加热固化成型的热固型复合材料结构件,其不仅可以提高整体结构的强度及韧性,其制作程序可以简化,也可以节省生产成本,降低不良率。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2011101695555A CN102837421A (zh) | 2011-06-22 | 2011-06-22 | 复合材料结构件制程及其结构 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2011101695555A CN102837421A (zh) | 2011-06-22 | 2011-06-22 | 复合材料结构件制程及其结构 |
Publications (1)
Publication Number | Publication Date |
---|---|
CN102837421A true CN102837421A (zh) | 2012-12-26 |
Family
ID=47365268
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN2011101695555A Pending CN102837421A (zh) | 2011-06-22 | 2011-06-22 | 复合材料结构件制程及其结构 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN102837421A (zh) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103331899A (zh) * | 2013-07-17 | 2013-10-02 | 厦门新旺新材料科技有限公司 | 一种新型复材加工成型气袋 |
CN113103707A (zh) * | 2021-04-27 | 2021-07-13 | 南充旭阳塑料制造有限公司 | 一种pet玄武岩纤维复合板材及其制备方法 |
Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4619374A (en) * | 1984-05-21 | 1986-10-28 | Ecodyne Corporation | Pressure vessel with an improved sidewall structure |
CN1429511A (zh) * | 2001-12-31 | 2003-07-16 | 厦门新凯复材科技有限公司 | 复材安全帽壳的制法 |
CN101041265A (zh) * | 2006-03-24 | 2007-09-26 | 王景辉 | 一种便于用碳素纤维成形异型壳体产品的制作方法 |
CN101913270A (zh) * | 2010-07-23 | 2010-12-15 | 哈尔滨工业大学 | 一种可折叠-展开的形状记忆支撑管及其制备方法 |
-
2011
- 2011-06-22 CN CN2011101695555A patent/CN102837421A/zh active Pending
Patent Citations (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4619374A (en) * | 1984-05-21 | 1986-10-28 | Ecodyne Corporation | Pressure vessel with an improved sidewall structure |
CN1429511A (zh) * | 2001-12-31 | 2003-07-16 | 厦门新凯复材科技有限公司 | 复材安全帽壳的制法 |
CN101041265A (zh) * | 2006-03-24 | 2007-09-26 | 王景辉 | 一种便于用碳素纤维成形异型壳体产品的制作方法 |
CN101913270A (zh) * | 2010-07-23 | 2010-12-15 | 哈尔滨工业大学 | 一种可折叠-展开的形状记忆支撑管及其制备方法 |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103331899A (zh) * | 2013-07-17 | 2013-10-02 | 厦门新旺新材料科技有限公司 | 一种新型复材加工成型气袋 |
CN103331899B (zh) * | 2013-07-17 | 2015-06-24 | 厦门新旺新材料科技有限公司 | 一种复材加工成型气袋 |
CN113103707A (zh) * | 2021-04-27 | 2021-07-13 | 南充旭阳塑料制造有限公司 | 一种pet玄武岩纤维复合板材及其制备方法 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN106103013B (zh) | 臂端工具 | |
CN102285017B (zh) | 碳纤维外壳的制造方法 | |
WO2013130184A3 (en) | Molded composite threads | |
EP2233625A4 (en) | Reinforcing fiber base of curved shape, layered product employing the same, preform, fiber-reinforced resin composite material, and processes for producing these | |
MX2014001308A (es) | Metodo para fabricar articulo formado mediante moldeado a baja presion. | |
CN102765198A (zh) | 复合材料真空辅助模压成型系统及成型方法 | |
WO2011101093A3 (de) | Verfahren zur herstellung von pellets aus faserverbundwerkstoffen | |
CN103770343B (zh) | 一种高性能纤维复合材料制品的制备方法 | |
US20190337243A1 (en) | Method for molding hollow vehicle part, hollow vehicle part and automobile | |
WO2011158172A3 (en) | Mould made of a composite material, as well as master and process for its manufacturing | |
CN101585236A (zh) | 复合材料异形产品成型工艺 | |
CN105346099A (zh) | 一种碳纤维复合材料薄壁曲线管件的制备方法 | |
CN105619840B (zh) | 碳纤维复合材料同步成型涂装工艺 | |
MY173821A (en) | Resin-soluble veils for composite article fabrication and methods of manufacturing the same | |
CN104015376A (zh) | 碳纤维复合材料混合成型方法 | |
CN107735252B (zh) | 加饰片、成形品的制造方法以及成形品 | |
CN107214975B (zh) | 一种模拟涂覆快速成型湿法模压工艺 | |
CN104893252A (zh) | 一种用于汽车上的碳纤维装饰条的制备方法 | |
CN105881929A (zh) | 一种连续纤维织物和lft复合壁板结构的制造方法 | |
CN102837421A (zh) | 复合材料结构件制程及其结构 | |
CN101417502A (zh) | 复合材料结构件及其制造方法 | |
CN207747277U (zh) | 一种多腔复合材料结构件及其成型模具 | |
CN109843564A (zh) | 复合片材及其制造方法 | |
CN103696123B (zh) | 化学纤维与天然木皮混合编织的复合材料及其制备方法 | |
CN104908376A (zh) | 自然纤维片材热塑性制作方法、片材和手机壳的制作方法 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C06 | Publication | ||
PB01 | Publication | ||
C10 | Entry into substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
WD01 | Invention patent application deemed withdrawn after publication |
Application publication date: 20121226 |