CN102728577A - Method for improving surface tension of glass plastic accessory - Google Patents
Method for improving surface tension of glass plastic accessory Download PDFInfo
- Publication number
- CN102728577A CN102728577A CN2012102057749A CN201210205774A CN102728577A CN 102728577 A CN102728577 A CN 102728577A CN 2012102057749 A CN2012102057749 A CN 2012102057749A CN 201210205774 A CN201210205774 A CN 201210205774A CN 102728577 A CN102728577 A CN 102728577A
- Authority
- CN
- China
- Prior art keywords
- glass plastic
- heating
- glass
- surface tension
- annex
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention provides a method for improving surface tension of a glass plastic accessory in the technical field of glass production. The method for improving the surface tension of the glass plastic accessory comprises the following steps of: 1) adding deionized water (3) into a heating container (1) for heating the glass plastic accessory; 2) before the glass plastic accessory (2) is put into the heating container (1), heating the deionized water (3), and then putting the glass plastic accessory (2) into the heating container (1) for hot boiling; and 3) continuously heating the deionized water (3) in the heating container (1) for 20 to 60 minutes. By adopting the technical scheme, under the condition that the material of the glass plastic accessory is not damaged, residual release agent or grease on the surface of the plastic accessory can be well removed, an optimal cleaning effect is achieved, and the thermal stability of the glass plastic accessory in a bonding technology is improved. Meanwhile, adverse effects of chemical reagents adopted in the prior art on human body and environment can be avoided, and an environment-friendly effect is achieved.
Description
Technical field
The invention belongs to field of glass production technology, more particularly, relate to a kind of process that improves glass plastic attachment surface tension force.
Background technology
For improving the surface tension of glass plastic annex, improve the stability of glass plastic annex in technique for sticking, need the glass plastic parts surface is cleaned.In the prior art, be to adopt butanone or alcohol that the glass plastic annex is soaked, dries processing.But existing this method, the chemical reagent use amount is bigger, and cost is higher, and discarded butanone or alcohol have negative effect to human body, environment, are unfavorable for environmental protection.Meanwhile, even segment glass plastics annex is after using butanone or alcohol-pickled processing, still handles and do not fall material surface releasing agent, grease, thereby influence the stability of glass plastic annex in barbola work.
Summary of the invention
Technical problem to be solved by this invention is: to the deficiency of prior art; A kind of negative effect that can avoid the chemical reagent of glass plastic annex in bonding to human body, environment is provided, improves the process of the raising glass plastic attachment surface tension force of glass plastic attachment surface tension force simultaneously.
Solve above-described technical problem, the technical scheme that the present invention takes is:
The present invention is a kind of process that improves glass plastic attachment surface tension force, and the step of the process of described raising glass plastic attachment surface tension force is:
1) in the heating container that is used for heating glass plastics annex, adds deionized water;
2) in heating container, put into the glass plastic annex before, add hot deionized water, put into the glass plastic annex then and carry out heat and boil;
3) deionized water in the heating container is continued heating 20-60min.
Described glass plastic annex is carried out heat when boiling, different glass plastic annexes should be in batches glass container heat boil or in different glass containers heat boil.
The glass plastic annex is carried out heat when boiling, change deionized water when each heat is boiled.
Before in heating container, putting into the glass plastic annex, the temperature of the ion that anhydrates is heated between 90 ℃-100 ℃.
When the deionized water in the heating container is continued heating, the heating-up temperature of deionized water is remained between 90 ℃-100 ℃.
When the deionized water in the heating container is continued heating, be controlled at heat time heating time between 30-40min, after described glass plastic annex heat is boiled completion, the glass plastic annex dried, and then the glass plastic annex is carried out subsequent job.
Described heating container is set to the structure through the Electric heating heating.
Adopt technical scheme of the present invention, can obtain following beneficial effect:
The process of raising glass plastic attachment surface tension force of the present invention; Do not destroying under the glass plastic annex material situation; The process of using elevated temperature heat to boil; Not only can better remove releasing agent, the grease of working of plastics remained on surface, reach best cleaning effect, improve the stability of glass plastic annex in technique for sticking.Simultaneously, the process that adopts heat to boil can be avoided the negative effect of available technology adopting chemical reagent to human body, environment, reaches the effect of environmental protection.
Description of drawings
The mark of facing down among expressed content of each accompanying drawing of this specification and the figure is made briefly bright:
Fig. 1 is the structural representation of the heating container of raising glass plastic attachment surface tension force;
Fig. 2 is the process chart of the process of raising glass plastic attachment surface tension force of the present invention;
Mark among the figure: 1, heating container; 2, glass plastic annex; 3, deionized water.
The specific embodiment
Contrast accompanying drawing below; Through the description to embodiment, the effect of mutual alignment between the shape of specific embodiments of the invention such as related each member, structure, the each several part and annexation, each several part and operation principle etc. are done further to specify:
Shown in accompanying drawing 1, accompanying drawing 2, the present invention is a kind of process that improves glass plastic attachment surface tension force, and the step of the process of described raising glass plastic attachment surface tension force is:
1) in the heating container 1 that is used for heating glass plastics annex, adds deionized water 3;
2) in heating container 1, put into glass plastic annex 2 before, add hot deionized water 3, put into glass plastic annex 2 then and carry out heat and boil;
3) deionized water in the heating container 13 is continued heating 20-60min.
Described glass plastic annex 2 is carried out heat when boiling, different glass plastic annexes 2 should be in batches glass container 1 heat boil or in different glass container 1 heat boil.
Glass plastic annex 2 is carried out heat when boiling, change deionized water 3 when each heat is boiled.The deionized water that each heat must more renew when boiling, the glass plastic annex of unlike material can not mix and carries out poach simultaneously, because the heat of mixing is boiled influencing the stability of glass plastic annex in technique for sticking greatly.
Before in heating container 1, putting into glass plastic annex 2, the temperature of the ion 3 that anhydrates is heated between 90 ℃-100 ℃.
When the deionized water in the heating container 13 is continued heating, the heating-up temperature of deionized water 3 is remained between 90 ℃-100 ℃.
When the deionized water in the heating container 13 is continued heating, be controlled at heat time heating time between 30-40min, after described glass plastic annex 2 heat are boiled completion, glass plastic annex 2 dried, and then glass plastic annex 2 is carried out subsequent job.
Described heating container 1 is set to the structure through the Electric heating heating.
The process of raising glass plastic attachment surface tension force of the present invention; Do not destroying under the glass plastic annex material situation; The process of using elevated temperature heat to boil; Not only can better remove releasing agent, the grease of working of plastics remained on surface, reach best cleaning effect, improve the stability of glass plastic annex in technique for sticking.Simultaneously, the process that adopts heat to boil can be avoided the negative effect of available technology adopting chemical reagent to human body, environment, reaches the effect of environmental protection.
Combine accompanying drawing that the present invention has been carried out exemplary description above; Obviously the concrete realization of the present invention does not receive the restriction of aforesaid way; As long as the various improvement of having adopted method design of the present invention and technical scheme to carry out; Or design of the present invention and technical scheme are directly applied to other occasions without improving, all in protection scope of the present invention.
Claims (7)
1. process that improves glass plastic attachment surface tension force, it is characterized in that: the step of the process of described raising glass plastic attachment surface tension force is:
1) in the heating container that is used for heating glass plastics annex (1), adds deionized water (3);
2) it is preceding in heating container (1), to put into glass plastic annex (2), adds hot deionized water (3), puts into glass plastic annex (2) then and carries out heat and boil;
3) deionized water (3) in the heating container (1) is continued heating 20-60min.
2. the process of raising glass plastic attachment surface tension force according to claim 1; It is characterized in that: described glass plastic annex (2) is carried out heat when boiling, different glass plastic annexes (2) should be in batches glass container (1) heat boil or in different glass container (1) heat boil.
3. the process of raising glass plastic attachment surface tension force according to claim 1 and 2 is characterized in that: glass plastic annex (2) is carried out heat when boiling, change deionized water (3) when each heat is boiled.
4. the process of raising glass plastic attachment surface tension force according to claim 3 is characterized in that: it is preceding in heating container (1), to put into glass plastic annex (2), and the temperature of the ion (3) that will anhydrate is heated between 90 ℃-100 ℃.
5. the process of raising glass plastic attachment surface tension force according to claim 4 is characterized in that: when the deionized water (3) in the heating container (1) is continued heating, the heating-up temperature of deionized water (3) is remained between 90 ℃-100 ℃.
6. the process of raising glass plastic attachment surface tension force according to claim 5; It is characterized in that: when the deionized water (3) in the heating container (1) is continued heating; Be controlled at heat time heating time between 30-40min; After described glass plastic annex (2) heat is boiled completion, glass plastic annex (2) is dried, and then glass plastic annex (2) is carried out subsequent job.
7. the process of raising glass plastic attachment surface tension force according to claim 6 is characterized in that: described heating container (1) is set to the structure through the Electric heating heating.