CN102697197A - Manufacture method for woolen sweater with ironed diamonds - Google Patents

Manufacture method for woolen sweater with ironed diamonds Download PDF

Info

Publication number
CN102697197A
CN102697197A CN2012102099205A CN201210209920A CN102697197A CN 102697197 A CN102697197 A CN 102697197A CN 2012102099205 A CN2012102099205 A CN 2012102099205A CN 201210209920 A CN201210209920 A CN 201210209920A CN 102697197 A CN102697197 A CN 102697197A
Authority
CN
China
Prior art keywords
woollen sweater
clothing
sweater
rhinestone
ironing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012102099205A
Other languages
Chinese (zh)
Inventor
杜士良
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TAICANG SHARTEX SHENTAI SWEATER CO Ltd
Original Assignee
TAICANG SHARTEX SHENTAI SWEATER CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TAICANG SHARTEX SHENTAI SWEATER CO Ltd filed Critical TAICANG SHARTEX SHENTAI SWEATER CO Ltd
Priority to CN2012102099205A priority Critical patent/CN102697197A/en
Publication of CN102697197A publication Critical patent/CN102697197A/en
Pending legal-status Critical Current

Abstract

The invention discloses a manufacture method for a woolen sweater with ironed diamonds. The method is characterized by comprising the steps of making clothes, stitching, pre-inspecting, ironing, designing, ironing diamonds, after-finishing, inspecting quality and packaging. The manufacture method is applicable to industrialized production; by changing the production process of the sweater, the manufacture of the sweater and diamond ironing can be carried out on the same assembly line, so that the production procedures can be simplified, the production efficiency is improved, the production cost is reduced, and the market competitiveness is improved advantageously; and the pre-inspecting and after-finishing are added in the production process, so that operating staff can control the production process better, and finished product ratio is increased.

Description

A kind of preparation method that has the woollen sweater of rhinestone
Technical field
The present invention relates to a kind of preparation method of woollen sweater, especially a kind of preparation method that has the woollen sweater of rhinestone.
Background technology
The Along with people's growth in the living standard also no longer only is confined in the warming pursuit the pursuit of wearing clothes, and people prefer fashionable, clothes beautiful in colour.
Now; Domestic woollen sweater industry is with considerable scale; And the problem that woollen sweater market exists also becomes increasingly conspicuous, the assimilation of Design of Woolen Sweater thinking, and the aspect competition mainly shows on design and the style; In the face of such phenomenon, the design level of woollen sweater has become the key factor of the woollen sweater market competitiveness.
Summary of the invention
Goal of the invention: the objective of the invention is provides a kind of pattern various in order to overcome the deficiency of prior art, the preparation method of the woollen sweater that has rhinestone of good visual effect.
Technical scheme: in order to solve the problems of the technologies described above, a kind of preparation method that has the woollen sweater of rhinestone of the present invention, it is characterized in that: this preparation method may further comprise the steps:
(a) clothing: make the clothing body of woollen sweater, sleeve, collar;
(b) sew up: with wool underwear body, it is an integral body that sleeve, collar are connected;
(c) preceding inspection: the woollen sweater after inspection is sewed up, to screen out clothing defective;
(d) whole scalding: press woollen sweater with flatiron, ironing temperature is 80 ℃-90 ℃;
(e) design: layout is as rhinestone;
(f) rhinestone: with vapour iron brill is bonded on the woollen sweater, described brill is that SW bores in Austria of 14 tangent planes, and ironing temperature is 150 ℃-175 ℃;
(g) back arrangement: cut off the end of a thread on the woollen sweater, order the dress button;
(h) quality inspection;
(i) packing:, transport and dispatch from the factory with the clothing packing.
Design in the said step (e) is treated to adopt diamond ironing machine to arrange after design is accomplished.
Beneficial effect: the present invention is applicable to suitability for industrialized production, through changing the production procedure of woollen sweater, makes woollen sweater make with rhinestone and on same streamline, produces; Simplify production stage, enhance productivity, reduce production costs; Help improving the market competitiveness; Owing to increased preceding inspection and back arrangement step in process of production, make operating personnel can control production process better again, improve yield rate.
The specific embodiment
Below in conjunction with embodiment the present invention is done further detailed description, should understand these embodiment only be used to the present invention is described and be not used in the restriction scope of the present invention.
Embodiment 1:
(a) clothing: make the clothing body of woollen sweater, sleeve, collar;
(b) sew up: with wool underwear body, it is an integral body that sleeve, collar are connected;
(c) preceding inspection: the woollen sweater after inspection is sewed up, to screen out clothing defective;
(d) whole scalding: press woollen sweater with flatiron, ironing temperature is 80 ℃;
(e) design: layout, treat to adopt diamond ironing machine to arrange after design is accomplished;
(f) rhinestone: with vapour iron brill is bonded on the woollen sweater, described brill is that SW bores in Austria of 14 tangent planes, and ironing temperature is 150 ℃;
(g) back arrangement: cut off the end of a thread on the woollen sweater, order the dress button;
(h) quality inspection;
(i) packing:, transport and dispatch from the factory with the clothing packing.
Embodiment 2:
(a) clothing: make the clothing body of woollen sweater, sleeve, collar;
(b) sew up: with wool underwear body, it is an integral body that sleeve, collar are connected;
(c) preceding inspection: the woollen sweater after inspection is sewed up, to screen out clothing defective;
(d) whole scalding: press woollen sweater with flatiron, ironing temperature is 85 ℃;
(e) design: layout, treat to adopt diamond ironing machine to arrange after design is accomplished;
(f) rhinestone: with vapour iron brill is bonded on the woollen sweater, described brill is that SW bores in Austria of 14 tangent planes, and ironing temperature is 160 ℃;
(g) back arrangement: cut off the end of a thread on the woollen sweater, order the dress button;
(h) quality inspection;
(i) packing:, transport and dispatch from the factory with the clothing packing.
Embodiment 3
(a) clothing: make the clothing body of woollen sweater, sleeve, collar;
(b) sew up: with wool underwear body, it is an integral body that sleeve, collar are connected;
(c) preceding inspection: the woollen sweater after inspection is sewed up, to screen out clothing defective;
(d) whole scalding: press woollen sweater with flatiron, ironing temperature is 90 ℃;
(e) design: layout, treat to adopt diamond ironing machine to arrange after design is accomplished;
(f) rhinestone: with vapour iron brill is bonded on the woollen sweater, described brill is that SW, 175 ℃ of ironing temperatures bore in Austria of 14 tangent planes;
(g) back arrangement: cut off the end of a thread on the woollen sweater, order the dress button;
(h) quality inspection;
(i) packing:, transport and dispatch from the factory with the clothing packing.

Claims (2)

1. preparation method that has the woollen sweater of rhinestone, it is characterized in that: this preparation method may further comprise the steps:
(a) clothing: make the clothing body of woollen sweater, sleeve, collar;
(b) sew up: with wool underwear body, it is an integral body that sleeve, collar are connected;
(c) preceding inspection: the woollen sweater after inspection is sewed up, to screen out clothing defective;
(d) whole scalding: press woollen sweater with flatiron, ironing temperature is 80 ℃-90 ℃;
(e) design: layout is as rhinestone;
(f) rhinestone: with vapour iron brill is bonded on the woollen sweater, described brill is that SW bores in Austria of 14 tangent planes, and ironing temperature is 150 ℃-175 ℃;
(g) back arrangement: cut off the end of a thread on the woollen sweater, adorn button surely;
(h) quality inspection;
(i) packing:, transport and dispatch from the factory with the clothing packing.
2. a kind of preparation method that has the woollen sweater of rhinestone according to claim 1 is characterized in that: the design in the said step (e), and after accomplishing, design adopt diamond ironing machine to arrange.
CN2012102099205A 2012-06-25 2012-06-25 Manufacture method for woolen sweater with ironed diamonds Pending CN102697197A (en)