CN102687964A - Method for strengthening drug slow release property in summer sleeping mat - Google Patents

Method for strengthening drug slow release property in summer sleeping mat Download PDF

Info

Publication number
CN102687964A
CN102687964A CN2012101452204A CN201210145220A CN102687964A CN 102687964 A CN102687964 A CN 102687964A CN 2012101452204 A CN2012101452204 A CN 2012101452204A CN 201210145220 A CN201210145220 A CN 201210145220A CN 102687964 A CN102687964 A CN 102687964A
Authority
CN
China
Prior art keywords
sustained release
pressing
adhesive
summer sleeping
sleeping mat
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2012101452204A
Other languages
Chinese (zh)
Other versions
CN102687964B (en
Inventor
张哲玮
黄吉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anji Lvning Bamboo & Wood Industry Co Ltd
Original Assignee
Anji Lvning Bamboo & Wood Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anji Lvning Bamboo & Wood Industry Co Ltd filed Critical Anji Lvning Bamboo & Wood Industry Co Ltd
Priority to CN2012101452204A priority Critical patent/CN102687964B/en
Publication of CN102687964A publication Critical patent/CN102687964A/en
Application granted granted Critical
Publication of CN102687964B publication Critical patent/CN102687964B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention relates to a method for strengthening drug slow release property in a summer sleeping mat, belonging to a drug slow release technology field in vitro. A method for strengthening drug slow release property in the summer sleeping mat comprises the following steps: 1. stirring uniformly and obtaining a functional binder after mixing a traditional Chinese medicine powder, a binder and an adsorption slow-releasing agent; 2. taking the functional binder as a binder for manufacturing the summer sleeping mat. The adsorption slow-releasing agent is a porosity material and diluents are simple organic solvents whose carbon number of carbon chains is not more than three. The method in the invention enables the traditional Chinese medicine to have a slow-releasing effect by mixing the traditional Chinese medicine powder, the binder and the adsorption slow-releasing agent and taking the mixture as the functional binder. The method overcomes the technology problem that the medicine adhered to household wares is susceptible to water and easily dissipates in prior art and achieves the purpose that the traditional Chinese medicine can make an impression for a long time after being applied to products such as bamboo mats by people.

Description

A kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance
Technical field
The present invention relates to a kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance, belong to external medicament slow release technical field.
Background technology
Existing mat normally directly is woven into the single face mat by bamboo, grass or rattan.These mats usually cause human body to be discharged in use because of not absorbing water sweat can't be absorbed, and body local is in the environment that is full of sweat, and these places are easy to generate prickly heat, occur red and swollen even infect acarid.Like application number is 02217064.2 Chinese utility model patent, discloses a kind of mat, the positive dishes served at a feast layer that is compiled into for paper slip of this mat, and dishes served at a feast layer is compound through the substrate layer of middle resin adhesive linkage and reverse side, and tape edge forms all around then.Substrate layer is layer of cloth or elastic fibrous layer or spongy layer.The paper slip width is controlled at 1~5 millimeter scope, and paper slip is that the scraps of paper of narrow length form through flattening after twisting again.Therefore the medicine of expecting easily in this mat, placing absorbing sweat material and antibiosis anti-acarien is to solve the problems of the technologies described above.But directly place medicine and the medicine problem of approach exhaustion in a short time can occur.
Summary of the invention
The objective of the invention is for solving the problems of the technologies described above, a kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance is provided.
The objective of the invention is to be achieved through following technical scheme:
A kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance is characterized in that, may further comprise the steps:
1. after Chinese traditional powder, adhesive and adsorptivity sustained release agent being the mixed of 3 ︰, 25~28 ︰ 3~8 with weight ratio, stir, placed 20~30 minutes, make functional adhesive;
2. be viscose glue with said functional adhesive, be used for the making of summer sleeping mat;
Step 1. in, being prepared under 15~25 ℃ of the temperature of functional adhesive carried out, and avoids the sunlight direct projection;
Step 2. in, be viscose glue with said functional adhesive, resin added is 0.1~0.2g/cm 2, adopt the mode of exerting pressure for a long time to carry out pressing, pressure is not more than 0.5kg/cm 2, pressing-in temp is 25~45 ℃, the time of exerting pressure was not less than 2 hours;
Said adsorptivity sustained release agent is a porous material;
Said diluent is that carbon number is no more than 3 simple organic solvent on the carbochain.
The present invention mixes the back as the technical scheme that functional viscose glue uses with Chinese medicine medicine, adsorptivity sustained release agent and adhesive with certain proportion, makes the Chinese medicine medicine can play the effect of slowly-releasing.
Preferred as technique scheme, said pressing is the pulsed pressing, and said pulsed pressing is for to carry out pressing according to the mode of certain frequency change pressure, and said frequency is 3~10 times/second.
Because be mixed with inviscid composition in the adhesive, so adhesive property has certain influence, adopts the impact style of pulse to make and bondingly becomes more firm.
Preferred as technique scheme, preceding half section of said pressing process be the pulsed pressing, the second half section is to stablize pressing; Said pulsed pressing is for to carry out pressing according to the mode of certain frequency change pressure, and said frequency is 3~10 times/second; Said stable pressing is to carry out pressing with the constant mode of pressure stability.
Preferred as technique scheme also contains diluent and anticorrisive agent in the said functional adhesive, and the weight ratio of said diluent and anticorrisive agent and said functional adhesive is 1 ︰ 30~40; The method for using of said diluent is this diluent and mix with said adhesive and adsorptivity sustained release agent after Chinese traditional powder mixes earlier again, makes said functional adhesive; The method for using of said anticorrisive agent is to treat to sneak into said anticorrisive agent again after Chinese traditional powder and said adhesive and adsorptivity sustained release agent mix, and makes said functional adhesive.
Preferred as technique scheme, said adsorptivity sustained release agent is selected from one or more in porous aluminium oxide, activated carbon powder and the ion exchange resin; Said diluent is selected from one or more in acetone, the toluene.
Preferred as technique scheme, step 1. in, said weight ratio is 3 ︰, 27~28 ︰ 4~6; Step 2. in, pressing-in temp is 35~45 ℃, the time of exerting pressure is 3~5 hours.
Preferred as technique scheme, said frequency is 5~6 times/second.
Preferred as technique scheme, said adsorptivity sustained release agent be by bamboo must activated carbon powder, said diluent is an acetone.
Preferred as technique scheme, said adhesive are a kind of in epoxyn, the agent of phenolic resins viscose, the polyacrylate adhesive.
The present invention has following technique effect:
The present invention mixes the back with Chinese medicine medicine, adhesive and adsorptivity sustained release agent and uses as functional adhesive; Make said Chinese medicine medicine have the effect of slowly-releasing; Overcome the medicine that is attached in the prior art in the household wares and be afraid of that tide is prone to the dissipation technical problem, realized that people are applied to Chinese medicine the purpose that can play a role for a long time behind the product such as bamboo mat.The new application form of the health-related Chinese medicine of knowing clearly is started in the appearance of this technology, is also opening up new developing direction for household goods such as bamboo mat, floor, wardrobes.
The specific embodiment
This specific embodiment only is to explanation of the present invention; It is not a limitation of the present invention; Those skilled in the art can make any modification to present embodiment as required after reading this specification, but as long as in claim scope of the present invention, all receive the protection of Patent Law.
Embodiment one
A kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance may further comprise the steps:
1. after Chinese traditional powder, adhesive and adsorptivity sustained release agent being the mixed of 3 ︰, 25 ︰ 3 with weight ratio, stir, placed 20~30 minutes, make functional adhesive;
2. be viscose glue with said functional adhesive, be used for the making of summer sleeping mat;
Step 1. in, being prepared under 15 ℃ of the temperature of functional adhesive carried out, and avoids the sunlight direct projection;
Step 2. in, be viscose glue with said functional adhesive, resin added is 0.1g/cm 2, adopt the mode of exerting pressure for a long time to carry out pressing, pressure is not more than 0.5kg/cm 2, pressing-in temp is 25 ℃, the time of exerting pressure was not less than 2 hours;
Said adsorptivity sustained release agent is the porous aluminium oxide; Said adhesive is an epoxyn.
Embodiment two
A kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance may further comprise the steps:
1. after Chinese traditional powder, adhesive and adsorptivity sustained release agent being the mixed of 3 ︰, 25 ︰ 4 with weight ratio, stir, placed 20~30 minutes, make functional adhesive;
2. be viscose glue with said functional adhesive, be used for the making of summer sleeping mat;
Step 1. in, being prepared under 18 ℃ of the temperature of functional adhesive carried out, and avoids the sunlight direct projection;
Step 2. in, be viscose glue with said functional adhesive, resin added is 0.1g/cm 2, adopt the mode of exerting pressure for a long time to carry out pressing, pressure is not more than 0.5kg/cm 2, pressing-in temp is 25~45 ℃, the time of exerting pressure was not less than 2 hours;
Said adsorptivity sustained release agent is an activated carbon powder; Said adhesive is the agent of phenolic resins viscose.
Said pressing is the pulsed pressing, and said pulsed pressing is for to carry out pressing according to the mode of certain frequency change pressure, and said frequency is 3 times/second.
Embodiment three
A kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance may further comprise the steps:
1. after Chinese traditional powder, adhesive and adsorptivity sustained release agent being the mixed of 3 ︰, 26 ︰ 5 with weight ratio, stir, placed 20~30 minutes, make functional adhesive;
2. be viscose glue with said functional adhesive, be used for the making of summer sleeping mat;
Step 1. in, being prepared under 20 ℃ of the temperature of functional adhesive carried out, and avoids the sunlight direct projection;
Step 2. in, be viscose glue with said functional adhesive, resin added is 0.12g/cm 2, adopt the mode of exerting pressure for a long time to carry out pressing, pressure is 0.2kg/cm 2, pressing-in temp is 35 ℃, the time of exerting pressure was not less than 2 hours;
Said adsorptivity sustained release agent is an ion exchange resin; Said adhesive is the polyacrylate adhesive.
Preceding half section of said pressing process is the pulsed pressing, and the second half section is for stablizing pressing; Said pulsed pressing is for to carry out pressing according to the mode of certain frequency change pressure, and said frequency is 5 times/second; Said stable pressing is to carry out pressing with the constant mode of pressure stability.
Also contain diluent in the said functional adhesive, the weight ratio of said diluent and said functional adhesive is 1 ︰ 30; The method for using of said diluent is this diluent and mix with said adhesive and adsorptivity sustained release agent after Chinese traditional powder mixes earlier again, makes said functional adhesive.Said diluent is a toluene.
Embodiment four
A kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance may further comprise the steps:
1. after Chinese traditional powder, adhesive and adsorptivity sustained release agent being the mixed of 3 ︰, 26 ︰ 6 with weight ratio, stir, placed 20~30 minutes, make functional adhesive;
2. be viscose glue with said functional adhesive, be used for the making of summer sleeping mat;
Step 1. in, being prepared under 25 ℃ of the temperature of functional adhesive carried out, and avoids the sunlight direct projection;
Step 2. in, be viscose glue with said functional adhesive, resin added is 0.15g/cm 2, adopt the mode of exerting pressure for a long time to carry out pressing, pressure is not more than 0.5kg/cm 2, pressing-in temp is 35 ℃, the time of exerting pressure was not less than 2 hours;
Said adsorptivity sustained release agent is the porous aluminium oxide; Said adhesive is an epoxyn.
Preceding half section of said pressing process is the pulsed pressing, and the second half section is for stablizing pressing; Said pulsed pressing is for to carry out pressing according to the mode of certain frequency change pressure, and said frequency is 6 times/second; Said stable pressing is to carry out pressing with the constant mode of pressure stability.
Also contain diluent and anticorrisive agent in the said functional adhesive, the weight ratio of said diluent and anticorrisive agent and said functional adhesive is 1 ︰ 35; The method for using of said diluent is this diluent and mix with said adhesive and adsorptivity sustained release agent after Chinese traditional powder mixes earlier again, makes said functional adhesive; The method for using of said anticorrisive agent is to treat to sneak into said anticorrisive agent again after Chinese traditional powder and said adhesive and adsorptivity sustained release agent mix, and makes said functional adhesive.Said diluent is a toluene.
Embodiment five
A kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance may further comprise the steps:
1. after Chinese traditional powder, adhesive and adsorptivity sustained release agent being the mixed of 3 ︰, 27 ︰ 8 with weight ratio, stir, placed 20~30 minutes, make functional adhesive;
2. be viscose glue with said functional adhesive, be used for the making of summer sleeping mat;
Step 1. in, being prepared under 25 ℃ of the temperature of functional adhesive carried out, and avoids the sunlight direct projection;
Step 2. in, be viscose glue with said functional adhesive, resin added is 0.2g/cm 2, adopt the mode of exerting pressure for a long time to carry out pressing, pressure is not more than 0.5kg/cm 2, pressing-in temp is 40 ℃, the time of exerting pressure was not less than 2 hours;
Said adsorptivity sustained release agent is the active carbon that bamboo one-tenth is arranged; Said adhesive is the polyacrylate adhesive.
Preceding half section of said pressing process is the pulsed pressing, and the second half section is for stablizing pressing; Said pulsed pressing is for to carry out pressing according to the mode of certain frequency change pressure, and said frequency is 7 times/second; Said stable pressing is to carry out pressing with the constant mode of pressure stability.
Also contain diluent and anticorrisive agent in the said functional adhesive, the weight ratio of said diluent and anticorrisive agent and said functional adhesive is 1 ︰ 35; The method for using of said diluent is this diluent and mix with said adhesive and adsorptivity sustained release agent after Chinese traditional powder mixes earlier again, makes said functional adhesive; The method for using of said anticorrisive agent is to treat to sneak into said anticorrisive agent again after Chinese traditional powder and said adhesive and adsorptivity sustained release agent mix, and makes said functional adhesive.Said diluent is an acetone.
Embodiment six
A kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance may further comprise the steps:
1. after Chinese traditional powder, adhesive and adsorptivity sustained release agent being the mixed of 3 ︰, 28 ︰ 5 with weight ratio, stir, placed 20~30 minutes, make functional adhesive;
2. be viscose glue with said functional adhesive, be used for the making of summer sleeping mat;
Step 1. in, being prepared under 25 ℃ of the temperature of functional adhesive carried out, and avoids the sunlight direct projection;
Step 2. in, be viscose glue with said functional adhesive, resin added is 0.2g/cm 2, adopt the mode of exerting pressure for a long time to carry out pressing, pressure is not more than 0.5kg/cm 2, pressing-in temp is 45 ℃, the time of exerting pressure was not less than 2 hours;
Said adsorptivity sustained release agent is an active carbon; Said adhesive is an epoxyn.
Preceding half section of said pressing process is the pulsed pressing, and the second half section is for stablizing pressing; Said pulsed pressing is for to carry out pressing according to the mode of certain frequency change pressure, and said frequency is 8 times/second; Said stable pressing is to carry out pressing with the constant mode of pressure stability.
Also contain diluent and anticorrisive agent in the said functional adhesive, the weight ratio of said diluent and anticorrisive agent and said functional adhesive is 1 ︰ 38; The method for using of said diluent is this diluent and mix with said adhesive and adsorptivity sustained release agent after Chinese traditional powder mixes earlier again, makes said functional adhesive; The method for using of said anticorrisive agent is to treat to sneak into said anticorrisive agent again after Chinese traditional powder and said adhesive and adsorptivity sustained release agent mix, and makes said functional adhesive.Said diluent is an acetone.
Embodiment seven
A kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance may further comprise the steps:
1. after Chinese traditional powder, adhesive and adsorptivity sustained release agent being the mixed of 3 ︰, 28 ︰ 8 with weight ratio, stir, placed 20~30 minutes, make functional adhesive;
2. be viscose glue with said functional adhesive, be used for the making of summer sleeping mat;
Step 1. in, being prepared under 25 ℃ of the temperature of functional adhesive carried out, and avoids the sunlight direct projection;
Step 2. in, be viscose glue with said functional adhesive, resin added is 0.2g/cm 2, adopt the mode of exerting pressure for a long time to carry out pressing, pressure is not more than 0.5kg/cm 2, pressing-in temp is 45 ℃, the time of exerting pressure was not less than 2 hours;
Said adsorptivity sustained release agent is a macroreticular resin; Said adhesive is the agent of phenolic resins viscose.
Preceding half section of said pressing process is the pulsed pressing, and the second half section is for stablizing pressing; Said pulsed pressing is for to carry out pressing according to the mode of certain frequency change pressure, and said frequency is 10 times/second; Said stable pressing is to carry out pressing with the constant mode of pressure stability.
Also contain diluent and anticorrisive agent in the said functional adhesive, the weight ratio of said diluent and anticorrisive agent and said functional adhesive is 1 ︰ 40; The method for using of said diluent is this diluent and mix with said adhesive and adsorptivity sustained release agent after Chinese traditional powder mixes earlier again, makes said functional adhesive; The method for using of said anticorrisive agent is to treat to sneak into said anticorrisive agent again after Chinese traditional powder and said adhesive and adsorptivity sustained release agent mix, and makes said functional adhesive.Said diluent is an ethanol.

Claims (9)

1. a method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance is characterized in that, may further comprise the steps:
1. after Chinese traditional powder, adhesive and adsorptivity sustained release agent being the mixed of 3 ︰, 25~28 ︰ 3~8 with weight ratio, stir, placed 20~30 minutes, make functional adhesive;
2. be viscose glue with said functional adhesive, be used for the making of summer sleeping mat;
Step 1. in, being prepared under 15~25 ℃ of the temperature of functional adhesive carried out, and avoids the sunlight direct projection;
Step 2. in, be viscose glue with said functional adhesive, resin added is 0.1~0.2g/cm 2, adopt the mode of exerting pressure for a long time to carry out pressing, pressure is not more than 0.5kg/cm 2, pressing-in temp is 25~45 ℃, the time of exerting pressure was not less than 2 hours;
Said adsorptivity sustained release agent is a porous material;
Said diluent is that carbon number is no more than 3 simple organic solvent on the carbochain.
2. a kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance according to claim 1; It is characterized in that: said pressing is the pulsed pressing; Said pulsed pressing is for to carry out pressing according to the mode of certain frequency change pressure, and said frequency is 3~10 times/second.
3. a kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance according to claim 1 is characterized in that: preceding half section of said pressing process is the pulsed pressing, and the second half section is for stablizing pressing; Said pulsed pressing is for to carry out pressing according to the mode of certain frequency change pressure, and said frequency is 3~10 times/second; Said stable pressing is to carry out pressing with the constant mode of pressure stability.
4. a kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance according to claim 1; It is characterized in that: also contain diluent and anticorrisive agent in the said functional adhesive, the weight ratio of said diluent and anticorrisive agent and said functional adhesive is 1 ︰ 30~40; The method for using of said diluent is this diluent and mix with said adhesive and adsorptivity sustained release agent after Chinese traditional powder mixes earlier again, makes said functional adhesive; The method for using of said anticorrisive agent is to treat to sneak into said anticorrisive agent again after Chinese traditional powder and said adhesive and adsorptivity sustained release agent mix, and makes said functional adhesive.
5. a kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance according to claim 1 is characterized in that: said adsorptivity sustained release agent is selected from one or more in porous aluminium oxide, activated carbon powder and the ion exchange resin; Said diluent is selected from one or more in acetone, the toluene.
6. a kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance according to claim 1 is characterized in that: step 1. in, said weight ratio is 3 ︰, 27~28 ︰ 4~6; Step 2. in, pressing-in temp is 35~45 ℃, the time of exerting pressure is 3~5 hours.
7. according to claim 2 or 3 described a kind of methods of strengthening summer sleeping mat Chinese traditional medicine sustained release performance, it is characterized in that: said frequency is 5~6 times/second.
8. a kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance according to claim 5 is characterized in that: said adsorptivity sustained release agent is the activated carbon powder that is got by bamboo, and said diluent is an acetone.
9. a kind of method of strengthening summer sleeping mat Chinese traditional medicine sustained release performance according to claim 1 is characterized in that: said adhesive is a kind of in epoxyn, the agent of phenolic resins viscose, the polyacrylate adhesive.
CN2012101452204A 2012-05-11 2012-05-11 Method for strengthening drug slow release property in summer sleeping mat Expired - Fee Related CN102687964B (en)