CN102589342A CN2012100769999A CN201210076999A CN102589342A CN 102589342 A CN102589342 A CN 102589342A CN 2012100769999 A CN2012100769999 A CN 2012100769999A CN 201210076999 A CN201210076999 A CN 201210076999A CN 102589342 A CN102589342 A CN 102589342A
Authority
CN
China
Prior art keywords
copper pipe
pipe
welding
nuclear power
air cooler
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2012100769999A
Other languages
English (en)
Other versions
CN102589342B (zh
Inventor
车作文
刘宏
付秀昀
荆云涛
刘万里
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HARBIN AIR-CONDITIONER Co Ltd
Original Assignee
HARBIN AIR-CONDITIONER Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HARBIN AIR-CONDITIONER Co Ltd filed Critical HARBIN AIR-CONDITIONER Co Ltd
Priority to CN201210076999.9A priority Critical patent/CN102589342B/zh
Publication of CN102589342A publication Critical patent/CN102589342A/zh
Application granted granted Critical
Publication of CN102589342B publication Critical patent/CN102589342B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Images

Abstract

本发明涉及核电站应急柴油机房空冷器的管箱与薄壁铜管的连接技术,具体为核电站应急发电系统空冷器铜管端部焊接防止裂纹装置。其特点是:在靠近铜管插入管箱端部处,设有环形槽,环形槽与管箱端部处之间有间隙k。第一步由数控钻滑槽刀在已钻好的管箱孔周围划出环形槽;第二步用丙酮仔细清理擦洗焊接部位20mm面积区域,第三步预热焊接部位110℃-130℃;第四步由深孔管端自动氩弧焊机将管端焊上镍合金材料;第五步由胀管器插入铜管内旋转电动胀管机使胀管器变大铜管贴胀在管箱内孔壁上,使铜管牢固的连接在碳钢板管箱上。在靠近铜管插入管箱端部处,设有环形槽,环形槽与管箱端部处之间有间隙k。焊点覆盖铜管与间隙k,使铜管与管箱牢固连接。本发明的优点是:结构简单、成本低廉、强度焊安全可靠,结构简单、耐压力,焊接变形小,贴胀方便,好加工。

Description

核电站应急发电系统空冷器铜管端部焊接防止裂纹装置
技术领域:本发明涉及核电站应急柴油机房空冷器的管箱与薄壁铜管的连接技术,具体为核电站应急发电系统空冷器铜管端部焊接防止裂纹装置。
背景技术:在核电领域内,空冷器是发电时为了安全在出现断电时应急柴油机房发电用空气冷却器散热调节柴油机温度的主要设备,为了解决空冷器散热翅片管中的薄壁铜管与钢管箱的连接问题,人们通常胀接,使穿入铝翅片的铜管内的介质进行冷却柴油机,而薄壁铜管胀接在一般领域可行,在关键领域安全系数要求高时和强度焊加贴胀的方法相比会差很多。
发明内容:本发明的目的在于提供一种结构简单、成本低廉、加工、制造方便、使用灵活、省时、省力的核电站应急发电系统空冷器铜管端部焊接防止裂纹装置。本发明的目的是这样实现的:它包含铜管、翅片、管箱、连接法兰,其特征在于:在靠近铜管插入管箱端部处,设有环形槽,环形槽与管箱端部处之间有间隙k。核电站应急发电系统空冷器铜管端部焊接防止裂纹装置制备工艺方法是:第一步由数控钻滑槽刀在已钻好的管箱孔周围划出环形槽;第二步用丙酮仔细清理擦洗焊接部位20mm面积区域,第三步预热焊接部位110℃-130℃;第四步由深孔管端自动氩弧焊机将管端焊上镍合金材料;第五步由胀管器插入铜管内旋转电动胀管机使胀管器变大铜管贴胀在管箱内孔壁上,使铜管牢固的连接在碳钢板管箱上。焊点覆盖铜管与间隙k,使铜管与管箱牢固连接。环形槽的宽度)是2-5mm。环形槽与管箱端部处之间有间隙k是1-3mm。本发明的优点是:结构简单、成本低廉、强度焊安全可靠,结构简单、耐压力,焊接变形小,贴胀方便,好加工。
附图说明:图1是本发明结构原理示意图;图2是本发明局部放大的A向结构原理示意图;图3是本发明铜管与管箱焊接结构原理示意图。L-环形槽的深度。
具体实施方式:它包含铜管1、翅片2、管箱3、连接法兰5,其特征在于:在靠近铜管1插入管箱3端部处,设有环形槽4,环形槽4与管箱3端部处之间有间隙k。核电站应急发电系统空冷器铜管端部焊接防止裂纹装置制备工艺方法是:第一步由数控钻滑槽刀在已钻好的管箱3孔周围划出环形槽4;第二步用丙酮仔细清理擦洗焊接部位20mm面积区域,第三步预热焊接部位110℃-130℃;第四步由深孔管端自动氩弧焊机将管端焊上镍合金材料;第五步由胀管器插入铜管1内旋转电动胀管机使胀管器变大铜管1贴胀在管箱3内孔壁上,使铜管1牢固的连接在碳钢板管箱3上。焊点6覆盖铜管1与间隙k,使铜管1与管箱3牢固连接。环形槽的宽度G是2-5mm。环形槽与管箱端部处之间有间隙k是1-3mm。L是2-5mm。本发明工作原理及工作过程是:铜管腔1外层是翅片2、铜管腔1,两端分别插入带环形槽4的管箱3中,使铜管腔1与管箱3实现贯通连接,工作完成。

Claims (5)

1.一种核电站应急发电系统空冷器铜管端部焊接防止裂纹装置,它包含铜管、翅片、管箱、连接法兰,其特征在于:在靠近铜管插入管箱端部处,设有环形槽,环形槽与管箱端部处之间有间隙k。
2.一种核电站应急发电系统空冷器铜管端部焊接防止裂纹装置制备工艺方法,其特征在于:第一步由数控钻滑槽刀在已钻好的管箱孔周围划出环形槽;第二步用丙酮仔细清理擦洗焊接部位20mm面积区域,第三步预热焊接部位110℃-130℃;第四步由深孔管端自动氩弧焊机将管端焊上镍合金材料;第五步由胀管器插入铜管内旋转电动胀管机使胀管器变大铜管贴胀在管箱内孔壁上,使铜管牢固的连接在碳钢板管箱上。
3.根据权利要求1所述的一种核电站应急发电系统空冷器铜管端部焊接防止裂纹装置,其特征在于:焊点覆盖铜管与间隙k,使铜管与管箱牢固连接。
4.根据权利要求1所述的一种核电站应急发电系统空冷器铜管端部焊接防止裂纹装置,其特征在于:环形槽的宽度G是2-5mm。
5.根据权利要求1所述的一种核电站应急发电系统空冷器铜管端部焊接防止裂纹装置,其特征在于:环形槽与管箱端部处之间的间隙k是1-3mm。
CN201210076999.9A 2012-03-22 2012-03-22 核电站应急发电系统空冷器铜管端部焊接防止裂纹装置 Active CN102589342B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201210076999.9A CN102589342B (zh) 2012-03-22 2012-03-22 核电站应急发电系统空冷器铜管端部焊接防止裂纹装置

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201210076999.9A CN102589342B (zh) 2012-03-22 2012-03-22 核电站应急发电系统空冷器铜管端部焊接防止裂纹装置

Publications (2)

Publication Number Publication Date
CN102589342A true CN102589342A (zh) 2012-07-18
CN102589342B CN102589342B (zh) 2015-09-30

Family

ID=46478341

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201210076999.9A Active CN102589342B (zh) 2012-03-22 2012-03-22 核电站应急发电系统空冷器铜管端部焊接防止裂纹装置

Country Status (1)

Country Link
CN (1) CN102589342B (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103769726A (zh) * 2014-02-14 2014-05-07 中国船舶重工集团公司第七�三研究所 一种可减少残余应力的管子与管板焊接方法的结构
CN105108369A (zh) * 2015-09-14 2015-12-02 无锡市创新化工设备有限公司 一种防法兰焊接变形的结构及焊接方法

Citations (15)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US1390835A (en) * 1920-08-17 1921-09-13 Gen Electric Method of manufacturing nozzle-diaphragms for elastic-fluid turbines
US2474023A (en) * 1944-02-17 1949-06-21 British Thomson Houston Co Ltd Method of gas-shielded alternating current arc welding
CN1209376A (zh) * 1997-08-22 1999-03-03 株式会社神户制钢所 气体保护电弧焊接用药芯焊丝
CN2608934Y (zh) * 2002-12-16 2004-03-31 张永胜 复合式换热管空冷器
CN2742260Y (zh) * 2004-09-13 2005-11-23 台州市精艺管件有限公司 铜管接头
CN1861309A (zh) * 2005-05-13 2006-11-15 株式会社神户制钢所 非镀铜焊丝
CN101074085A (zh) * 2007-06-06 2007-11-21 中国核工业华兴建设有限公司 核电站环形轨道箱形吊车梁组装焊接方法
CN101112733A (zh) * 2007-08-30 2008-01-30 沈阳飞机工业(集团)有限公司 潜弧焊接工艺
CN101154472A (zh) * 2006-09-29 2008-04-02 中国核动力研究设计院 一体化低温核供热堆
CN201318881Y (zh) * 2008-10-31 2009-09-30 哈尔滨空调股份有限公司 复合管式空冷器装置
CN201600050U (zh) * 2009-09-28 2010-10-06 哈尔滨空调股份有限公司 复合管式空气冷却器管束装置
CN101925792A (zh) * 2008-10-07 2010-12-22 三菱重工业株式会社 管接头和集管箱的焊接结构
CN102109293A (zh) * 2011-01-10 2011-06-29 哈尔滨空调股份有限公司 石化换热空冷器翅片管定位条装置
CN202041101U (zh) * 2011-03-22 2011-11-16 哈尔滨空调股份有限公司 管箱局部堆焊空冷器装置
CN202582344U (zh) * 2012-03-22 2012-12-05 哈尔滨空调股份有限公司 核电站应急发电系统空冷器铜管端部焊接防止裂纹装置

Patent Citations (15)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US1390835A (en) * 1920-08-17 1921-09-13 Gen Electric Method of manufacturing nozzle-diaphragms for elastic-fluid turbines
US2474023A (en) * 1944-02-17 1949-06-21 British Thomson Houston Co Ltd Method of gas-shielded alternating current arc welding
CN1209376A (zh) * 1997-08-22 1999-03-03 株式会社神户制钢所 气体保护电弧焊接用药芯焊丝
CN2608934Y (zh) * 2002-12-16 2004-03-31 张永胜 复合式换热管空冷器
CN2742260Y (zh) * 2004-09-13 2005-11-23 台州市精艺管件有限公司 铜管接头
CN1861309A (zh) * 2005-05-13 2006-11-15 株式会社神户制钢所 非镀铜焊丝
CN101154472A (zh) * 2006-09-29 2008-04-02 中国核动力研究设计院 一体化低温核供热堆
CN101074085A (zh) * 2007-06-06 2007-11-21 中国核工业华兴建设有限公司 核电站环形轨道箱形吊车梁组装焊接方法
CN101112733A (zh) * 2007-08-30 2008-01-30 沈阳飞机工业(集团)有限公司 潜弧焊接工艺
CN101925792A (zh) * 2008-10-07 2010-12-22 三菱重工业株式会社 管接头和集管箱的焊接结构
CN201318881Y (zh) * 2008-10-31 2009-09-30 哈尔滨空调股份有限公司 复合管式空冷器装置
CN201600050U (zh) * 2009-09-28 2010-10-06 哈尔滨空调股份有限公司 复合管式空气冷却器管束装置
CN102109293A (zh) * 2011-01-10 2011-06-29 哈尔滨空调股份有限公司 石化换热空冷器翅片管定位条装置
CN202041101U (zh) * 2011-03-22 2011-11-16 哈尔滨空调股份有限公司 管箱局部堆焊空冷器装置
CN202582344U (zh) * 2012-03-22 2012-12-05 哈尔滨空调股份有限公司 核电站应急发电系统空冷器铜管端部焊接防止裂纹装置

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
汪东明: "国内外换热器管子管板焊接技术综述", 《压力容器》 *

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103769726A (zh) * 2014-02-14 2014-05-07 中国船舶重工集团公司第七�三研究所 一种可减少残余应力的管子与管板焊接方法的结构
CN105108369A (zh) * 2015-09-14 2015-12-02 无锡市创新化工设备有限公司 一种防法兰焊接变形的结构及焊接方法

Also Published As

Publication number Publication date
CN102589342B (zh) 2015-09-30

Similar Documents

Publication Publication Date Title
WO2011071315A3 (ko) 형상기억합금을 이용한 공구 홀더 및 공구 고정방법
CN109396770B (zh) 一种胀接鼓包u形换热管的更换方法以及特制直角镗刀
CN102589342A (zh) 核电站应急发电系统空冷器铜管端部焊接防止裂纹装置
TW201515751A (zh) 利用攪拌摩擦焊接將管件連接至元件的方法和由其製成的結構
AU2013224000A8 (en) Method and machine for forge welding of tubular articles and exothermic flux mixture and method of manufacturing an exothermic flux mixture
CN105312742A (zh) 一种焊接工艺
CN110867318B8 (zh) 一种电力变压器散热冷却系统制作方法
CN105499719A (zh) 一种螺母攻丝机
CN103386540A (zh) 换热管与管板氩弧焊时换热管内壁的保护工装
CN204135685U (zh) 金属管件定位钻孔拔边机
CN104690483A (zh) 油田废旧射孔枪内盲孔复合修复工艺
CN202582344U (zh) 核电站应急发电系统空冷器铜管端部焊接防止裂纹装置
CN103192230A (zh) 深孔加工方法及制备得到的注浆块
CN102848571A (zh) 一种塑料薄壁管锥口热熔焊接装置及热熔焊接方法
CN104646977A (zh) 大型汽车用热交换器埋丝钎焊加工方法
CN211105684U (zh) 一种电熔连接装置
CN104117779A (zh) 钻具稳定器合金块的焊接方法
CN206439522U (zh) 一种爆炸焊接金属复合锥形管
CN203751100U (zh) 风塔平台梁冲孔工装
CN105014246A (zh) 一种用于异型薄壁锥管的焊接夹具
CN203418217U (zh) 换热管与管板氩弧焊时换热管内壁的保护工装
CN104227421A (zh) 金属管件定位钻孔拔边机
CN207071820U (zh) 一种枪钻的钻柄快速夹头
CN104384883A (zh) 冷却器管板的加工方法
CN104439673B (zh) 表面张力贮箱通道用电子束焊接及热处理工装及方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant