CN102582196A - 一种用于反光罩的复合材料的制造方法 - Google Patents
一种用于反光罩的复合材料的制造方法 Download PDFInfo
- Publication number
- CN102582196A CN102582196A CN2011100028573A CN201110002857A CN102582196A CN 102582196 A CN102582196 A CN 102582196A CN 2011100028573 A CN2011100028573 A CN 2011100028573A CN 201110002857 A CN201110002857 A CN 201110002857A CN 102582196 A CN102582196 A CN 102582196A
- Authority
- CN
- China
- Prior art keywords
- adhesive
- reflective film
- composite
- compound
- reflection shield
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种用于反光罩的复合材料的制造方法,其制作步骤为:①在反射薄膜的一面涂覆粘胶剂;②将反射薄膜与粘胶剂一同加热;③将金属材料通过粘胶剂与反射薄膜复合;④在反射薄膜的另一面复合保护膜。与现有技术相比,本发明的积极效果是:加工工艺简单、粘胶剂固化时间短,从而缩短了整个加工周期。同时实现设备国产化,大大降低了成本。
Description
技术领域
本发明涉及一种层状产品的制造方法,具体而言,是一种用于反光罩的符合材料的制造方法。
背景技术
在一般背光模块或液晶显示器中,通常以冷阴极管(CCLF)作为光源发光构件,并且通过导光板将光源转换成平面发光源。为了让冷阴极管所发出的光线都能有效地导入导光板中,通常会采用反射罩结构反射光线,用以提高冷阴极管发光的使用效率。
目前液晶屏反光罩的制造方法为:将反光薄膜材料粘合于金属基料上,然后进行冲压,制成各种形状。该方法的制造设备由德国和日本进口,不但设备投资巨大、原材料成本高,而且粘合剂的固化期长,致使生产率低,延长了交货周期。
中国专利“一种反光罩生产方法”(ZL 200610167772.x)提供了一种反光罩的生产方法,通过包括有放卷装置、清洗装置、烘干装置、涂抹粘合剂装置、加热装置,压合反光膜装置、冷却装置、压合保护膜装置和复卷装置的生产装置完成反光罩复合材料的生产。不仅步骤复杂、加热温度高,还需要用水冷却。这不仅增加了生产的成本,同时对环境造成了污染,又浪费了水资源。
因此,我们需要一种成本低、无毒性、步骤简单、消耗环境资源少的发光罩生产方法。
发明内容
本发明的目的在于提供一种用于反光罩的符合材料的制造方法。
为了解决上述问题本发明的技术方案是这样的:
一种用于反光罩的复合材料的制造方法,其制作步骤为:
(1)在反射薄膜的一面涂覆粘胶剂;
(2)将反射薄膜与粘胶剂一同加热;
(3)将金属材料通过粘胶剂与反射薄膜复合;
(4)在反射薄膜的另一面复合保护膜。
所述加热为三级式连续加热,加热温度分别为90℃、82℃、60℃,加热方式为烘箱加热。
所述金属材料与反射薄膜通过复合滚轮复合。
所述保护膜与反射薄膜通过复合滚轮复合。
所述复合滚轮的温度为60℃。
与现有技术相比,本发明的积极效果是:加工工艺简单、无毒性、消耗少、粘胶剂固化时间短,缩短了整个加工周期。同时实现设备国产化,大大降低了成本。
附图说明
下面结合附图和具体实施方式来详细说明本发明;
图1为实现本发明加工工艺的实施例。
图2为本发明制备的反光罩复合材料。
图中标号为:1—反射薄膜放置装置、2—上胶机构、3—加热部件、4—金属材料放置装置、5—复合滚轮、6—复合材料收卷装置、7—保护膜放置装置、8~11—表示传送方向的箭头、20—反光罩复合材料、21—保护膜、22—反射薄膜、23—粘胶剂、24—金属材料。
具体实施方式
为了使本发明实现的技术手段、创作特征、达成目的与功效易于明白了解,下面结合具体图示,进一步阐述本发明。
图1所示的是为实现本发明方法的设备。其中反射薄膜放置装置1用于放置反射薄膜22卷。上胶机构2用于为反射薄膜22涂覆粘胶剂23。加热部件3由3个烘箱组成,为涂覆有粘胶剂23的反射薄膜22提供3种温度的连续加热,使粘胶剂22处于融化状态,便于其与金属材料24复合。金属材料放置装置4用于放置金属材料24卷。复合滚轮5用于将涂覆有粘胶剂23的反射薄膜22、金属片24以及保护膜21复合。复合滚轮5的温度为60℃。收卷装置6是用于将复合之后的复合材料20收卷。
如图1所示,复合材料的加工步骤为:
(1)将反射薄膜22卷与金属材料24卷分别放入反射薄膜放置装置1和金属材料放置装置4上;
(2)反射薄膜22在滚轮和传送带的带动下,经过上胶机构2,由上胶机构2在反射薄膜22的一面涂覆粘胶剂23;
(3)涂覆有粘胶剂23的反射薄膜22经过由3个烘箱组成的加热部件3加热,所述3个烘箱的温度从左到右分别为90℃、82℃、60℃;
(4)加热后的涂覆有粘胶剂23的反射薄膜22通过复合滚轮5与金属材料24及保护膜21复合,获得反光罩复合材料20;所述复合滚轮5设有温度,温度为60℃;
(5)复合材料20经由收卷装置6收卷即可。
复合过程中通过滚轮及传送带,使各原料在机器上运转。图中箭头8表示的是反射薄膜22的传送方向,箭头9表示的是金属材料24的传送方向,箭头10标示的是保护膜21的传送方向,箭头11表示的是反光罩复合材料20的传送方向。
所述反射薄膜22为聚对苯二甲酸乙二醇酯反射薄膜,所述金属材料24为金属铝或不锈钢,所述保护膜21为聚乙烯,所述粘胶剂由聚脂系聚氨脂树脂和多聚异氰酸脂按重量比7.5(±0.5):1.7(±0.1)的比例混合而成。
与现有技术相比,本发明的积极效果是:①加工工艺简单、无毒性、加热温度低、无需用水冷却,对环境的消耗低;②粘胶剂固化时间短,从而缩短了整个加工周期;③实现设备国产化,大大降低了成本。
Claims (5)
1.一种用于反光罩的复合材料的制造方法,其特征在于,其制作步骤为:
(1)在反射薄膜的一面涂覆粘胶剂;
(2)将反射薄膜与粘胶剂一同加热;
(3)将金属材料通过粘胶剂与反射薄膜复合;
(4)在反射薄膜的另一面复合保护膜。
2.根据权利要求1所述的用于反光罩的复合材料的制造方法,其特征在于,所述加热为三级式连续加热,加热温度分别为90℃、82℃、60℃。
3.根据权利要求1所述的用于反光罩的复合材料的制造方法,其特征在于,所述金属材料与反射薄膜通过复合滚轮复合。
4.根据权利要求1所述的用于反光罩的复合材料的制造方法,其特征在于,所述保护膜与反射薄膜通过复合滚轮复合。
5.根据权利要求3或4所述的用于反光罩的复合材料的制造方法,其特征在于,所述复合滚轮的温度为60℃。