CN102582156A - 超音速火焰铝粉融合铁复合板生产流水线 - Google Patents

超音速火焰铝粉融合铁复合板生产流水线 Download PDF

Info

Publication number
CN102582156A
CN102582156A CN201210030252XA CN201210030252A CN102582156A CN 102582156 A CN102582156 A CN 102582156A CN 201210030252X A CN201210030252X A CN 201210030252XA CN 201210030252 A CN201210030252 A CN 201210030252A CN 102582156 A CN102582156 A CN 102582156A
Authority
CN
China
Prior art keywords
production line
aluminium powder
inlet
aluminium
hypersonic flame
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201210030252XA
Other languages
English (en)
Inventor
王宝根
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Gongshang University
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201210030252XA priority Critical patent/CN102582156A/zh
Publication of CN102582156A publication Critical patent/CN102582156A/zh
Pending legal-status Critical Current

Abstract

一种超音速火焰铝粉融合铁复合板生产流水线,其包括布置在生产流水线入口部分的开卷机、入口夹送和入口剪,布置在生产流水线加工部分的三辊纠偏机和检测台,以及布置在生产流水线出口部分的出口剪、出口夹送和卷取机,其特点是:它还包括布置在生产流水线加工部分的超音速火焰铝喷涂机、冷轧机和静电涂油机,其中超音速火焰铝粉喷涂机布置在入口剪之后,冷轧机布置在超音速火焰铝粉喷涂机之后。本发明解决了现有问题,提供一种利用超音速火焰喷涂机在铁板上复合铝粉的生产流水线,其生产的铝粉融合铁复合板代替紧缺的有色金属,减少贵重有色金属的消耗,使其具有节能环保、加工方便、装饰效果好及成本低等特点。

Description

超音速火焰铝粉融合铁复合板生产流水线
一、技术领域
本发明涉及一种板材生产流水线,尤其是一种超音速火焰铝粉融合铁复合板生产流水线。
二、背景技术
随着经济的发展和社会的进步以及及物质文化水平的提高,人们越来越注重生活的质量和家具以及公共设施的装修,大大加剧了具有豪华装饰效果和具有良好防腐性能的有色金属在建筑装饰行业上的应用。但是有色金属的资源相对紧缺,国内国际的有色金属价格节节攀升,加之有色金属的冶炼属于高耗能、高污染项目,对大自然危害大,成本也很高。在这个倡导绿色环保,经济节约型的社会,就更需要研发一种经济适用的复合板作为装饰建筑材料代替原有贵重有色金属。
三、发明内容
本发明的目的是要解决上述现有问题,提供一种利用超音速火焰喷涂机在铁板上复合铝粉的生产流水线,其生产的铝铁复合板代替紧缺的有色金属,减少贵重有色金属的消耗,使其具有节能环保、加工方便、装饰效果好及成本低等特点。
本发明的目的是采用如下方案实现的:一种多层金属复合板,以铁板为基板,铝为面板,形成多层金属合板,即铁-铝二层复合板,即在铁板上铝。
在铁板上复合铝时,使用超音速火焰铝粉喷涂机,即在铁板上撤铝粉后,利用超音速火焰将铝粉复合到铁板上,使铝粉与铁板结合形成复合板的的铝层,再进行冷轧平整。
一种超音速火焰铝粉融合铁复合板生产流水线,其包括布置在生产流水线入口部分的开卷机、入口夹送和入口剪,布置在生产流水线加工部分的三辊纠偏机和检测台,以及布置在生产流水线出口部分的出口剪、出口夹送和卷取机,其特点是:它还包括布置在生产流水线加工部分的超音速火焰铝粉喷涂机、冷轧机和静电涂油机,其中超音速火焰铝粉喷涂机布置在入口剪之后,其与冷轧机配套使用完成铝粉与铁板的复合,冷轧机布置在超音速火焰铝粉喷涂机之后;所述静电涂油机布置在检测台后方,方便对复合加工后的复合板进行防腐处理。
本发明采用上述方案的有益效果是:1)制造方便,大大降低了成本;2)利用低廉的材料复合成一种新型复合板材,其拥有有色金属豪华、高档的装饰效果;3)代替贵重有色金属,满足了大众化的需求;4)简单、方便及实用,超音速火焰铝粉融合铁结合力好,冷轧后板面比较平滑、美观,且进行涂油防腐处理,这样利用板材再做产品时不用再进行电镀。
四、附图说明
图1是本发明超音速火焰铝粉融合铁复合板生产流水线的结构示意图。
对各幅附图中的标号说明如下:
a-入口部分;b-加工部分;c-出口部分;1-开卷机;2-入口夹送;3-入口剪;4-超音速火焰铝粉喷涂机;5-冷轧机;6-三辊纠偏机;7-检测台;8-静电涂油机;9-出口剪;10-出口夹送;11-卷取机。
五、具体实施方式
下面结合附图对本发明超音速火焰铝粉融合铁复合板生产流水线的具体实施方式作详细描述。
一种多层金属复合板,以铁板为基板,铝为面板,形成多层金属合板,即铁-铝二层复合板,即在铁板上铝。
在铁板上复合铝时,使用超音速火焰铝粉喷涂机4,即在铁板上撒铝粉后,利用超音速火焰将铝粉复合到铁板上,使铝粉与铁板结合形成复合板的的铝层,再进行冷轧平整。
如图1所示,一种超音速火焰铝粉融合铁复合板生产流水线,其包括布置在生产流水线入口部分a的开卷机1、入口夹送2和入口剪3,布置在生产流水线加工部分b的三辊纠偏机6和检测台7,布置在生产流水线出口部分c的出口剪9、出口夹送10和卷取机11,以及布置在生产流水线加工部分b的超音速火焰铝粉喷涂机4、冷轧机5和静电涂油机8。图中虚线表示复合板。
超音速火焰铝粉喷涂机4布置在入口剪3之后,其与冷轧机5配套使用,冷轧机5布置在超音速火焰铝粉喷涂机3之后。
静电涂油机8布置在检测台7后方,方便对复合加工后的复合板进行防腐处理。
开机后,各机器启动,比如开卷机1、超音速火焰铝粉喷涂机3、静电涂油机8、出口剪9、出口夹送10和卷取机11等,此时开卷机1将成卷的铁展开送入入口夹送2,经过入口剪3后进入超音速火焰铝粉喷涂机4进行超音速火焰铝粉喷涂,喷涂后的复合板进入冷轧机5,经冷轧机5轧薄轧平后的复合板进入三辊纠偏机6进入纠偏,然后进入检测台7进行检测,确认无问题后进入静电涂油机8内进行防腐处理,最后出口剪9、出口夹送10送到卷取机11进行卷取,当卷取到需要的大小时,由出口剪9剪断复合板,然后取出成卷的铝粉铁复合板进行装箱打包即可。

Claims (2)

1.一种多层金属复合板,其特征是:一种多层金属复合板,以铁板为基板,铝为面板,形成多层金属合板,即铁-铝二层复合板,即在铁板上铝。
2.一种超音速火焰铝粉融合铁复合板生产流水线,其包括布置在生产流水线入口部分(a)的开卷机(1)、入口夹送(2)和入口剪(3),布置在生产流水线加工部分(b)的三辊纠偏机(6)和检测台(7),以及布置在生产流水线出口部分(c)的出口剪(8)、出口夹送(10)和卷取机(11),其特征是:它还包括布置在生产流水线加工部分(b)的超音速火焰铝粉喷涂机(4)、冷轧机(5)和静电涂油机(8),其中超音速火焰铝粉喷涂机(4)布置在入口剪(3)之后,其与冷轧机(5)配套使用完成铝粉与铁板的复合,冷轧机(5)布置在超音速火焰铝粉喷涂机(4)之后;所述静电涂油机(8)布置在检测台(7)后方,方便对复合加工后的复合板进行防腐处理。
CN201210030252XA 2012-02-10 2012-02-10 超音速火焰铝粉融合铁复合板生产流水线 Pending CN102582156A (zh)