CN102581014A - 生产薄壁无缝钢管的工艺 - Google Patents

生产薄壁无缝钢管的工艺 Download PDF

Info

Publication number
CN102581014A
CN102581014A CN2012100256220A CN201210025622A CN102581014A CN 102581014 A CN102581014 A CN 102581014A CN 2012100256220 A CN2012100256220 A CN 2012100256220A CN 201210025622 A CN201210025622 A CN 201210025622A CN 102581014 A CN102581014 A CN 102581014A
Authority
CN
China
Prior art keywords
tubes
rolling
seamless steel
sizing
thin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012100256220A
Other languages
English (en)
Inventor
王国亮
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2012100256220A priority Critical patent/CN102581014A/zh
Publication of CN102581014A publication Critical patent/CN102581014A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种生产薄壁无缝钢管的工艺,包括步骤如下:加热,将管坯在加热炉中加热到1150℃以上;穿孔,经穿孔机对加热后的管坯进行穿孔,制成毛管;二次均热,将穿孔后制成的毛管送入斜底式加热炉中进行短时加热;轧制,将经过二次均热后的毛管穿在限动芯棒上,然后经过三辊斜轧机进行缩径、减壁、延伸轧制,形成荒管;脱管,轧制后的荒管从限动芯棒上脱出;定径整形,将荒管通过定径机组,进行定径、整形,形成热成品管;冷却,热成品管经过步进冷床进行冷却;成品收集,冷却后的热成品管进行校直、切头、检验、打包、标记入库,形成商品管。其解决了生产薄壁无缝钢管在轧制过程中降温快不易再轧制的生产难题,改变了薄壁无缝钢管生产以冷拔代替热轧的不合理产品结构,能够降低能耗、缩减了设备投资成本、提高了生产无缝钢管的效率。

Description

生产薄壁无缝钢管的工艺
技术领域
本发明属于钢管轧制工艺技术领域,具体涉及一种生产薄壁无缝钢管的工艺。
背景技术
我国经过多年的发展,无缝钢管的生产能力和产量已经连续几年排名第一。国内拥有了各种类型的无缝钢管热轧及冷拔机组,因历史发展的原因,技术布局参差不齐,落后的冷拔机组及技术占有很大的比例。特别是在薄壁无缝钢管生产技术领域内,由于穿孔后的毛管温度过低无法热轧。所以还运用着传统的穿孔冷拔等工艺,其能耗高、成材率低、污染环境严重已经严重影响了无缝钢管生产制造能力的提高。
发明内容
本发明的目的在于解决现有技术中存在的问题而提供一种生产薄壁无缝钢管的工艺。其解决了生产薄壁无缝钢管在轧制过程中降温快不易再轧制的生产难题,改变了薄壁无缝钢管生产以冷拔代替热轧的不合理产品结构,能够降低能耗、缩减了设备投资成本、提高了生产无缝钢管的效率。
本发明的技术方案是这样实现的:
生产薄壁无缝钢管的工艺,其特征在于包括如下步骤:
1)、加热,将管坯在加热炉中加热到1150℃以上;
2)、穿孔,经穿孔机对加热后的管坯进行穿孔,制成毛管;
3)、二次均热,将穿孔后制成的毛管送入斜底式加热炉中进行短时加热;
4)、轧制,将经过二次均热后的毛管穿在限动芯棒上,然后经过三辊斜轧机进行缩径、减壁、延伸轧制,形成荒管;
5)、脱管,轧制后的荒管从限动芯棒上脱出;
6)、定径整形,将荒管通过定径机组,进行定径、整形,形成热成品管;
7)、冷却,热成品管经过步进冷床进行冷却;
 8)、成品收集,冷却后的热成品管进行校直、切头、检验、打包、标记入库,形成商品管。
所述的步骤2)中的穿孔机为二辊斜轧式穿孔机。
所述的步骤3)中的二次均热至850-1050摄氏度,均热时间为3-5分钟。
所述的步骤6)中的定径机组为5-15架定径机连续布置组成。
本发明的积极效果:
1、传统冷拔加工工艺需要的酸洗,磷化,皂化环境污染较大,新工艺对环境不产生污染,有利于环评是环境影响。
2、相比传统工艺,生产效率提高2~3倍。
3、新工艺材料利用率高,每吨钢管生产效益提高20%左右。
4、固定设备投入少,生产周期短。
附图说明
图1为生产薄壁无缝钢管的工艺流程图。
图中:1、管坯加热炉,2、穿孔机组,3、进料机构,4、出料翻料机构,5 、斜底式加热炉,6、 燃气炉,7、旋转进料机构、限动芯棒机构,8、三辊斜轧机组,9、定径机组,10、步进冷床。
具体实施方式
实施例:结合如图1所示,对本发明生产薄壁无缝钢管的工艺实例作进一步的描述:生产薄壁无缝钢管的工艺,其特征在于包括如下步骤:
1)、加热,将直径为50-100毫米的管坯在加热炉中加热到1150℃以上;
2)、穿孔,经穿孔机对加热后的管坯进行穿孔,制成外径为53-103毫米的毛管;
3)、二次均热,将穿孔后制成的毛管送入斜底式加热炉中进行短时加热;
4)、轧制,将经过二次均热后的毛管穿在限动芯棒上,然后经过三辊斜轧机进行缩径、减壁、延伸轧制,形成荒管,相对于管坯来说,缩径在10-15毫米、减壁在0.5-1毫米、延伸轧制延伸率为1.2);
5)、脱管,轧制后的荒管从限动芯棒上脱出,通过三辊轧机的旋转、抱管及传料升降将轧制后的荒管带出;
6)、定径整形,将荒管通过定径机组,进行定径、整形,形成热成品管,其符合GB/T8162-1999标准;
7)、冷却,热成品管经过步进冷床进行冷却;
8)、成品收集,冷却后的热成品管进行校直、切头、检验、打包、标记入库,形成商品管。
所述的步骤2)中的穿孔机为二辊斜轧式穿孔机。
所述的步骤3)中的二次均热至850-1050摄氏度,均热时间为3-5分钟。
所述的步骤6)中的定径机组为5-15架定径机连续布置组成。
管坯在管坯加热炉中加热到1150℃以上时,经穿孔机组轧制成毛管,由进料机构送入斜底式加热炉加热到900℃以上时,由出料及翻料机构传到旋转进料机构及限动芯棒机构,跑车运动将毛管预穿在限动芯棒上,启动旋转进料,将毛管旋转送入三辊斜轧机组进行轧制,在轧制过程中通过液压限动芯棒机构的运行,进行缩径、减壁、延伸轧制,形成荒管;轧制后的荒管从限动芯棒上脱出,最后荒管通过定径机组进行定径整形,形成热成品管;定径后的热成品管经过步进冷床进行冷却;最终冷却后的热成品管进行校直、切头、检验、打包、标记入库,形成商品管。管坯加热炉与斜底式加热炉通过燃气炉供气。

Claims (4)

1.生产薄壁无缝钢管的工艺,其特征在于包括如下步骤:
1)、加热,将管坯在加热炉中加热到1150℃以上;
2)、穿孔,经穿孔机对加热后的管坯进行穿孔,制成毛管;
3)、二次均热,将穿孔后制成的毛管送入斜底式加热炉中进行短时加热;
4)、轧制,将经过二次均热后的毛管穿在限动芯棒上,然后经过三辊斜轧机进行缩径、减壁、延伸轧制,形成荒管;
5)、脱管,轧制后的荒管从限动芯棒上脱出;
6)、定径整形,将荒管通过定径机组,进行定径、整形,形成热成品管;
7)、冷却,热成品管经过步进冷床进行冷却;
8)、成品收集,冷却后的热成品管进行校直、切头、检验、打包、标记入库,形成商品管。
2.根据权利要求1所述的工艺,其特征在于:所述的步骤2)中的穿孔机为二辊斜轧式穿孔机。
3.根据权利要求1所述的工艺,其特征在于:所述的步骤3)中的二次均热至850-1050摄氏度,均热时间为3-5分钟。
4.根据权利要求1所述的工艺,其特征在于:所述的步骤6)中的定径机组为5-15架定径机连续布置组成。
CN2012100256220A 2012-02-07 2012-02-07 生产薄壁无缝钢管的工艺 Pending CN102581014A (zh)