CN102476826A - 一种降低四氯化钛生产过程中损耗的方法及装置 - Google Patents

一种降低四氯化钛生产过程中损耗的方法及装置 Download PDF

Info

Publication number
CN102476826A
CN102476826A CN2010105632508A CN201010563250A CN102476826A CN 102476826 A CN102476826 A CN 102476826A CN 2010105632508 A CN2010105632508 A CN 2010105632508A CN 201010563250 A CN201010563250 A CN 201010563250A CN 102476826 A CN102476826 A CN 102476826A
Authority
CN
China
Prior art keywords
titanium tetrachloride
titanium
production process
loss
condensing surface
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2010105632508A
Other languages
English (en)
Inventor
蒙钧
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guiyang Aluminum Magnesium Design and Research Institute Co Ltd
Original Assignee
Guiyang Aluminum Magnesium Design and Research Institute Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guiyang Aluminum Magnesium Design and Research Institute Co Ltd filed Critical Guiyang Aluminum Magnesium Design and Research Institute Co Ltd
Priority to CN2010105632508A priority Critical patent/CN102476826A/zh
Publication of CN102476826A publication Critical patent/CN102476826A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种降低四氯化钛生产过程中损耗的方法及装置,在采用现有的富钛料氯化生产四氯化钛方法进行四氯化钛生产时,本发明对富钛料氯化生产四氯化钛生产线的收尘冷凝器底部进行加热,使收尘冷凝器内部底部的温度保持在140℃~160℃,这样即可降低四氯化钛生产过程中四氯化钛的损耗,并提高钛金属实收率。在对富钛料氯化生产四氯化钛生产线的收尘冷凝器底部进行加热时,最好是对其生产线中的2#收尘冷凝器底部进行加热。本发明具有能提高钛金属实收率、减少环境污染、简化生产流程和减少操作人员、提高能源的利用率等优点。

Description

一种降低四氯化钛生产过程中损耗的方法及装置
技术领域
本发明涉及一种降低四氯化钛生产过程中损耗的方法及装置,属于富钛料氯化生产四氯化钛技术领域。
背景技术
目前,在现有的富钛料氯化生产四氯化钛的工艺流程中,在其生产线的氯化炉出炉的四氯化钛混合气温度为600~1000℃,该混合气体通常经过四氯化钛生产线中的收尘冷凝器降温到160~200℃,在收尘冷凝器冷凝降温过程中由于为降低气流速度,往往将混合气体中的高沸点物和固态沉降达到除尘的作用,这样很容易引起收尘冷凝器底部有部分四氯化钛气冷凝而变为液态,该液态的四氯化钛沿收尘气内表面与收尘渣一起排出,这不仅会使四氯化钛损失,而且还同时由于收尘渣的粒度较小,当四氯化钛液体与之混合后形成浆状物较难排出,并在处理过程中造成污染环境(特别是生产线中的2#收尘冷凝器这种现象更为严重)。在生产实践中由于环境温度的变化和产能的调节,四氯化钛的冷凝量较大,并且在冬季冷凝量更大,其四氯化钛的损失也就更多。因此现有的富钛料氯化生产四氯化钛生产工艺及装置还是不够理想。
发明内容
本发明的目的是:提供一种既能减少四氯化钛的损失、同时又能保证收尘冷凝器底部排渣顺利的、并且热效率高、能减少环境污染的降低四氯化钛生产过程中损耗的方法及装置,从而克服现有技术的不足。
本发明的技术方案是这样实现的:本发明的一种降低四氯化钛生产过程中损耗的方法,包括采用现有的富钛料氯化生产四氯化钛的方法,在采用现有的富钛料氯化生产四氯化钛方法进行四氯化钛生产时,对富钛料氯化生产四氯化钛生产线的收尘冷凝器底部进行加热,使收尘冷凝器内部底部的温度保持在140℃~160℃,这样即可降低四氯化钛生产过程中四氯化钛的损耗,并提高钛金属实收率。
在对收尘冷凝器进行加热时,其加热温度为160℃~200℃。
用于本发明方法的一种降低四氯化钛生产过程中损耗的装置,包括富钛料氯化生产四氯化钛生产线中的收尘冷凝器,在收尘冷凝器的底部设有加热装置。
上述加热装置为燃气加热装置、空气加热装置、蒸汽加热装置或电加热装置。
由于采用了上述技术方案,本发明将收尘冷凝器内部底部的温度保持在140℃~160℃,这样即可使收尘冷凝器底部收尘渣的温度高于四氯化钛的沸点(136.5℃),使四氯化钛处于气化状态,从而有效的消除了现有技术所存在的问题。因此,本发明与现有技术相比,本发明具有以下优点:
1、减少了四氯化钛生产过程中的损失,提高了钛金属实收率;
2、减少了四氯化钛生产过程中的环境污染;
3、由于不需要对收尘冷凝器中形成的浆状物进行处理,因此简化了生产流程和减少了生产岗位与操作人员,从而有效地提高了劳动生产率和降低了生产成本; 
4、由于减少了四氯化钛生产过程中的损失,因此有效地提高了能源的利用率,达到了节能的目的。
附图说明
图1为本发明的结构示意图。
附图的中箭头方向表示在生产过程中四氯化钛混合气的流动方向。
具体实施方式
下面结合附图和实施例对本发明作进一步的说明。
本发明的实施例:在采用现有的富钛料氯化生产四氯化钛方法进行四氯化钛生产时,按照本发明的一种降低四氯化钛生产过程中损耗的方法对现有的富钛料氯化生产四氯化钛生产线进行改造后再进行生产,即对富钛料氯化生产四氯化钛生产线的收尘冷凝器1的底部进行加热,使收尘冷凝器1内部底部的温度保持在140℃~160℃,这样即可降低四氯化钛生产过程中四氯化钛的损耗,并提高钛金属实收率;在对富钛料氯化生产四氯化钛生产线的收尘冷凝器1底部进行加热时,最好特别是对其生产线中的2#收尘冷凝器1的底部进行加热即成。
在对对现有的富钛料氯化生产四氯化钛生产线进行改造时,采用本发明的一种降低四氯化钛生产过程中损耗的装置,该装置包括现有的富钛料氯化生产四氯化钛生产线中的收尘冷凝器1,在收尘冷凝器1的底部安装上加热装置2;其加热装置2可采用现有的燃气加热装置、空气加热装置、蒸汽加热装置或电加热装置,通过这些加热装置的热媒:热空气、蒸汽或导热油等进行间接加热。在对收尘冷凝器1进行加热时,将加热装置2的加热温度控制在160℃~200℃范围即可。

Claims (4)

1.一种降低四氯化钛生产过程中损耗的方法,包括采用富钛料氯化生产四氯化钛的方法,其特征在于:在采用现有的富钛料氯化生产四氯化钛方法进行四氯化钛生产时,对富钛料氯化生产四氯化钛生产线的收尘冷凝器底部进行加热,使收尘冷凝器内部底部的温度保持在140℃~160℃,这样即可降低四氯化钛生产过程中四氯化钛的损耗,并提高钛金属实收率。
2.根据权利要求1所述的降低四氯化钛生产过程中损耗的方法,其特征在于:在对收尘冷凝器进行加热时,其加热温度为160℃~200℃。
3.一种降低四氯化钛生产过程中损耗的装置,包括富钛料氯化生产四氯化钛生产线中的收尘冷凝器(1),其特征在于:在收尘冷凝器(1)的底部设有加热装置(2)。
4.根据权利要求3所述的降低四氯化钛生产过程中损耗的装置,其特征在于:加热装置(2)为燃气加热装置、空气加热装置、蒸汽加热装置或电加热装置。
CN2010105632508A 2010-11-29 2010-11-29 一种降低四氯化钛生产过程中损耗的方法及装置 Pending CN102476826A (zh)