CN102357557A - Steel strip cold rolling and winding method without additional lining paper - Google Patents

Steel strip cold rolling and winding method without additional lining paper Download PDF

Info

Publication number
CN102357557A
CN102357557A CN2011102106986A CN201110210698A CN102357557A CN 102357557 A CN102357557 A CN 102357557A CN 2011102106986 A CN2011102106986 A CN 2011102106986A CN 201110210698 A CN201110210698 A CN 201110210698A CN 102357557 A CN102357557 A CN 102357557A
Authority
CN
China
Prior art keywords
steel strip
strip surface
oil
rolling
lining paper
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2011102106986A
Other languages
Chinese (zh)
Other versions
CN102357557B (en
Inventor
刘铭豪
赵海波
邢勇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Angang Lianzhong Guangzhou Stainless Steel Co ltd
Original Assignee
Lianzhong (guangzhou) Stainless Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Lianzhong (guangzhou) Stainless Steel Co Ltd filed Critical Lianzhong (guangzhou) Stainless Steel Co Ltd
Priority to CN 201110210698 priority Critical patent/CN102357557B/en
Publication of CN102357557A publication Critical patent/CN102357557A/en
Application granted granted Critical
Publication of CN102357557B publication Critical patent/CN102357557B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention discloses a steel strip cold rolling and winding method without additional lining paper. The method comprises the following steps: 1) detecting a profile: a steel strip surface detection system performs profile detection for a steel strip surface, wherein the steel strip surface detection system automatically performs the investigation operation for the non-normal profile, and a step 2) is performed if the detected profile is normal; 2) spraying rolled oil: a oil spraying system sprays the rolled oil on the steel strip surface, after the excess rolled oil is removed by the initial oil scraping, the rolled oil is uniformly distributed on the steel strip surface, then treatments of rolling and winding are performed. According to the present invention, with the protection due to the extrusion resistance of the rolled oil, the case of direct contacting between the steel strip surfaces can not be generated, wherein the direct contacting between the steel strip surfaces can cause the crack, such that the friction between the steel coils is effectively reduced, the protection is provided for the steel strip surface; because the convex part of the non-normal profile does not exist, such that the chiseled mark destruction between the steel strips can not be generated, the good steel strip quality is ensured while the use of the high-cost lining paper is avoided, the step of the lining paper adding is avoided so as to save the production cost.

Description

A kind of cold rolling rolling method of steel band that does not add lining paper
Technical field
The invention belongs to the stainless-steel cold-rolling field, be specifically related to a kind of cold rolling rolling method of steel band that does not add lining paper.
Background technology
When stainless steel carries out cold rolling batching; Because the steel band template through hot rolling is handled is different, comprises normal template and improper template, improper template such as wedge shape template, bimodal pattern etc.; One side of wedge shape template can exceed small height than opposite side; The bimodal pattern steel plate then has slight convexity in the both sides of steel plate, when wedge shape template or bimodal pattern steel plate when carrying out cold rolling rolling, between the steel band because bimodal or its raised area of wedge shape template can cause the local contact of steel strip surface; Cause steel strip surface cut to occur, influence the steel band quality.
Be to reduce friction mutually between the stainless-steel sheet, the way that adopts at present is the special-purpose lining paper of liner between stainless-steel sheet, preventing that producing loose winding between the stainless-steel roll produces the cutter trace with friction, thus the assurance product quality.But, because the temperature of cold-rolled steel coils is generally at 120 ℃, sometimes up to 150 ℃; Therefore, lining paper needs heat resistance preferably, with thermal degradation or the carbonization that prevents the part fiber; Can not occur influencing isolation effect because of paper strength descends; To the demanding while of lining paper, the cost of lining paper is higher, in coil of strip, adds the cost that lining paper has also just increased production and processing.
Summary of the invention
The object of the present invention is to provide and a kind ofly can protect the cold rolling rolling method of the intact steel band that does not add lining paper of steel strip surface, so that when guaranteeing the steel band quality, save production cost.
The cold rolling rolling method of steel band that does not add lining paper according to the invention; Comprise the steps: 1), detect template: the steel strip surface detection system is carried out template to steel strip surface and is detected, and for improper template, investigates operation automatically; If it is normal to detect template, then get into step 2); 2) spray rolls and prolongs oil: injection system steel strip surface evenly spray roll and prolong oil, remove unnecessary rolling through preliminary frizing and prolong after the oil, make to roll and prolong oil and be evenly distributed in steel strip surface, roll then and prolong rolling.
Preferably, the said saponification value of prolonging oil of rolling is greater than the every gram of 7mg potassium hydroxide.
Preferably, said roll prolong oil saponification value be the every grams of 10 mg potassium hydroxide.
Preferably, said steel strip surface detection system will move steel strip surface data input picture treatment system and analyze identification through being arranged at the face scan light electric coupling image high speed video system of hot rolling roller-way upper and lower.
Adopt the cold rolling rolling method of steel band that does not add lining paper according to the invention, before cold rolling, earlier template is carried out on the surface of steel band and detect, for detected improper template; Then send alarm or investigate operation automatically by the steel strip surface detection system; The detection system testing result be template normal after, by injection system steel strip surface is sprayed to roll uniformly and prolongs oil, roll the crush resistance of prolonging oil itself and help protecting steel strip surface can directly not contact breaking; The all right friction that effectively reduces between the coil of strip of oil is prolonged in rolling of evenly covering; Effectively steel strip surface is protected,, can better be guaranteed that can not occur cutting a hole trace between steel band and the steel band destroys owing to there is not the bossing of improper template; When having guaranteed that equally the steel band quality is intact; Also can avoid the use of the higher lining paper of cost, remove the step of adding lining paper from, thereby save production cost effectively.
Description of drawings
Fig. 1 does not add the cold rolling rolling flowage structure of the steel band sketch map of lining paper for the present invention.
The specific embodiment
Below in conjunction with accompanying drawing, the present invention is further described.
The cold rolling rolling method of steel band that does not add lining paper according to the invention; Comprise the steps: 1), detect template: the steel strip surface detection system is carried out template to steel strip surface and is detected, and for improper template, investigates operation automatically; If it is normal to detect template, then get into step 2); 2) spray rolls and prolongs oil: injection system steel strip surface evenly spray roll and prolong oil, remove unnecessary rolling through preliminary frizing and prolong after the oil, make to roll and prolong oil and be evenly distributed in steel strip surface, roll then and prolong rolling.
What the present invention was different with mode in the past is before cold rolling, just to have preestablished and detected the surface of steel band being carried out template, for detected improper template; Then send alarm or investigate operation automatically, improper template is in time investigated by the steel strip surface detection system, the detection system testing result be template normal after; By injection system steel strip surface is sprayed to roll uniformly and prolong oil; Roll and prolong crush resistance of oil itself and help protecting steel strip surface can directly not contact breaking, the effectively friction between the minimizing coil of strip of oil is prolonged in rolling of evenly covering, and effectively steel strip surface is protected; When having guaranteed that equally the steel band quality is intact; Also can avoid the use of the higher lining paper of cost, remove the step of adding lining paper from, thereby save production cost effectively.
For guaranteeing that better the steel strip surface quality is intact; The said saponification value of prolonging oil of rolling is greater than the every gram of 7mg potassium hydroxide (7mgKOH/g); For example, roll the saponification value of prolonging oil and can be the every gram of 7.2mg potassium hydroxide (7.2mgKOH/g), the every gram of 7.4mg potassium hydroxide (7.4mgKOH/g), the every gram of 7.6mg potassium hydroxide (7.6mgKOH/g), the every gram of 7.8mg potassium hydroxide (7.8mgKOH/g), the every gram of 7.9mg potassium hydroxide (7.9mgKOH/g), the every gram of 8.2mg potassium hydroxide (8.2mgKOH/g), the every gram of 8.4mg potassium hydroxide (8.4mgKOH/g), the every gram of 8.7mg potassium hydroxide (8.7mgKOH/g), the every gram of 9.0mg potassium hydroxide (9.0mgKOH/g), the every gram of 9.2mg potassium hydroxide (9.2mgKOH/g), the every gram of 9.4mg potassium hydroxide (9.4mgKOH/g), the every gram of 9.6mg potassium hydroxide (9.6mgKOH/g), the every gram of 9.8mg potassium hydroxide (9.8mgKOH/g), the every gram of 9.9mg potassium hydroxide (9.9mgKOH/g), the every gram of 10mg potassium hydroxide (10mgKOH/g) or the every gram of 10.3mg potassium hydroxide (10.3mgKOH/g) etc.As embodiment preferably, select that to roll the saponification value of prolonging oil be the every gram of 10mg potassium hydroxide (10mgKOH/g) for use, it is high more to roll the saponification value of prolonging oil; Roll the anti-extrusion performance of prolonging oil also can rise thereupon; Spray oil film behind the coil of strip surface is not easy to break, and can evenly cover steel strip surface, plays the effect of protection coil of strip; Thereby avoid the mutual friction generates cutter of coil of strip trace; Through practical proof, to roll and prolong oily viscosity and saponification value through control template, raising for the coil of strip of discharging thickness less than 0.8 millimeter, intact the rolling of milling train can not added lining paper and well guaranteed crudy.
In addition; For improving recognition effect to steel strip surface; When steel strip surface is detected; The steel strip surface detection system will move steel strip surface data input picture treatment system and analyze identification through being arranged at the face scan light electric coupling image high speed video system of hot rolling roller-way upper and lower, and its accuracy of identification is high.
More than the technical scheme that the embodiment of the invention provided has been carried out detailed introduction; Used concrete example among this paper the principle and the embodiment of the embodiment of the invention are set forth, the explanation of above embodiment only is applicable to the principle that helps to understand the embodiment of the invention; Simultaneously, for one of ordinary skill in the art, according to the embodiment of the invention, the part that on the specific embodiment and range of application, all can change, in sum, this description should not be construed as limitation of the present invention.

Claims (4)

1. the cold rolling rolling method of steel band that does not add lining paper is characterized in that, comprises the steps: 1), detect template: the steel strip surface detection system is carried out template to steel strip surface and is detected; For improper template; Automatically investigate operation,, then get into step 2) if it is normal to detect template; 2) spray rolls and prolongs oil: injection system steel strip surface evenly spray roll and prolong oil, remove unnecessary rolling through preliminary frizing and prolong after the oil, make to roll and prolong oil and be evenly distributed in steel strip surface, roll then and prolong rolling.
2. the cold rolling rolling method of steel band that does not add lining paper according to claim 1 is characterized in that, the said saponification value of prolonging oil of rolling is greater than the every gram of 7mg potassium hydroxide.
3. the cold rolling rolling method of steel band that does not add lining paper according to claim 2 is characterized in that, said roll prolong oil saponification value be the every grams of 10 mg potassium hydroxide.
4. the cold rolling rolling method of steel band that does not add lining paper according to claim 1; It is characterized in that; Said steel strip surface detection system will move steel strip surface data input picture treatment system and analyze identification through being arranged at the face scan light electric coupling image high speed video system of hot rolling roller-way upper and lower.
CN 201110210698 2011-07-26 2011-07-26 Steel strip cold rolling and winding method without additional lining paper Expired - Fee Related CN102357557B (en)