CN102329925A - 一种经改善疲劳寿命的杆件类构件 - Google Patents

一种经改善疲劳寿命的杆件类构件 Download PDF

Info

Publication number
CN102329925A
CN102329925A CN201110136043A CN201110136043A CN102329925A CN 102329925 A CN102329925 A CN 102329925A CN 201110136043 A CN201110136043 A CN 201110136043A CN 201110136043 A CN201110136043 A CN 201110136043A CN 102329925 A CN102329925 A CN 102329925A
Authority
CN
China
Prior art keywords
rod piece
rod member
center
goods
stress
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201110136043A
Other languages
English (en)
Inventor
钱云春
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201110136043A priority Critical patent/CN102329925A/zh
Publication of CN102329925A publication Critical patent/CN102329925A/zh
Pending legal-status Critical Current

Abstract

本发明提供一种经改善疲劳寿命的杆件类构件,一杆件类长型金属构件的外表面被感应线圈快速加热的后并以淬火剂喷雾加以冷却,而在处理的同时此杆件承受足以使杆件的中间部份趋近降伏而使杆件稍微拉长的拉力。杆件上的拉力被释放后,则杆件的已冷却的外层上可获得高度的残余压缩表面应力,其构成一环形部份且稍微缩短了杆件,直到表层的压缩应力与作用在杆件的中央部份的拉应力相等为止,藉此便能大大地改进杆件的疲劳寿命。

Description

一种经改善疲劳寿命的杆件类构件
技术领域
本发明涉及一种杆件类构件,尤其是一种经改善疲劳寿命的杆件类构件。
背景技术
本发明提供一种经改善疲劳寿命的杆件类构件,一杆件类长型金属构件的外表面被感应线圈快速加热的后并以淬火剂喷雾加以冷却,而在处理的同时此杆件承受足以使杆件的中间部份趋近降伏而使杆件稍微拉长的拉力。杆件上的拉力被释放后,则杆件的已冷却的外层上可获得高度的残余压缩表面应力,其构成一环形部份且稍微缩短了杆件,直到表层的压缩应力与作用在杆件的中央部份的拉应力相等为止,藉此便能大大地改进杆件的疲劳寿命。
发明内容
针对上述问题,本发明提供一种经改善疲劳寿命的杆件类构件。
本发明提供一种经改善疲劳寿命的杆件类构件,一杆件类长型金属构件的外表面被感应线圈快速加热的后并以淬火剂喷雾加以冷却,而在处理的同时此杆件承受足以使杆件的中间部份趋近降伏而使杆件稍微拉长的拉力。杆件上的拉力被释放后,则杆件的已冷却的外层上可获得高度的残余压缩表面应力,其构成一环形部份且稍微缩短了杆件,直到表层的压缩应力与作用在杆件的中央部份的拉应力相等为止,藉此便能大大地改进杆件的疲劳寿命。一种由承受外负荷及/或弯曲负荷时其疲劳寿命已有改进的细长轴向延伸构件所构成的制品,包括:一具有作用在小面积上的高残余压缩应力的外环构件;以及一和该外环构件一体成型的内心子,此内心子具有作用在大面积上的残余应力,以便当无拉外力时在相对方向上的内力可相等,其中该轴向延伸金属构件系一全长均为圆形横断面的轴向伸长杆件,其中该轴向延伸构件系一全长均具有固定的内径及外径的轴向长管状构件,该内心子的构造系管状的,一种由细长轴向延伸金属元件所构成的制品,具有于迅速加热至高温同时遭受轴向应力时能在熔化前先软化的特性,其后迅速将的冷却以于外层产生高残余压缩应力,俾于遭受外负荷及/或弯曲负荷时能改进其疲劳寿命,此制品包括:一薄层外构件,具有作用于小面积上的至少10,000psi的高残余压缩应力;以及一与该外构件一体成型的内心子,具有作用在大面积上的向第二方向的残余拉应力,俾当无外力时在相对方向上的内力可相等,其中该轴向延伸金属元件系一全长尚为圆形横断面的轴向细长杆件,其中该轴向延伸金属元件系一元件全长均具有固定的内径及外径的轴向细长管状构件,该内心子的构造系管状的。一种由细长轴向延伸元件所能成的制品,于遭受外拉伸负荷及/或弯曲负荷时其疲劳寿命已有改进,包括:一外构件,具有作用于小面积上至少10,000psi的高残余压缩应力;以及一与该外构件一体成型的内心子,此内心子具有作用在大面积上的残余拉应力,俾当无外力时在相对方向上的内力可相等,其中该细长轴向延伸元件系一至少其长度的主要部分均为圆形横断面的杆件,其中该细长轴向延伸元件系一元件全长均具有固定的内径及外径的管状构件,该内心子的构造系管状的。
具体实施方式
本发明提供一种经改善疲劳寿命的杆件类构件,一杆件类长型金属构件的外表面被感应线圈快速加热的后并以淬火剂喷雾加以冷却,而在处理的同时此杆件承受足以使杆件的中间部份趋近降伏而使杆件稍微拉长的拉力。杆件上的拉力被释放后,则杆件的已冷却的外层上可获得高度的残余压缩表面应力,其构成一环形部份且稍微缩短了杆件,直到表层的压缩应力与作用在杆件的中央部份的拉应力相等为止,藉此便能大大地改进杆件的疲劳寿命。一种由承受外负荷及/或弯曲负荷时其疲劳寿命已有改进的细长轴向延伸构件所构成的制品,包括:一具有作用在小面积上的高残余压缩应力的外环构件;以及一和该外环构件一体成型的内心子,此内心子具有作用在大面积上的残余应力,以便当无拉外力时在相对方向上的内力可相等,其中该轴向延伸金属构件系一全长均为圆形横断面的轴向伸长杆件,其中该轴向延伸构件系一全长均具有固定的内径及外径的轴向长管状构件,该内心子的构造系管状的,一种由细长轴向延伸金属元件所构成的制品,具有于迅速加热至高温同时遭受轴向应力时能在熔化前先软化的特性,其后迅速将的冷却以于外层产生高残余压缩应力,俾于遭受外负荷及/或弯曲负荷时能改进其疲劳寿命,此制品包括:一薄层外构件,具有作用于小面积上的至少10,000psi的高残余压缩应力;以及一与该外构件一体成型的内心子,具有作用在大面积上的向第二方向的残余拉应力,俾当无外力时在相对方向上的内力可相等,其中该轴向延伸金属元件系一全长尚为圆形横断面的轴向细长杆件,其中该轴向延伸金属元件系一元件全长均具有固定的内径及外径的轴向细长管状构件,该内心子的构造系管状的。一种由细长轴向延伸元件所能成的制品,于遭受外拉伸负荷及/或弯曲负荷时其疲劳寿命已有改进,包括:一外构件,具有作用于小面积上至少10,000psi的高残余压缩应力;以及一与该外构件一体成型的内心子,此内心子具有作用在大面积上的残余拉应力,俾当无外力时在相对方向上的内力可相等,其中该细长轴向延伸元件系一至少其长度的主要部分均为圆形横断面的杆件,其中该细长轴向延伸元件系一元件全长均具有固定的内径及外径的管状构件,该内心子的构造系管状的。

Claims (3)

1.一种由承受外负荷及/或弯曲负荷时其疲劳寿命已有改进的细长轴向延伸构件所构成的制品,包括:一具有作用在小面积上的高残余压缩应力的外环构件;以及一和该外环构件一体成型的内心子,此内心子具有作用在大面积上的残余应力,以便当无拉外力时在相对方向上的内力可相等。
2.如申请专利范围第1项的制品,其中该轴向延伸金属构件是一全长均为圆形横断面的轴向伸长杆件。
3.如申请专利范围第1项的制品,其中该轴向延伸构件是一全长均具有固定的内径及外径的轴向长管状构件,该内心子的构造系管状的。
CN201110136043A 2011-05-24 2011-05-24 一种经改善疲劳寿命的杆件类构件 Pending CN102329925A (zh)