CN102287049B - 防腐抗渗保温屋面的施工方法 - Google Patents

防腐抗渗保温屋面的施工方法 Download PDF

Info

Publication number
CN102287049B
CN102287049B CN 201110137494 CN201110137494A CN102287049B CN 102287049 B CN102287049 B CN 102287049B CN 201110137494 CN201110137494 CN 201110137494 CN 201110137494 A CN201110137494 A CN 201110137494A CN 102287049 B CN102287049 B CN 102287049B
Authority
CN
China
Prior art keywords
insulation layer
cement
rubber cement
layer
construction
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201110137494
Other languages
English (en)
Other versions
CN102287049A (zh
Inventor
葛加君
华菊芬
班新华
谢春海
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kunming Erjian Construction (group) Co Ltd
Original Assignee
Kunming Erjian Construction (group) Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kunming Erjian Construction (group) Co Ltd filed Critical Kunming Erjian Construction (group) Co Ltd
Priority to CN 201110137494 priority Critical patent/CN102287049B/zh
Publication of CN102287049A publication Critical patent/CN102287049A/zh
Application granted granted Critical
Publication of CN102287049B publication Critical patent/CN102287049B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种防腐抗渗保温屋面的施工方法,包括清理基层、铺设保温层、涂刷胶浆、铺贴防水层、施工保护层等步骤。本发明施工方便,形成的屋面起到了抗老化、延长使用寿命的效果,据对比试验显示,可延长屋面修补年限5年以上;保温效果比普通保温屋面提高热阻力36.5%。

Description

防腐抗渗保温屋面的施工方法
技术领域
本发明涉及一种防腐抗渗保温屋面的施工方法。
背景技术
现有的屋面施工时,把保温与防水进行分隔,一般做保温就不考虑防水,做防水就不考虑保温,不能互相兼得,影响工作效果。
发明内容
本发明的目的在于提供一种结构合理,兼具保温和防水双重功能的防腐抗渗保温屋面的施工方法。
本发明的技术解决方案是:
一种防腐抗渗保温屋面的施工方法,其特征是:包括下列步骤:
(1)清理基层:将基层表面的浮灰、油污、杂物清理干净,凸出部位剔平,使表面平整;
(2)铺设保温层:用聚氨酯硬泡体或沥青膨胀珍珠岩作保温层;
铺设聚氨酯硬泡体保温层时,采用现场连续喷涂施工方法,施工时,气温应为15~35℃,风速不超过5m/s,相对湿度应小于85%;
铺设沥青膨胀珍珠岩作保温层时,采用下列方法:a)先将膨胀珍珠岩散料倒在锅内预热并不断翻动,预热温度为100~120℃,然后倒入已熬好的沥青中拌合均匀;所述已熬好的沥青温度为190~240℃;沥青与膨胀珍珠岩的重量比例为1:0.7~0.8;
b)铺设时,采用木板分隔,进行“分仓”施工,每仓宽度为700~900mm;
c)保温层的虚铺厚度为设计厚度的130%,然后用木板拍实抹平至设计厚度;
d)抹找平层:施工找平层,找平层由下列重量比的材料制成:水泥:粗砂:细砂=1:2:1,找平层初凝后洒水养护;
(3)涂刷胶浆:先配置胶浆:在水平基层上施工时,胶浆的各组分重量比为:PⅡ32.5水泥:水:901胶=1:0.3:0.2;在侧面基层上施工时,胶浆的各组分重量比为:PⅡ32.5水泥:水:901胶=1:0.24~0.26:0.17~0.16;然后进行涂刷,胶浆涂刷厚度为3~5mm;
(4)铺贴防水层:将BAC防水卷材平铺在胶浆上,晾放24~48小时;
(5)施工保护层:在BAC防水卷材上再采用刚性砂浆或混凝土施工保护层。
在排气管和构筑物穿过保温层和防水层的管壁周边及构筑物四周,预留排气口;,女儿墙根部与保温层、防水层之间设温度缝,缝宽15~20mm,并贯穿到结果基层。
用聚氨酯硬泡体作保温层时:屋面及山墙、女儿墙的聚氨酯硬泡体保温层直接连续地喷涂至泛水高度,最低泛水高度不小于250mm;在天沟、檐沟的连接处聚氨酯硬泡体保温层实行连续喷涂,在无组织排水檐口,聚氨酯硬泡体实行连续喷到檐口端部;在伸出屋面的管道或通气管根部,根据泛水高度要求连续地直接喷涂;在屋顶垂直出入口处,聚氨酯硬泡体保温层收头连续喷涂至帽口;水落口防水保温层手头构造采用下列形式:横式水落口周围直径500mm范围内的坡度不小于2%,在山墙或女儿墙的横式水落口处,将聚氨酯硬泡体保温层连续地直接喷涂至水落口内。
本发明施工方便,形成的屋面起到了抗老化、延长使用寿命的效果,据对比试验显示,可延长屋面修补年限5年以上;保温效果比普通保温屋面提高热阻力36.5%。
下面结合实施例对本发明作进一步说明。
具体实施方式
一种防腐抗渗保温屋面的施工方法,包括下列步骤:
(1)清理基层:将基层表面的浮灰、油污、杂物清理干净,凸出部位剔平,使表面平整;
(2)铺设保温层:用聚氨酯硬泡体或沥青膨胀珍珠岩作保温层;
铺设聚氨酯硬泡体保温层时,采用现场连续喷涂施工方法,施工时,气温应为15~35℃,风速不超过5m/s,相对湿度应小于85%;
铺设沥青膨胀珍珠岩作保温层时,采用下列方法:a)先将膨胀珍珠岩散料倒在锅内预热并不断翻动,预热温度为100~120℃,然后倒入已熬好的沥青中拌合均匀;所述已熬好的沥青温度为190~240℃;沥青与膨胀珍珠岩的重量比例为1:0.7~0.8;
b)铺设时,采用木板分隔,进行“分仓”施工,每仓宽度为700~900mm;
c)保温层的虚铺厚度为设计厚度的130%,然后用木板拍实抹平至设计厚度;
d)抹找平层:施工找平层,找平层由下列重量比的材料制成:水泥:粗砂:细砂=1:2:1,找平层初凝后洒水养护;
(3)涂刷胶浆:先配置胶浆:在水平基层上施工时,胶浆的各组分重量比为:PⅡ32.5水泥:水:901胶=1:0.3:0.2;在侧面基层上施工时,胶浆的各组分重量比为:PⅡ32.5水泥:水:901胶=1:0.24~0.26:0.17~0.16;然后进行涂刷,胶浆涂刷厚度为3~5mm;
(4)铺贴防水层:将BAC防水卷材平铺在胶浆上,晾放24~48小时;
(5)施工保护层:在BAC防水卷材上再采用刚性砂浆或混凝土施工保护层。
在排气管和构筑物穿过保温层和防水层的管壁周边及构筑物四周,预留排气口;,女儿墙根部与保温层、防水层之间设温度缝,缝宽15~20mm,并贯穿到结果基层。
用聚氨酯硬泡体作保温层时:屋面及山墙、女儿墙的聚氨酯硬泡体保温层直接连续地喷涂至泛水高度,最低泛水高度不小于250mm;在天沟、檐沟的连接处聚氨酯硬泡体保温层实行连续喷涂,在无组织排水檐口,聚氨酯硬泡体实行连续喷到檐口端部;在伸出屋面的管道或通气管根部,根据泛水高度要求连续地直接喷涂;在屋顶垂直出入口处,聚氨酯硬泡体保温层收头连续喷涂至帽口;水落口防水保温层手头构造采用下列形式:横式水落口周围直径500mm范围内的坡度不小于2%,在山墙或女儿墙的横式水落口处,将聚氨酯硬泡体保温层连续地直接喷涂至水落口内。

Claims (2)

1.一种防腐抗渗保温屋面的施工方法,其特征是:包括下列步骤:
(1)清理基层:将基层表面的浮灰、油污、杂物清理干净,凸出部位剔平,使表面平整;
(2)铺设保温层:用沥青膨胀珍珠岩作保温层;
铺设沥青膨胀珍珠岩作保温层时,采用下列方法:a)先将膨胀珍珠岩散料倒在锅内预热并不断翻动,预热温度为100~120℃,然后倒入已熬好的沥青中拌合均匀;所述已熬好的沥青温度为190~240℃;沥青与膨胀珍珠岩的重量比例为1:0.7~0.8;
b)铺设时,采用木板分隔,进行“分仓”施工,每仓宽度为700~900mm;
c)保温层的虚铺厚度为设计厚度的130%,然后用木板拍实抹平至设计厚度;
d)抹找平层:施工找平层,找平层由下列重量比的材料制成:水泥:粗砂:细砂=1:2:1,找平层初凝后洒水养护;
(3)涂刷胶浆:先配置胶浆:在水平基层上施工时,胶浆的各组分重量比为:PⅡ32.5水泥:水:901胶=1:0.3:0.2;在侧面基层上施工时,胶浆的各组分重量比为:PⅡ32.5水泥:水:901胶=1:0.24~0.26:0.17~0.16;然后进行涂刷,胶浆涂刷厚度为3~5mm;
(4)铺贴防水层:将BAC防水卷材平铺在胶浆上,晾放24~48小时; 
(5)施工保护层:在BAC防水卷材上再采用刚性砂浆或混凝土施工保护层。
2.根据权利要求1所述的防腐抗渗保温屋面的施工方法,其特征是:在排气管和构筑物穿过保温层和防水层的管壁周边及构筑物四周,预留排气口,女儿墙根部与保温层、防水层之间设温度缝,缝宽15~20mm,并贯穿到结果基层。 
CN 201110137494 2011-05-26 2011-05-26 防腐抗渗保温屋面的施工方法 Expired - Fee Related CN102287049B (zh)