CN102285300A - Three-dimensional texture high-definition glass painting and processing method thereof - Google Patents

Three-dimensional texture high-definition glass painting and processing method thereof Download PDF

Info

Publication number
CN102285300A
CN102285300A CN201110168606A CN201110168606A CN102285300A CN 102285300 A CN102285300 A CN 102285300A CN 201110168606 A CN201110168606 A CN 201110168606A CN 201110168606 A CN201110168606 A CN 201110168606A CN 102285300 A CN102285300 A CN 102285300A
Authority
CN
China
Prior art keywords
glass substrate
shadow glue
line
shadow
glass
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201110168606A
Other languages
Chinese (zh)
Other versions
CN102285300B (en
Inventor
不公告发明人
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jinan Chuanghakka Science and Technology Development Co., Ltd.
Original Assignee
JINAN GUANGFA TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JINAN GUANGFA TECHNOLOGY Co Ltd filed Critical JINAN GUANGFA TECHNOLOGY Co Ltd
Priority to CN201110168606A priority Critical patent/CN102285300B/en
Publication of CN102285300A publication Critical patent/CN102285300A/en
Application granted granted Critical
Publication of CN102285300B publication Critical patent/CN102285300B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a three-dimensional texture high-definition glass painting and a processing method thereof. The three-dimensional texture high-definition glass painting comprises a glass substrate, a shadowless glue layer and a photo-cured glue layer which are glued into a whole in turn; and the outside of the photo-cured glue layer is provided with three-dimensional patterns. The processing method comprises the following steps of: making the shadowless glue layer on the glass substrate; and making the photo-cured glue layer on the shadowless glue layer. The glass substrate is not damaged, and two glue layers are arranged on the outside of the glass substrate, so that the structural strength of the glass substrate with the two glue layer is higher than that of the single glass substrate. The three-dimensional texture high-definition glass painting can refract various colors under the irradiation of sun light; the three-dimensional patterns are molded through a mold, the mold can be repeatedly used, and the cost is low; moreover, the manufacturing method is simple, and convenient to implement. The three-dimensional patterns are molded by the mold, and the definition of the three-dimensional patterns is higher than that of three-dimensional patterns formed by processes such as chemical etching, mechanical polishing, sand blasting and the like.

Description

A kind of cubic texture high-definition glass is drawn and processing method
Technical field
The present invention relates to a kind of glass-painting and processing method thereof of making the high definition picture effect, particularly a kind of glass-painting and processing method thereof of high definition picture cubic texture effect.
Background technology
It mainly is that picture is sticked on the glass plate that a little artistic glass that had is in the past drawn, and only can produce the less demanding simple art glass of definition is drawn no stereoeffect.Also having a kind of is to be compressed on the picture that forms stereoeffect on the glass surface by mould behind the glass sintering, or forms by processes such as chemical attack, mechanical grinding, sandblasts.These several cubic texture glass-paintings are to form picture by the destruction to glass substrate, and the structural strength of glass-painting is low, cracky, and energy-output ratio is big, and environment is had pollution, and the cost height of processing and fabricating.
Summary of the invention
The problem to be solved in the present invention is: provide the high cubic texture high-definition glass of a kind of structural strength to draw, and provide a kind of cubic texture high-definition glass to draw processing method, make its cubic texture high-definition glass that processes draw the structural strength height.
For addressing the above problem, cubic texture high-definition glass of the present invention is drawn and is comprised the glass substrate that is bonded to one successively, no shadow glue-line and light binding layer, and the outside of light binding layer has space pattern.
Can manifest specific image for the cubic texture high-definition glass is drawn, described no shadow glue-line is the first no shadow glue-line, is bonded with the plane picture layer that the second no shadow glue-line and pigment form between the glass substrate and the first no shadow glue-line successively.
Cubic texture high-definition glass method for making picture of the present invention comprises the steps:
(1) make no shadow glue-line: a keeps flat transparent glass substrate, falls a certain amount of no shadow glue on glass substrate, covers polyester film, pushes polyester film and no shadow glue is spread spare between glass substrate and polyester film; B adopts the ultraviolet ray irradiation to make no shadow adhesive curing; C takes polyester film off, forms the first no shadow glue-line on the glass substrate;
(2) make the light binding layer: a goes up a certain amount of light binding on the first no shadow glue-line, cover the mould of space pattern, and extrusion die makes light binding spread even between no shadow glue-line and mould and is full of mould; B adopts the ultraviolet ray irradiation that light binding is solidified; C takes mould off, forms the light binding layer that the outside has space pattern on the first no shadow glue-line.
In order to improve the bonding force of the light binding layer and the first no shadow glue-line, described step (1) afterwards step (2) to polish before the first no shadow glue-line upper surface around the wide edge of 2-3CM.
For the cubic texture high-definition glass picture that this method is made can manifest specific image, make plane picture layer: a before with print image plane also oven dry on transparent film in step (1); B, the no shadow glue of some of on glass substrate, falling, the printing surface that covers transparent film and make transparent film down, the extruding transparent film is spread no shadow glue to spare between glass substrate and transparent film; C adopts the ultraviolet ray irradiation to make no shadow adhesive curing; D takes transparent film off, and the pigment on the transparent film sticks on the no shadow glue, forms second no shadow glue-line and the plane image layer on the glass substrate; No shadow glue is on the plane picture layer that is poured on the glass substrate in the step poly-(1).
In order to improve curing rate, it is the 200-400 nanometer that ultraviolet wavelength is adopted in the curing of described no shadow glue, and be 300-500 second hardening time, and it is the 200-400 nanometer that ultraviolet wavelength is adopted in the curing of described light binding, and be 500-600 second hardening time.
In order to improve extrusion speed, the cold paperhanging machine extruding is all adopted in the extruding in described each step.
Beneficial effect of the present invention: cubic texture high-definition glass of the present invention is drawn on the light binding layer and forms space pattern, the light binding layer passes through the firm bonding structure of no shadow glue-line outside glass substrate, itself is not damaged glass substrate, and increase two-layer glue-line in its outside, higher than the structural strength of glass substrate itself.Cubic texture high-definition glass of the present invention is drawn under the irradiation of light of sunlight can reflect many each colors, and after increasing the plane picture layer, can also manifest specific high-definition image.The cubic texture high-definition glass that this cubic texture high-definition glass method for making picture processes is drawn the structural strength height.And the cubic texture pattern is by mould molding, and mould can be reused, and cost is low, and this preparation method is simple, and it is convenient to implement.Space pattern of the present invention is by mould molding, and is higher than the definition of the space pattern of technological formings such as chemical attack, mechanical grinding, sandblast.
Description of drawings
Fig. 1 is the structural representation of the cross section of the specific embodiment one drawn of cubic texture high-definition glass of the present invention; Fig. 2 is the structural representation of the cross section of the specific embodiment two drawn of cubic texture high-definition glass of the present invention;
Among the figure: 1, light binding layer, 2, the first no shadow glue-line, 3, glass substrate, 4, the plane picture layer, 5, the second no shadow glue-line.
The specific embodiment
Specific embodiment one
A kind of cubic texture high-definition glass is as shown in Figure 1 drawn, and it comprises glass substrate 3, first no shadow glue-line 2 and the light binding layer 1 that is bonded to one successively, and the outside of light binding layer 1 has space pattern.
The preparation method that this cubic texture high-definition glass is drawn comprises the steps:
1, clean and dry up or dry naturally transparent glass substrate 3 waters or alcohol wash with hair-dryer.This step purpose is in order to improve the image quality after the cubic texture high-definition glass is drawn as shape, and the adhesion that improves glass substrate 3 and no shadow glue.
2, glass substrate 3 is kept flat, fall a certain amount of no shadow glue on glass substrate 3, the glass substrate 3 of 1 square meter falls the no shadow glue of 50-60ml.Cover polyester film, the extruding polyester film is spread no shadow glue between glass substrate 3 and polyester film even.The extruding polyester film can carry out in cold paperhanging machine, also can scrape pressure with rubber roll roll-in or scraper plate by hand.
3, adopt the ultraviolet ray irradiation to make no shadow adhesive curing; Ultraviolet wavelength 200-400 nanometer, be 300-500 second hardening time.
4, scratch flowing to glass substrate 3 no shadow glue all around along the edge of glass substrate 3, take polyester film off, form the first no shadow glue-line 2 on the glass substrate 3.
5, use 300 orders or 400 purpose liquid honings, the first no shadow glue-line, 2 upper surface edges, the width of polishing is 2-3CM.
6, glass substrate 3 is kept flat, the first no shadow glue-line 2 is gone up a certain amount of light binding up on the first no shadow glue-line 2, cover the mould of space pattern again, and extrusion die makes light binding spread even between no shadow glue-line and mould and is full of mould; Mould can adopt the soft transparent plastics, has on the transparent plastic with the cubic texture high-definition glass to draw the corresponding space pattern of space pattern, and the glass of 1 square meter needs the light binding of 80-100ml generally speaking.Extrusion die can carry out in cold paperhanging machine, also can scrape pressure with rubber roll roll-in or scraper plate by hand.
7, adopt the ultraviolet ray irradiation that light binding is solidified; Ultraviolet wavelength 200-400 nanometer, 500-600 second hardening time.
8, scratch flowing to glass substrate 3 light binding all around along the edge of glass substrate 3, again mould is taken off, form the light binding layer 1 that the outside has space pattern on the first no shadow glue-line 2.
9, use cutter to handle glass substrate 3 edges, the cutter edge of a knife is downward, neat get final product of glass substrate 3 edge cuts, and makes glass substrate 3 edge-smoothings with the polish edge of glass substrate 3 of sand plate.
10, the impurity that uses alcohol will remain in step 9 aftershaping cubic texture high-definition glass picture surface is at last wiped.Step 9 and 10 purpose are that the cubic texture high-definition glass is drawn is more attractive in appearance.
Specific embodiment two
A kind of cubic texture high-definition glass is as shown in Figure 2 drawn, and it comprises glass substrate 3, the second no shadow glue-line 5, plane picture layer 4, first no shadow glue-line 2 and the light binding layer 1 that is bonded to one successively, and the outside of light binding layer 1 has space pattern.
The preparation method that this cubic texture high-definition glass is drawn comprises the steps:
1, clean and dry up or dry naturally transparent glass substrate 3 waters or alcohol wash with hair-dryer.
2, with print image plane also oven dry on transparent film; Fall the no shadow glue of some on glass substrate 3, the glass substrate 3 of 1 square meter is put into the no shadow glue of 50-60ml, the printing surface that covers transparent film and make transparent film down, the extruding transparent film is spread no shadow glue to spare between glass substrate 3 and transparent film; The extruding transparent film can carry out in cold paperhanging machine, also can scrape pressure with rubber roll roll-in or scraper plate by hand.
3, adopt the ultraviolet ray irradiation to make no shadow adhesive curing; Ultraviolet wavelength 200-400 nanometer, be 300-500 second hardening time.
4, scratch flowing to glass substrate 3 no shadow glue all around along the edge of glass substrate 3, take transparent film off, the pigment on the transparent film sticks on the no shadow glue, forms second no shadow glue-line 5 and the plane image layer 4 on the glass substrate 3.
5, glass substrate 3 is kept flat, plane picture layer 4 falls a certain amount of no shadow glue up on the plane picture layer 4 on the glass substrate 3, and the glass substrate 3 of 1 square meter is put into the no shadow glue of 50-60ml.Cover polyester film, the extruding polyester film is spread no shadow glue between glass substrate 3 and polyester film even.The extruding polyester film can carry out in cold paperhanging machine, also can scrape pressure with rubber roll roll-in or scraper plate by hand.
6, adopt the ultraviolet ray irradiation to make no shadow adhesive curing; Ultraviolet wavelength 200-400 nanometer, be 300-500 second hardening time.
7, scratch flowing to glass substrate 3 no shadow glue all around along the edge of glass substrate 3, take polyester film off, form the first no shadow glue-line 2 on the second no shadow glue-line 5 of glass substrate 3.
8, use the edge of 300 orders or 400 purpose liquid honings, first no shadow glue-line 2 upper surfaces, the width of polishing is 2-3CM.
9, glass substrate 3 is kept flat, the first no shadow glue-line 2 is gone up a certain amount of light binding up on the first no shadow glue-line 2, cover the mould of space pattern again, and extrusion die makes light binding spread even between the first no shadow glue-line and mould and is full of mould; Mould can adopt the soft transparent plastics, has on the transparent plastic with the cubic texture high-definition glass to draw the corresponding space pattern of space pattern, and the glass of 1 square meter needs the light binding of 80-100ml generally speaking.Extrusion die can carry out in cold paperhanging machine, also can scrape pressure with rubber roll roll-in or scraper plate by hand.
10, adopt the ultraviolet ray irradiation that light binding is solidified; Ultraviolet wavelength 200-400 nanometer, 500-600 second hardening time.
11, scratch flowing to glass substrate 3 light binding all around along the edge of glass substrate 3, again mould is taken off, form the light binding layer 1 that the outside has space pattern on the first no shadow glue-line 2.
12, use cutter to handle glass substrate 3 edges, the cutter edge of a knife is downward, neat get final product of glass substrate 3 edge cuts, and makes glass substrate 3 edge-smoothings with the polish edge of glass substrate 3 of sand plate.
13, the impurity that uses alcohol will remain in step 12 forming stereo texture high-definition glass picture surface is at last wiped and is got final product.
The shop of the various glue described in this patent is even to be meant that glue has been expressed to the layer dielectric edge, and the glue layer between the two layer medium does not have bubble, if there is bubble to drive bubble out of from medium edge with rubber roll.

Claims (7)

1. a cubic texture high-definition glass is drawn, and it is characterized in that: comprise the glass substrate that is bonded to one successively, no shadow glue-line and light binding layer, the outside of light binding layer has space pattern.
2. cubic texture high-definition glass according to claim 1 is drawn, and it is characterized in that: described no shadow glue-line is the first no shadow glue-line, is bonded with the plane picture layer that the second no shadow glue-line and pigment form between the glass substrate and the first no shadow glue-line successively.
3. a cubic texture high-definition glass method for making picture is characterized in that: comprise the steps:
Make no shadow glue-line: a keeps flat transparent glass substrate, falls a certain amount of no shadow glue on glass substrate, covers polyester film, and the extruding polyester film is spread no shadow glue to spare between glass substrate and polyester film; B adopts the ultraviolet ray irradiation to make no shadow adhesive curing; C takes polyester film off, forms the first no shadow glue-line on the glass substrate;
Make the light binding layer: a goes up a certain amount of light binding on the first no shadow glue-line, cover the mould of space pattern, and extrusion die makes light binding spread even between no shadow glue-line and mould and is full of mould; B adopts the ultraviolet ray irradiation that light binding is solidified; C takes mould off, forms the light binding layer that the outside has space pattern on the first no shadow glue-line.
4. cubic texture high-definition glass method for making picture according to claim 3 is characterized in that: described step (1) afterwards step (2) to polish before the first no shadow glue-line upper surface around the wide edge of 2-3CM.
5. according to claim 3 or 4 described cubic texture high-definition glass method for making picture, it is characterized in that: make plane picture layer: a before with print image plane also oven dry on transparent film in step (1); B, the no shadow glue of some of on glass substrate, falling, the printing surface that covers transparent film and make transparent film down, the extruding transparent film is spread no shadow glue to spare between glass substrate and transparent film; C adopts the ultraviolet ray irradiation to make no shadow adhesive curing; D takes transparent film off, and the pigment on the transparent film sticks on the no shadow glue, forms second no shadow glue-line and the plane image layer on the glass substrate; No shadow glue is on the plane picture layer that is poured on the glass substrate in the step poly-(1).
6. cubic texture high-definition glass method for making picture according to claim 5, it is characterized in that: it is the 200-400 nanometer that ultraviolet wavelength is adopted in the curing of described no shadow glue, be 300-500 second hardening time, it is the 200-400 nanometer that ultraviolet wavelength is adopted in the curing of described light binding, and be 500-600 second hardening time.
7. cubic texture high-definition glass method for making picture according to claim 5 is characterized in that: the cold paperhanging machine extruding is all adopted in the extruding in described each step.
CN201110168606A 2011-06-22 2011-06-22 Three-dimensional texture high-definition glass painting and processing method thereof Active CN102285300B (en)