CN102197934B - 水晶框 - Google Patents

水晶框 Download PDF

Info

Publication number
CN102197934B
CN102197934B CN 201110025782 CN201110025782A CN102197934B CN 102197934 B CN102197934 B CN 102197934B CN 201110025782 CN201110025782 CN 201110025782 CN 201110025782 A CN201110025782 A CN 201110025782A CN 102197934 B CN102197934 B CN 102197934B
Authority
CN
China
Prior art keywords
crystal frame
glue
glass
picture
dust
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201110025782
Other languages
English (en)
Other versions
CN102197934A (zh
Inventor
刘义贤
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANGHAI NANBING ENVIRONMENTAL PROTECTION TECHNOLOGY CO., LTD.
Original Assignee
刘义贤
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 刘义贤 filed Critical 刘义贤
Priority to CN 201110025782 priority Critical patent/CN102197934B/zh
Publication of CN102197934A publication Critical patent/CN102197934A/zh
Application granted granted Critical
Publication of CN102197934B publication Critical patent/CN102197934B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种水晶框,所述水晶框包括玻璃、环氧树脂、固化剂。构成水晶框的胶水的组分以及各组分占胶水总重量百分比为:环氧树脂67%,固化剂33%;照片存放在水晶框中,具有保存时间长,照片不易褪色,表面光泽透亮。因此市场运用前景很广泛,本发明的水晶框的有益效果有:(1)制作成本低;(2)生产过程操作简单。

Description

水晶框
技术领域
本发明涉及一种装饰品,具体涉及一种水晶框。
背景技术
水晶框能够长时间保存图片,而且画面细腻而清晰、光滑而不刺眼,并具有立体感,欣赏性极强,由于画纸与空气彻底隔离,具有清晰度高,色彩艳丽,永不褪色、防水、防晒、可擦洗等特点,因此,在日常生活广泛的被运用,具有较好的经济价值。水晶框的使用场所包括办公、家居、商场、礼堂、学校,作为婚庆、生日、家居摆挂件非常的适宜。
发明内容
本发明所要解决的技术问题是提供一种防晒、防水、可擦洗的水晶框。
本发明的一种水晶框,包括玻璃、环氧树脂、固化剂,将玻璃表面用自粘胶贴上图片,然后用环氧树脂和固化剂配备成待用的水晶框胶水,将配备好的水晶框胶水搅拌均匀后倒在粘好图片的玻璃面上,用刮板刮平,然后进行排泡,排完泡之后等待凝固即是本产品。
所述待用胶水的重量为玻璃的平方米的1.2倍;
所述固化剂为聚醚氨;
本发明的优点有:(1)生产工艺简单;(2)生产成本低;(3)无毒害性。
具体实施方式
为了了解本发明,下面详细阐述一下本发明:
实施例1:制备水晶框
按如下重量百分比配料:
环氧树脂67%;
固化剂33%。
步骤:
a)首先准备无尘房,房间内安装好恒温装置,恒温装置能控制在30℃-70℃之间调节;
b)无尘房内设制好操作台,操作台面必须保持水平;
c)把需要规格的玻璃或镜片表面上贴上图片,图片与玻璃粘合的胶水可选择自粘胶或双面胶;
d)把贴好图片的玻璃放在操作台面上:
e)操作时先不用打开温控装置;
f)按玻璃规格大小比例配好水晶框胶水,水晶框胶水标准比例:玻璃的平方米×1.2倍(千克),水晶框胶水搅拌均匀;
g)把搅均匀胶水倒在粘好图片的玻璃面上,用刮板刮平,然后进行排泡;
h)排泡方法
1)真空排泡:把刮平胶水的玻璃板放入真空机内抽2分钟真空。
2)用火排泡:用丁烷装上火枪,在AB胶面上快速平扫,在气流的作用下,气泡自然破裂;
i)完成破泡后,打开温控开关、温度控制在40℃左右,操作人员离开无尘房;
j)无尘房内温度必须要25℃以上,25℃以下无法完全凝固,温度越高凝固时间就越短。8小时凝固;
k)完全凝固后即可取出包装。
水晶框的凝固和硬化时间:
编号 无尘房内温度 凝固时间 硬化时间 备注
1 25℃ 8小时 150小时 恒温
2 30℃ 6小时 130小时 恒温
3 35℃ 5小时 110小时 恒温
4 40℃ 4小时 90小时 恒温
5 45℃ 3小时 72小时 恒温
6 50℃ 2.5小时 60小时 恒温
7 60℃ 2小时 48小时 恒温
实施例2:制备水晶框
按如下重量百分比配料:
环氧树脂75%;
固化剂25%。
步骤:
a)首先准备无尘房,房间内安装好恒温装置,恒温装置能控制在30℃-70℃之间调节;
b)无尘房内设制好操作台,操作台面必须保持水平;
c)把需要规格的玻璃或镜片表面上贴上图片,图片与玻璃粘合的胶水可选择自粘胶或双面胶;
d)把贴好图片的玻璃放在操作台面上:
e)操作时先不用打开温控装置;
f)按玻璃规格大小比例配好水晶框胶水,水晶框胶水标准比例:玻璃的平方米×1.2倍(千克),水晶框胶水搅拌均匀;
g)把搅均匀胶水倒在粘好图片的玻璃面上,用刮板刮平,然后进行排泡;
h)排泡方法
1)真空排泡:把刮平胶水的玻璃板放入真空机内抽2分钟真空。
2)用火排泡:用丁烷装上火枪,在AB胶面上快速平扫,在气流的作用下,气泡自然破裂;
i)完成破泡后,打开温控开关、温度控制在40℃左右,操作人员离开无尘房;
j)无尘房内温度必须要25℃以上,25℃以下无法完全凝固,温度越高凝固时间就越短。8小时凝固;
k)完全凝固后即可取出包装。
水晶框的凝固和硬化时间:
编号 无尘房内温度 凝固时间 硬化时间 备注
1 25℃ 8小时 150小时 恒温
2 30℃ 6小时 130小时 恒温
3 35℃ 5小时 110小时 恒温
4 40℃ 4小时 90小时 恒温
5 45℃ 3小时 72小时 恒温
6 50℃ 2.5小时 60小时 恒温
7 60℃ 2小时 48小时 恒温
本发明的范围不受所述具体实施方案的限制,所述实施方案只欲作为阐明本发明各个方面的例子,本发明范围内还包括功能等同的方法和组分。实际上,除了本文所述的内容外,本领域技术人员参照上文的描述可以容易地掌握对本发明的多种改进。所述改进也落入所附权利要求书的范围之内。

Claims (3)

1.一种水晶框,包括玻璃、环氧树脂、固化剂,构成水晶框的胶水的组分以及各组分占水晶框胶水总重量百分比为:环氧树脂67%;固化剂33%,其特征在于,制备步骤为:
a)首先准备无尘房,房间内安装好恒温装置,恒温装置能控制在30℃-70℃之间调节;
b)无尘房内设制好操作台,操作台面必须保持水平;
c)把需要规格的玻璃或镜片表面上贴上图片,图片与玻璃粘合的胶水可选择自粘胶或双面胶;
d)把贴好图片的玻璃放在操作台面上:
e)操作时先不用打开温控装置;
f)按玻璃规格大小比例配好水晶框胶水,水晶框胶水搅拌均匀;
g)把搅均匀胶水倒在粘好图片的玻璃面上,用刮板刮平,然后进行排泡;
h)排泡方法
1)真空排泡:把刮平胶水的玻璃板放入真空机内抽2分钟真空;
2)用火排泡:用火枪装上丁烷,在AB胶面上快速平扫,在气流的作用下,气泡自然破裂;
i)完成破泡后,打开温控开关、温度控制在40℃左右,操作人员离开无尘房;
j)无尘房内温度必须要25℃以上,25℃以下无法完全凝固,温度越高凝固时间就越短,8小时凝固;
k)完全凝固后即可取出包装。
2.根据权利要求1所述的一种水晶框,其特征为:所述固化剂为聚醚氨。
3.根据权利要求1所述的一种水晶框,其特征为:所述水晶框胶水的需要配比的重量为玻璃面积×1.2倍(千克),其中,玻璃面积的单位为平方米。
CN 201110025782 2011-01-24 2011-01-24 水晶框 Expired - Fee Related CN102197934B (zh)