CN102161613A - 氟代苯的除水方法 - Google Patents
氟代苯的除水方法 Download PDFInfo
- Publication number
- CN102161613A CN102161613A CN2010105987469A CN201010598746A CN102161613A CN 102161613 A CN102161613 A CN 102161613A CN 2010105987469 A CN2010105987469 A CN 2010105987469A CN 201010598746 A CN201010598746 A CN 201010598746A CN 102161613 A CN102161613 A CN 102161613A
- Authority
- CN
- China
- Prior art keywords
- fluorobenzene
- water
- removal agent
- moisture
- dewatering
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及电池电解液技术领域,具体公开了一种新型的锂离子电池电解液添加剂——氟代苯的除水方法。本发明采取的技术方案是:在氟代苯中加入不溶于氟代苯且又能吸附水分的除水剂。除水剂为硅铝酸盐氧化物、活性炭、硅胶、硫酸钡或活性氧化铝,除水剂的加入量为氟代苯重量的1~10%。本发明在氟代苯中加入一种或几种除水剂,可以简单、快速的除去氟代苯中的水分,从而减少将其添加到锂离子电池电解液中而带来负面影响。本发明方法简单,满足了高品质电解液对氟代苯的要求。
Description
技术领域
本发明涉及电池电解液技术领域,具体公开了一种新型的锂离子电池电解液添加剂——氟代苯的除水方法。
背景技术
氟代苯是工业上一种重要的有机溶剂,应用范围非常广泛。近年来,随着科学技术的不断进步,氟代苯的用途得到不断的开发,目前高纯非水氟代苯已经成功应用于锂离子电池电解液中,相对于通常的含碳酸酯电解液相比,加入较大含量的氟代苯可以改善电池的性能,从电池的低温性能、电池寿命和高温放电能力来看,均有明显的优点。
氟代苯在生产、运输、储存过程中都可能带来水分,若水分过高,会影响锂离子电池电解液的水分,过高的水分对电池的电化学性能有一定的影响,通常电解液中水分控制在30ppm以内或者更低。以传统的生产工艺,氟代苯中水分偏高,无法满足高品质电池级要求。
发明内容
本发明采取的技术方案是:所述的氟代苯的除水方法,其特点是:在氟代苯中加入不溶于氟代苯且又能吸附水分的除水剂。
除水剂为硅铝酸盐氧化物、活性炭、硅胶、硫酸钡或活性氧化铝,除水剂的加入量为氟代苯重量的1~10%。优选地,除水剂的加入量为氟代苯重量的5~10%。进一步优选地,除水剂的加入量为氟代苯重量的8%。
本发明的工艺流程:在充氩气的手套箱中(水分<10ppm、氧份<10ppm)中进行氟代苯的除水:按比例将氟代苯置入不锈钢的钢瓶中(钢瓶用充高纯氩气抽真空置换三次),加入氟代苯重量的1~10%量的除水剂,密封后摇晃5—10分钟,使氟代苯和除水剂充分接触,静置3-5小时后再摇晃5—10分钟,取样测试处理后的氟代苯水分;上述过程温度控制在20~30℃,时间为3~5小时,取样检测达到要求后将脱水剂和氟代苯过滤后即得到高品质要求的氟代苯。
本发明的有益效果是:氟代苯中加入一种或几种除水剂,可以简单、快速的除去氟代苯中的水分,从而减少将其添在加到锂离子电池电解液中而带来负面影响。本发明方法简单,能有效降低氟代苯中水分含量,满足了高品质电解液对氟代苯的要求。
具体实施方式
下面以具体实施例对本发明作进一步的说明,但本发明不受下述实施例的限定。
实施例1
氟代苯,纯度为99.95%,水分84ppm。取上述氟代苯500g,置入不锈钢的钢瓶中(钢瓶用充高纯氩气抽真空置换三次),然后加入50 g的硅铝酸盐,密封后摇晃5分钟,使氟代苯和除水剂充分接触,静置3小时后再摇晃5分钟,于20℃处理3~4小时,处理后水分为9.3ppm(采用Metrohm KF-831型(瑞士万通)库仑水分测试仪测定)。
实施例2
氟代苯,纯度为99.93%,水分104ppm。取上述氟代苯500g,置入不锈钢的钢瓶中(钢瓶用充高纯氩气抽真空置换三次),然后加入25 g 的活性炭,密封后摇晃8分钟,使氟代苯和除水剂充分接触,静置5小时后再摇晃8分钟,于20℃处理5小时,处理后水分为7.3ppm(采用Metrohm KF-831型(瑞士万通)库仑水分测试仪测定)。
实施例3
氟代苯,纯度为99.96%,水分95ppm。取上述氟代苯500g,置入不锈钢的钢瓶中(钢瓶用充高纯氩气抽真空置换三次),然后加入25 g的硫酸钡和15 g活性氧化铝,密封后摇晃10分钟,使氟代苯和除水剂充分接触,静置3小时后再摇晃10分钟,于25℃处理3小时,处理后水分为6.8ppm(采用Metrohm KF-831型(瑞士万通)库仑水分测试仪测定)。
以上所述仅是本发明的较佳实施方式,故凡依本发明专利申请范围所述的构造、特征及原理所做的等效变化或修饰,均包括于本发明专利申请范围内。
Claims (5)
1.氟代苯的除水方法,其特征在于:在氟代苯中加入不溶于氟代苯且又能吸附水分的除水剂;除水剂为硅铝酸盐氧化物、活性炭、硅胶、硫酸钡或活性氧化铝的其中一种。
2.根据权利要求1所述的氟代苯的除水方法,其特征在于:除水剂的加入量为氟代苯重量的1~10%。
3. 根据权利要求1所述的氟代苯的除水方法,其特征在于:除水剂的加入量为氟代苯重量的5~10%。
4.根据权利要求1所述的氟代苯的除水方法,其特征在于:除水剂的加入量为氟代苯重量的8%。
5.根据权利要求1所述的氟代苯的除水方法,其特征在于:工艺方法如下:在水分<10ppm、氧份<10ppm的充氩气的手套箱中进行氟代苯的除水:按比例将氟代苯置入不锈钢的钢瓶中(钢瓶用充高纯氩气抽真空置换三次),加入氟代苯重量1~10%量的除水剂,密封后摇晃5—10分钟,使氟代苯和除水剂充分接触,静置3-5小时后再摇晃5—10分钟,取样分析测试处理后的氟代苯水分;上述过程温度控制在20~30℃,时间为3~5小时,取样检测达到要求后将脱水剂和氟代苯过滤后即得到产品氟代苯。