CN102085629A - Process for treating wood grain on surface of wood floor board - Google Patents
Process for treating wood grain on surface of wood floor board Download PDFInfo
- Publication number
- CN102085629A CN102085629A CN2010105531282A CN201010553128A CN102085629A CN 102085629 A CN102085629 A CN 102085629A CN 2010105531282 A CN2010105531282 A CN 2010105531282A CN 201010553128 A CN201010553128 A CN 201010553128A CN 102085629 A CN102085629 A CN 102085629A
- Authority
- CN
- China
- Prior art keywords
- face
- floor
- wood
- floor board
- polishing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention provides a process for treating wood grain on the surface of a wood floor board, comprising the following steps: processing a groove and tongue on a moulded floor board; polishing the end face of the floor board by virtue of a sanding machine or by adopting a manual matting way and blasting sand on the polished end face; brushing a tintlating on the end face of the floor board and drying and curing the tintlating; producing a concavo-convex polishing scratch region on the end face of the floor board by virtue of a polishing machine or by adopting the manual matting way; carrying out surface colour retouching on the polishing scratch region; and carrying out painting applications on the floor board. After tinting, polishing and surface colour retouching are carried out in the invention, the grain of the wood floor board is clearer, and the floor board is provided with the concavo-convex polishing scratch region in natural aberration, thus the senses of beauty and obsolescence indicating loss of time can be obtained from perception.
Description
Technical field
The present invention relates to the treatment process of wood floors, the Wood grain processing technique on a kind of specifically wood floors surface.
Background technology
Along with growth in the living standard, people are also more and more stricter for the requirement of living environment, and wood floors have natural wood grain as a kind of sheet material of high-quality, therefore, also more and more are subjected to doting on of consumers in general.At present, the wood floors of being sold on the market, the treatment process of its wood grain is comparatively single, and the texture on floor can slowly disappear the overall aesthetic on reduction floor through after wearing and tearing.
Summary of the invention
At above the deficiencies in the prior art and defective, the object of the present invention is to provide the Wood grain processing technique on a kind of wood floors surface.
The objective of the invention is by realizing by the following technical solutions:
The Wood grain processing technique on a kind of wood floors surface may further comprise the steps:
A, tongue and groove processing is carried out on the floor of moulding;
The mode of b, use sander or hand-sand is polished the end face on floor, and the end face sandblast after polishing;
C, end face brushes tint lating on the floor, and described tint lating is carried out dry solidification, and the moisture of this tint lating is dried to 6~15%;
The mode of d, employing sander or hand-sand grinds concavo-convex polishing scratch zone at the floor end face;
E, carry out complexion in the polishing scratch zone of floor end face and repair look and handle;
F, oil paint coating is carried out on the floor.
As the preferred technical solution of the present invention, the sandblast degree of depth of the floor end face in the described b step is 0.1~1mm.
As the preferred technical solution of the present invention, before the described c step, also comprise: use tenonen that circular arc chamfering or " V " shape chamfering are carried out in four end limits of floor end face, the arc length or the hypotenuse length of this circular arc chamfering or " V " shape chamfering are 0.3~6.5mm.
As the preferred technical solution of the present invention, adopt coating roller or manual mode to brush tint lating in the described c step at the floor end face.
As the preferred technical solution of the present invention, the length on described floor is 300~2200mm, and width is 58~220mm, and thickness is 9~22mm.
Compared with prior art, after the present invention repaiies the look processing by painted, polishing, complexion, the texture of wood floors is more clear, and has the concavo-convex polishing scratch zone of nature aberration on the floor, make the embodiment more true to nature of natural wood grain, simultaneously, it is local through wearing and tearing, fading appears in color, has a kind of aesthetic feeling and old sense of years loss from sense organ.
The specific embodiment
Below the specific embodiment of the present invention is described.
The Wood grain processing technique on this wood floors surface may further comprise the steps:
Wood floors processing technology through routine is processed as square floor with log material, the length on this floor, width, thickness, can be according to different floor specifications, different settings, comparatively preferred scheme: its length is 300~2200mm, width is 58~220mm, and thickness is 9~22mm.
First step: tongue and groove processing is carried out on the floor of this moulding, when assembling, so that splicing on the floor.
Second step: the mode of use sander or hand-sand is polished the end face on floor, and the end face sandblast after polishing, and the sandblast degree of depth is 0.1~1mm.
Third step: use tenonen that circular arc chamfering or " V " shape chamfering are carried out in four end limits of floor end face, the arc length or the hypotenuse length of this circular arc chamfering or " V " shape chamfering are 0.3~6.5mm.
The 4th step: adopt coating roller or manual mode, end face brushes tint lating on the floor, and described tint lating is carried out dry solidification, and the moisture of this tint lating is dried to 6~15%.
The 5th step: the mode that adopts sander or hand-sand, in conjunction with the natural texture of timber, grind concavo-convex polishing scratch zone with nature aberration at the floor end face, make the embodiment more true to nature of natural wood grain, simultaneously, it is local, and fading appears in color through wearing and tearing, has a kind of aesthetic feeling and old sense of years loss from sense organ.
The 6th step: use application machine or craft, different color and lusters is applied to the polishing scratch zone of floor end face uniformly, carry out complexion and repair look and handle, make wooden contrast color and the visual contrast effect that presents the different depths in conjunction with self natural texture.
The 7th step: oil paint coating is carried out on the floor.
The above is preferred embodiment of the present invention only, is not to be used for limiting practical range of the present invention; Every according to equivalence variation and modification that the present invention did, all covered by the scope of claims of the present invention.
Claims (5)
1. the Wood grain processing technique on a wood floors surface is characterized in that, may further comprise the steps:
A, tongue and groove processing is carried out on the floor of moulding;
The mode of b, use sander or hand-sand is polished the end face on floor, and the end face sandblast after polishing;
C, end face brushes tint lating on the floor, and described tint lating is carried out dry solidification, and the moisture of this tint lating is dried to 6~15%;
The mode of d, employing sander or hand-sand grinds concavo-convex polishing scratch zone at the floor end face;
E, carry out complexion in the polishing scratch zone of floor end face and repair look and handle;
F, oil paint coating is carried out on the floor.
2. the Wood grain processing technique on wood floors according to claim 1 surface is characterized in that: the sandblast degree of depth of the floor end face in the described b step is 0.1~1mm.
3. the Wood grain processing technique on wood floors according to claim 1 surface, it is characterized in that, before the described c step, also comprise: use tenonen that circular arc chamfering or " V " shape chamfering are carried out in four end limits of floor end face, the arc length or the hypotenuse length of this circular arc chamfering or " V " shape chamfering are 0.3~6.5mm.
4. the Wood grain processing technique on wood floors according to claim 1 surface is characterized in that: adopt coating roller or manual mode to brush tint lating at the floor end face in the described c step.
5. the Wood grain processing technique on wood floors according to claim 1 surface is characterized in that: the length on described floor is 300~2200mm, and width is 58~220mm, and thickness is 9~22mm.