CN102061074A - 绿色环保夜光无卤阻燃聚碳酸酯挤出片材料 - Google Patents
绿色环保夜光无卤阻燃聚碳酸酯挤出片材料 Download PDFInfo
- Publication number
- CN102061074A CN102061074A CN2010105754609A CN201010575460A CN102061074A CN 102061074 A CN102061074 A CN 102061074A CN 2010105754609 A CN2010105754609 A CN 2010105754609A CN 201010575460 A CN201010575460 A CN 201010575460A CN 102061074 A CN102061074 A CN 102061074A
- Authority
- CN
- China
- Prior art keywords
- halogen
- free
- percent
- retardant
- polycarbonate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开一种绿色环保夜光无卤阻燃聚碳酸酯挤出片材料,是由以下成分按重量比组成,聚碳酸酯:47.5-96%;复合无卤阻燃剂:1-35%;消烟剂:1.0-3.0%;夜光剂:0.1-6.0%;抗氧剂:0.1-2.0%;润滑剂:0.1-2.0%;其他助剂:1.3-5.5%。本发明绿色环保夜光无卤阻燃聚碳酸酯挤出片材料,综合机械性能优良,不含卤素,产品外观美观,同时,又赋予其夜光功能,同时他的夜光功能完全不需能量输入,仅仅依靠自身吸收后再在无光线时释放出来发光,并且生产采购方便,同时也符合所有的环保要求,具有较好的社会与经济价值,这样全面提高了产品竞争力。
Description
技术领域
本发明涉及一种有机高分子复合材料,更具体地说,是涉及一种绿色环保夜光无卤阻燃聚碳酸酯挤出片材料。本发明还涉及制作这种绿色环保夜光无卤阻燃聚碳酸酯挤出片材料的方法。
背景技术
聚碳酸酯片材目前已经在被广泛使用,出于安全性考虑,越来越多的地方开始要求使用阻燃的聚碳酸酯片材,而无卤阻燃化,又是当前全社会积极努力的方向,如何用无卤阻燃的技术方法生产聚碳酸酯片材,同时,又赋予其夜光功能,同时他的夜光功能完全不需能量输入,仅仅依靠自身吸收后再在无光线时释放出来发光,生产这种具有较好的社会与经济价值的环保材料已成为一个亟待解决的问题。
发明内容
本发明的目的在于,提供一种不含卤素且仅仅依靠自身吸收后再在无光线时释放出来发光的绿色环保夜光无卤阻燃聚碳酸酯挤出片材料。
本发明提供的技术方案如下:一种绿色环保夜光无卤阻燃聚碳酸酯挤出片材料,由以下成分按重量比组成,聚碳酸酯:47.5-96%;复合无卤阻燃剂:1-35%;消烟剂:1.0-3.0%;夜光剂:0.1-6.0%;抗氧剂:0.1-2.0%;润滑剂:0.1-2.0%;其他助剂:1.3-5.5%。
本发明所述的绿色环保夜光无卤阻燃聚碳酸酯挤出片材料的制备方法,包括如下步骤:先将聚碳酸酯用120度烘干,然后与抗氧剂、复合无卤阻燃剂、消烟剂、夜光剂、润滑剂、其他助剂按照比例称量后在混料机中低速混合10分钟,后再及时经平行同向双螺杆挤出机在一定强度剪切的螺杆组合情况下,在保持良好真空压力状态下,用一定螺杆转速混炼挤出,水冷拉条切粒经过筛分脱水制得绿色环保夜光无卤阻燃聚碳酸酯挤出片材料。
本发明绿色环保夜光无卤阻燃聚碳酸酯挤出片材料,综合机械性能优良,不含卤素,产品外观美观,同时,又赋予其夜光功能,同时他的夜光功能完全不需能量输入,仅仅依靠自身吸收后再在无光线时释放出来发光,并且生产采购方便,同时也符合所有的环保要求,具有较好的社会与经济价值,这样全面提高了产品竞争力。
具体实施方式
以下是本发明所述的绿色环保夜光无卤阻燃聚碳酸酯挤出片材料的实施例,并不因此限定本发明的保护范围。
实施例一,提供一种绿色环保夜光无卤阻燃聚碳酸酯挤出片材料,由以下成分按重量比组成,聚碳酸酯:87.0%,复合无卤阻燃剂:5%;消烟剂:2.2%;抗氧剂:1.0%,夜光剂:3.0%;润滑剂:0.3%;其他助剂:1.5%。
先将聚碳酸酯用120度烘干4小时,然后与抗氧剂、复合无卤阻燃剂、消烟剂、夜光剂、润滑剂、其他助剂按照比例称量后在混料机中低速混合10分钟,混料机采用低速混合,不锈钢材质,搅拌叶应与筒壁间隙小于0.5厘米,原辅料混合效果应目视各种粒子和粉末基本均匀,没有明显团块或集聚,然后再及时经平行同向双螺杆挤出机在一定强度剪切的螺杆组合情况下,双螺杆挤出机使用36长径比,在保持良好真空压力状态下,用一定螺杆转速混炼挤出,水冷拉条切粒经过筛分脱水制得绿色环保夜光无卤阻燃聚碳酸酯挤出片材料。
以上所述,仅为本发明的具体实施方式,但本发明的保护范围并不局限于此,任何熟悉本领域的技术人员在本发明所揭露的技术范围内,可不经过创造性劳动想到的变化或替换,都应涵盖在本发明的保护范围之内。因此,本发明的保护范围应该以权利要求书所限定的保护范围为准。
Claims (2)
1.一种绿色环保夜光无卤阻燃聚碳酸酯挤出片材料,其特征在于:是由以下成分按重量比组成,聚碳酸酯:47.5-96%;复合无卤阻燃剂:1-35%;消烟剂:1.0-3.0%;夜光剂:0.1-6.0%;抗氧剂:0.1-2.0%;润滑剂:0.1-2.0%;其他助剂:1.3-5.5%。
2.一种绿色环保夜光无卤阻燃聚碳酸酯挤出片材料的制备方法,其特征在于,包括如下步骤:先将聚碳酸酯用120度烘干,然后与抗氧剂、复合无卤阻燃剂、消烟剂、夜光剂、润滑剂、其他助剂按照比例称量后在混料机中低速混合10分钟,后再及时经平行同向双螺杆挤出机在一定强度剪切的螺杆组合情况下,在保持良好真空压力状态下,用一定螺杆转速混炼挤出,水冷拉条切粒经过筛分脱水制得绿色环保夜光无卤阻燃聚碳酸酯挤出片材料。