CN101914861B - 一种奶面纸的生产方法 - Google Patents

一种奶面纸的生产方法 Download PDF

Info

Publication number
CN101914861B
CN101914861B CN2010102369120A CN201010236912A CN101914861B CN 101914861 B CN101914861 B CN 101914861B CN 2010102369120 A CN2010102369120 A CN 2010102369120A CN 201010236912 A CN201010236912 A CN 201010236912A CN 101914861 B CN101914861 B CN 101914861B
Authority
CN
China
Prior art keywords
facial tissue
paper
milk facial
treatment
milk
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN2010102369120A
Other languages
English (en)
Other versions
CN101914861A (zh
Inventor
高晓明
詹金春
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
FUJIAN JIANNING LIANFENG MILL PAPER Co Ltd
Original Assignee
FUJIAN JIANNING LIANFENG MILL PAPER Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by FUJIAN JIANNING LIANFENG MILL PAPER Co Ltd filed Critical FUJIAN JIANNING LIANFENG MILL PAPER Co Ltd
Priority to CN2010102369120A priority Critical patent/CN101914861B/zh
Publication of CN101914861A publication Critical patent/CN101914861A/zh
Application granted granted Critical
Publication of CN101914861B publication Critical patent/CN101914861B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及造纸工艺领域,尤其涉及奶面纸的生产方法。本发明的奶面纸的生产方法,包括如下步骤:将商品纸将碎解处理;进行打浆处理;加入助剂;进行抄造处理;进行脱水处理和压榨处理;进行干燥处理;在圆筒卷纸机上卷取;放置以均衡水分处理,放置时间是24小时;经湿润机进行湿润处理;送入压光机热压光处理后即成奶面纸。本发明采用如上技术方案,实现了一种定量要求是22g/m2-40g/m2的透明度高、强度高的超薄奶面纸。

Description

一种奶面纸的生产方法
技术领域
本发明涉及造纸工艺领域,尤其涉及奶面纸的生产方法。
背景技术
奶面纸是属于特种纸,广泛应用于轻工日用品(如玻璃制品、工艺美术制品等)、食品(如蜜饯、巧克力、蛋糕、面包、各种点心衬垫、保鲜速冻食品等)、水果以及药品等包装行业,属于高档商品包装材料。奶面纸具有强度高、透气性好和柔软性高的优点,不仅抗菌保鲜,而且使用后的废纸又能够自然降解。
轻工制品类包装用纸的定量要求是40g/m2以上,如何降低定量要求,生产出一种更薄、透明度更高且强度足够高的奶面纸,已经成为业内亟待解决的问题。
发明内容
本发明就是针对上述的问题,提出一种奶面纸的生产方法,可以生产出定量要求是22g/m2-40g/m2的透明度高、强度高的超薄奶面纸。
本发明的奶面纸的生产方法,包括如下步骤:
a.将商品纸浆碎解处理;
b.进行打浆处理,纸浆的打浆度为80-90°SR,湿重为5.0-6.0g;
c.加入助剂,助剂包括钛白粉50kg/吨浆、CaCO3150kg/吨浆;
d.进行抄造处理,抄造条件是上网浓度0.3%,上网平均纤维长度1.1mm,纸机抄造车速160米/分钟;
e.进行脱水处理和压榨处理;
f.进行干燥处理;
g.在圆筒卷纸机上卷取;
h.放置以均衡水分处理,放置时间是24小时;
i.经湿润机进行湿润处理;
j.送入压光机热压光处理后即成奶面纸。
进一步的,所述的步骤f详细是烘缸温度95°进行干燥处理。
进一步的,所述的步骤i详细是经湿润机进行湿润处理,使湿润后纸页水份达18%-20%。
本发明采用如上技术方案,实现了一种定量要求是22g/m2-40g/m2的透明度高、强度高的超薄奶面纸。
具体实施方式
本发明的奶面纸的生产方法,包括如下步骤:将商品纸将碎解处理;进行打浆处理,加入助剂,进行抄造处理,进行脱水处理和压榨处理,进行干燥处理,在圆筒卷纸机上卷取,放置以均衡水分处理,经湿润机进行湿润处理,送入压光机热压光处理后即成奶面纸。
实施例1:
本发明的优选实施例具体是:将商品纸浆碎解处理→进行打浆处理,纸浆的打浆度为80-90°SR,湿重为5.0-6.0g→加入助剂,助剂包括钛白粉50kg/吨浆、CaCO3150kg/吨浆→进行抄造处理,抄造条件是上网浓度0.3%,上网平均纤维长度1.1mm,纸机抄造车速160米/分钟→进行脱水处理和压榨处理→进行干燥处理,烘缸温度95°→在圆筒卷纸机上卷取→放置以均衡水分处理,放置时间是24小时→经湿润机进行湿润处理,使湿润后纸页水份达18%-20%→送入压光机热压光处理后即成奶面纸。
尽管结合优选实施方案具体展示和介绍了本发明,但所属领域的技术人员应该明白,在不脱离所附权利要求书所限定的本发明的精神和范围内,在形式上和细节上可以对本发明做出各种变化,均为本发明的保护范围。

Claims (3)

1.一种奶面纸的生产方法,其特征是:包括步骤:
a.将商品纸浆碎解处理;
b.进行打浆处理,纸浆的打浆度为80-90°SR,湿重为5.0-6.0g;
c.加入助剂,助剂包括钛白粉50kg/吨浆、CaCO3150kg/吨浆;
d.进行抄造处理,抄造条件是上网浓度0.3%,上网平均纤维长度1.1mm,纸机抄造车速160米/分钟;
e.进行脱水处理和压榨处理;
f.进行干燥处理;
g.在圆筒卷纸机上卷取;
h.放置以均衡水分处理,放置时间是24小时;
i.经湿润机进行湿润处理;
j.送入压光机热压光处理后即成奶面纸。
2.根据权利要求1所述的奶面纸的生产方法,其特征是:所述的步骤f进一步是烘缸温度95°进行干燥处理。
3.根据权利要求1所述的奶面纸的生产方法,其特征是:所述的步骤i进一步是经湿润机进行湿润处理,使湿润后纸页水份达18%-20%。
CN2010102369120A 2010-07-23 2010-07-23 一种奶面纸的生产方法 Active CN101914861B (zh)