CN101875553B CN2010101327031A CN201010132703A CN101875553B CN 101875553 B CN101875553 B CN 101875553B CN 2010101327031 A CN2010101327031 A CN 2010101327031A CN 201010132703 A CN201010132703 A CN 201010132703A CN 101875553 B CN101875553 B CN 101875553B
Authority
CN
China
Prior art keywords
inkpad
attapulgite
alcohol
color
attapulgite clay
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN2010101327031A
Other languages
English (en)
Other versions
CN101875553A (zh
Inventor
许盛英
许庆华
蒋文兰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nantong Sanlian Petrochemical Equipment Manufacture Co Ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2010101327031A priority Critical patent/CN101875553B/zh
Publication of CN101875553A publication Critical patent/CN101875553A/zh
Application granted granted Critical
Publication of CN101875553B publication Critical patent/CN101875553B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Inks, Pencil-Leads, Or Crayons (AREA)

Abstract

本发明公开了一种彩色醇基凹凸棒手印泥及其生产方法,其技术方案的要点是,将高粘凹凸棒石粘土粉和锐钛型钛白粉加入彩色溶液中进行搅拌,搅拌均匀后为混合物,将乙醇稀释液加入混合物中进行搅拌,搅拌均匀后为半成品,将半成品铺平放在框架内,用平整的木板把半成品压平和压光,密封包装为彩色醇基凹凸棒手印泥的成品。打开密封包装的彩色醇基凹凸棒手印泥,将手或脚按压在手印泥上,即可留下清晰的手脚纹理,彩色醇基凹凸棒手印泥具有质地细腻、柔软可塑性好、压制的手印纹理清晰、固化后收缩率小、强度好不变形的特点。调整配料的重量百分比,可以生产各种不同色彩的手印泥,彩色醇基凹凸棒手印泥适用于制作手足印记。

Description

彩色醇基凹凸棒手印泥及其生产方法
技术领域
本发明涉及印泥,具体涉及一种彩色醇基凹凸棒手印泥及其生产方法。
背景技术
用手印泥为宝宝做一份值得珍藏童年记忆,在特别的日子为我们留下一个美好、真实的见证,是手印泥记录我们手足印记的珍贵纪念品,馈赠朋友的最佳礼物。
将取印者的手按压在印泥上,即可留下清晰恒久的美好印记,手印泥固化后应具有真实、立体、坚固不变形、便于永久保存。
目前市场上销售的手印泥,是由石膏粉、香料和色素组成,石膏粉与水混合后凝固速度太快,造成压在手印泥上的手印清晰度较差,强度低耐水性能不好。
发明内容
本发明的目的是克服现有技术中不足之处,提供一种彩色醇基凹凸棒手印泥及其生产方法。
彩色醇基凹凸棒手印泥由高粘凹凸棒石粘土粉、乙醇、锐钛型钛白粉、聚乙酸乙烯酯、棕榈酸异辛酯、苋菜红、胭脂红、柠檬黄、日落黄、靛蓝、亮蓝和去离子水组成。
凹凸棒石粘土在含水的情况下具有较高的可塑性,稳定性好,凹凸棒石粘土的硬度为莫氏2~3度;凹凸棒石粘土潮湿时呈粘性,粘度可达到3000mPa·s以上,凹凸棒石粘土干燥后收缩率小,且不产生龟裂,高粘凹凸棒石粘土粉是采用提高凹凸棒石粘土粘度的加工工艺生产的粉状凹凸棒石粘土。
乙醇是一种易燃、易挥发的无色透明液体,它的水溶液具有特殊的、令人愉快的香味,并略带刺激性,是很好的稀释剂、有机溶剂和消毒剂。
锐钛型钛白粉具有优异的水分散性和卓越的光学性能,色相稳定性,粒度分布好,具有高光泽、高消色力、高遮盖力的特点。
聚乙酸乙烯酯是一种白色粘稠液体或淡黄色细粉或玻璃状块,无臭,透明,韧性强,不溶于水,溶于乙醇,遇光、热不易变色,不易老化,对酸、碱比较稳定。
棕榈酸异辛酯为无色透明油状液体,不溶于水,能与醇和油脂等有机溶剂混溶。对皮肤的亲和性好,具有优越的分散性和铺展性,可有效降低膏体堵塞毛孔的可能性。
苋菜红、胭脂红、柠檬黄、日落黄、靛蓝和亮蓝是人工合成色素,具有色泽鲜艳、着色力强、稳定性好、无臭无味、易溶于水和成本低廉的特点。
本发明通过下述技术方案予以实现:
1、彩色醇基凹凸棒手印泥的配料按重量百分比由下列组分组成:高粘凹凸棒石粘土粉55~75%、乙醇稀释液5~25%、锐钛型钛白粉0.1~10%、苋菜红0.0001~1%、胭脂红0.0001~1%、柠檬黄0.0001~1%、日落黄0.0001~1%、靛蓝0.0001~1%、亮蓝0.0001~1%和去离子水15~25%。
所述乙醇稀释液的配料按重量百分比由下列组分组成:乙醇85~95%、聚乙酸乙烯酯0.1~10%和棕榈酸异辛酯0.1~5%。
2、彩色醇基凹凸棒手印泥的生产方法:(1)先将去离子水加入已经运转的搅拌机内,再加入苋菜红、胭脂红、柠檬黄、日落黄、靛蓝和亮蓝搅拌为彩色溶液;(2)将高粘凹凸棒石粘土粉和锐钛型钛白粉加入彩色溶液中进行搅拌,搅拌均匀后为彩色醇基凹凸棒手印泥的混合物;(3)将乙醇稀释液加入彩色醇基凹凸棒手印泥的混合物中进行搅拌,搅拌均匀后为彩色醇基凹凸棒手印泥的半成品;(4)将彩色醇基凹凸棒手印泥的半成品铺平放在框架内,用平整的木板把彩色醇基凹凸棒手印泥的半成品压平和压光,密封包装为彩色醇基凹凸棒手印泥的成品。
所述框架是一种用于放置和保存彩色醇基凹凸棒手印泥的装饰品。
所述高粘凹凸棒石粘土粉是采用提高凹凸棒石粘土粘度的加工工艺生产的凹凸棒石粘土,其特征在于,从矿区开采的凹凸棒石粘土,需要经过30~120天的自然风化;改性处理方法是:以重量百分比计算,取自然风化后的凹凸棒石粘土94~98%,均匀加入2~6%碳酸钠,共同输入浸泡池中,加入清水进行浸泡陈化,浸泡时间为72~120小时;取浸泡后的凹凸棒石粘土,输入搅拌机中进行搅拌,并将搅拌后的凹凸棒石粘土,经挤压机挤成薄片,其厚度控制在0.5~2毫米,将凹凸棒石粘土薄片,进行晾晒,晾晒后的凹凸棒石粘土薄片,其含水量≤15%;配料以重量百分比计算:晾晒后的凹凸棒石粘土94~98%、高吸水树脂0.5~5%和纤维素0.5~3%,将上述配料进行搅拌,搅拌均匀后输入磨机中进行磨粉,颗粒细度≤0.074毫米。
上述生产工艺是采用由本发明人于2005年6月20日申请的“提高凹凸棒石粘土粘度的加工工艺”,中国专利授权公告号为:CN 1317067C,授权公告日:2007年5月23日。
彩色醇基凹凸棒手印泥的使用方法:打开密封包装的彩色醇基凹凸棒手印泥,将手或脚按压在手印泥上,5秒钟后缓慢离开手印泥,即可留下清晰的手脚纹理,8小时后,彩色醇基凹凸棒手印泥完成了固化过程,有利于永久的保存。
彩色醇基凹凸棒手印泥具有质地细腻、柔软可塑性好、色泽艳丽、压制的手印纹理清晰、固化后收缩率小、强度好不变形、不产生龟裂和耐水性能好的特点。
调整彩色醇基凹凸棒手印泥配料的重量百分比,可以生产各种不同色彩的彩色醇基凹凸棒手印泥。
彩色醇基凹凸棒手印泥适用于制作手足印记。
具体实施方式
下面结合实施例对本发明作进一步的描述:
1、彩色醇基凹凸棒手印泥的配料按重量百分比由下列组分组成:高粘凹凸棒石粘土粉60%、乙醇稀释液18%、锐钛型钛白粉5.5%、苋菜红0.3%、胭脂红0.1996%、柠檬黄0.0001%、日落黄0.0001%、靛蓝0.0001%、亮蓝0.0001%和去离子水16%。
所述乙醇稀释液的配料按重量百分比由下列组分组成:乙醇90%、聚乙酸乙烯酯6%和棕榈酸异辛酯4%。
2、彩色醇基凹凸棒手印泥的生产方法:(1)先将去离子水加入已经运转的搅拌机内,再加入苋菜红、胭脂红、柠檬黄、日落黄、靛蓝和亮蓝;(2)将高粘凹凸棒石粘土粉和锐钛型钛白粉加入已经溶有苋菜红、胭脂红、柠檬黄、日落黄、靛蓝和亮蓝的去离子水中进行搅拌,搅拌均匀后为彩色醇基凹凸棒手印泥的混合物;(3)将乙醇稀释液加入彩色醇基凹凸棒手印泥的混合物中进行搅拌,搅拌均匀后为彩色醇基凹凸棒手印泥的半成品;(4)将彩色醇基凹凸棒手印泥的半成品铺平放在框架内,用平整的木板把彩色醇基凹凸棒手印泥的半成品压平和压光,密封包装为彩色醇基凹凸棒手印泥的成品。
所述框架是一种用于放置和保存彩色醇基凹凸棒手印泥的装饰品。

Claims (1)

1.一种彩色醇基凹凸棒手印泥,其特征在于,彩色醇基凹凸棒手印泥的配料按重量百分比由下列组分组成:高粘凹凸棒石粘土粉55~75%、乙醇稀释液5~25%、锐钛型钛白粉0.1~10%、苋菜红0.0001~1%、胭脂红0.0001~1%、柠檬黄0.0001~1%、日落黄0.0001~1%、靛蓝0.0001~1%、亮蓝0.0001~1%和去离子水15~25%;
所述乙醇稀释液的配料按重量百分比由下列组分组成:乙醇85~95%、聚乙酸乙烯酯0.1~10%和棕榈酸异辛酯0.1~5%;
所述彩色醇基凹凸棒手印泥的生产方法:(1)先将去离子水加入已经运转的搅拌机内,再加入苋菜红、胭脂红、柠檬黄、日落黄、靛蓝和亮蓝搅拌为彩色溶液;(2)将高粘凹凸棒石粘土粉和锐钛型钛白粉加入彩色溶液中进行搅拌,搅拌均匀后为彩色醇基凹凸棒手印泥的混合物;(3)将乙醇稀释液加入彩色醇基凹凸棒手印泥的混合物中进行搅拌,搅拌均匀后为彩色醇基凹凸棒手印泥的半成品;(4)将彩色醇基凹凸棒手印泥的半成品铺平放在框架内,用平整的木板把彩色醇基凹凸棒手印泥的半成品压平和压光,密封包装为彩色醇基凹凸棒手印泥的成品;
所述框架是一种用于放置和保存彩色醇基凹凸棒手印泥的装饰品;
所述高粘凹凸棒石粘土粉是采用提高凹凸棒石粘土粘度的加工工艺生产的凹凸棒石粘土,从矿区开采的凹凸棒石粘土,需要经过30~120天的自然风化;改性处理方法是:以重量百分比计算,取自然风化后的凹凸棒石粘土94~98%,均匀加入2~6%碳酸钠,共同输入浸泡池中,加入清水进行浸泡陈化,浸泡时间为72~120小时;取浸泡后的凹凸棒石粘土,输入搅拌机中进行搅拌,并将搅拌后的凹凸棒石粘土,经挤压机挤成薄片,其厚度控制在0.5~2毫米,将凹凸棒石粘土薄片,进行晾晒,晾晒后的凹凸棒石粘土薄片,其含水量≤15%;配料以重量百分比计算:晾晒后的凹凸棒石粘土94~98%、高吸水树脂0.5~5%和纤维素0.5~3%,将上述配料进行搅拌,搅拌均匀后输入磨机中进行磨粉,颗粒细度≤0.074毫米。
CN2010101327031A 2010-03-26 2010-03-26 彩色醇基凹凸棒手印泥及其生产方法 Active CN101875553B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2010101327031A CN101875553B (zh) 2010-03-26 2010-03-26 彩色醇基凹凸棒手印泥及其生产方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2010101327031A CN101875553B (zh) 2010-03-26 2010-03-26 彩色醇基凹凸棒手印泥及其生产方法

Publications (2)

Publication Number Publication Date
CN101875553A CN101875553A (zh) 2010-11-03
CN101875553B true CN101875553B (zh) 2011-07-20

Family

ID=43018249

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2010101327031A Active CN101875553B (zh) 2010-03-26 2010-03-26 彩色醇基凹凸棒手印泥及其生产方法

Country Status (1)

Country Link
CN (1) CN101875553B (zh)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN112754110A (zh) * 2021-01-25 2021-05-07 江西服装学院 一种印模箱及脚部鞋楦模型构建系统

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1597088A (zh) * 2004-07-17 2005-03-23 兰州理工大学 凹凸棒石粘土脱硫吸附催化剂制备方法
CN1693425A (zh) * 2005-05-19 2005-11-09 许庆华 废柴油的净化方法

Family Cites Families (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6093669A (en) * 1995-11-30 2000-07-25 Oil-Dri Corporation Of America Method for selecting raw material for bleaching clay
NL1020554C2 (nl) * 2002-05-08 2003-11-11 Stichting Energie Werkwijze voor het ontzwavelen van aardgas.
JP2008221126A (ja) * 2007-03-13 2008-09-25 Hokkaido Univ 表面改質珪質頁岩及びこれを用いた水の浄化処理方法

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1597088A (zh) * 2004-07-17 2005-03-23 兰州理工大学 凹凸棒石粘土脱硫吸附催化剂制备方法
CN1693425A (zh) * 2005-05-19 2005-11-09 许庆华 废柴油的净化方法

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
JP特开2008-221126A 2008.09.25

Also Published As

Publication number Publication date
CN101875553A (zh) 2010-11-03

Similar Documents

Publication Publication Date Title
KR100732249B1 (ko) 금 및/또는 은 나노입자를 함유하는 화장료용 안료 조성물
CN101565571B (zh) 速溶水彩颜料及其生产方法
CN105238115A (zh) 水粉颜料及其制备方法
CN101875553B (zh) 彩色醇基凹凸棒手印泥及其生产方法
CN101875550B (zh) 粉状彩色凹凸棒手印泥及其生产方法
CN101875545B (zh) 油性凹凸棒橡皮泥及其生产方法
CN102961312A (zh) 美白防皱滋润面膜
CN101875544B (zh) 醇基凹凸棒手印泥及其生产方法
CN107149562B (zh) 由深到浅变色的粉底预混料、粉底组合物及其制备方法
CN101875546B (zh) 黑色凹凸棒橡皮泥及其生产方法
CN101973732B (zh) 金色凹凸棒软陶泥的生产方法
CN101875552B (zh) 粉状凹凸棒手印泥及其生产方法
CN101973059B (zh) 白色凹凸棒软陶泥的生产方法
CN106336154A (zh) 一种环保型水包沙多彩涂料及其制备方法
JP4826989B2 (ja) 藍入り石けんとその製造方法
KR101128034B1 (ko) 금형에 의한 패턴의 비누 각인에 따른 각인의 충진물과 이를 이용한 비누의 제조방법
CN101973735B (zh) 蓝色凹凸棒软陶泥的生产方法
CN101875540B (zh) 红色凹凸棒橡皮泥及其生产方法
CN1189524C (zh) 花泥画颜料及其制造方法
CN102531510A (zh) 一种高硬度石膏香薰工艺品及其制备方法
CN101973060B (zh) 荧光彩色凹凸棒软陶泥的生产方法
CN101973729A (zh) 红色凹凸棒软陶泥的生产方法
US20040231562A1 (en) Gelled carrier composition for surface colorants and associated methods of use
CN101973733B (zh) 紫色凹凸棒软陶泥的生产方法
CN101973063B (zh) 棕色凹凸棒软陶泥的生产方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
ASS Succession or assignment of patent right

Owner name: JIANGSU BAITENG TECHNOLOGY CO., LTD.

Free format text: FORMER OWNER: XU SHENGYING

Effective date: 20120718

C41 Transfer of patent application or patent right or utility model
COR Change of bibliographic data

Free format text: CORRECT: ADDRESS; FROM: 211700 HUAIAN, JIANGSU PROVINCE TO: 213164 CHANGZHOU, JIANGSU PROVINCE

TR01 Transfer of patent right

Effective date of registration: 20120718

Address after: 213164 building four, block B, building 1, Changzhou science and Education City, Jiangsu

Patentee after: Jiangsu 5ipatent Technology Co.,Ltd.

Address before: 211700 Huaian City, Jiangsu province Xuyi County Xu town Jin Yuan Road No. 22-1 Building 2 room 205

Patentee before: Xu Shengying

ASS Succession or assignment of patent right

Owner name: NANTONG SANLIAN PETROCHEMICAL EQUIPMENT MANUFACTUR

Free format text: FORMER OWNER: JIANGSU BAITENG TECHNOLOGY CO., LTD.

Effective date: 20131121

C41 Transfer of patent application or patent right or utility model
COR Change of bibliographic data

Free format text: CORRECT: ADDRESS; FROM: 213164 CHANGZHOU, JIANGSU PROVINCE TO: 226200 NANTONG, JIANGSU PROVINCE

TR01 Transfer of patent right

Effective date of registration: 20131121

Address after: 226200, Fuyuan Road 1658, Qidong Economic Development Zone, Nantong, Jiangsu

Patentee after: Nantong Sanlian Petrochemical Equipment Manufacture Co., Ltd.

Address before: 213164 building four, block B, building 1, Changzhou science and Education City, Jiangsu

Patentee before: Jiangsu 5ipatent Technology Co.,Ltd.