CN101864212A CN 201010213543 CN201010213543A CN101864212A CN 101864212 A CN101864212 A CN 101864212A CN 201010213543 CN201010213543 CN 201010213543 CN 201010213543 A CN201010213543 A CN 201010213543A CN 101864212 A CN101864212 A CN 101864212A
Authority
CN
China
Prior art keywords
parts
wear
printing
printing ink
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201010213543
Other languages
English (en)
Inventor
马宁一
马羽
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JURONG CITY XINGWEN PACKING CO Ltd
Original Assignee
JURONG CITY XINGWEN PACKING CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JURONG CITY XINGWEN PACKING CO Ltd filed Critical JURONG CITY XINGWEN PACKING CO Ltd
Priority to CN 201010213543 priority Critical patent/CN101864212A/zh
Publication of CN101864212A publication Critical patent/CN101864212A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Laminated Bodies (AREA)
  • Cartons (AREA)
  • Inks, Pencil-Leads, Or Crayons (AREA)

Abstract

本发明公开了一种用于耐磨瓦楞纸箱的印刷油墨,该印刷油墨成分重量配比为:成膜树脂25-35份、水35-45份、蜡15-25%,所述成膜树脂中成分重量配比为:丙烯酰胺和聚氨酯(C3H8N2O)20-25份、水35-45份、腊(CnH2n+2)15-20份、助剂10-20份。所述助剂为双胺C9H15NO2。本发明能提高瓦楞纸箱图文耐磨性能,在长距离运输中,即使箱体堆码间摩擦也不会掉色。

Description

一种用于耐磨瓦楞纸箱的印刷油墨
技术领域
本发明涉及一种瓦楞纸箱,具体地说是一种能提高瓦楞纸箱图文耐磨性能的用于耐磨瓦楞纸箱的印刷油墨。
背景技术
目前对家用电器、精密电子机电产品、食品药品等纸包装产品的质量要求越来越高,普通纸包装箱、木包装、EPS包装因其包装的质量、档次和环保因素已不能适应市场和客户的需求,不符合国家及美日韩、欧盟等国对绿色包装的环保要求。
瓦楞纸箱(彩箱)是目前应用最广泛的工业产品外包装物,可大规模生产,工艺简单,成本低,可回收,无污染,符合国家相关产业政策和绿色环保要求。但是,普通瓦楞纸箱(彩箱)的图文耐磨性主要依靠采用不同的材质来控制和提高,这会直接影响其生产成本。现有瓦楞纸箱印刷用油墨成分主要有成膜树脂25-35%、水35-45%、蜡15-25%等组成,印刷图文耐磨次数在200-400次左右,图文耐磨性能差,在长距离运输中,箱体堆码间摩擦容易掉色;而且在长时间堆放中,也易出现脱墨和掉色现象,影响成品包装的外观和销售。
发明内容
为了克服现有技术存在的问题,本发明的目的是提供一种用于耐磨瓦楞纸箱的印刷油墨,该印刷油墨能提高瓦楞纸箱图文耐磨性能,在长距离运输中,即使箱体堆码间摩擦也不会掉色。
本发明的目的是通过以下技术方案来实现的:
一种用于耐磨瓦楞纸箱的印刷油墨,其特征在于:该印刷油墨成分重量配比为:成膜树脂25-35份、水35-45份、蜡15-25%,所述成膜树脂中成分重量配比为:丙烯酰胺和聚氨酯(C3H8N2O)20-25份、水35-45份、腊(CnH2n+2)15-20份、助剂10-20份,其中,丙烯酰胺和聚氨酯之间的重量配比为:丙烯酰胺1-2份,聚氨酯为1-2份。
本发明所述助剂为双胺C9H15NO2
本发明中印刷油墨成分重量配比优选为:成膜树脂30份、水40份、蜡20份,成膜树脂中成分重量配比为:丙烯酰胺和聚氨酯(C3H8N2O)22份、水30份、腊(CnH2n+2)18份、助剂C9H15NO215份。
本发明改变普通印刷用水性油墨中的成份,并合理调配各种添加剂的成分比例,生产出符合耐磨要求的瓦楞纸箱。在采用了本发明所述的油墨印刷后的纸箱,其箱面之间往返摩擦5000次不脱墨、不掉色,纸箱物理性能和外观质量保持稳定,且生产成本不变。
研究表明:采用本发明所述的印刷油墨生产的纸箱,箱面相向,上层箱面用500g砝码重压,往返摩擦为一次,连续摩擦5000次,箱面印刷图文不脱墨、不掉色,光泽清晰、鲜艳。
与现有技术相比,本发明能提高瓦楞纸箱图文耐磨性能,在长距离运输中,即使箱体堆码间摩擦也不会掉色。
具体实施方式
实施例1
一种本发明所述的用于耐磨瓦楞纸箱的印刷油墨,该印刷油墨成分重量配比为:成膜树脂30份、水40份、蜡20份,成膜树脂中成分重量配比为:丙烯酰胺和聚氨酯(C3H8N2O)22份,其中,丙烯酰胺1份,聚氨酯为1份。水30份、腊(CnH2n+2)18份、助剂15份,助剂为双胺C9H15NO2
采用本发明生产出符合耐磨要求的瓦楞纸箱,其箱面之间往返摩擦5000次不脱墨、不掉色,纸箱物理性能和外观质量保持稳定,且生产成本不变。
实施例2
一种用于耐磨瓦楞纸箱的印刷油墨,其特征在于:该印刷油墨成分重量配比为:成膜树脂25份、水35份、蜡15%,所述成膜树脂中成分重量配比为:丙烯酰胺和聚氨酯(C3H8N2O)20份,其中,丙烯酰胺1份,聚氨酯为2份、水35份、腊(CnH2n+2)15份、助剂10份,助剂为双胺C9H15NO2
研究表明:采用本发明所述的印刷油墨生产的纸箱,箱面相向,上层箱面用500g砝码重压,往返摩擦为一次,连续摩擦5000次,箱面印刷图文不脱墨、不掉色,光泽清晰、鲜艳。
实施例3
一种用于耐磨瓦楞纸箱的印刷油墨,其特征在于:该印刷油墨成分重量配比为:成膜树脂35份、水45份、蜡25%,所述成膜树脂中成分重量配比为:丙烯酰胺和聚氨酯(C3H8N2O)25份,其中,丙烯酰胺2份,聚氨酯为1份、水45份、腊(CnH2n+2)20份、助剂20份,所述助剂为双胺C9H15NO2

Claims (3)

1.一种用于耐磨瓦楞纸箱的印刷油墨,其特征在于:该印刷油墨成分重量配比为:成膜树脂25-35份、水35-45份、蜡15-25%,所述成膜树脂中成分重量配比为:丙烯酰胺和聚氨酯20-25份、水35-45份、腊15-20份、助剂10-20份,其中,丙烯酰胺和聚氨酯之间的重量配比为:丙烯酰胺1-2份,聚氨酯为1-2份。
2.根据权利要求1所述的用于耐磨瓦楞纸箱的印刷油墨,其特征在于:所述助剂为双胺C9H15NO2
3.根据权利要求2所述的用于耐磨瓦楞纸箱的印刷油墨,其特征在于:该印刷油墨成分重量配比为:成膜树脂30份、水40份、蜡20份,成膜树脂中成分重量配比为:丙烯酰胺和聚氨酯(C3H8N2O)22份、水30份、腊(CnH2n+2)18份、双胺C9H15NO215份。
CN 201010213543 2010-06-30 2010-06-30 一种用于耐磨瓦楞纸箱的印刷油墨 Pending CN101864212A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201010213543 CN101864212A (zh) 2010-06-30 2010-06-30 一种用于耐磨瓦楞纸箱的印刷油墨

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201010213543 CN101864212A (zh) 2010-06-30 2010-06-30 一种用于耐磨瓦楞纸箱的印刷油墨

Publications (1)

Publication Number Publication Date
CN101864212A true CN101864212A (zh) 2010-10-20

Family

ID=42956150

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201010213543 Pending CN101864212A (zh) 2010-06-30 2010-06-30 一种用于耐磨瓦楞纸箱的印刷油墨

Country Status (1)

Country Link
CN (1) CN101864212A (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109252423A (zh) * 2018-11-20 2019-01-22 合肥绿普包装材料有限公司 一种提升瓦楞纸箱表面印刷性能的处理方法

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US20060063871A1 (en) * 2004-09-21 2006-03-23 Johnson Polymer, Llc Stabilized water-borne polymer compositions for use as water-based coatings
CN101125977A (zh) * 2006-08-15 2008-02-20 东莞市英科水墨有限公司 一种水性柔版印刷油墨及其制备方法
CN101585904A (zh) * 2008-05-21 2009-11-25 北京高盟燕山科技有限公司 一种水性油墨用连接料树脂的制备方法与应用

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US20060063871A1 (en) * 2004-09-21 2006-03-23 Johnson Polymer, Llc Stabilized water-borne polymer compositions for use as water-based coatings
CN101125977A (zh) * 2006-08-15 2008-02-20 东莞市英科水墨有限公司 一种水性柔版印刷油墨及其制备方法
CN101585904A (zh) * 2008-05-21 2009-11-25 北京高盟燕山科技有限公司 一种水性油墨用连接料树脂的制备方法与应用

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN109252423A (zh) * 2018-11-20 2019-01-22 合肥绿普包装材料有限公司 一种提升瓦楞纸箱表面印刷性能的处理方法
CN109252423B (zh) * 2018-11-20 2019-05-17 东莞龙成纸业有限公司 一种提升瓦楞纸箱表面印刷性能的处理方法

Similar Documents

Publication Publication Date Title
CN101857785A (zh) 一种用于高强耐水瓦楞纸箱的粘合剂
CN101864212A (zh) 一种用于耐磨瓦楞纸箱的印刷油墨
CN204488144U (zh) 一种质轻高阻隔耐刮擦彩色纸铝塑奶粉包装复合结构
CN103540153A (zh) 一种柔性高分子塑料
CN108589402A (zh) 一种木纹包装纸
CN103305056B (zh) 烟标用印刷白卡纸白墨
CN102936438B (zh) 水性油墨式食品日期带
CN206969244U (zh) 一种环保物流包装盒
CN201817747U (zh) 防水牛卡白板纸
CN205631614U (zh) 一种多层环保酒盒包装纸
CN202298347U (zh) 一种涂覆树脂的卡纸
CN206438344U (zh) 一种新型环保装饰纸
CN206034194U (zh) 一种转移镀铝型吸塑纸卡
CN204622739U (zh) 包装膜
CN110528315A (zh) 一种抗水性碳纤维瓦楞纸
CN204399600U (zh) 用于包装机的隔离板
CN202987667U (zh) 一种一纸成型包装盒
CN101481509A (zh) 一种防静电包装材料
CN103526636B (zh) 一种水性高光光油在低品质纸张上的印刷工艺
CN202298362U (zh) 一种涂覆树脂的环保型卡纸
CN201567505U (zh) 双面定位数码防伪纸及包装盒
CN104710873A (zh) 一种丝印油墨
CN106281181A (zh) 一种包装箱用环保胶水
CN105169720A (zh) 一种环保实用玩具
CN205343954U (zh) 一种防水保温秸秆纤维包装材料

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C12 Rejection of a patent application after its publication
RJ01 Rejection of invention patent application after publication

Application publication date: 20101020