CN101779671B - 凹凸棒游泳池杀菌灭藻剂 - Google Patents

凹凸棒游泳池杀菌灭藻剂 Download PDF

Info

Publication number
CN101779671B
CN101779671B CN200910263385XA CN200910263385A CN101779671B CN 101779671 B CN101779671 B CN 101779671B CN 200910263385X A CN200910263385X A CN 200910263385XA CN 200910263385 A CN200910263385 A CN 200910263385A CN 101779671 B CN101779671 B CN 101779671B
Authority
CN
China
Prior art keywords
concave
clay rod
convex clay
attapulgites
swimming pool
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN200910263385XA
Other languages
English (en)
Other versions
CN101779671A (zh
Inventor
许庆华
王傲乾
许盛英
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Qidong Jiangtian Ecological Farm Co Ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN200910263385XA priority Critical patent/CN101779671B/zh
Publication of CN101779671A publication Critical patent/CN101779671A/zh
Application granted granted Critical
Publication of CN101779671B publication Critical patent/CN101779671B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种凹凸棒游泳池杀菌灭藻剂,其技术方案的要点是,凹凸棒游泳池杀菌灭藻剂由高粘凹凸棒石粘土、活性凹凸棒石粘土、硫酸铜、聚合氯化铝、十二烷基二甲基苄基氯化铵和二氧化氯组成。将凹凸棒游泳池杀菌灭藻剂的配料加入搅拌机内进行搅拌,搅拌混合均匀后包装为凹凸棒游泳池杀菌灭藻剂的成品。凹凸棒游泳池杀菌灭藻剂能杀死游泳池水中的病毒、细菌、原生生物、藻类、真菌和各种孢子及孢子形成的菌体;凹凸棒游泳池杀菌灭藻剂不但能杀灭水中的藻类,还能杀死池底与砖缝内的苔藻,去除水中的氨氮、异味和浊度,使游泳池池水清澈、干净,达到国家标准。凹凸棒游泳池杀菌灭藻剂适用于游泳池循环水杀菌灭藻和吸附异味。

Description

凹凸棒游泳池杀菌灭藻剂
技术领域
本发明涉及杀菌灭藻剂,具体涉及一种凹凸棒游泳池杀菌灭藻剂。
背景技术
随着人们的生活水平提高,游泳池及水上娱乐项目得到了迅速的发展。当前人们越来越注重加强自身锻炼和健康娱乐,游泳及水上休闲活动也成为人们的首选项目,游泳池水质卫生和水处理技术也越来越受到人们的普遍重视和关注,游泳池水质的清澈洁净直接关系到人们的健康和安全。
游泳池水质好坏对人群健康影响较大,部分传染病经游泳池水相互传播,如传染性皮肤病、眼结膜炎、肠道传染病和真菌病等,游泳池水质污染时有发生,特别是炎热夏季日益突出;
游泳池水中的尿素来源于人体的分泌物、排泄物,游泳池水中尿素含量偏高,氨氮超标是表明水体受人体排泄物污染的重要指标之一,游泳池水中尿素含量增加和细菌数的增多呈正比例;
绿藻又称青苔,常出现在游泳池的池水、池壁、池底中,导致水质变色混浊,卫生不达标。水的营养化是造成绿藻泛滥的原因。池水中过多的绿藻导致底层的绿藻因阳光被阻隔而无法进行光合作用,进而死亡,变成污泥而衍生出厌氧性细菌,更加速水质恶化,游泳池中长绿藻对管理者而言是最头痛的问题。
发明内容
本发明的目的是克服现有技术中不足之处,提供一种凹凸棒游泳池杀菌灭藻剂。
凹凸棒游泳池杀菌灭藻剂由高粘凹凸棒石粘土、活性凹凸棒石粘土、硫酸铜、聚合氯化铝、十二烷基二甲基苄基氯化铵和二氧化氯组成。
所述高粘凹凸棒石粘土是采用提高凹凸棒石粘土粘度的加工工艺生产的凹凸棒石粘土,凹凸棒石粘土在含水的情况下具有较高的可塑性,在高温和盐水中稳定性好,密度小,凹凸棒石粘土潮湿时呈粘性,其粘度可达到3000mPa·s以上,能加快杀菌灭藻剂絮凝的沉淀速度和提高灭藻的效率。
所述活性凹凸棒石粘土,是用硫酸加入凹凸棒石粘土原矿中进行酸化,再经过高温焙烧为活性凹凸棒石粘土,凹凸棒石粘土酸化改性处理后,具有较好的吸附氨氮、除异味性功能。
硫酸铜水溶液有强力的杀菌灭藻作用,本发明选用粉状硫酸铜。
聚合氯化铝能除菌、除臭、除油、除浊和除重金属盐,絮凝沉淀速度快,适用PH值范围宽,对管道设备无腐蚀性,本发明选用粉状聚合氯化铝。
十二烷基二甲基苄基氯化铵具有广谱、高效的杀菌灭藻能力,能有效地控制水中菌藻繁殖和粘泥生长,并具有良好的粘泥剥离作用和一定的分散、渗透作用,同时具有一定的去油、除臭能力和缓蚀作用,本发明选用粉状十二烷基二甲基苄基氯化铵。
二氧化氯是一种广谱、高效的灭菌剂,能杀死病毒、细菌、原生生物、藻类、真菌和各种孢子及孢子形成的菌体;可杀灭所有细菌繁殖体和许多致病菌、细菌繁殖体、肝炎病毒、噬菌体和细菌芽孢,受温度和氨影响小,本发明选用粉状二氧化氯。
本发明通过下述技术方案予以实现:
1、凹凸棒游泳池杀菌灭藻剂的配料按重量百分比由下列组分组成:高粘凹凸棒石粘土30~55%、活性凹凸棒石粘土15~40%、硫酸铜0.1~15%、聚合氯化铝0.1~12%、十二烷基二甲基苄基氯化铵0.1~10%和二氧化氯0.01~10%。
2、凹凸棒游泳池杀菌灭藻剂的生产方法:将凹凸棒游泳池杀菌灭藻剂的配料加入搅拌机内进行搅拌,搅拌混合均匀后包装为凹凸棒游泳池杀菌灭藻剂的成品。
所述高粘凹凸棒石粘土是采用提高凹凸棒石粘土粘度的加工工艺生产的凹凸棒石粘土,其特征在于,从矿区开采的凹凸棒石粘土,需要经过30~120天的自然风化;改性处理方法是:以重量百分比计算,取自然风化后的凹凸棒石粘土94~98%,均匀加入2~6%碳酸钠,共同输入浸泡池中,加入清水进行浸泡陈化,浸泡时间为72~120小时;取浸泡后的凹凸棒石粘土,输入搅拌机中进行搅拌,并将搅拌后的凹凸棒石粘土,经挤压机挤成薄片,其厚度控制在0.5~2毫米,将凹凸棒石粘土薄片,进行晾晒,晾晒后的凹凸棒石粘土薄片,其含水量≤15%;配料以重量百分比计算:晾晒后的凹凸棒石粘土94~98%、高吸水树脂0.5~5%和纤维素0.5~3%,将上述配料进行搅拌,搅拌均匀后输入磨机中进行磨粉,颗粒细度≤0.074毫米。
上述生产工艺是采用由本发明人于2005年6月20日申请的“提高凹凸棒石粘土粘度的加工工艺”,中国专利授权公告号为:CN 1317067C,授权公告日:2007年5月23日。
所述活性凹凸棒石粘土的生产方法是:①稀硫酸的配制,按重量百分比由下列组分组成:浓度98%的硫酸3~5%,水95~97%;②酸化处理的配料,按重量百分比由下列组分组成:凹凸棒石粘土原矿55~65%,稀硫酸35~45%,将稀硫酸缓慢加入凹凸棒石粘土原矿中进行酸化处理;③挤压:将酸化后的凹凸棒石粘土,通过挤压机进行挤压为片状物,片状物的厚度≤3毫米;④焙烧:凹凸棒石粘土的片状物输送到焙烧炉内进行焙烧,焙烧时间为1.5~3小时,焙烧温度控制在320~450℃,焙烧后的凹凸棒石粘土片状物为活性凹凸棒石粘土半成品;⑤将活性凹凸棒石粘土半成品输入磨机中进行磨粉,颗粒细度≤0.074毫米。
⑤将活性凹凸棒石粘土半成品输入磨机中进行磨粉,颗粒细度≤0.074毫米;
凹凸棒游泳池杀菌灭藻剂能杀死游泳池水中的病毒、细菌、原生生物、藻类、真菌和各种孢子及孢子形成的菌体;可杀灭所有细菌繁殖体和许多致病菌、细菌繁殖体、肝炎病毒、噬菌体和细菌芽孢,具有杀菌消毒有效时间长,杀菌消毒效率高的特点。
凹凸棒游泳池杀菌灭藻剂将会吸附着在藻类的表面,不但能杀灭水中的藻类,还能杀死池底与砖缝内的苔藻,达到快速杀灭藻的效果,死亡的藻类沉淀于池底,再用吸污机以水底吸尘方式排除。
凹凸棒游泳池杀菌灭藻剂可有效去除水中的氨氮、异味和浊度,使游泳池池水清澈、干净,达到国家标准。
凹凸棒游泳池杀菌灭藻剂适用于游泳池循环水杀菌灭藻和吸附异味。
具体实施方式
下面结合实施例对本发明作进一步的描述:
1、凹凸棒游泳池杀菌灭藻剂的配料按重量百分比由下列组分组成:高粘凹凸棒石粘土40%、活性凹凸棒石粘土35%、硫酸铜10%、聚合氯化铝8%、十二烷基二甲基苄基氯化铵4%和二氧化氯3%。
2、凹凸棒游泳池杀菌灭藻剂的生产方法:将凹凸棒游泳池杀菌灭藻剂的配料加入搅拌机内进行搅拌,搅拌混合均匀后包装为凹凸棒游泳池杀菌灭藻剂的成品。
所述高粘凹凸棒石粘土是采用提高凹凸棒石粘土粘度的加工工艺生产的凹凸棒石粘土,其特征在于,从矿区开采的凹凸棒石粘土,需要经过30~120天的自然风化;改性处理方法是:以重量百分比计算,取自然风化后的凹凸棒石粘土97%,均匀加入3%碳酸钠,共同输入浸泡池中,加入清水进行浸泡陈化,浸泡时间为72小时;取浸泡后的凹凸棒石粘土,输入搅拌机中进行搅拌,并将搅拌后的凹凸棒石粘土,经挤压机挤成薄片,其厚度控制在0.5~2毫米,将凹凸棒石粘土薄片,进行晾晒,晾晒后的凹凸棒石粘土薄片,其含水量≤15%;配料以重量百分比计算:晾晒后的凹凸棒石粘土96%、高吸水树脂3%和纤维素1%,将上述配料进行搅拌,搅拌均匀后输入磨机中进行磨粉,颗粒细度≤0.074毫米。
所述活性凹凸棒石粘土的生产方法是:①稀硫酸的配制,按重量百分比由下列组分组成:浓度98%的硫酸3%,水97%;②酸化处理的配料,按重量百分比由下列组分组成:凹凸棒石粘土原矿58%,稀硫酸42%,将稀硫酸缓慢加入凹凸棒石粘土原矿中进行酸化处理;③挤压:将酸化后的凹凸棒石粘土,通过挤压机进行挤压为片状物,片状物的厚度≤3毫米;④焙烧:凹凸棒石粘土的片状物输送到焙烧炉内进行焙烧,焙烧时间为2小时,焙烧温度控制在320~350℃,焙烧后的凹凸棒石粘土片状物为活性凹凸棒石粘土半成品;⑤将活性凹凸棒石粘土半成品输入磨机中进行磨粉,颗粒细度≤0.074毫米。

Claims (1)

1.一种凹凸棒游泳池杀菌灭藻剂,其特征在于,凹凸棒游泳池杀菌灭藻剂的配料按重量百分比由下列组分组成:高粘凹凸棒石粘土30~55%、活性凹凸棒石粘土15~40%、硫酸铜0.1~15%、聚合氯化铝0.1~12%、十二烷基二甲基苄基氯化铵0.1~10%和二氧化氯0.01~10%;
所述高粘凹凸棒石粘土是采用提高凹凸棒石粘土粘度的加工工艺生产的凹凸棒石粘土,从矿区开采的凹凸棒石粘土,需要经过30~120天的自然风化;改性处理方法是:以重量百分比计算,取自然风化后的凹凸棒石粘土94~98%,均匀加入2~6%碳酸钠,共同输入浸泡池中,加入清水进行浸泡陈化,浸泡时间为72~120小时;取浸泡后的凹凸棒石粘土,输入搅拌机中进行搅拌,并将搅拌后的凹凸棒石粘土,经挤压机挤成薄片,其厚度控制在0.5~2毫米,将凹凸棒石粘土薄片,进行晾晒,晾晒后的凹凸棒石粘土薄片,其含水量≤15%;配料以重量百分比计算:晾晒后的凹凸棒石粘土94~98%、高吸水树脂0.5~5%和纤维素0.5~3%,将上述配料进行搅拌,搅拌均匀后输入磨机中进行磨粉,颗粒细度≤0.074毫米;
所述活性凹凸棒石粘土的生产方法是:①稀硫酸的配制,按重量百分比由下列组分组成:浓度98%的硫酸3~5%,水95~97%;②酸化处理的配料,按重量百分比由下列组分组成:凹凸棒石粘土原矿55~65%,稀硫酸35~45%,将稀硫酸缓慢加入凹凸棒石粘土原矿中进行酸化处理;③挤压:将酸化后的凹凸棒石粘土,通过挤压机进行挤压为片状物,片状物的厚度≤3毫米;④焙烧:凹凸棒石粘土的片状物输送到焙烧炉内进行焙烧,焙烧时间为1.5~3小时,焙烧温度控制在320~450℃,焙烧后的凹凸棒石粘土片状物为活性凹凸棒石粘土半成品;⑤将活性凹凸棒石粘土半成品输入磨机中进行磨粉,颗粒细度≤0.074毫米;
所述凹凸棒游泳池杀菌灭藻剂的生产方法:将凹凸棒游泳池杀菌灭藻剂的配料加入搅拌机内进行搅拌,搅拌混合均匀后包装为凹凸棒游泳池杀菌灭藻剂的成品。
CN200910263385XA 2009-12-21 2009-12-21 凹凸棒游泳池杀菌灭藻剂 Active CN101779671B (zh)