CN101775869A - Stereo-shield energy saving insulating brick and preparation method thereof - Google Patents

Stereo-shield energy saving insulating brick and preparation method thereof Download PDF

Info

Publication number
CN101775869A
CN101775869A CN200910265845A CN200910265845A CN101775869A CN 101775869 A CN101775869 A CN 101775869A CN 200910265845 A CN200910265845 A CN 200910265845A CN 200910265845 A CN200910265845 A CN 200910265845A CN 101775869 A CN101775869 A CN 101775869A
Authority
CN
China
Prior art keywords
energy saving
stereo
insulating brick
weight portion
saving insulating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN200910265845A
Other languages
Chinese (zh)
Other versions
CN101775869B (en
Inventor
朱国春
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhu Guochun
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2009102658452A priority Critical patent/CN101775869B/en
Publication of CN101775869A publication Critical patent/CN101775869A/en
Application granted granted Critical
Publication of CN101775869B publication Critical patent/CN101775869B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention relates to a stereo-shield energy saving insulating brick and a preparation method thereof. The stereo-shield energy saving insulating brick has the functions of energy saving, light weight, environmental protection and sound insulation. The slurry materials of the stereo-shield energy saving insulating brick comprise the following components in parts by weight: 0.6 to 0.8 part of cement, 1.5 to 2.0 parts of gravel, 1.0 to 1.5 parts of sand, 0.3 to 0.6 part of pulverized fuel ash, 0.5 to 2.0 parts of slag, 0.3 to 0.6 parts of building rubbish, 0.01 to 0.025 part of EPS granule, and the balance of water. The stereo-shield energy saving insulating brick has the advantages of food sound insulation effect, high bearing strength, good heat insulation and heat preservation effect and low manufacturing cost.

Description

Stereo-shield energy saving insulating brick and preparation method
Technical field
The present invention relates to a kind of stereo-shield energy saving insulating brick and preparation method, belong to brick and make the field with energy-conservation, lightweight, environmental protection, sound insulation function.
Background technology
Notice of authorization CN title " concrete bearing insulating brick ", the concrete mixed material that this brick is made up of cement, water, sand and aggregate chips adds foam grain and the water reducing agent mixing is formed, and its weight proportion is as follows: cement 1 weight portion, water 0.16-0.55 weight portion, sand 0-1.5 weight portion, aggregate chips 1.5-6 weight portion, foam grain 0.002-0.06 weight portion, water reducing agent 0-0.03 weight portion.Its weak point: the one, soundproof effect is not good; The 2nd, load bearing stength is low; The 3rd, heat insulation and preservation effect is not good.
Summary of the invention
Purpose of design: avoid the weak point in the background technology, design a kind of stereo-shield energy saving insulating brick and preparation method with energy-conservation, lightweight, environmental protection, sound insulation function.
Design scheme: in order to realize above-mentioned purpose of design.1, the EPS particle adopts the design of 0.01~0.025 weight portion, is one of technical characterictic of the present invention.The purpose of doing like this is: eps foam is a kind of thermoplastic, through after the foamable, every cubic metre of volume contains ten thousand independent closed bubbles of 300--600, the contain air volume is more than 98%, and the thermal conductivity of air is very little and be closed in the foam and can not convection current, so EPS is the very superior material of a kind of heat preservation and insulation.The present invention utilizes this characteristic of EPS just, makes made stereo-shield energy saving insulating brick have good heat-insulation and heat-preservation and sound insulation function.2, slag adopts the design of 0.5~1.0 weight portion, is two of technical characterictic of the present invention.The purpose of doing like this is: slag claims molten slag again.The melt that floats over liquid surfaces such as metal that generates in the pyrometallurgical processes, it is formed based on oxide, also often contains sulfide and carries little metal secretly.The component of slag is adjusted by adding an amount of flux (lime, quartz, fluorite etc.).Its blast furnace slag can be made cement raw material, and the present invention utilizes this characteristic just, and the composition of slag as stereo-shield energy saving insulating brick constituted, and improves the load bearing stength of stereo-shield energy saving insulating brick.3, flyash adopts the design of 0.3~0.6 weight portion, is three of technical characterictic of the present invention.The purpose of doing like this is: the one, and the main oxides of the chemical compound power plants flyash of flyash consists of: SiO2, AL2O3, FeO, Fe2O3, CaO, TiO2, MgO, K2O, Na2O, SO3, MnO etc. also have P2O5 etc. in addition.Wherein silica, titanium oxide be from clay, the rock page or leaf; Iron oxide is mainly from pyrite; Magnesia and calcium oxide are from its corresponding carbonate and sulfate; The 2nd, because flyash is a kind of artificial pozzolana mixed material, itself slightly or do not have a hydraulic gelling property, but when existing with powdery and water, can be at normal temperature, particularly under hydrothermal treatment consists (stream curing) condition, with calcium hydroxide or other alkaline earth metal hydroxide generation chemical reactions, generate compound with hydraulic gelling property, become a kind of gaining in strength and the material of durability; The 3rd, adding coal ash in concrete, a large amount of cement and fines have promptly been saved, reduced water supply volume again, improved the workability of concrete mix, strengthened concrete pumpability simultaneously, and reduced concrete creep, the reduce heat of hydration, heat energy dilatancy, improve concrete impervious ability and increase concrete ground modification property.4, building waste adopts the design of 0.3~0.6 weight portion, is four of technical characterictic of the present invention.The purpose of doing like this is: building waste mostly is solid waste greatly, generally produces in process of construction or in the old building maintenance, demolishing process.Its mainly by soil, dregs, the mortar that is scattered and concrete, pick concrete pile crown that masonry that cutter produces and broken concrete, piling cuts down and other discarded object etc. and form; utilize discarded building concrete and discarded masonry, useless brick and tile to produce coarse-fine aggregate; can be used for the building block of production respective strengths grade, have advantage such as realize building waste minimizing, resource, saving natural resources, preserve the ecological environment.
Technical scheme 1: stereo-shield energy saving insulating brick, constitute the stereo-shield energy saving insulating brick slurry by cement, stone, building waste, sand, flyash, slag, EPS particle and water, its heavy reason proportioning is as follows: cement 0.6~0.8 weight portion, stone 1.5~2.0 weight portions, sand 1.0~1.5 weight portions, flyash 0.3~0.6 weight portion, slag 0.5~1.0 weight portion, building waste 0.3~0.6 weight portion, EPS particle 0.01~0.025 weight portion, remainder is a water.
Technical scheme 2: the preparation method of stereo-shield energy saving insulating brick, (1) gets cement, stone, building waste, sand, flyash, slag, EPS particle by the proportioning weighing balance, and the error in dipping of each prong material is no more than 2%; (2) batching earlier stone, building waste, sand, slag are poured into the mixer hopper wetting after, then cement, flyash, EPS particle are poured successively into the mixer hopper and are added entry while stirring and stir into and mix slurry; (3) slurry is delivered to brick equipment, the brick machine is pressed into six round bricks of specification, promptly gets stereo-shield energy saving insulating brick after the natural curing.
The present invention compares with background technology, and the one, soundproof effect is good; The 2nd, the load bearing stength height; The 3rd, heat insulation and preservation effect is good; The 4th, low cost of manufacture.
The specific embodiment
Embodiment 1: stereo-shield energy saving insulating brick, constitute the stereo-shield energy saving insulating brick slurry by cement, stone, sand, flyash, slag, building waste, EPS particle and water, its weight proportion is as follows: cement 0.6~0.8 weight portion, stone 1.5~2.0 weight portions, sand 1.0~1.5 weight portions, flyash 0.3~0.6 weight portion, slag 0.5~1.0 weight portion, building waste 0.3~0.6 weight portion, EPS particle 0.01~0.025 weight portion, remainder is a water.Described EPS particle grain size is less than 0.5mm.
Embodiment 2: on the basis of embodiment 1, and cement 0.6 weight portion, stone 1.5 weight portions, sand 1.0 weight portions, flyash 0.3 weight portion, slag 0.5 weight portion, building waste 0.3 weight portion, EPS particle 0.01 weight portion, remainder is a water.
Embodiment 3: on the basis of embodiment 1, and cement 0.8 weight portion, stone 2.0 weight portions, sand 1.5 weight portions, flyash 0.6 weight portion, slag 1.0 weight portions, building waste 0.6 weight portion, EPS particle 0.025 weight portion, remainder is a water.
Embodiment 4: on the basis of embodiment 1, and cement 0.7 weight portion, stone 1.75 weight portions, sand 1.25 weight portions, flyash 0.45 weight portion, slag 0.75 weight portion, building waste 0.45 weight portion, EPS particle 0.0175 weight portion, remainder is a water.
Embodiment 5: on the basis of embodiment 1, the preparation method of stereo-shield energy saving insulating brick is characterized in that: (1) gets cement, stone, sand, flyash, slag, building waste, EPS particle by the proportioning weighing balance, and the error in dipping of each prong material is no more than 2%; (2) batching earlier stone, building waste, sand, slag are poured into the mixer hopper wetting after, then cement, flyash, EPS particle are poured successively into the mixer hopper and are added entry while stirring and stir into and mix slurry; (3) slurry is delivered to brick equipment, the brick machine is pressed into six round bricks of specification 240 * 240 * 90, promptly gets stereo-shield energy saving insulating brick after the natural curing.
What need understand is: though the foregoing description is to the present invention's detailed text description of contrasting; but these text descriptions; it is simple description to mentality of designing of the present invention; rather than to the restriction of mentality of designing of the present invention; any combination, increase or modification that is no more than mentality of designing of the present invention all falls within the scope of protection of the present invention.

Claims (3)

1. stereo-shield energy saving insulating brick, it is characterized in that constituting the stereo-shield energy saving insulating brick slurry by cement, stone, sand, flyash, slag, EPS particle and water, its weight proportion is as follows: cement 0.6~0.8 weight portion, stone 1.5~2.0 weight portions, sand 1.0~1.5 weight portions, flyash 0.3~0.6 weight portion, slag 0.5~1.0 weight portion, building waste 0.3~0.6 weight portion, EPS particle 0.01~0.025 weight portion, remainder is a water.
2. stereo-shield energy saving insulating brick according to claim 1 is characterized in that: the EPS particle grain size is less than 0.5mm.
3. the preparation method of stereo-shield energy saving insulating brick according to claim 1, it is characterized in that: (1) gets cement, stone, sand, flyash, slag, building waste, EPS particle by the proportioning weighing balance, and the error in dipping of each prong material is no more than 2%; (2) batching earlier stone, sand, slag, building waste are poured into the mixer hopper wetting after, then cement, flyash, EPS particle are poured successively into the mixer hopper and are added entry while stirring and stir into and mix slurry; (3) slurry is delivered to brick equipment, the brick machine is pressed into six round bricks of specification, promptly gets stereo-shield energy saving insulating brick after the natural curing.
CN2009102658452A 2009-12-29 2009-12-29 Stereo-shield energy saving insulating brick and preparation method thereof Expired - Fee Related CN101775869B (en)