CN101708988B CN2009102303949A CN200910230394A CN101708988B CN 101708988 B CN101708988 B CN 101708988B CN 2009102303949 A CN2009102303949 A CN 2009102303949A CN 200910230394 A CN200910230394 A CN 200910230394A CN 101708988 B CN101708988 B CN 101708988B
Authority
CN
China
Prior art keywords
orders
conductive powder
cement
ceramic tile
static ceramic
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN2009102303949A
Other languages
English (en)
Other versions
CN101708988A (zh
Inventor
袁国梁
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shandong Electric Shield Polytron Technologies Inc
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2009102303949A priority Critical patent/CN101708988B/zh
Publication of CN101708988A publication Critical patent/CN101708988A/zh
Application granted granted Critical
Publication of CN101708988B publication Critical patent/CN101708988B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Road Paving Structures (AREA)

Abstract

一种防静电陶瓷砖用复合导电粉,其特征在于按照重量百分数计,由方解石60%-95%,硼砂2%-20%和三氧化二铝含量≥98%的氧化铝1%-20%混合而成。其静电导电性能稳定,易施工,成本低。

Description

防静电陶瓷砖铺贴用复合导电粉
技术领域
本发明属于建筑材料的技术领域,具体涉及一种铺贴防静电陶瓷砖的复合导电粉。
背景技术
静电现象在信息产业、纺织工业、石油化工、塑料和橡胶工业、油漆工业等的生产、加工和使用过程中最非常普遍的。静电电荷的积聚将可能造成很大的危害,如静电放电时产生的电磁波可能干扰精密电子仪器的工作,甚至造成自动化电子设备的误动作;在医药上引尘、引菌;医疗手术上引起电颤事故;矿山、石油化工上引起火灾、爆炸;在电子工业上引起集成电路破坏;在纺织上引起纤维聚集等等。在防静电的建筑材料中,目前研究与应用最多的是聚合物防静电涂料和地面材料,这些材料是在聚合物中添加金属和碳黑等导电物质制成的,如环氧合三聚氰胺防静电涂料、地板等。近几年这类材料虽在抗老化、抗污、耐磨等方面有所改进,但难以解决耐久性和防火性能欠佳等问题。
目前防静电陶瓷砖已经被各行业广泛应用,但是按照以前使用铁丝网或铜带施工比较复杂,成本高。并且时间久了易氧化,很难保证体积电阻的稳定性。如果用一种复合粉体混合在施工时的水泥里面,能达到预期的效果就解决了以上问题。
发明内容
本发明所要解决的技术问题是提供一种防静电陶瓷砖用复合导电粉,静电导电性能稳定永久不变,易施工,成本低。
本发明一种防静电陶瓷砖用复合导电粉,其特征在于按照重量百分数计,由方解石60%-95%,硼砂2%-20%和三氧化二铝含量为≥98%的氧化铝1%-20%混合而成。
其制备方法可按照以下方式制造:
第一步:将粒度为80目~120目的方解石和粒度为80目~120目不低于工业纯的硼砂用V型混料机充分混合均匀;
第二步:将粒度为150目~200目,三氧化二铝质量含量为≥98%的氧化铝和第一步混合好的基体用V型混料机充分混合均匀,即获得防静电陶瓷砖用复合导电粉。
本发明所制备的防静电陶瓷砖用复合导电粉,材料体积电阻为105Ω-109Ω。其制造工艺先进合理,施工简单、实用,性能稳定。
本发明的导电粉使用方法为:
1、湿铺
将一定比例的导电粉掺入水泥和沙子中搅拌均匀后加水,搅拌均匀铺贴。导电粉∶水泥∶沙子=1.2~3.4∶100∶200~250(重量比),水泥标号为325,沙子为小颗粒的细沙。
2、干铺
先铺找平层,将导电粉按一定比例掺入水泥和沙子中搅拌均匀后加水,均匀铺好找平层。导电粉∶水泥∶沙子=1.2~3.4∶100∶200~250(重量比),水泥标号为325,沙子为小颗粒的细沙。
铺砖时在砖背面抹找的水泥膏制作时应将导电粉加入水泥中干拌均匀后加水搅拌(导电粉∶水泥=1.2~3.4∶100,同标号水泥)。
本发明与现有技术相比,具有如下优点和效果:
1、所制造的防静电陶瓷砖用复合导电粉,其静电导电性能稳定。
2、比用铁丝网、铜带为导体材料连接的施工方案要简单、易施工,成本低。
3、对生产技术和生产环境的要求相对较低易于生产。
具体实施方式
以下结合实施例来说明,以下实施例的百分数未作特别说明均指质量百分数:
实施例1:
1、筛选:将方解石、硼砂分别用80目筛网筛选备用;氧化铝用150目筛网筛选备用。
2、混料:80%的方解石、2%的硼砂和12%的氧化铝一起放入混料机中充分混合均匀。
经电性能检测,产品体积电阻率为3.6×107Ω。该产品可用作防静电陶瓷砖铺贴施工用的复合导电粉。
实施例2:
1、筛选:将方解石、硼砂分别用100目筛网筛选备用;氧化铝用200目筛网筛选备用。
2、混料:65%的方解石、15%的硼砂和20%的氧化铝一起放入混料机中充分混合均匀。
经电性能检测,产品体积电阻率为6.0×107Ω。该产品可用作防静电陶瓷砖铺贴施工用的复合导电粉。
实施例3:
1、筛选:将方解石、硼砂分别用80目筛网筛选备用;氧化铝用150目筛网筛选备用。
2、混料:90%的方解石、8%的硼砂和2%的氧化铝一起放入混料机中充分混合均匀。
经电性能检测,产品体积电阻率为1.7×107Ω。该产品可用作防静电陶瓷砖铺贴施工用的复合导电粉。
实施例4:
将水泥(325号,下同)∶实施例1制备的防静电陶瓷砖用复合导电粉按照97.5∶2.5的质量比混合即获得导电水泥。
将导电水泥∶沙∶水按照1∶2.5∶0.4的质量比充分混合均匀预铺在地面,厚3厘米。
将3厘米的混合料铺平后,再将导电水泥∶水按照100∶35的质量比制成水泥浆,涂在砖的背面3至4毫米,平稳的铺在铺平的混合料上即可。
经电性能检测,施工体积电阻率为2.6×108Ω。
实施例5:
将水泥∶实施例1制备的防静电陶瓷砖用复合导电粉按照97∶3的质量比混合即获得导电水泥。
将导电水泥∶沙∶水按照1∶2.5∶0.4的质量比充分混合均匀预铺在地面,厚3厘米。
将3厘米的混合料铺平后,再将导电水泥∶水按照100∶35的质量比制成水泥浆,涂在砖的背面3至4毫米,平稳的铺在铺平的混合料上即可。
经电性能检测,施工体积电阻率为6.1×107Ω。
实施例6:
将水泥∶实施例2制备的防静电陶瓷砖用复合导电粉按照97∶3的质量比混合即获得导电水泥。
将导电水泥∶沙∶水按照1∶2.5∶0.4的质量比充分混合均匀预铺在地面,厚3厘米。
将3厘米的混合料铺平后,再将导电水泥∶水按照100∶35的质量比制成水泥浆,涂在砖的背面3至4毫米,平稳的铺在铺平的混合料上即可。
经电性能检测,施工体积电阻率为2.3×107Ω。
实施例7:
将水泥∶实施例3制备的防静电陶瓷砖用复合导电粉按照97.5∶2.5的质量比混合即获得导电水泥。
将导电水泥∶沙∶水按照1∶2.5∶0.4的质量比充分混合均匀预铺在地面,厚3厘米。
将3厘米的混合料铺平后,再将导电水泥∶水按照100∶35的质量比制成水泥浆,涂在砖的背面3至4毫米,平稳的铺在铺平的混合料上即可。
经电性能检测,施工体积电阻率为5.8×107Ω。

Claims (5)

1.一种复合导电粉在防静电陶瓷砖生产中的应用,其特征在于:复合粉体由60%-95wt%方解石,硼砂2%-20wt%和含量为98%的氧化铝1%-20wt%组成,方解石粒度为80目-120目,硼砂为80目-120目,氧化铝为150目-200目,将复合粉体与水泥和沙子干混后再加入水制成水泥浆料,用于陶瓷砖铺贴。
2.根据权利要求书1所述的复合导电粉在防静电陶瓷砖生产中的应用,其特征在于:复合导电粉与水泥、沙子用量重量比例为:导电粉:水泥:沙子=1.2-3.4:100:200-250。
3.根据权利要求书1所述的复合导电粉在防静电陶瓷砖生产中的应用,其特征在于:方解石粒度为80目,硼砂粒度为80目,氧化铝粒度为150目。
4.根据权利要求1所述的复合导电粉在防静电陶瓷砖生产中的应用,其特征在于:方解石粒度为100目,硼砂粒度为100目,氧化铝粒度为200目。
5.一种添加有权利要求1所述的复合导电粉的水泥浆,其特征在于:导电粉、水泥和沙子的用量重量比例为导电粉:水泥:沙子=1.2-3.4:100:200-250。
CN2009102303949A 2009-11-24 2009-11-24 防静电陶瓷砖铺贴用复合导电粉 Active CN101708988B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2009102303949A CN101708988B (zh) 2009-11-24 2009-11-24 防静电陶瓷砖铺贴用复合导电粉

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2009102303949A CN101708988B (zh) 2009-11-24 2009-11-24 防静电陶瓷砖铺贴用复合导电粉

Publications (2)

Publication Number Publication Date
CN101708988A CN101708988A (zh) 2010-05-19
CN101708988B true CN101708988B (zh) 2011-09-14

Family

ID=42401800

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2009102303949A Active CN101708988B (zh) 2009-11-24 2009-11-24 防静电陶瓷砖铺贴用复合导电粉

Country Status (1)

Country Link
CN (1) CN101708988B (zh)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102795799B (zh) * 2012-09-10 2013-11-06 山东电盾科技有限公司 防静电水泥用防静电粉、制备方法及其应用方法
CN105924133A (zh) * 2016-04-25 2016-09-07 山东电盾科技有限公司 防静电陶瓷砖及其制备方法
CN109181391B (zh) * 2018-09-20 2021-04-09 杭州电盾装饰材料有限公司 无机复合导电粉及其制备方法和应用

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101042013A (zh) * 2007-04-21 2007-09-26 淄博统一陶瓷有限公司 防静电复古生态砖
CN101463645A (zh) * 2008-12-05 2009-06-24 北京工业大学 一种抗静电瓷砖及其制造方法
CN101475364A (zh) * 2009-02-02 2009-07-08 山东瓦伦蒂诺陶瓷有限公司 防静电陶瓷砖用防静电粉

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101042013A (zh) * 2007-04-21 2007-09-26 淄博统一陶瓷有限公司 防静电复古生态砖
CN101463645A (zh) * 2008-12-05 2009-06-24 北京工业大学 一种抗静电瓷砖及其制造方法
CN101475364A (zh) * 2009-02-02 2009-07-08 山东瓦伦蒂诺陶瓷有限公司 防静电陶瓷砖用防静电粉

Also Published As

Publication number Publication date
CN101708988A (zh) 2010-05-19

Similar Documents

Publication Publication Date Title
CN105810294B (zh) 一种水性导电银浆及其制备方法
CN105976893A (zh) 无铅石墨烯/纳米银复合电子银浆及其制备方法
CN108091839A (zh) 一种锂硫电池正极浆料的制备方法
CN109841834A (zh) 一种复合导电剂、其制备方法及在正极浆料的应用
CN103275552A (zh) 一种碳系电热油墨及其制备方法
CN102277109B (zh) 一种环保型光固化导电银胶的制备方法
CN101708988B (zh) 防静电陶瓷砖铺贴用复合导电粉
CN108305704A (zh) 一种石墨烯基高导电碳浆及其制备方法
CN103740252A (zh) 一种抗静电聚氨酯水性涂料及其制备方法
CN108711625A (zh) 一种用于锂离子电池正极材料的石墨烯复合导电剂的制备方法
CN1552657A (zh) 复相导电基元混凝土
CN101085845A (zh) 一种导电纤维母粒及其制备方法
CN100348682C (zh) 一种抗静电涂料及其制备方法
CN101514281A (zh) 一种封装led的导电银胶及其制备方法
Chi et al. Effects of magnetic field treatment on dielectric properties of CCTO@ Ni/PVDF composite with low concentration of ceramic fillers
CN102262915B (zh) 一种基于大功率led 芯片贴装用环保型银导体浆料及其制备方法
CN105255330B (zh) 一种碳纤维热固性粉末电磁屏蔽涂料的制备方法
CN106830691A (zh) 一种石墨烯掺杂型电子浆料用玻璃粉及其制备方法
CN105199564A (zh) 一种热固性粉末电磁屏蔽涂料
CN104310907A (zh) 一种电磁屏蔽抹面砂浆及其制备方法
KR20160044356A (ko) 전도성 페이스트의 제조방법 및 이로부터 제조된 전도성 페이스트
CN106128554A (zh) 一种抗老化晶硅太阳能电池背电极银浆
CN105199563A (zh) 一种热固性粉末电磁屏蔽涂料
CN109574601A (zh) 一种建筑石墨混凝土及其制备方法
CN105219210A (zh) 一种纳米防腐导电涂料

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
ASS Succession or assignment of patent right

Owner name: TAN AILI

Free format text: FORMER OWNER: YUAN GUOLIANG

Effective date: 20110829

C41 Transfer of patent application or patent right or utility model
C53 Correction of patent of invention or patent application
CB03 Change of inventor or designer information

Inventor after: Tan Aili

Inventor after: Yuan Guoliang

Inventor before: Yuan Guoliang

COR Change of bibliographic data

Free format text: CORRECT: INVENTOR; FROM: YUAN GUOLIANG TO: TAN AILI YUAN GUOLIANG

TA01 Transfer of patent application right

Effective date of registration: 20110829

Address after: 255100 3-2-201, Geng Jia village, Zichuan District, Shandong, Zibo

Applicant after: Tan Aili

Address before: Yang Zhai Ceramic Industrial Park Zichuan District 255100 Shandong city of Zibo province Zibo Tongyi Ceramics Co. Ltd

Applicant before: Yuan Guoliang

ASS Succession or assignment of patent right

Owner name: SHANDONG DIANDUN TECHNOLOGY CO., LTD.

Free format text: FORMER OWNER: TAN AILI

Effective date: 20120328

C41 Transfer of patent application or patent right or utility model
COR Change of bibliographic data

Free format text: CORRECT: ADDRESS; FROM: 255100 ZIBO, SHANDONG PROVINCE TO: 255185 ZIBO, SHANDONG PROVINCE

TR01 Transfer of patent right

Effective date of registration: 20120328

Address after: 255185 Shandong Province, Zibo city Zichuan District Ceramic Industrial Park

Patentee after: Shandong Diandun Technology Co.,Ltd.

Address before: 255100 3-2-201, Geng Jia village, Zichuan District, Shandong, Zibo

Patentee before: Tan Aili

C56 Change in the name or address of the patentee
CP01 Change in the name or title of a patent holder

Address after: 255185 Shandong Province, Zibo city Zichuan District Ceramic Industrial Park

Patentee after: SHANDONG ELECTRIC SHIELD POLYTRON TECHNOLOGIES Inc.

Address before: 255185 Shandong Province, Zibo city Zichuan District Ceramic Industrial Park

Patentee before: Shandong Diandun Technology Co.,Ltd.

PE01 Entry into force of the registration of the contract for pledge of patent right
PE01 Entry into force of the registration of the contract for pledge of patent right

Denomination of invention: Compound conductive powder for anti-static ceramic tile

Effective date of registration: 20200107

Granted publication date: 20110914

Pledgee: Zibo Zichuan District sub branch of China Post Savings Bank Co.,Ltd.

Pledgor: SHANDONG ELECTRIC SHIELD POLYTRON TECHNOLOGIES Inc.

Registration number: Y2020990000023

PC01 Cancellation of the registration of the contract for pledge of patent right
PC01 Cancellation of the registration of the contract for pledge of patent right

Date of cancellation: 20210716

Granted publication date: 20110914

Pledgee: Zibo Zichuan District sub branch of China Post Savings Bank Co.,Ltd.

Pledgor: SHANDONG ELECTRIC SHIELD POLYTRON TECHNOLOGIES Inc.

Registration number: Y2020990000023

PE01 Entry into force of the registration of the contract for pledge of patent right
PE01 Entry into force of the registration of the contract for pledge of patent right

Denomination of invention: Composite conductive powder for anti-static ceramic tile paving

Effective date of registration: 20211125

Granted publication date: 20110914

Pledgee: Zibo Zichuan District sub branch of China Post Savings Bank Co.,Ltd.

Pledgor: SHANDONG ELECTRIC SHIELD POLYTRON TECHNOLOGIES Inc.

Registration number: Y2021980013248

PC01 Cancellation of the registration of the contract for pledge of patent right

Date of cancellation: 20230711

Granted publication date: 20110914

Pledgee: Zibo Zichuan District sub branch of China Post Savings Bank Co.,Ltd.

Pledgor: SHANDONG ELECTRIC SHIELD POLYTRON TECHNOLOGIES Inc.

Registration number: Y2021980013248

PC01 Cancellation of the registration of the contract for pledge of patent right