CN101614078A - 从凝固的混凝土中取出钢管的方法 - Google Patents
从凝固的混凝土中取出钢管的方法 Download PDFInfo
- Publication number
- CN101614078A CN101614078A CN200810048201A CN200810048201A CN101614078A CN 101614078 A CN101614078 A CN 101614078A CN 200810048201 A CN200810048201 A CN 200810048201A CN 200810048201 A CN200810048201 A CN 200810048201A CN 101614078 A CN101614078 A CN 101614078A
- Authority
- CN
- China
- Prior art keywords
- steel pipe
- heating wire
- concrete
- solidifies
- melted
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
从凝固的混凝土中取出钢管的方法,是在混凝土浇筑之前,将钢管可能被混凝土浇筑的部位,包裹上在常温情况下是固体,超过一定温度时被融化的材料,再将电热丝缠绕在上面,在电热丝外再包裹上常温情况下是固体,超过一定温度被融化的材料,使电热丝夹在这种材料的中间。当混凝土浇筑完毕后,钢管需要拆除时,在电热丝两端连接上电源,电热丝升温,夹在电热丝内外的材料迅速融化,混凝土与钢管之间便有了一定的间隙,钢管就能方便地从混凝土中取出。
Description
技术领域:
本发明属于建筑施工领域,具体涉及一种从凝固的混凝土中取出钢管的方法。
背景技术:
在建筑行业中,钢管起着支撑架结构的作用。混凝土浇筑完毕,到施工后期。脚手架、钢管需要拆除。但有些钢管被埋在混凝土中,无法取出。外露部位只得被割除,而割下来的钢管因太短也不能再利用,因而造成极大的浪费。
发明内容:
本发明的目的在于针对现有技术的缺陷,提供一种可以从凝固的混凝土中取出钢管的方法。使钢管在建筑施工领域的利用率大大的提高,减少浪费,降低施工成本。
本发明的技术方案如下:在混凝土浇筑之前,将钢管可能被混凝土浇筑的部位,包裹上在常温情况下是固体,超过一定温度时被融化的材料,再将电热丝缠绕在上面,在电热丝外再包裹上常温情况下是固体,超过一定温度被融化的材料,使电热丝夹在这种材料的中间。当混凝土浇筑完毕,到施工后期,钢管需要拆除时,在电热丝两端连接上电源,电热丝升温,夹在电热丝内外的材料迅速融化,混凝土与钢管之间便有了一定的间隙,钢管就能方便地从混凝土中取出。
本发明可将常温情况下是固体,超过一定温度时被融化的材料选择用塑料布来包裹钢管和电热丝。也可以选择在常温情况下是固体,到150度以下时被融化的材料包裹钢管和电热丝。
附图说明
图1从凝固的混凝土中取出钢管方法的示意图;
其中:1钢管、2包裹钢管的塑料布、3电热丝、4包裹电热丝的塑料布、5混凝土。
具体实施方式:本发明根据施工的地理位置和季节环境温度的变化,包裹钢管的塑料布的厚度为0.9-9毫米,包裹电热丝上塑料布的厚度同样为0.9-9毫米。
下面参照附图详述本发明。
参照附图,钢管1外径上被混凝土浇筑的部位包有包裹钢管的塑料布2,电热丝3缠绕在包裹钢管的塑料布2上面。电热丝3外再包上包裹电热丝的塑料布4,电热丝3被紧紧包裹在中间,外面才是混凝土5。
为了施工安全防止电热丝烧断或漏电,电热丝3的外径上包有绝缘层,电热丝3通电时的温度可选择在150度以下。
该方法使钢管在建筑施工领域的利用率大大的提高,减少浪费,降低施工成本。
Claims (6)
1、从凝固的混凝土中取出钢管的方法,其特征在于将钢管(1)可能被混凝土浇筑的部位,包裹上在常温情况下是固体,超过一定温度时被融化的材料,再将电热丝(3)缠绕在上面,在电热丝外再包裹上常温情况下是固体,超过一定温度被融化的材料,使电热丝(3)夹在这种材料的中间。
2、根据权利要求1所述从凝固的混凝土中取出钢管的方法,其特征在于可将常温情况下是固体,超过一定温度时被融化的材料选择用塑料布来包裹钢管和电热丝。
3、根据权利要求1所述从凝固的混凝土中取出钢管的方法,其特征在于可以选择在常温情况下是固体,到150度以下时被融化的材料包裹钢管和电热丝。
4、根据权利要求1、2所述从凝固的混凝土中取出钢管的方法,其特征在于包裹钢管的塑料布(2)的厚度为0.9-9毫米,包裹电热丝塑料布(4)的厚度同样为0.9-9毫米。
5、根据权利要求1所述从凝固的混凝土中取出钢管的方法,其特征在于电热丝3的外径上包有绝缘层。
6、根据权利要求1所述从凝固的混凝土中取出钢管的方法,其特征在于电热丝3通电时的温度可选择在150度以下。