CN101474550A - 一种用于室内的环保装饰材料 - Google Patents
一种用于室内的环保装饰材料 Download PDFInfo
- Publication number
- CN101474550A CN101474550A CNA2008101814139A CN200810181413A CN101474550A CN 101474550 A CN101474550 A CN 101474550A CN A2008101814139 A CNA2008101814139 A CN A2008101814139A CN 200810181413 A CN200810181413 A CN 200810181413A CN 101474550 A CN101474550 A CN 101474550A
- Authority
- CN
- China
- Prior art keywords
- activated carbon
- adhesive
- environment friendly
- granular activated
- shaped activated
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种用于室内的环保装饰材料,以颗粒活性炭为基料制作,选择颗粒活性炭,加水搅拌混合均匀,形成潮湿状活性炭,再加入聚酰胺粘合剂或丙烯酸聚合物乳液,搅拌均匀后,按装饰材料的要求确定形状尺寸,通过挤压成型后进行干燥,本发明除可制作室内各种装饰材料外,还可作为各种装饰品的载体,具有长期吸附室内有害气体、净化室内空气的作用,确保人们的身体健康。
Description
技术领域:
本发明涉及一种净化室内空气的装饰材料,特别是涉及一种用于室内的环保装饰材料。
背景技术:
目前,现代家装材料所含化学成份较多,其散发的有毒气体长期充斥在室内,加之人为吸烟和室内空气的流通产生的各种对人体有害的气体,长期影响着人们的身体健康,例如各种材质的天花板、地板和各种工艺品及装饰画,所采用的各种材料均含有部分有害物质,长期污染室内空气,影响着人们的身体健康,特别是室内装饰画,其结构主要是由画框、背板和粘贴在背板上的各种画组成,由于该种画灵活多变,立体感强,观赏性好,所以得到人们的普遍喜爱,大多家庭都有或多或少的装饰画进行点缀,人们在欣赏画的同时,也受着有害气体的危害,加之其它各种装饰材料散发的有害气体,使人们的居住、生活和工作环境长期处于空气污染状态,而解决的办法常用开窗通风、使用换气扇等,这都是一时的,不能长期解决问题,目前还没有一种可随时、长期净化室内空气、祛除室内有害气体的装饰材料。
发明内容:
本发明针对现有技术不足,提供一种用于室内的环保装饰材料,所要解决的技术问题是合理选材、确定制作工艺,可生产用于室内的各种可长期吸附室内有害气体、净化室内空气的环保装饰材料,既起到装饰的效果,又能达到环保要求,本发明所采取的技术方案如下:
本发明是一种用于室内的环保装饰材料,其特征在于以5-80目颗粒活性炭为基料制作。
上述环保装饰材料的具体制作工艺如下:
(1)在5-80目的范围内选择一个目数范围的颗粒活性炭;
(2)在选择好的颗粒活性炭中加水搅拌,混合均匀,形成潮湿状活性炭,活性炭与水的比例为1:0.25-0.50;
(3)在潮湿状活性炭中加入粘合剂,潮湿状活性炭和粘合剂按重量配比为:潮湿状活性炭70-80%、粘合剂20-30%,并搅拌均匀;
(4)按装饰材料的要求确定形状和尺寸,通过挤压成型;
(5)进行干燥,干燥温度在80-150℃之间,时间为2-5小时。
上述粘合剂可选择聚酰胺粘合剂或丙烯酸聚合物乳液。
与现有技术相比,本发明除可制作室内各种装饰材料外,还可作为各种装饰品的载体,选用5-80目颗粒活性炭挤压成型有透气、透水的特性,具有长期吸附室内有害气体、净化室内空气的作用,确保人们的身体健康。
具体实施方式:
本发明以颗粒活性炭为基料制作,具体制作工艺如下:
一、
(1)选择5-10目的颗粒活性炭;
(2)加水搅拌,活性炭与水的比例为1:0.25,混合均匀,形成潮湿状活性炭;
(3)在潮湿状活性炭中加入聚酰胺粘合剂或丙烯酸聚合物乳液,按重量配比为:潮湿状活性炭70%、聚酰胺粘合剂或丙烯酸聚合物乳液30%,并搅拌均匀;
(4)按装饰材料的要求确定形状尺寸,通过挤压成型;
(5)进行干燥,干燥温度在80-150℃之间,时间2-5小时。
二、
(1)选择50-80目的颗粒活性炭;
(2)加水搅拌,活性炭与水的比例为1:0.50,混合均匀,形成潮湿状活性炭;
(3)在潮湿状活性炭中加入聚酰胺粘合剂或丙烯酸聚合物乳液,按重量配比为:潮湿状活性炭80%、聚酰胺粘合剂或丙烯酸聚合物乳液20%,并搅拌均匀;
(4按装饰材料的要求确定形状尺寸,通过挤压成型;
(5)进行干燥,干燥温度在80-150℃之间,时间2-5小时。
三、
(1)选择24-50目的颗粒活性炭;
(2)加水搅拌,活性炭与水的比例为1:0.35,混合均匀,形成潮湿状活性炭;
(3)在潮湿状活性炭中加入聚酰胺粘合剂或丙烯酸聚合物乳液,按重量配比为:潮湿状活性炭75%、聚酰胺粘合剂或丙烯酸聚合物乳液25%,并搅拌均匀;
(4按装饰材料的要求确定形状尺寸,通过挤压成型;
(5)进行干燥,干燥温度在80-150℃之间,时间2-5小时。
Claims (4)
1、一种用于室内的环保装饰材料,其特征在于选用5-80目颗粒活性炭为基料。
2、一种权利要求1所述环保装饰材料的制作工艺,其特征在于:
(1)在5-80目的范围内选择一个目数范围的颗粒活性炭;
(2)在选择好的颗粒活性炭中加水搅拌,混合均匀,形成潮湿状活性炭,活性炭与水的比例为1:0.25-0.50;
(3)在潮湿状活性炭中加入粘合剂,潮湿状活性炭和粘合剂按重量配比为:潮湿状活性炭70-80%、粘合剂20-30%,并搅拌均匀;
(4)按装饰材料的要求确定形状和尺寸,通过挤压成型;
(5)进行干燥,干燥温度在80-150℃之间,时间为2-5小时。
3、根据权利要求2所述的制作工艺,其特征在于粘合剂选用聚酰胺粘合剂。
4、根据权利要求2所述的制作工艺,其特征在于粘合剂选用丙烯酸聚合物乳液。