CN101429421A - 环保型散煤覆盖抑制剂及其制备方法 - Google Patents

环保型散煤覆盖抑制剂及其制备方法 Download PDF

Info

Publication number
CN101429421A
CN101429421A CNA200810232714XA CN200810232714A CN101429421A CN 101429421 A CN101429421 A CN 101429421A CN A200810232714X A CNA200810232714X A CN A200810232714XA CN 200810232714 A CN200810232714 A CN 200810232714A CN 101429421 A CN101429421 A CN 101429421A
Authority
CN
China
Prior art keywords
carboxymethyl cellulose
inhibitor
environment
coal
water
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA200810232714XA
Other languages
English (en)
Inventor
程爱华
端木合顺
王旭东
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Xian University of Science and Technology
Original Assignee
Xian University of Science and Technology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Xian University of Science and Technology filed Critical Xian University of Science and Technology
Priority to CNA200810232714XA priority Critical patent/CN101429421A/zh
Publication of CN101429421A publication Critical patent/CN101429421A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种环保型散煤覆盖抑制剂,所述抑制剂由以下质量百分比的原料组成:羧甲基纤维素0.05-2.00%,丙三醇0.50-2.50%,余量为水。本发明还提供了一种环保型散煤覆盖抑制剂的制备方法,制备过程为;在反应釜中加入水量的80%,再加入羧甲基纤维素,启动反应釜进行搅拌,待所述羧甲基纤维素全部溶解后再加入丙三醇,搅拌混匀后最后加入剩余的20%水量,搅拌均匀,即为成品。本发明产品配方合理、原料易购,由于原料为有机物,故喷洒后不会影响煤的燃烧值,且该产品成本低廉,使用方便,抑尘防损效果明显,经济及生态效益显著;其生产工艺简单,在加工、使用过程中无二次污染,使用安全,无毒副作用。

Description

环保型散煤覆盖抑制剂及其制备方法
技术领域
本发明涉及一种防煤尘抑制剂及其制备方法,具体涉及一种环保型散煤覆盖抑制剂及其制备方法。
背景技术
长期以来,煤炭作为基础能源,在我国能源的生产与消费结构中一直占据主导地位。据有关专家预测,到2050年,煤炭在我国一次能源中的比重仍将占据50%以上。在煤炭的储存和运输过程中,会产生大量煤尘,不仅会造成煤炭损失,造成自然资源浪费,还会对环境造成严重污染。此外,对于煤堆来说,扬尘还可能引发安全事故。有些火力发电厂的露天贮煤厂,由于煤尘飞扬,可使供热管道、缆等处因沉积粉尘自燃而造成火灾。目前采用的方法主要有加盖法和喷淋抑尘剂法。其中喷淋抑尘剂法由于施工简单、省时省工、容易实施而受到广泛关注。目前研究开发的抑尘剂大多数为黏结剂(50%)和湿润剂(44%)。湿润剂主要由表面活性剂和某些无机盐、卤化物组成;无机黏结剂主要有卤化物、氧化钙、煤灰、泥土、黏土、石膏、高岭土、酸等,有机黏结剂主要有原油、橄榄油废渣、石油渣油、木质素衍生物、煤渣油、沥青、石蜡、聚合物等;这些抑尘剂,或是加工工艺较为复杂,或是成本较高,或是有一定的毒副作用和腐蚀作用,因此,为了节约宝贵的煤炭资源、减少对环境的污染,研究价廉易得的、无二次污染的散煤覆盖抑尘剂势在必行。
发明内容
本发明所要解决的技术问题在于针对上述现有技术中的不足,提供一种成本低廉,使用安全方便,抑尘防损效果明显,在加工、使用过程中无二次污染且喷洒后不会影响煤的燃烧值的环保型散煤覆盖抑制剂。
为解决上述技术问题,本发明的技术方案是:一种环保型散煤覆盖抑制剂,其特征在于所述抑制剂由以下质量百分比的原料组成:
羧甲基纤维素0.05-2.00%,丙三醇0.50-2.50%,余量为水。
本发明的优选技术方案是:一种环保型散煤覆盖抑制剂,其特征在于所述抑制剂由以下质量百分比的原料组成:
羧甲基纤维素0.1-1.50%,丙三醇1.0-2.00%,余量为水。
本发明的最佳技术方案是:一种环保型散煤覆盖抑制剂,其特征在于所述抑制剂由以下质量百分比的原料组成:
羧甲基纤维素0.3%,丙三醇1.0%,余量为水。
本发明的另一目的是提供一种工艺简单的环保型散煤覆盖抑制剂的制备方法,其特征在于包括以下步骤:
(1)按质量百分比计,在反应釜中加入水量的80%,再加入羧甲基纤维素,启动反应釜,搅拌1~2小时,待所述羧甲基纤维素全部溶解;
(2)在反应釜中再加入丙三醇,搅拌混匀后加入剩余的20%水量,搅拌均匀,即为成品。
发明原料中羧甲基纤维素具有粘合、助悬、增稠、乳化、缓释等作用,能形成良好胶膜,喷洒于散煤表面,形成具有一定强度的固化层;丙三醇具有很强的吸水性,可保持煤层表面的润湿性,起到一定的抑尘效果,此外,加入丙三醇,可改变煤层表面的憎水性,使覆盖抑尘剂容易吸附在煤层表面,增加了固化层的厚度。
本发明与现有技术相比具有以下优点:本发明产品配方合理、原料易购,由于原料为有机物,故喷洒后不会影响煤的燃烧值;其生产工艺简单,在加工、使用过程中无二次污染,使用安全,无毒副作用,且该产品成本低廉,使用方便,抑尘防损效果明显,经济及生态效益显著。
下面通过实施例对本发明的技术方案做进一步的详细描述,但本发明的保护范围不仅仅限于以下实施例。
具体实施方式
实施例1
在反应釜中加入19.744kg的水,加入羧甲基纤维素0.075kg;启动反应釜,搅拌1小时待羧甲基纤维素全部溶解;加入丙三醇0.250kg,搅拌混匀后加入4.931kg水,搅拌均匀即成成品。喷洒在煤堆表面,单位面积喷洒量为3kg/m2,煤堆喷洒覆盖抑尘剂溶液后第2天,在煤堆表面形成1层连续完整的硬壳,壳体经过16天风吹、日晒、雨淋后保持完整、没有裂隙。
实施例2
在反应釜中加入39.488kg的水,加入羧甲基纤维素0.150kg;启动反应釜,搅拌1.5小时待羧甲基纤维素全部溶解;加入丙三醇0.500kg,搅拌混匀后加入9.862kg的水,搅拌均匀即成成品。卡车装满原煤,以单位面积喷洒量为3kg/m2喷淋覆盖抑尘剂,卡车从神木行至西安段,选择路况复杂、颠簸起伏的路段,以80km/h~120km/h的速度行驶,未发现扬尘现象。固化层平均厚度在10mm左右,粘结层未破裂。
实施例3
在反应釜中加入78.976kg的水,加入羧甲基纤维素0.300kg;启动反应釜,搅拌2小时待羧甲基纤维素全部溶解;加入丙三醇1.000kg,搅拌混匀后加入19.724kg的水,搅拌均匀即成成品。以单位面积喷洒量为3kg/m2喷洒覆盖抑尘剂于运煤火车煤料表面,运煤火车运行约800公里,与未喷洒覆盖抑尘剂相比,煤料损失减少约98%。
实施例4
在反应釜中加入79.560kg的水,加入羧甲基纤维素0.050kg;启动反应釜,搅拌1.2小时待羧甲基纤维素全部溶解;加入丙三醇0.500kg,搅拌混匀后加入19.890kg的水,搅拌均匀即成成品。
实施例5
在反应釜中加入76.400kg的水,加入羧甲基纤维素2.000kg;启动反应釜,搅拌1.6小时待羧甲基纤维素全部溶解;加入丙三醇2.500kg,搅拌混匀后加入19.100kg的水,搅拌均匀即成成品。
实施例6
在反应釜中加入77.200kg的水,加入羧甲基纤维素1.500kg;启动反应釜,搅拌1.3小时待羧甲基纤维素全部溶解;加入丙三醇2.000kg,搅拌混匀后加入19.300kg的水,搅拌均匀即成成品。
实施例7
在反应釜中加入78.976kg的水,加入羧甲基纤维素0.100kg;启动反应釜,搅拌1.7小时待羧甲基纤维素全部溶解;加入丙三醇1.000kg,搅拌混匀后加入19.924kg的水,搅拌均匀即成成品。
本发明产品的用法用量:通过喷洒器,按单位面积喷洒量3kg/m2向散煤堆表层均匀喷洒本发明散煤覆盖抑尘剂水溶液。

Claims (4)

1.一种环保型散煤覆盖抑制剂,其特征在于所述抑制剂由以下质量百分比的原料组成:
羧甲基纤维素0.05-2.00%,丙三醇0.50-2.50%,余量为水。
2.根据权利要求1所述的一种环保型散煤覆盖抑制剂,其特征在于所述抑制剂由以下质量百分比的原料组成:
羧甲基纤维素0.1-1.50%,丙三醇1.0-2.00%,余量为水。
3.根据权利要求1所述的一种环保型散煤覆盖抑制剂,其特征在于所述抑制剂由以下质量百分比的原料组成:
羧甲基纤维素0.3%,丙三醇1.0%,余量为水。
4.一种制备如权利要求1所述环保型散煤覆盖抑制剂的方法,其特征在于包括以下步骤:
(1)按质量百分比计,在反应釜中加入总水量的80%,再加入羧甲基纤维素,启动反应釜,搅拌1~2小时,待所述羧甲基纤维素全部溶解;
(2)在反应釜中再加入丙三醇,搅拌混匀后加入剩余的20%水量,搅拌均匀,即为成品。
CNA200810232714XA 2008-12-22 2008-12-22 环保型散煤覆盖抑制剂及其制备方法 Pending CN101429421A (zh)