CN101402806B - 一种脱墨剂及其制备方法 - Google Patents
一种脱墨剂及其制备方法 Download PDFInfo
- Publication number
- CN101402806B CN101402806B CN2008102018292A CN200810201829A CN101402806B CN 101402806 B CN101402806 B CN 101402806B CN 2008102018292 A CN2008102018292 A CN 2008102018292A CN 200810201829 A CN200810201829 A CN 200810201829A CN 101402806 B CN101402806 B CN 101402806B
- Authority
- CN
- China
- Prior art keywords
- deinking agent
- percent
- sodium
- ethanol
- span
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明公开了一种脱墨剂及其制备方法,组分按体积百分比组成包括:环己酮10%~30%;乙醇30%~50%;乙二醇丁醚5%~10%;司班-802%~5%;过硼酸钠0.1%~1%;碳酸钠0.1%~1%;十二烷基苯磺酸钠0.1%~1%;其余为水。本发明能够轻松脱除油墨、记号笔、喷漆等的墨迹,性能稳定,成本较低,无毒无害,对环境没有污染。
Description
技术领域
本发明涉及一种能够脱除油墨、记号笔、喷漆墨迹的脱墨剂及其制备方法。
背景技术
现有的脱墨剂是一种高新科技的产品,能够使油墨、记号笔、喷漆等迅速溶解,质量稳定,无毒无害,对环境无污染,但是由于成本较高,价格没有竞争力,故在市场上没能推广使用。
发明内容
本发明所要解决的技术问题是提供一种低成本能够脱除油墨、记号笔、喷漆墨迹的脱墨剂及其制备方法。
本发明采用的技术方案:一种脱墨剂,由下列组分按体积百分比组成:
环己酮10%~30%
乙醇30%~50%
乙二醇丁醚5%~10%
司班-802%~5%
过硼酸钠0.1%~1%
碳酸钠0.1%~1%
十二烷基苯磺酸钠0.1%~1%
其余为水。
根据上述组分按体积百分比组成的脱墨剂的制备方法,包括下列步骤:
a.将乙醇与水混合加热至50~70℃,加入十二烷基苯磺酸钠、过硼酸钠、碳酸钠,搅拌后使固体完全溶解;
b.待固体完全溶解后加入环己酮、乙二醇丁醚,在50~70℃下,用搅拌器搅拌30分钟,搅拌速度为800~1000转/分钟,使其混合均匀;
c.加入司班-80,继续搅拌,30分钟后停止搅拌和加热;
d.最后将反应产物冷却至室温,得到所述脱墨剂。
发明的有益效果:本发明能够轻松脱除油墨、记号笔、喷漆等的墨迹,性能稳定,成本较低,无毒无害,对环境没有污染。
具体实施方式
下面通过实施例对本发明进一步详细描述,一种脱墨剂,由下列组分按体积百分比组成:
环己酮10%~30%
乙醇30%~50%
乙二醇丁醚5%~10%
司班-802%~5%
过硼酸钠0.1%~1%
碳酸钠0.1%~1%
十二烷基苯磺酸钠0.1%~1%
其余为水。
根据上述组分按体积百分比组成的脱墨剂的制备方法,包括下列步骤:
a.将乙醇与水混合加热至50~70℃,加入十二烷基苯磺酸钠、过硼酸钠、碳酸钠,搅拌后使固体完全溶解;
b.待固体完全溶解后加入环己酮、乙二醇丁醚,在50~70℃下,用搅拌器搅拌30分钟,搅拌速度为800~1000转/分钟,使其混合均匀;
c.加入司班-80,继续搅拌,30分钟后停止搅拌和加热;
d.最后将反应产物冷却至室温,得到所述脱墨剂。
实施例1
配方:
环己酮15ml;乙醇40ml;乙二醇丁醚7ml;
司班-803ml;过硼酸钠0.3g;碳酸钠0.3g
十二烷基苯磺酸钠0.5g;其余为水
制备工艺:
1、将40ml乙醇与35ml水混合加热至55℃,加入0.5g十二烷基苯磺酸钠、0.3g过硼酸钠、0.3g碳酸钠,搅拌至固体完全溶解。
2、固体完全溶解后加入15ml环己酮、7ml乙二醇丁醚,在恒温55℃条件下,用搅拌器搅拌30分钟,搅拌速度为800转/分钟,使其混合均匀。
3、加入3ml司班-80,继续搅拌,30分钟后停止搅拌和加热。
4、将上述反应物在水域中冷却至室温,得到产品。
实施例2
配方:
环己酮20ml;乙醇50ml;乙二醇丁醚5ml;
司班-803ml;过硼酸钠0.2g;碳酸钠0.2g
十二烷基苯磺酸钠0.3g;其余为水
制备工艺:
1、将50ml乙醇与22ml水混合加热至60℃,加入0.3g十二烷基苯磺酸钠、0.2g过硼酸钠、0.2g碳酸钠,搅拌至固体完全溶解。
2、固体完全溶解后加入20ml环己酮、10ml乙二醇丁醚,在恒温60℃条件下,用搅拌器搅拌30分钟,搅拌速度为900转/分钟,使其混合均匀。
3、加入3ml司班-80,继续搅拌,30分钟后停止搅拌和加热。
4、将上述反应物在水域中冷却至室温,得到产品。
所述内容仅为本发明构思下的基本说明,而依据本发明的技术方案所作的任何等效变换,均应属于本发明的保护范围。
Claims (2)
1.一种脱墨剂,由下列组分按体积百分比组成:
环己酮10%~30%
乙醇30%~50%
乙二醇丁醚5%~10%
司班-802%~5%
过硼酸钠0.1%~1%
碳酸钠0.1%~1%
十二烷基苯磺酸钠0.1%~1%
其余为水。
2.根据权利要求1所述组分按体积百分比组成的脱墨剂的制备方法,包括下列步骤:
a.将乙醇与水混合加热至50~70℃,加入十二烷基苯磺酸钠、过硼酸钠、碳酸钠,搅拌后使固体完全溶解;
b.待固体完全溶解后加入环己酮、乙二醇丁醚,在50~70℃下,用搅拌器搅拌30分钟,搅拌速度为800~1000转/分钟,使其混合均匀;
c.加入司班-80,继续搅拌,30分钟后停止搅拌和加热;
d.最后将反应产物冷却至室温,得到所述脱墨剂。