CN101328412B - 一种清洁型热回收炼焦炉炉门柔性密封方法 - Google Patents

一种清洁型热回收炼焦炉炉门柔性密封方法 Download PDF

Info

Publication number
CN101328412B
CN101328412B CN 200810055334 CN200810055334A CN101328412B CN 101328412 B CN101328412 B CN 101328412B CN 200810055334 CN200810055334 CN 200810055334 CN 200810055334 A CN200810055334 A CN 200810055334A CN 101328412 B CN101328412 B CN 101328412B
Authority
CN
China
Prior art keywords
furnace door
door
protecting sheet
sealing
lower edge
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN 200810055334
Other languages
English (en)
Other versions
CN101328412A (zh
Inventor
杨晓杰
武文斌
张留峰
杨生斌
曹峰亮
崔智�
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanxi Qinxin Energy Group Co Ltd
Original Assignee
孙宏原
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 孙宏原 filed Critical 孙宏原
Priority to CN 200810055334 priority Critical patent/CN101328412B/zh
Publication of CN101328412A publication Critical patent/CN101328412A/zh
Application granted granted Critical
Publication of CN101328412B publication Critical patent/CN101328412B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种清洁型热回收炼焦炉炉门柔性密封方法,包括以下步骤:a、将原来的上炉门改为和炭化室宽度一样长的下沿,并把下沿高度降到平行于保护板;b、在上炉门上弧段上铣出半圆弧槽;c、在半圆弧槽内粘有石棉圆绳,凸出来的一半石棉绳和上保护板平面接触;d、将下炉门改为炉门本体和四条带燕尾槽的可拆卸铸铁条;e、将下炉门四周密封面铸铁条高度调整到同一平面;f、燕尾槽内人工嵌入陶瓷纤维扁绳,形成一个柔性密封体,利用安装下炉门的大车压力,使扁绳外凸部分压扁,成平面与上炉门下沿和中、下保护板充分接触。本发明将炉门密封形式从硬性面接触改为柔性密封,解决了炼焦过程中密封不严、焦炉无组织进风的问题,提高全焦产率,减少了资源浪费。

Description

一种清洁型热回收炼焦炉炉门柔性密封方法
一、技术领域
本发明属于一种密封工艺技术,具体涉及一种清洁型热回收炼焦炉炉门密封方法。 
二、背景技术:
目前,国内外环保要求都有所提高,2000年山西省化工设计院自主研发了环保效果较好的QRD-2000清洁型热回收捣固式炼焦炉。从2000年到现在国内外上马建设的清洁型热回收捣固式炼焦炉有80多家,但由于该炉型负压操作,炉门密封要求较严,同时该技术又属于一种新生事物、新型技术,不太成熟。炉门密封一直采用刚性硬密封,密封效果差,出现了因从炉门无组织进风量大而化焦严重的问题,造成了资源浪费和企业经济效益降低。 
三、发明内容:
本发明就是要解决现有清洁型热回收捣固式炼焦炉炉门硬密封方法中存在的密封效果差、无组织进风量大、化焦严重的问题。 
本发明通过以下技术方案实现:一种清洁型热回收炼焦炉炉门柔性密封方法,包括以下步骤: 
a、将上炉门从原来高出保护板和宽于炭化室宽度的下沿,改为和炭化室宽度一样长的下沿,并把下沿高度降到平行于保护板; 
b、在上炉门上弧段和上保护板接触部位铣出半圆弧槽; 
c、在半圆弧槽内用粘结剂将石棉圆绳粘住,凸出来的一半石棉绳和上保护板平面接触,利用安装上炉门的大车压力,使石棉圆绳压扁成平面 与保护板充分接触, 
d、将下炉门由原来的整体设计改为五个分体组合而成,分别为炉门本体和四条带燕尾槽的可拆卸铸铁条,四条带燕尾槽的可拆卸铸铁条通过耐热螺栓与炉门本体联接; 
e、将下炉门四周密封面铸铁条高度调整到同一平面; 
f、燕尾槽内人工嵌入耐高温性好、弹性变形恢复性好和重复利用次数多的陶瓷纤维扁绳,嵌到位后,形成一个柔性密封体,利用安装下炉门的大车压力,使扁绳外凸部分压扁,成平面与上炉门下沿和中、下保护板充分接触。 
本发明方法通过对炉门结构和炉门密封材料的改进,使炉门密封形式改为柔性密封,从而改变原硬性面接触密封不严、泄漏严重、焦炉无组织进风的现状,降低化焦率,提高全焦产率,减少资源浪费,提高企业经济效益和社会效益。 
四、具体实施方式:
一种清洁型热回收炼焦炉炉门柔性密封方法,包括以下步骤: 
a、将上炉门从原来高出保护板和宽于炭化室宽度的下沿,改为和炭化室宽度一样长的下沿,并把下沿高度降到平行于保护板; 
b、在上炉门上弧段和上保护板接触部位铣出半圆弧槽; 
c、在半圆弧槽内用粘结剂将石棉圆绳粘住,凸出来的一半石棉绳和上保护板平面接触,利用安装上炉门的大车压力,使石棉圆绳压扁成平面与保护板充分接触, 
d、将下炉门由原来的整体设计改为五个分体组合而成,分别为炉门本体和四条带燕尾槽的可拆卸铸铁条,四条带燕尾槽的可拆卸铸铁条通过 耐热螺栓与炉门本体联接; 
e、将下炉门四周密封面铸铁条高度调整到同一平面; 
f、燕尾槽内人工嵌入耐高温性好、弹性变形恢复性好和重复利用次数多的陶瓷纤维扁绳,嵌到位后,形成一个柔性密封体,利用安装下炉门的大车压力,使扁绳外凸部分压扁,成平面与上炉门下沿和中、下保护板充分接触。 

Claims (1)

1.一种清洁型热回收炼焦炉炉门柔性密封方法,包括以下步骤:
a.将上炉门从原来高出保护板和宽于炭化室宽度的下沿,改为和炭化室宽度一样长的下沿,并把下沿高度降到平行于保护板; 
b.在上炉门上弧段和上保护板接触部位铣出半圆弧槽;
c.在半圆弧槽内用粘结剂将石棉圆绳粘住,凸出来的一半石棉圆绳和上保护板平面接触,利用安装上炉门的大车压力,使石棉圆绳压扁成平面与保护板充分接触;
d.将下炉门由原来的整体设计改为五个分体组合而成,分别为炉门本体和四条带燕尾槽的可拆卸铸铁条,四条带燕尾槽的可拆卸铸铁条通过耐热螺栓与炉门本体联接;
e.将下炉门四周密封面铸铁条高度调整到同一平面;
f.燕尾槽内人工嵌入耐高温性好、弹性变形恢复性好和重复利用次数多的陶瓷纤维扁绳,嵌到位后,形成一个柔性密封体,利用安装下炉门的大车压力,使扁绳外凸部分压扁,成平面与上炉门下沿和中、下保护板充分接触。
CN 200810055334 2008-07-03 2008-07-03 一种清洁型热回收炼焦炉炉门柔性密封方法 Active CN101328412B (zh)