CN101153200A - 防水涂料制备方法 - Google Patents

防水涂料制备方法 Download PDF

Info

Publication number
CN101153200A
CN101153200A CNA2006100158275A CN200610015827A CN101153200A CN 101153200 A CN101153200 A CN 101153200A CN A2006100158275 A CNA2006100158275 A CN A2006100158275A CN 200610015827 A CN200610015827 A CN 200610015827A CN 101153200 A CN101153200 A CN 101153200A
Authority
CN
China
Prior art keywords
present
added
anhydrous
coating material
waterproof coating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CNA2006100158275A
Other languages
English (en)
Inventor
张云波
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhonghong Tianjin Industry Co Ltd
Original Assignee
Zhonghong Tianjin Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhonghong Tianjin Industry Co Ltd filed Critical Zhonghong Tianjin Industry Co Ltd
Priority to CNA2006100158275A priority Critical patent/CN101153200A/zh
Publication of CN101153200A publication Critical patent/CN101153200A/zh
Pending legal-status Critical Current

Abstract

一种防水涂料制备方法,将无水煤焦油、无水酚油投入到加热釜内,搅拌后,加入聚氯乙烯粉、邻苯二甲酸二辛酯、硬脂酸钡,搅拌后,加热,加入滑石粉,保温,停止加热,冷却,停止搅拌,即可。本发明的优点:具有耐候性和弹性、延伸性、粘结性,低温时涂膜不脆裂、不龟裂,高温时不流淌;无污染,防水效果好。

Description

防水涂料制备方法
技术领域
本发明涉及一种防水涂料制备方法。
背景技术
目前,采用油毡纸涂盖石油沥青方法作建筑物防水渗漏,因效果差逐渐被淘汰,而新兴防水卷材成本高,不易普及推广;橡胶改性石油沥青防水涂料,粘结强度差,低温涂膜水裂。
发明内容
本发明的目的在于克服上述的缺陷,提供一种防水涂料制备方法。
本发明的技术方案是:一种防水涂料制备方法,其特征在于:将26%无水煤焦油、21%无水酚油投入到加热釜内,搅拌后,加入2.0%聚氯乙烯粉、0.8%邻苯二甲酸二辛酯、0.2%硬脂酸钡,搅拌后,加热至130-140℃,加入45-55%滑石粉,保温5-10分钟后,停止加热,冷却至40℃,停止搅拌,即可。
本发明具有以下优点:具有优良的耐候性和较高的弹性、延伸性、粘结性,低温时涂膜不脆裂、不龟裂,高温时不流淌;无污染,防水效果好。
具体实施方式
实施例:-种防水涂料制备方法,将26%无水煤焦油、21%无水酚油投入到加热釜内,搅拌后,加入2.0%聚氯乙烯粉、0.8%邻苯二甲酸二辛酯、0.2%硬脂酸钡,搅拌后,加热至130-140℃,加入45-55%滑石粉,保温5-10分钟后,停止加热,冷却至40℃,停止搅拌,即可。

Claims (1)

1.一种防水涂料制备方法,其特征在于:将26%无水煤焦油、21%无水酚油投入到加热釜内,搅拌后,加入2.0%聚氯乙烯粉、0.8%邻苯二甲酸二辛酯、0.2%硬脂酸钡,搅拌后,加热至130-140℃,加入45-55%滑石粉,保温5-10分钟后,停止加热,冷却至40℃,停止搅拌,即可。
CNA2006100158275A 2006-09-25 2006-09-25 防水涂料制备方法 Pending CN101153200A (zh)