CN101109208A - 防水保温一体保护层屋面工法 - Google Patents
防水保温一体保护层屋面工法 Download PDFInfo
- Publication number
- CN101109208A CN101109208A CNA2006101079124A CN200610107912A CN101109208A CN 101109208 A CN101109208 A CN 101109208A CN A2006101079124 A CNA2006101079124 A CN A2006101079124A CN 200610107912 A CN200610107912 A CN 200610107912A CN 101109208 A CN101109208 A CN 101109208A
- Authority
- CN
- China
- Prior art keywords
- roofing
- water
- precast plate
- construction method
- insulation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
本发明公开了一种防水保温一体保护层屋面工法,其特征是先制作保温预制板,然后将保温预制板粘贴在屋面上,再在保温预制板上涂刮粘结剂,将防水卷材粘贴到保温预制板上,完成防水保温一体保护层屋面构件的制作。本发明集防水保温于一体,其现场施工简单,且不受天气变化的影响,施工效率高。
Description
技术领域
本发明涉及一种建筑屋面防水保温保护层制作工艺方法,特别是一种防水保温一体保护层屋面制作方法。
背景技术
现有技术中公开了一种专利号为ZL01207676.7的硬泡聚氨酯抗裂保护层屋面,它是先将屋顶基层清理干净,对预制楼板的屋面先用20-30cm卷材点粘空铺或喷涂一层防水涂料层,然后将异氰酸酯和聚醚按比例混合配料,用喷枪喷涂,形成聚氨酯保护层,然后再做聚合物抗裂砂浆面层,在施工现场完成制作整个屋面构件。采用该方法因需现场喷涂聚氨酯保温层及做聚合物抗裂砂浆面层,现场施工受天气影响较大,施工效率低。
发明内容
本发明的目的是想提供一种制作防水保温一体保护层屋面新的工艺方法,该方法不受天气影响,现场施工简单,施工效率高。
为实现本发明的上述目的所采用技术方案是:一种防水保温一体保护层屋面工法,其特征是先制作保温预制板,将保温预制板粘贴在屋面上,然后在屋面保温预制板上涂刮粘结剂,再将防水卷材粘贴到保温预制板上,完成防水保温一体保护层屋面构件的制作。
所述的保温预制板,可采用聚氨酯预制板、酚醛预制板、发泡聚苯乙烯或挤出聚苯乙烯预制板的至少一种。
所述的粘结剂最好采用改性沥青热熔涂料或水泥胶或聚氨酯防水涂料。
所述的防水卷材可采用SBS或APP防水卷材、聚乙烯丙纶防水卷材或聚氯乙烯防水卷材。
本发明的上述工艺中,最好用聚合物砂浆将保温预制板粘贴在屋面上。
改性沥青热熔涂料的施工厚度大于或等于3mm时,或聚氨酯防水涂料厚度大于等于1.2mm时,可作为一道防水层,以增加防水效果。
本发明由于采用先制作保温预制板的施工方法,这样给屋顶施工带来了方便,不仅施工简单、施工效率大大提高,而且不受天气的影响,采用粘结剂将防水卷材牢固地粘贴到保温层上,可以有效地起到防水的作用,本发明集防水保温于一体,适合于平楼顶及瓦屋面的防水保温。
具体实施方式
下面结合具体实施的例子对本发明做进一步详细的描述。
1、先制作硬质聚氨酯或者酚醛保温预制板,将屋顶基面清理干净,并找平,用聚合物砂浆将保温预制板粘贴在屋面上作为保温层,然后在保温层上涂刮SBS改性沥青热熔涂料粘结剂,再将SBS或者APP防水卷材粘贴到保温层上,完成防水保温一体保护层屋面构件制作。当SBS改性沥青热熔涂料的厚度大于或等于3mm时,可作为一道防水层。
2、先制作发泡聚苯乙烯或挤出聚苯乙烯保温预制板,将屋顶基面清理干净,并找平,用聚合物砂浆将保温预制板粘贴在屋面上作为保温层,然后在保温层上涂刮水泥胶,再将聚乙烯丙纶防水卷材粘贴到保温层上,完成防水保温一体保护层屋面构件的制作。
3、先制作发泡聚苯乙烯或挤出聚苯乙烯保温预制板,将屋顶基面清理干净,并找平,用聚合物砂浆将保温预制板粘贴在屋面上作为保温层,然后在保温层上涂刮聚氨酯防水涂料粘结剂,再将聚氯乙烯(PVC)防水卷材粘贴到保温层上,完成制作防水保温一体保护层屋面构件的制作。当聚氨酯防水涂料厚度达到或超过1.2mm时可以作为一道防水层。
Claims (5)
1.一种防水保温一体保护层屋面工法,其特征是先制作保温预制板,将保温预制板粘贴在屋面上,再在保温预制板上涂刮粘结剂,然后将防水卷材粘贴到保温预制板上,完成防水保温一体保护层屋面构件的制作。
2.按照权利要求1所述的防水保温一体保护层屋面工法,其特征是所述的保温预制板可采用聚氨酯预制板、酚醛预制板、发泡聚苯乙烯或挤出聚苯乙烯预制板的至少一种。
3.按照权利要求2所述的防水保温一体保护层屋面工法,其特征是所述的粘结剂可采用改性沥青热熔涂料、水泥胶或聚氨酯防水涂料。
4.按照权利要求1、2或3所述的防水保温一体保护层屋面工法,其特征是所述的防水卷材可采用SBS或APP防水卷材、聚乙烯丙纶防水卷材、聚氯乙烯防水卷材。
5.按照权利要求4所述的防水保温一体保护层屋面工法,其特征是用聚合物砂浆将保温预制板粘贴在屋面上。