CN100389843C - 防变形竹剑及其制造方法 - Google Patents
防变形竹剑及其制造方法 Download PDFInfo
- Publication number
- CN100389843C CN100389843C CNB2004100666536A CN200410066653A CN100389843C CN 100389843 C CN100389843 C CN 100389843C CN B2004100666536 A CNB2004100666536 A CN B2004100666536A CN 200410066653 A CN200410066653 A CN 200410066653A CN 100389843 C CN100389843 C CN 100389843C
- Authority
- CN
- China
- Prior art keywords
- bamboo
- sword
- epee
- deformation
- tabasheer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种防变形竹剑及其制造方法,该竹剑由四片竹片组合而成,各竹片的一端为柄部而另端为剑尖部,柄部以铁片固定或增用黏胶黏合加工形成握柄呈圆柱状,各竹片的外表面为竹青部,内壁为竹黄部,两侧形成接触面,其中在各竹黄部上涂有防水层。制造时,增加一道涂防水材料工序,将防水材料漆或油或蜡均匀地涂布在各竹片的竹黄部上(蜡是热涂)。如果竹黄部有内膜时,可在涂布前先将残留内膜去除,因竹子种类而异。由于竹剑的竹黄部被防水层覆盖,竹片内部的水分不易挥发,外部的水分也不易渗入。因此,竹剑不会随着天气变化而产生变形,不会影响竹剑的使用。
Description
技术领域
本发明是一种剑道用的竹剑,尤其是一种可以防止变形的竹剑及其制造方法。
背景技术
剑道运动中,剑是必不可少的器械。为了避免人身伤害,练习和比赛中使用的是具有弹性软式的竹剑。
一般的竹剑主要将圆竹筒剖开,由四片竹片,经多道工序将外表竹青及切削面抛光、抛蜡、抛亮,组合成剑体,然后于剑体外加上皮套、刀锷等配件制成,如图4所示。
如图5所示,为图4所示现有竹剑剑体的横剖面图。剑体由四片竹片40组成,各竹片40的柄部用铁片固定或增用黏胶(胶水)黏合加工形成握柄呈圆柱状(图4被包覆于握柄处皮套中),竹片的剑尖部(末端)未黏合,而是利用套索和皮套(如图4所示)贴合紧固在一起以免向外弹出。
然而,竹剑的竹片40虽经干燥处理,仍含有一定的水分,一般在10%-14%左右。各竹片的外表面为竹青部41,内壁为竹黄部42。竹青部41致密性好,水分不易挥发。竹黄部42则密度较低,壁面呈无数个毛细孔形态,内含水分会随天气而变化。当空气中的湿度高时,水分会被竹黄毛细孔吸入,致使竹片40胀开。天气干燥时,竹黄部内的水分又会从微孔中挥发使竹片40收缩。这样一来,竹片常常发生变形,影响竹剑的使用。
发明内容
本发明主要目的是在于提供一种竹剑,其可有效防止竹片内含水分随天气而变化,使竹片不致变形。
为达成上述目的,本发明提供了一种防变形竹剑,由四片竹片组合而成,各竹片的一端为柄部而相对柄部的另一端为剑尖部,柄部以铁片固定或增用黏胶黏合加工形成握柄呈圆柱状,各竹片的外表面为竹青部,内壁为竹黄部,两侧形成接触面,其中在各竹黄部上涂有防水层。
上述的防变形竹剑,各竹片的接触面上涂有防水层。
本发明还提供了一种上述竹剑的制造方法,该制造方法中增加一道涂防水层工序,将防水材料均匀地涂布在各竹片的竹黄部上。
上述竹剑的制造方法的涂防水层工序还包括将防水材料涂布在各竹片的接触面上。
上述的防水层材料可用漆、油或蜡等材料。
本发明制造的竹剑,其竹黄部被防水层覆盖,竹片内部的水分不易挥发,外部的水分也不易渗入。因此,竹剑不会随着天气变化而产生变形,不会影响竹剑的使用。
附图简述
图1是本发明竹剑未加装皮套、剑锷等配件时的外观示意图。
图2是本发明竹剑沿图1中“A-A”的放大剖视图。
图3是本发明另一实施方式的放大剖视图。
图4是现有竹剑的成品外观示意图。
图5是现有竹剑沿图4中“B-B”的放大剖视图。
具体实施方式
如图1、2所示,本发明的竹剑由四片竹片10组合而成,图1竹剑的竹片头部用铁片固定或增用黏胶或胶水黏合加工形成握柄呈圆柱状,剑尖(末端)未黏合。各竹片10的外表面为竹青部11,内壁为竹黄部13,两侧形成接触面12,各竹黄部13上涂有防水层20,使竹片内的水分不易挥发,外部的水分也不易渗入竹黄部13。在本实施方式中,该防水层20为漆层。其他如油、蜡等防水材料也可应用在本发明中。
制造时,加入一道防水层工序,将防水材料漆或油或蜡均匀地涂布在各竹片的竹黄部13上(蜡是热涂),使竹片内的含水率保持稳定。如果竹黄部有内膜时,可在涂布前先将残留的内膜去除,因竹子种类而异。
如图3所示,根据本发明的另一实施方式,各竹片10的接触面12上亦可涂上防水材料,进一步防止水分的挥发或渗入。
Claims (10)
1.一种防变形竹剑,由四片竹片组合而成,各竹片的一端为柄部,而相对柄部的另一端为剑尖部,柄部以铁片固定或增用黏胶黏合加工形成握柄呈圆柱状,各竹片的外表面为竹青部,内壁为竹黄部,两侧形成接触面,其特征在于,各竹黄部上涂有防水层。
2.如权利要求1所述的防变形竹剑,其特征在于,各竹片的接触面上涂有防水层。
3.如权利要求1或2所述的防变形竹剑,其特征在于,该防水层为漆层。
4.如权利要求1或2所述的防变形竹剑,其特征在于,该防水层为油层。
5.如权利要求1或2所述的防变形竹剑,其特征在于,该防水层为蜡层。
6.一种防变形竹剑的制造方法,该竹剑由四片竹片组合而成,各竹片的一端为柄部而相对柄部的另一端为剑尖部,柄部以铁片固定或增用黏胶黏合加工形成握柄,其呈圆柱状,各竹片的外表面为竹青部,内壁为竹黄部,两侧形成接触面,其特征在于,该竹剑的制造方法中增加一道涂防水层工序,将防水材料均匀地涂在各竹片的竹黄部上。
7.如权利要求6所述的防变形竹剑的制造方法,其特征在于,该方法的涂防水层工序还包括将防水材料涂在各竹片的接触面上。
8.如权利要求6或7所述的防变形竹剑的制造方法,其特征在于,该防水材料为漆。
9.如权利要求6或7所述的防变形竹剑的制造方法,其特征在于,该防水材料为油。
10.如权利要求6或7所述的防变形竹剑的制造方法,其特征在于,该防水材料为蜡。