CN100368505C - 一种等离子显示器用荧光粉浆料 - Google Patents

一种等离子显示器用荧光粉浆料 Download PDF

Info

Publication number
CN100368505C
CN100368505C CNB2005100961423A CN200510096142A CN100368505C CN 100368505 C CN100368505 C CN 100368505C CN B2005100961423 A CNB2005100961423 A CN B2005100961423A CN 200510096142 A CN200510096142 A CN 200510096142A CN 100368505 C CN100368505 C CN 100368505C
Authority
CN
China
Prior art keywords
parts
fluorescent powder
carrier
plasma display
carriers
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNB2005100961423A
Other languages
English (en)
Other versions
CN1766031A (zh
Inventor
许彦旗
陆康宁
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sichuan Sterope Orion Display Co., Ltd.
Original Assignee
SICHUAN STEROPE ORION DISPLAY CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SICHUAN STEROPE ORION DISPLAY CO Ltd filed Critical SICHUAN STEROPE ORION DISPLAY CO Ltd
Priority to CNB2005100961423A priority Critical patent/CN100368505C/zh
Publication of CN1766031A publication Critical patent/CN1766031A/zh
Application granted granted Critical
Publication of CN100368505C publication Critical patent/CN100368505C/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种等离子显示器用荧光粉浆料,含质量份数为10~40份的荧光粉粉体、60~90份的载体和0.1~1份的甲苯。本发明在荧光粉浆料中加入了甲苯,可以对载体中的有机树脂进行改性,大大增强了有机溶剂对树脂的溶解能力,从而使荧光粉颗粒在载体中分散更加均匀,使用本发明的荧光粉浆料进行印刷,浆料的涂敷性能明显改善,烧结后的荧光粉层致密性显著提高。

Description

一种等离子显示器用荧光粉浆料
技术领域
本发明属于显示技术领域,具体涉及一种等离子显示器用荧光粉浆料。
背景技术
彩色交流等离子体显示器是利用气体放电产生的紫外线激发涂敷在显示单元内的荧光粉从而实现彩色显示的,制作在后面板上的障壁,把显示区域分隔成小的显示单元,顺序涂敷红(R)、绿(G)、蓝(B)三色荧光粉。每一个显示像素由红(R)、绿(G)、蓝(B)三个子像素构成,三种颜色的可见光经加法混色而实现全色显示。各个显示单元内的荧光粉不仅涂敷在障壁的沟底,还要附着在障壁的两侧,荧光粉涂层要求均匀致密。
荧光粉浆料是将固体荧光粉微粒均匀分散在有机载体中制成的。作为用于上述各色荧光粉的化合物,已知的包括发红光的(Y,Ga)BO3:Eu3+、Y2O3:Eu3+,发绿光的Zn2SiO4:Mn2+,发蓝光的BaMgAl10O17:Eu2+。载体由有机溶剂和有机树脂组成,有机树脂起到粘结剂的作用,如乙基纤维素、丙稀酸树脂等;有机溶剂用来溶解有机树脂,常用的有松油醇、醋酸丁基卡必醇、丁基卡必醇等。现有的有机树脂在溶入有机溶剂时,经常出现溶解不充分的现象。荧光粉的粉体在有机树脂溶剂不充分的载体中的分散性很差,而且极易产生二次团聚的颗粒。
另外,目前把荧光粉涂敷到显示单元内大多是采用丝网印刷的方法。漏印版上与各显示单元相对的位置,是镂空的,而其它区域是密封的。具有一定粘度的荧光粉浆料在刮刀的挤压力作用下,填充进与上述漏印版上镂空区域相对应的上述障壁分隔开的显示单元内,荧光粉浆料经干燥、烧结处理后,浆料中的载体挥发出来,只有荧光粉粉体附着在显示单元的内壁上。
在印刷时,刮刀下压漏印版丝网的张力是不均匀的,刮刀两侧的张力大,中间位置的张力小,由于张力不均匀,挤压进显示单元的荧光粉浆料的量就会随之不均匀。在显示图像时,荧光粉数量不同的显示单元,发出可见光的强度会不同。而且,随着基板尺寸的扩大,这种不均匀性会变得更加明显。
发明内容
本发明的目的在于克服上述现有技术的缺点,提供了一种可以改善传统丝网印刷荧光粉方法中浆料排出量的精度,提高显示屏全屏均匀亮度的等离子显示器用荧光粉浆料。
为达到上述目的,本发明采用的制备方法是:含质量份数为10~40份的荧光粉粉体、60~90份的载体和0.1~1份的甲苯。
本发明的荧光粉粉体为发红光的(Y,Ga)BO3:Eu3+、Y2O3:Eu3+、发绿光的Zn2SiO4:Mn2+或者发蓝光的BaMgAl10O17:Eu2+;载体中含有10~40份的乙基纤维素和60~90份有机溶剂松油醇、醋酸丁基卡必醇或丁基卡必醇。
本发明在荧光粉浆料中加入了甲苯,可以对载体中的有机树脂进行改性,大大增强了有机溶剂对树脂的溶解能力,从而使荧光粉颗粒在载体中分散更加均匀,使用本发明的荧光粉浆料进行印刷,浆料的涂敷性能明显改善,烧结后的荧光粉层致密性显著提高。
具体实施方式
实施例1:本发明的荧光粉浆料含质量份数为10份的发红光的(Y,Ga)BO3:Eu3+、90份载体和1份的甲苯,该载体中含有40份的乙基纤维素和60份的松油醇。
实施例2:本发明的荧光粉浆料含质量份数为30份的发红光的Y2O3:Eu3+、70份载体和0.8份的甲苯,该载体中含有10份的乙基纤维素和90份的醋酸丁基卡必醇。
实施例3:本发明的荧光粉浆料含质量份数为40份的发绿光的Zn2SiO4:Mn2+、60份载体和0.5份的甲苯,该载体中含有15份的乙基纤维素和85份的丁基卡必醇。
实施例4:本发明的荧光粉浆料含质量份数为20份的发蓝光的BaMgAl10O17:Eu2+、80份载体和0.1份的甲苯,该载体中含有30份的乙基纤维素和70份的松油醇。
实施例5:本发明的荧光粉浆料含质量份数为35份的发红光的(Y,Ga)BO3:Eu3+、65份载体和0.6份的甲苯,该载体中含有25份的乙基纤维素和75份的松油醇。
实施例6:本发明的荧光粉浆料含质量份数为25份的发绿光的Zn2SiO4:Mn2+、75份载体和0.3份的甲苯,该载体中含有35份的乙基纤维素和65份的丁基卡必醇。
本发明的荧光粉浆料,相对传统的荧光粉浆料,粘度降低。用丝网印刷法制作荧光粉膜,一次印刷后,挤入显示单元内的浆料比较少,所以,使用这种荧光粉浆料,需要重复(印刷-干燥)过程两次或者两次以上。由于浆料的涂敷性能得到改善,而且粘度降低,又经过了多次印刷过程,大大缓解了一次印刷造成的浆料排出量的不均匀性。

Claims (7)

1.一种等离子显示器用荧光粉浆料,其特征在于:含质量份数为10~40份的荧光粉粉体、60~90份的载体和0.1~1份的甲苯;所说的荧光粉粉体为发红光的(Y,Ga)BO3:Eu3+、Y2O3:Eu3+、发绿光的Zn2SiO4:Mn2+或者发蓝光的BaMgAl10O17:Eu2+;所说的载体中含有10~40份的乙基纤维素和60~90份有机溶剂松油醇、醋酸丁基卡必醇或丁基卡必醇。
2.根据权利要求1所述的等离子显示器用荧光粉浆料,其特征在于:含质量份数为10份的发红光的(Y,Ga)BO3:Eu3+、90份载体和1份的甲苯,该载体中含有40份的乙基纤维素和60份的松油醇。
3.根据权利要求1所述的等离子显示器用荧光粉浆料,其特征在于:荧光粉浆料含质量份数为30份的发红光的Y2O3:Eu3+、70份载体和0.8份的甲苯,该载体中含有10份的乙基纤维素和90份的醋酸丁基卡必醇。
4.根据权利要求1所述的等离子显示器用荧光粉浆料,其特征在于:荧光粉浆料含质量份数为40份的发绿光的Zn2SiO4:Mn2+、60份载体和0.5份的甲苯,该载体中含有15份的乙基纤维素和85份的丁基卡必醇。
5.根据权利要求1所述的等离子显示器用荧光粉浆料,其特征在于:荧光粉浆料含质量份数为20份的发蓝光的BaMgAl10O17:Eu2+、80份载体和0.1份的甲苯,该载体中含有30份的乙基纤维素和70份的松油醇。
6.根据权利要求1所述的等离子显示器用荧光粉浆料,其特征在于:荧光粉浆料含质量份数为35份的发红光的(Y,Ga)BO3:Eu3+、65份载体和0.6份的甲苯,该载体中含有25份的乙基纤维素和75份的松油醇。
7.根据权利要求1所述的等离子显示器用荧光粉浆料,其特征在于:荧光粉浆料含质量份数为25份的发绿光的Zn2SiO4:Mn2+、75份载体和0.3份的甲苯,该载体中含有35份的乙基纤维素和65份的丁基卡必醇。
CNB2005100961423A 2005-10-13 2005-10-13 一种等离子显示器用荧光粉浆料 Expired - Fee Related CN100368505C (zh)