CN100357215C - Cement reinforcement agent, its preparation and application - Google Patents
Cement reinforcement agent, its preparation and application Download PDFInfo
- Publication number
- CN100357215C CN100357215C CNB2006100379206A CN200610037920A CN100357215C CN 100357215 C CN100357215 C CN 100357215C CN B2006100379206 A CNB2006100379206 A CN B2006100379206A CN 200610037920 A CN200610037920 A CN 200610037920A CN 100357215 C CN100357215 C CN 100357215C
- Authority
- CN
- China
- Prior art keywords
- cement
- kilograms
- intensifier
- sodium
- adds
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
Description
Claims (2)