CA2844874C - Procede de recuperation de molybdene de qualite technique a partir de solutions acides diluees de lixiviation, hautement concentrees en arsenic provenant de residus metallurgiques - Google Patents
Procede de recuperation de molybdene de qualite technique a partir de solutions acides diluees de lixiviation, hautement concentrees en arsenic provenant de residus metallurgiques Download PDFInfo
- Publication number
- CA2844874C CA2844874C CA2844874A CA2844874A CA2844874C CA 2844874 C CA2844874 C CA 2844874C CA 2844874 A CA2844874 A CA 2844874A CA 2844874 A CA2844874 A CA 2844874A CA 2844874 C CA2844874 C CA 2844874C
- Authority
- CA
- Canada
- Prior art keywords
- solution
- molybdenum
- recovery
- technical grade
- pls
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
La présente invention concerne un procédé de récupération de molybdène de qualité technique à partir de solutions acides diluées de lixiviation, hautement concentrées en arsenic, ledit procédé comprenant les étapes consistant à: (a) mettre en contact une solution acide de lixiviation préalablement filtrée provenant de la lixiviation des poussières de fonderie avec une résine anionique d'échange d'ions; (b) laver à l'eau la résine chargée; (c) extraire le molybdène de la résine d'échange d'ions avec une solution régénérante alcaline d'ammonium à une valeur de pH comprise entre 8 et 12, pour former du molybdate d'ammonium en solution; (d) laver à l'eau, la résine déchargée; (e) ajouter des sels de magnésium et/ou de fer à la solution ammoniacale récupérée pour obtenir un précipité qui est soumis à l'étape d'élimination de l'arsenic, et une solution qui contient le molybdate d'ammonium en solution; (f) ajouter de l'acide sulfurique à la solution ammoniacale exempte d'arsenic, pour précipiter le molybdène sous forme de molybdate d'ammonium dans un milieu acide à une valeur de pH comprise entre 1,5 et 4; (g) séparer le précipité formé par filtration du molybdate et remettre en circulation la solution obtenue dans la solution initiale de solution acide de lixiviation; (h) calciner le précipité séparé pour obtenir du trioxyde de molybdène et de l'ammoniac; et (i) récupérer l'ammoniac séparé en vue de son renvoi ultérieur dans le processus en tant que solution régénérante recirculée.
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
PCT/IB2012/054308 WO2013030741A2 (fr) | 2011-08-26 | 2012-08-24 | Procédé de récupération de molybdène de qualité technique à partir de solutions acides diluées de lixiviation, hautement concentrées en arsenic provenant de résidus métallurgiques |
Publications (2)
Publication Number | Publication Date |
---|---|
CA2844874A1 CA2844874A1 (fr) | 2013-03-07 |
CA2844874C true CA2844874C (fr) | 2018-01-02 |
Family
ID=50614356
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CA2844874A Active CA2844874C (fr) | 2012-08-24 | 2012-08-24 | Procede de recuperation de molybdene de qualite technique a partir de solutions acides diluees de lixiviation, hautement concentrees en arsenic provenant de residus metallurgiques |
Country Status (1)
Country | Link |
---|---|
CA (1) | CA2844874C (fr) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN111945018B (zh) * | 2020-09-15 | 2022-11-11 | 昆明理工大学 | 一种利用阴离子树脂和赤泥处理含砷溶液中砷的方法 |
-
2012
- 2012-08-24 CA CA2844874A patent/CA2844874C/fr active Active
Also Published As
Publication number | Publication date |
---|---|
CA2844874A1 (fr) | 2013-03-07 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP5994912B2 (ja) | スカンジウムの回収方法 | |
CA2847833C (fr) | Procede pour purifier de l'oxyde de zinc | |
JP6176491B2 (ja) | 塩化ニッケル水溶液の脱銅方法 | |
AU2019211653A1 (en) | Method for producing high-purity scandium oxide | |
EP4077751A1 (fr) | Récupération de vanadium à partir de matériaux de scories | |
JP6798078B2 (ja) | イオン交換処理方法、スカンジウムの回収方法 | |
JP6319362B2 (ja) | スカンジウム回収方法 | |
US9279168B2 (en) | Process for recovery of technical grade molybdenum from diluted leaching acid solutions (PLS), with highly concentrated arsenic, from metallurgical residues | |
CA2844874C (fr) | Procede de recuperation de molybdene de qualite technique a partir de solutions acides diluees de lixiviation, hautement concentrees en arsenic provenant de residus metallurgiques | |
WO2015125821A1 (fr) | Procédé de récupération de scandium | |
JP7276042B2 (ja) | スカンジウムの回収方法、並びにイオン交換処理方法 | |
JP7276043B2 (ja) | スカンジウムの回収方法、並びにイオン交換処理方法 | |
JP6888359B2 (ja) | 金属酸化鉱の製錬方法 | |
KR20220080109A (ko) | 아연 함유 원료에서 아연을 회수하는 개선된 공정 | |
JP7327276B2 (ja) | スカンジウムの回収方法 | |
JP7338283B2 (ja) | スカンジウムの回収方法 | |
WO2013030741A2 (fr) | Procédé de récupération de molybdène de qualité technique à partir de solutions acides diluées de lixiviation, hautement concentrées en arsenic provenant de résidus métallurgiques | |
WO2021010180A1 (fr) | Procédé de récupération de scandium | |
AU2014101275A4 (en) | Process for purifying zinc oxide | |
Angelov et al. | Ionexchange operations for copper and zinc recovery and arsenic removal at the Devnya Waste Treatment Plant, Bulgaria |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
EEER | Examination request |
Effective date: 20140211 |