CA1257526A - Compound for protecting the internal surface of a pipeline against corrosion method of producing same and method of protecting the internal surface of a pipeline against corrosion using this compound - Google Patents
Compound for protecting the internal surface of a pipeline against corrosion method of producing same and method of protecting the internal surface of a pipeline against corrosion using this compoundInfo
- Publication number
- CA1257526A CA1257526A CA000493200A CA493200A CA1257526A CA 1257526 A CA1257526 A CA 1257526A CA 000493200 A CA000493200 A CA 000493200A CA 493200 A CA493200 A CA 493200A CA 1257526 A CA1257526 A CA 1257526A
- Authority
- CA
- Canada
- Prior art keywords
- compound
- pipeline
- water
- internal surface
- protecting
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23F—NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C23F11/00—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent
- C23F11/08—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids
- C23F11/18—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids using inorganic inhibitors
- C23F11/187—Mixtures of inorganic inhibitors
- C23F11/188—Mixtures of inorganic inhibitors containing phosphates
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23F—NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- C23F11/00—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent
- C23F11/08—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids
- C23F11/18—Inhibiting corrosion of metallic material by applying inhibitors to the surface in danger of corrosion or adding them to the corrosive agent in other liquids using inorganic inhibitors
- C23F11/184—Phosphorous, arsenic, antimony or bismuth containing compounds
Landscapes
- Chemical & Material Sciences (AREA)
- Inorganic Chemistry (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Preventing Corrosion Or Incrustation Of Metals (AREA)
- Manufacture And Refinement Of Metals (AREA)
Applications Claiming Priority (14)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| SU3797903 | 1984-10-17 | ||
| SU3798009 | 1984-10-17 | ||
| SU3798009 | 1984-10-17 | ||
| SU3798012 | 1984-10-17 | ||
| SU3798052 | 1984-10-17 | ||
| SU3798005 | 1984-10-17 | ||
| SU3798052 | 1984-10-17 | ||
| SU3798005 | 1984-10-17 | ||
| SU3797906 | 1984-10-17 | ||
| SU3798012 | 1984-10-17 | ||
| SU3798002 | 1984-10-17 | ||
| SU3798002 | 1984-10-17 | ||
| SU843797903A SU1368560A1 (ru) | 1984-10-17 | 1984-10-17 | Устройство дл нанесени антикоррозионного покрыти на внутреннюю поверхность трубопровода |
| SU3797906 | 1985-10-17 |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| CA1257526A true CA1257526A (en) | 1989-07-18 |
Family
ID=27567252
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| CA000493200A Expired CA1257526A (en) | 1984-10-17 | 1985-10-17 | Compound for protecting the internal surface of a pipeline against corrosion method of producing same and method of protecting the internal surface of a pipeline against corrosion using this compound |
Country Status (9)
| Country | Link |
|---|---|
| US (1) | US4828796A (enExample) |
| AT (1) | AT394059B (enExample) |
| AU (2) | AU5195386A (enExample) |
| CA (1) | CA1257526A (enExample) |
| DE (2) | DE3590524C2 (enExample) |
| FR (1) | FR2571745B1 (enExample) |
| GB (1) | GB2180031A (enExample) |
| HU (1) | HUT40498A (enExample) |
| WO (1) | WO1986002426A1 (enExample) |
Families Citing this family (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5137657A (en) * | 1991-04-24 | 1992-08-11 | Merck & Co., Inc. | Synergistic combination of sodium silicate and orthophosphate for controlling carbon steel corrosion |
| JPH06228721A (ja) * | 1992-12-02 | 1994-08-16 | Praxair St Technol Inc | 耐溶融金属侵食性シール材およびその製造方法 |
| DE4321883C2 (de) * | 1993-07-01 | 2003-05-15 | Henkel Kgaa | Wäßrige Silicatlösungen mit hohen Orthophosphatgehalten und Verfahren zur Korrosionsschutzbehandlung von Trinkwasserleitungen |
| JP2003534902A (ja) | 2000-06-01 | 2003-11-25 | シー.エイチ.オー.シー.エス.インコーポレイテッド | 酸素ラインを洗浄するためのシステムおよび方法 |
| SE537355C2 (sv) * | 2013-08-27 | 2015-04-14 | Scana Subsea Ab | Anordning för ytbehandling av rör och rördelar |
| US11879094B2 (en) | 2022-06-03 | 2024-01-23 | Halliburton Energy Services, Inc. | Enhancing friction reduction and protection of wellbore equipment during hydraulic fracturing |
Family Cites Families (17)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US2426394A (en) * | 1943-04-15 | 1947-08-26 | Hall Lab Inc | Water-soluble glass composition |
| NL92131C (enExample) * | 1956-03-29 | |||
| DE1200756B (de) * | 1962-07-24 | 1965-09-09 | Giulini Ges Mit Beschraenkter | Behandlung von chloridhaltigen Brauchwaessern mit Phosphaten |
| NL6909042A (enExample) * | 1968-06-19 | 1969-12-23 | ||
| US3960576A (en) * | 1973-06-25 | 1976-06-01 | Betz Laboratories, Inc. | Silicate-based corrosion inhibitor |
| SU600109A1 (ru) * | 1974-02-01 | 1978-03-30 | Татарский Государственный Научно-Исследовательский И Проектный Институт Нефтяной Промышленности | Способ остекловывани внутренней поверхности металлической трубы |
| US3973056A (en) * | 1974-06-06 | 1976-08-03 | American Gas Association, Inc. | Inhibition of stress-corrosion cracking of steel pipeline |
| US3974047A (en) * | 1975-06-02 | 1976-08-10 | The B. F. Goodrich Company | Electrolytic cation exchange process for conjoint manufacture of chlorine and phosphate salts |
| US4085063A (en) * | 1976-10-06 | 1978-04-18 | Westinghouse Electric Corporation | Non-chromate pitting and general corrosion inhibitors for aluminum products and method |
| JPS60593B2 (ja) * | 1978-06-26 | 1985-01-09 | 住友金属工業株式会社 | 循環水配管系における電縫鋼管の溝状腐食防止方法 |
| DE2963154D1 (en) * | 1978-07-19 | 1982-08-12 | Ciba Geigy Ag | Corrosion inhibitors; compositions for protecting ferrous metals and the protected metals |
| US4405493A (en) * | 1979-02-03 | 1983-09-20 | The British Petroleum Company Limited | Corrosion inhibitors, method of producing them and protective coatings containing them |
| WO1983002628A1 (en) * | 1982-01-29 | 1983-08-04 | Kuhn, Vincent R. | Method of and composition for inhibiting corrosion of iron base metals |
| DE3227592C1 (de) * | 1982-07-21 | 1983-07-21 | Mannesmann AG, 4000 Düsseldorf | Verfahren zum Herstellen einer abriebfesten und korrosionsbestaendigen Zementmoertelauskleidung in Metallrohren |
| US4431563A (en) * | 1982-07-21 | 1984-02-14 | The Dow Chemical Company | Inhibitors for acid gas conditioning solutions |
| DE3232615A1 (de) * | 1982-09-02 | 1984-03-08 | Henkel KGaA, 4000 Düsseldorf | Verfahren zur korrosionsschutzbehandlung wasserfuehrender systeme |
| US4604235A (en) * | 1984-05-23 | 1986-08-05 | J. T. Baker Chemical Company | Purification of monoclonal antibodies |
-
1985
- 1985-10-14 FR FR8515214A patent/FR2571745B1/fr not_active Expired
- 1985-10-16 US US06/882,887 patent/US4828796A/en not_active Expired - Fee Related
- 1985-10-16 DE DE3590524A patent/DE3590524C2/de not_active Expired - Lifetime
- 1985-10-16 AU AU51953/86A patent/AU5195386A/en not_active Abandoned
- 1985-10-16 GB GB08612585A patent/GB2180031A/en not_active Withdrawn
- 1985-10-16 WO PCT/SU1985/000089 patent/WO1986002426A1/ru not_active Ceased
- 1985-10-16 DE DE19853590524 patent/DE3590524T1/de not_active Ceased
- 1985-10-16 HU HU86136A patent/HUT40498A/hu unknown
- 1985-10-16 AT AT0903785A patent/AT394059B/de not_active IP Right Cessation
- 1985-10-17 CA CA000493200A patent/CA1257526A/en not_active Expired
-
1989
- 1989-10-23 AU AU43673/89A patent/AU4367389A/en not_active Abandoned
Also Published As
| Publication number | Publication date |
|---|---|
| GB8612585D0 (en) | 1986-07-02 |
| DE3590524C2 (enExample) | 1990-05-03 |
| ATA903785A (de) | 1991-07-15 |
| DE3590524T1 (de) | 1986-09-18 |
| HUT40498A (en) | 1986-12-28 |
| FR2571745B1 (fr) | 1988-10-28 |
| AU4367389A (en) | 1990-02-08 |
| US4828796A (en) | 1989-05-09 |
| AT394059B (de) | 1992-01-27 |
| GB2180031A (en) | 1987-03-18 |
| FR2571745A1 (fr) | 1986-04-18 |
| AU5195386A (en) | 1986-05-02 |
| WO1986002426A1 (fr) | 1986-04-24 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CA1131436A (en) | Corrosion inhibition treatments and method | |
| US3699052A (en) | Corrosion inhibitor composition containing a glycine,chelating agent,phosphoric or boric acid ester,and a water soluble divalent metal salt | |
| US3935125A (en) | Method and composition for inhibiting corrosion in aqueous systems | |
| US3973056A (en) | Inhibition of stress-corrosion cracking of steel pipeline | |
| US4818298A (en) | Method of removing deposits from the inside walls of a pipeline and applying protective coatings thereto | |
| US2742369A (en) | Corrosion inhibiting composition and method of using same | |
| CA1113238A (en) | Anti-corrosion composition | |
| KR100300501B1 (ko) | 수성시스템에서의부식방지방법 | |
| US20050042440A1 (en) | Magnesium workpiece and method for generation of an anti-corrosion coating on a magnesium workpiece | |
| CA1187765A (en) | Control of iron induced fouling in water systems | |
| US2322349A (en) | Corrosion resistant coating for metal surfaces | |
| US4828796A (en) | Method of protecting the internal surface of a pipeline against corrosion | |
| US2848299A (en) | Corrosion inhibition in water systems | |
| US4126469A (en) | Solution and procedure for depositing a protective precoating on surfaces of zinc-coated ferrous metal parts against corrosion in presence of water | |
| JPS6187890A (ja) | 金属基板上に亜鉛又はZn/Si/Pコ−テイングを与えるための電気メツキ組成物および方法 | |
| CA1306929C (en) | Process of producing phosphate coatings | |
| US4000076A (en) | Drilling mud having reduced corrosiveness | |
| US4110128A (en) | Solution and procedure for depositing a protective coating on galvanized steel parts, and solution regeneration procedure | |
| Watts | The application of X-ray photoelectron spectroscopy to the study of polymer-to-metal adhesion: Part 3 The influence of substrate surface chemistry on the cathodic disbondment process | |
| US5425914A (en) | Methods for inhibiting corrosion in cooling water systems | |
| US2813075A (en) | Treatment of corrosive water | |
| Gouda et al. | Failure of boiler tubes in power plants | |
| US3794596A (en) | Method of and composition for the prevention of scale | |
| CA2110461A1 (en) | Composition and methods for inhibiting the corrosion of low carbon steel in aqueous systems | |
| Raheem | Effect of mixed corrosion inhibitors in cooling water system |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| MKEX | Expiry |