BE445877A - - Google Patents
Info
- Publication number
- BE445877A BE445877A BE445877DA BE445877A BE 445877 A BE445877 A BE 445877A BE 445877D A BE445877D A BE 445877DA BE 445877 A BE445877 A BE 445877A
- Authority
- BE
- Belgium
- Prior art keywords
- electrolyte
- silicates
- protective layers
- electrolytic process
- metals
- Prior art date
Links
- 238000000034 method Methods 0.000 claims description 17
- 229910052751 metal Inorganic materials 0.000 claims description 13
- 239000002184 metal Substances 0.000 claims description 13
- 150000002739 metals Chemical class 0.000 claims description 9
- 238000000576 coating method Methods 0.000 claims description 5
- 239000011248 coating agent Substances 0.000 claims description 4
- 239000003792 electrolyte Substances 0.000 description 18
- 239000011241 protective layer Substances 0.000 description 11
- 150000004760 silicates Chemical class 0.000 description 10
- 239000000203 mixture Substances 0.000 description 6
- 150000003839 salts Chemical class 0.000 description 5
- 239000010410 layer Substances 0.000 description 3
- 239000004115 Sodium Silicate Substances 0.000 description 2
- 229910052782 aluminium Inorganic materials 0.000 description 2
- XAGFODPZIPBFFR-UHFFFAOYSA-N aluminium Chemical compound [Al] XAGFODPZIPBFFR-UHFFFAOYSA-N 0.000 description 2
- 238000005260 corrosion Methods 0.000 description 2
- 230000007797 corrosion Effects 0.000 description 2
- NTHWMYGWWRZVTN-UHFFFAOYSA-N sodium silicate Chemical compound [Na+].[Na+].[O-][Si]([O-])=O NTHWMYGWWRZVTN-UHFFFAOYSA-N 0.000 description 2
- 229910052911 sodium silicate Inorganic materials 0.000 description 2
- XLYOFNOQVPJJNP-UHFFFAOYSA-N water Substances O XLYOFNOQVPJJNP-UHFFFAOYSA-N 0.000 description 2
- KRHYYFGTRYWZRS-UHFFFAOYSA-M Fluoride anion Chemical compound [F-] KRHYYFGTRYWZRS-UHFFFAOYSA-M 0.000 description 1
- 229910019142 PO4 Inorganic materials 0.000 description 1
- 239000004411 aluminium Substances 0.000 description 1
- 150000001768 cations Chemical class 0.000 description 1
- 239000003518 caustics Substances 0.000 description 1
- 231100001010 corrosive Toxicity 0.000 description 1
- 210000003298 dental enamel Anatomy 0.000 description 1
- 238000006073 displacement reaction Methods 0.000 description 1
- 238000005259 measurement Methods 0.000 description 1
- 239000003973 paint Substances 0.000 description 1
- 239000002245 particle Substances 0.000 description 1
- 230000035699 permeability Effects 0.000 description 1
- 235000021317 phosphate Nutrition 0.000 description 1
- 150000003013 phosphoric acid derivatives Chemical class 0.000 description 1
- 230000001681 protective effect Effects 0.000 description 1
- 239000007787 solid Substances 0.000 description 1
- 239000000126 substance Substances 0.000 description 1
- 231100000331 toxic Toxicity 0.000 description 1
- 230000002588 toxic effect Effects 0.000 description 1
Classifications
-
- C—CHEMISTRY; METALLURGY
- C25—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
- C25D—PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C25D11/00—Electrolytic coating by surface reaction, i.e. forming conversion layers
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Chemical Treatment Of Metals (AREA)
Publications (1)
| Publication Number | Publication Date |
|---|---|
| BE445877A true BE445877A (pm) |
Family
ID=102150
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| BE445877D BE445877A (pm) |
Country Status (1)
| Country | Link |
|---|---|
| BE (1) | BE445877A (pm) |
-
0
- BE BE445877D patent/BE445877A/fr unknown
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| Larsen et al. | Effect of excess silicon and small copper content on intergranular corrosion of 6000-series aluminum alloys | |
| Finšgar et al. | Corrosion study of copper in the presence of benzotriazole and its hydroxy derivative | |
| WO2014103703A1 (ja) | ステンレス鋼の不動態化方法 | |
| Sherif | Effects of 3-amino-1, 2, 4-triazole-5-thiol on the inhibition of pure aluminum corrosion in aerated stagnant 3.5 wt.% NaCl solution as a corrosion inhibitor | |
| Sherif et al. | Effect of equal-channel angular pressing passes on the corrosion behavior of 1050 aluminum alloy in natural seawater | |
| FR3082528A1 (fr) | Composition aqueuse et procede de traitement de surface d'une piece en alliage d'aluminium mettant en œuvre une telle composition | |
| El Bakri et al. | Corrosion inhibition study of brass in simulated cooling water by triazole derivatives, cetyltrimethylammonium bromide and their mixture | |
| US2918416A (en) | Electrolytic process for hard surfacing aluminum | |
| Duraisamy et al. | Chemical Degradation of Epoxy‐Polyamide Primer by Electrochemical Impedance Spectroscopy | |
| BE445877A (pm) | ||
| Lehr et al. | Electrodeposition of polypyrrole on aluminium in the presence of sodium bis (2-ethylhexyl) sulfosuccinate | |
| Marunkić et al. | Cerium citrate as ecologically friendly corrosion inhibitor for AA7075 alloy | |
| Diplas et al. | Effect of copper on anodic activity of aluminum-lead model alloy in chloride solution | |
| Knudsen et al. | Anodising as pre-treatment before organic coating of extruded and cast aluminium alloys | |
| Sherif et al. | Electrochemical corrosion behavior of Fe64/Ni36 and Fe55/Ni45 alloys in 4.0% sodium chloride solutions | |
| Grgur et al. | The influence of chloride anions on the pitting corrosion of aluminum alloy en 46000 | |
| FR2510807A1 (fr) | Feuille composite en aluminium pour condensateurs electrolytiques | |
| Zang et al. | Facile constructing of interlocking structure for improving anti-corrosion performance of adenine film on copper | |
| BE561524A (fr) | Procede de fabrication de revetements pour les surfaces de magnesium | |
| BE406710A (pm) | ||
| Šćepanović et al. | Impedance response of aluminum alloys with varying Mg content in Al–Mg systems during exposure to chloride corrosion environment | |
| KR101456176B1 (ko) | 스핀코팅법을 이용하여 철(Fe) 기판 표면을 산화 그래핀 박막으로 코팅하는 방법 및 이로부터 제조된 내 부식성이 향상된 철(Fe) 기판 | |
| Lee et al. | The Effect of Annealing Heat Treatment by Anodic Polarization Impedance Experiments for Cu-10% Ni Alloy | |
| JPS60218498A (ja) | 光輝焼鈍ステンレス鋼の耐食性向上法 | |
| KR100485469B1 (ko) | 경질양극산화피막 처리된 알루미늄 표면에 붕산을포함하는 피막의 형성방법 |