ATA983A - METHOD FOR MELTING AT LEAST PARTLY REDUCED IRON ORE - Google Patents
METHOD FOR MELTING AT LEAST PARTLY REDUCED IRON OREInfo
- Publication number
- ATA983A ATA983A AT0000983A AT983A ATA983A AT A983 A ATA983 A AT A983A AT 0000983 A AT0000983 A AT 0000983A AT 983 A AT983 A AT 983A AT A983 A ATA983 A AT A983A
- Authority
- AT
- Austria
- Prior art keywords
- melting
- iron ore
- reduced iron
- partly reduced
- partly
- Prior art date
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21B—MANUFACTURE OF IRON OR STEEL
- C21B13/00—Making spongy iron or liquid steel, by direct processes
- C21B13/0006—Making spongy iron or liquid steel, by direct processes obtaining iron or steel in a molten state
- C21B13/0013—Making spongy iron or liquid steel, by direct processes obtaining iron or steel in a molten state introduction of iron oxide into a bath of molten iron containing a carbon reductant
- C21B13/002—Reduction of iron ores by passing through a heated column of carbon
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21B—MANUFACTURE OF IRON OR STEEL
- C21B2100/00—Handling of exhaust gases produced during the manufacture of iron or steel
- C21B2100/40—Gas purification of exhaust gases to be recirculated or used in other metallurgical processes
- C21B2100/44—Removing particles, e.g. by scrubbing, dedusting
Landscapes
- Engineering & Computer Science (AREA)
- Chemical & Material Sciences (AREA)
- Manufacturing & Machinery (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Manufacture Of Iron (AREA)
- Manufacture And Refinement Of Metals (AREA)
Priority Applications (4)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
AT0000983A AT376241B (en) | 1983-01-03 | 1983-01-03 | METHOD FOR MELTING AT LEAST PARTLY REDUCED IRON ORE |
DE19833345106 DE3345106A1 (en) | 1983-01-03 | 1983-12-13 | Process for smelting at least partially reduced iron ore |
JP58252451A JPS59133308A (en) | 1983-01-03 | 1983-12-28 | Refinement for at least partially reduced iron ore |
SE8307241A SE8307241L (en) | 1983-01-03 | 1983-12-30 | PROCEDURE FOR MELTING OF ATMINSTONE SOME REDUCED IRON ORE |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
AT0000983A AT376241B (en) | 1983-01-03 | 1983-01-03 | METHOD FOR MELTING AT LEAST PARTLY REDUCED IRON ORE |
Publications (2)
Publication Number | Publication Date |
---|---|
ATA983A true ATA983A (en) | 1984-03-15 |
AT376241B AT376241B (en) | 1984-10-25 |
Family
ID=3479154
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
AT0000983A AT376241B (en) | 1983-01-03 | 1983-01-03 | METHOD FOR MELTING AT LEAST PARTLY REDUCED IRON ORE |
Country Status (4)
Country | Link |
---|---|
JP (1) | JPS59133308A (en) |
AT (1) | AT376241B (en) |
DE (1) | DE3345106A1 (en) |
SE (1) | SE8307241L (en) |
Families Citing this family (26)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DD226157A3 (en) * | 1983-06-01 | 1985-08-14 | Bandstahlkombinat Matern Veb | METHOD FOR PRODUCING LIQUID RAW STEEL AND REDUCTION GAS IN A SEPARATOR REFRIGERATOR |
DE3438487A1 (en) * | 1984-10-17 | 1986-04-24 | Korf Engineering GmbH, 4000 Düsseldorf | METHOD FOR THE PRODUCTION OF RAW IRON |
AT381116B (en) * | 1984-11-15 | 1986-08-25 | Voest Alpine Ag | METHOD FOR THE PRODUCTION OF LIQUID PIPE IRON OR STEEL PRE-PRODUCTS AND DEVICE FOR IMPLEMENTING THE METHOD |
SU1479006A3 (en) * | 1984-11-26 | 1989-05-07 | Фоест-Альпине (Фирма) | Method of producing molten iron or steel products and reducing gas in melting gasifier |
AT382390B (en) * | 1985-03-21 | 1987-02-25 | Voest Alpine Ind Anlagen | METHOD FOR THE PRODUCTION OF LIQUID PIPE IRON OR STEEL PRE-PRODUCTS |
DE3787017T2 (en) * | 1987-06-30 | 1993-11-25 | Kawasaki Steel Co | Method and device for producing liquid metal from ore particles. |
DE3731851A1 (en) * | 1987-09-22 | 1989-04-06 | Voest Alpine Ind Anlagen | Process for producing a metal melt |
DE3737262A1 (en) * | 1987-11-03 | 1989-05-24 | Voest Alpine Ind Anlagen | METHOD FOR PRE-TREATING A PIECE OF CARBON CARRIER |
AT392289B (en) * | 1988-04-08 | 1991-02-25 | Voest Alpine Stahl Donawitz | METHOD FOR UTILIZING ZINC-CONTAINED DUST AND SLUDGE |
AT394201B (en) * | 1989-02-16 | 1992-02-25 | Voest Alpine Ind Anlagen | METHOD FOR GENERATING COMBUSTIBLE GASES IN A MELT-UP CARBURETTOR |
AT403055B (en) * | 1993-05-07 | 1997-11-25 | Voest Alpine Ind Anlagen | METHOD FOR RECYCLING IRONIC WASTE OR RESIDUES |
AT400725B (en) * | 1994-04-11 | 1996-03-25 | Voest Alpine Ind Anlagen | METHOD FOR PRODUCING A MELTING IRON |
AT405186B (en) * | 1994-10-17 | 1999-06-25 | Voest Alpine Ind Anlagen | INSTALLATION AND METHOD FOR THE PRODUCTION OF RAW IRON AND / OR IRON SPONGE |
AT405187B (en) * | 1994-12-01 | 1999-06-25 | Voest Alpine Ind Anlagen | METHOD FOR THE PRODUCTION OF IRON SPONGE AND SYSTEM FOR IMPLEMENTING THE METHOD |
KR100226897B1 (en) * | 1994-12-26 | 1999-10-15 | 이구택 | Agglomerate method of pre-reduction fine ore for molten pig iron |
EP0805786B1 (en) | 1995-01-24 | 1998-11-04 | Voest-Alpine Industrieanlagenbau Gmbh | Method of utilizing dusts produced during the reduction of iron ore |
AT405294B (en) * | 1995-04-24 | 1999-06-25 | Voest Alpine Ind Anlagen | METHOD FOR RECYCLING FERROUS CABINET RESIDUES AND PLANT FOR IMPLEMENTING THE METHOD |
AT405524B (en) | 1996-03-05 | 1999-09-27 | Voest Alpine Ind Anlagen | METHOD FOR PRODUCING LIQUID PIPE IRON OR LIQUID STEEL PRE-PRODUCTS AND METAL SPONGE |
AT404598B (en) | 1997-04-16 | 1998-12-28 | Voest Alpine Ind Anlagen | METHOD AND INSTALLATION FOR THE PRODUCTION OF LIQUID PIG IRON OR LIQUID STEEL PRE-PRODUCTS |
AT405054B (en) | 1997-06-18 | 1999-05-25 | Voest Alpine Ind Anlagen | METHOD AND PLANT FOR PRODUCING AN IRON MEL WITH THE USE OF IRON-CONTAINING RESIDUAL MATERIALS |
USRE39536E1 (en) * | 1997-07-04 | 2007-04-03 | Deutsche Voest-Alpine Industrieanlagenbau Gmbh | Method and plant utilizing fine coal in a melter gasifier |
AT407053B (en) | 1997-07-04 | 2000-12-27 | Voest Alpine Ind Anlagen | METHOD AND SYSTEM FOR THE PRODUCTION OF A METAL MELT IN A MELTING-UP CARBURETOR USING FINE COAL |
AT406272B (en) | 1997-11-10 | 2000-03-27 | Voest Alpine Ind Anlagen | METHOD FOR PRODUCING DIRECTLY REDUCED IRON, LIQUID PIPE IRON AND STEEL, AND SYSTEM FOR IMPLEMENTING THE METHOD |
AT407161B (en) * | 1998-11-27 | 2001-01-25 | Voest Alpine Ind Anlagen | METHOD FOR PRODUCING LIQUID PIG IRON |
AT505227B1 (en) | 2007-05-09 | 2012-07-15 | Siemens Vai Metals Tech Gmbh | PROCESS FOR THE MANUFACTURE OF FORMINGS |
US8999033B2 (en) * | 2010-12-15 | 2015-04-07 | Midrex Technologies, Inc. | Method and system for producing direct reduced iron and/or hot metal using brown coal |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3038795A (en) * | 1958-06-07 | 1962-06-12 | Rummel Roman | Process for smelting and reducing powdered or finely divided ores |
DE2843303C2 (en) * | 1978-10-04 | 1982-12-16 | Korf-Stahl Ag, 7570 Baden-Baden | Process and plant for the production of liquid pig iron and reducing gas in a melter gasifier |
MX153453A (en) * | 1979-07-16 | 1986-10-16 | Mindres Int Bv | IMPROVEMENTS IN METHOD AND APPARATUS FOR THE PRODUCTION OF CAST CAST IRON |
-
1983
- 1983-01-03 AT AT0000983A patent/AT376241B/en not_active IP Right Cessation
- 1983-12-13 DE DE19833345106 patent/DE3345106A1/en active Granted
- 1983-12-28 JP JP58252451A patent/JPS59133308A/en active Pending
- 1983-12-30 SE SE8307241A patent/SE8307241L/en not_active Application Discontinuation
Also Published As
Publication number | Publication date |
---|---|
SE8307241L (en) | 1984-07-04 |
JPS59133308A (en) | 1984-07-31 |
SE8307241D0 (en) | 1983-12-30 |
DE3345106A1 (en) | 1984-07-12 |
AT376241B (en) | 1984-10-25 |
DE3345106C2 (en) | 1987-02-05 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
AT376241B (en) | METHOD FOR MELTING AT LEAST PARTLY REDUCED IRON ORE | |
DE3880245D1 (en) | METHOD AND DEVICE FOR MELTING DOWN AND REDUCING IRON ORE. | |
DE3579942D1 (en) | METHOD FOR DETACHING INTERFERON. | |
ATA296785A (en) | METHOD FOR CONTINUOUS CASTING | |
AT376243B (en) | METHOD FOR MELTING AT LEAST PARTLY REDUCED IRON ORE | |
DE3578942D1 (en) | METHOD FOR HARDENING GELATINE. | |
DE3581226D1 (en) | METHOD AND DEVICE FOR MELTING BLOCKS. | |
DE3483426D1 (en) | METHOD FOR ELECTRICALLY DEPOSITING METALS. | |
AT379572B (en) | METHOD FOR MELTING SLAG | |
ATA355585A (en) | METHOD FOR REPLACING BRIDGE BEARINGS | |
DE3382683D1 (en) | METHOD FOR MELTING POLYAMIDES. | |
AT380697B (en) | METHOD FOR MELTING AT LEAST PARTLY REDUCED IRON ORE AND DEVICE FOR CARRYING OUT THIS METHOD | |
DE3877320D1 (en) | METHOD FOR CONTINUOUS MELTING OF STEEL. | |
DE3671247D1 (en) | METHOD FOR MELTING REDUCTION OF IRON ORE. | |
DE3484387D1 (en) | METHOD FOR DEFORMING METAL. | |
AT375402B (en) | METHOD FOR HEAT-TREATING RAILS | |
AT378005B (en) | METHOD FOR DEOXIDATING METAL MELT | |
AT376245B (en) | METHOD FOR SINTERING FINE-GRAINED IRON ORES | |
AT376242B (en) | METHOD FOR MELTING AT LEAST PARTLY REDUCED IRON ORE | |
DE3677122D1 (en) | METHOD FOR MELTING AND DIRECTLY FIXING METALS. | |
DE3580354D1 (en) | METHOD FOR EDITING VIDEO STILL IMAGES. | |
AT377214B (en) | METHOD FOR ELECTROSHELL WELDING | |
DE3360636D1 (en) | Direct reduction method for iron ores | |
DE3861025D1 (en) | METHOD FOR CLEANING METAL MELT. | |
DE3462925D1 (en) | Sulphur removing method during pig iron melting |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
REN | Ceased due to non-payment of the annual fee | ||
ELJ | Ceased due to non-payment of the annual fee |