WO2014201507A1 - Dérivés de lactone homosérine pour améliorer l'extraction des éléments minéraux pendant l'extraction biologique de minerais - Google Patents
Dérivés de lactone homosérine pour améliorer l'extraction des éléments minéraux pendant l'extraction biologique de minerais Download PDFInfo
- Publication number
- WO2014201507A1 WO2014201507A1 PCT/AU2014/000641 AU2014000641W WO2014201507A1 WO 2014201507 A1 WO2014201507 A1 WO 2014201507A1 AU 2014000641 W AU2014000641 W AU 2014000641W WO 2014201507 A1 WO2014201507 A1 WO 2014201507A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- biomining
- composition
- branched
- linear
- alkyl
- Prior art date
Abstract
La présente invention concerne des dérivés de lactone homosérine représentés par la formule (I) utilisés en tant qu'additifs pour l'extraction biologique de minerais. La présente invention concerne des opérations d'extraction biologique de minerais au moyen de l'additif d'extraction biologique de minerai pour améliorer l'extraction des minerais cibles.
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US201361837760P | 2013-06-21 | 2013-06-21 | |
US61/837,760 | 2013-06-21 |
Publications (2)
Publication Number | Publication Date |
---|---|
WO2014201507A1 true WO2014201507A1 (fr) | 2014-12-24 |
WO2014201507A8 WO2014201507A8 (fr) | 2015-06-25 |
Family
ID=52103700
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
PCT/AU2014/000641 WO2014201507A1 (fr) | 2013-06-21 | 2014-06-20 | Dérivés de lactone homosérine pour améliorer l'extraction des éléments minéraux pendant l'extraction biologique de minerais |
Country Status (1)
Country | Link |
---|---|
WO (1) | WO2014201507A1 (fr) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2024081705A1 (fr) * | 2022-10-14 | 2024-04-18 | Basf Se | Compositions de molécules organiques pour la lixiviation de minerai contenant des sulfures métalliques et leurs procédés de préparation et d'utilisation |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2001074801A1 (fr) * | 2000-03-30 | 2001-10-11 | University Of Nottingham | N-acyl homoserine lactones a activite immunosuppressive |
WO2014105679A1 (fr) * | 2012-12-27 | 2014-07-03 | Flsmidth A/S | Compositions et procédés de lixiviation de minerais |
-
2014
- 2014-06-20 WO PCT/AU2014/000641 patent/WO2014201507A1/fr active Application Filing
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2001074801A1 (fr) * | 2000-03-30 | 2001-10-11 | University Of Nottingham | N-acyl homoserine lactones a activite immunosuppressive |
WO2014105679A1 (fr) * | 2012-12-27 | 2014-07-03 | Flsmidth A/S | Compositions et procédés de lixiviation de minerais |
Non-Patent Citations (6)
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2024081705A1 (fr) * | 2022-10-14 | 2024-04-18 | Basf Se | Compositions de molécules organiques pour la lixiviation de minerai contenant des sulfures métalliques et leurs procédés de préparation et d'utilisation |
Also Published As
Publication number | Publication date |
---|---|
WO2014201507A8 (fr) | 2015-06-25 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Brandl et al. | Biomobilization of silver, gold, and platinum from solid waste materials by HCN-forming microorganisms | |
Petersen et al. | Competitive bioleaching of pyrite and chalcopyrite | |
Schippers et al. | Biomining: metal recovery from ores with microorganisms | |
Watling et al. | The resilience and versatility of acidophiles that contribute to the bio‐assisted extraction of metals from mineral sulphides | |
Tipre et al. | Bioleaching process for Cu–Pb–Zn bulk concentrate at high pulp density | |
Ewart et al. | The extraction of metals from ores using bacteria | |
Adams et al. | Biogenic sulphide for cyanide recycle and copper recovery in gold–copper ore processing | |
US8597933B2 (en) | Method of treating a sulphide mineral | |
EP0432935B1 (fr) | Procédé de récupération et reconcentration d'or de ses minerais | |
US5152969A (en) | Processes to recover and reconcentrate gold from its ores with microorganisms | |
Hao et al. | Comparative study on bioleaching of two different types of low-grade copper tailings by mixed moderate thermophiles | |
Jorjani et al. | Gold leaching from ores using biogenic lixiviants–A review | |
Devasia et al. | Bacterial leaching: biotechnology in the mining industry | |
AU2009251040B2 (en) | Method of leaching copper sulfide ore | |
Petersen et al. | Carbon dioxide and oxygen consumption during the bioleaching of a copper ore in a large isothermal column | |
CN103805777B (zh) | 一种强化黄铁矿微生物浸出的方法 | |
Dong et al. | Bioleaching of heavy metals from metal tailings utilizing bacteria and fungi: Mechanisms, strengthen measures, and development prospect | |
Martins et al. | Chalcopyrite bioleaching in chloride media: A mini-review | |
AU2016234208B2 (en) | Method of leaching copper from copper sulfide ore and method of evaluating iodine loss content of column leaching test of the copper sulfide ore | |
US20080207462A1 (en) | DNA fragments array from biomining microorganisms and method for detection of them | |
WO2014201507A1 (fr) | Dérivés de lactone homosérine pour améliorer l'extraction des éléments minéraux pendant l'extraction biologique de minerais | |
JP2013155416A (ja) | 黄銅鉱を含む硫化銅鉱からの銅の浸出方法 | |
JP2012017513A (ja) | 銅の浸出方法 | |
KR101575582B1 (ko) | 미생물을 이용한 시안 생산 및 농축 장치와 이를 이용한 자동차 폐촉매에서 백금족 금속 회수 | |
Norris et al. | Ore column leaching with thermophiles: II, polymetallic sulfide ore |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
121 | Ep: the epo has been informed by wipo that ep was designated in this application |
Ref document number: 14813752 Country of ref document: EP Kind code of ref document: A1 |
|
NENP | Non-entry into the national phase |
Ref country code: DE |
|
122 | Ep: pct application non-entry in european phase |
Ref document number: 14813752 Country of ref document: EP Kind code of ref document: A1 |