WO2014194475A1 - Solder-piercing feed wheel - Google Patents

Solder-piercing feed wheel Download PDF

Info

Publication number
WO2014194475A1
WO2014194475A1 PCT/CN2013/076727 CN2013076727W WO2014194475A1 WO 2014194475 A1 WO2014194475 A1 WO 2014194475A1 CN 2013076727 W CN2013076727 W CN 2013076727W WO 2014194475 A1 WO2014194475 A1 WO 2014194475A1
Authority
WO
WIPO (PCT)
Prior art keywords
blade
solder
wheel
edge
solder wire
Prior art date
Application number
PCT/CN2013/076727
Other languages
French (fr)
Chinese (zh)
Inventor
罗艺
Original Assignee
Luo Yi
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Luo Yi filed Critical Luo Yi
Priority to PCT/CN2013/076727 priority Critical patent/WO2014194475A1/en
Publication of WO2014194475A1 publication Critical patent/WO2014194475A1/en

Abstract

A solder-piercing feed wheel. The solder- piercing feed wheel comprises a blade (10) and clamping wheels (20) capable of clamping the blade (10). The number of the clamping wheels (20) is two. Sawtooth-shaped cutter points (11) are disposed on the rim of the blade (10). The clamping wheels (20) are used to clamp the blade (10) to only allow the cutter points (11) of the blade to be exposed; rigidity of the blade (10) is ensured through the thickness of the clamping wheels (20), and the blade is not bent and cannot easily be distorted. In addition, during work, the cutter points (11) align to the center line of a solder wire, and after the cutter points (11) pierce said solder wire, the edges of the clamping wheels (20) abut against the solder wire, thereby preventing puncture depth of the cutter points (11) piercing the solder wire from exceeding a standard, thus enabling the pierced holes to be connected, and preventing blockage of solder feed passages.

Description

一种破锡刀轮  Broken tin knife wheel 技术领域Technical field
本实用新型属于焊接设备领域,尤其涉及用于焊接的锡丝破锡装置。The utility model belongs to the field of welding equipment, in particular to a tin wire breaking device for welding.
背景技术Background technique
现有技术,在SMT焊接过程中需要对焊锡丝进行破锡,以保证焊锡丝内部高温阻焊剂的压力释放,通常情况下,破锡刀轮采用整体刀片进行破锡,对刀片的刚性要求极高,通常使用日本进口特种钢材制作此类刀片,成本非常高,而且此类刀片虽然刚性满足了,但在长期使用过程中,还是容易发生扭曲,导致刀片在焊锡丝上开孔无法形成直线,如果将刀片的厚度加大后,虽然满足刚性要求,但材料成本,还有加工成本仍然还是加大了,而且加工出来的刀片刀锋超宽会刺破焊锡丝,从而影响锡丝的卷送能力,很容易造成卷送过程中堵死送锡通道。In the prior art, the solder wire needs to be broken in the SMT soldering process to ensure the pressure release of the high temperature solder resist inside the solder wire. Under normal circumstances, the broken tin wheel uses the integral blade to break the tin, and the rigidity of the blade is extremely required. High, usually made of special steel imported from Japan, the cost is very high, and although the blade is rigid, but it is easy to be twisted during long-term use, the blade can not form a straight line in the solder wire. If the thickness of the blade is increased, although the rigidity requirement is met, the material cost and the processing cost are still increased, and the processed blade blade is too wide to pierce the solder wire, thereby affecting the winding ability of the tin wire. It is easy to cause the tin channel to be blocked during the winding process.
技术问题technical problem
本实用新型的目的在于提供一种破锡刀轮,旨在解决现有技术中刀片刚性不足的问题。The purpose of the utility model is to provide a broken tin wheel, which aims to solve the problem of insufficient rigidity of the blade in the prior art.
技术解决方案Technical solution
本实用新型是这样实现的,一种破锡刀轮,所述破锡刀轮包括刀片和可将所述刀片夹紧的夹轮,所述夹轮为两片,所述刀片边缘具有锯齿状刀锋。The utility model is realized as follows, a broken tin cutter wheel, the broken tin cutter wheel comprises a blade and a clamping wheel capable of clamping the blade, the clamping wheel is two pieces, and the edge of the blade has a zigzag shape Blade.
优选地,所述夹轮直径小于所述刀片直径,所述夹轮与所述刀片的直径差小于焊锡丝的直径。Preferably, the pin wheel diameter is smaller than the blade diameter, and the difference between the pin wheel and the blade is smaller than the diameter of the solder wire.
优选地,所述刀片的刀锋呈等腰三角形位于所述刀片的边缘。Preferably, the blade has an isosceles triangle at the edge of the blade.
优选地,所述刀片的刀锋呈直角三角形位于所述刀片的边缘,所述直角三角形的一条边的延长线垂直交汇所述刀片的圆心,所述直角三角形最小锐角向外形成所述刀锋尖锐部。Preferably, the blade has a right-angled triangle at the edge of the blade, and an extension line of one side of the right-angled triangle vertically intersects the center of the blade, and the right-angled triangle has the smallest acute angle to form the sharp edge of the blade outward. .
优选地,所述刀片的刀锋截面呈由单边斜面所形成的尖锐状。Preferably, the blade has a sharp cross section formed by a single bevel.
优选地,所述刀片的刀锋截面呈由双边斜面所形成的尖锐状等腰三角形。Preferably, the blade has a blade cross section that is a sharp isosceles triangle formed by a double bevel.
有益效果Beneficial effect
依借上述技术方案,本实用新型所采用的夹轮夹紧所述刀片只露出所述刀片的刀锋,充分利用夹轮的厚度保证了所述刀片的刚性,不但不会发生折弯也不易发生扭曲变形,工作过程中,所述刀锋对正焊锡丝的中心线,刺入所述焊锡丝后,所述夹轮的边缘抵住所述焊锡丝,防止所述刀锋刺入焊锡丝的深度超标从而使破锡孔连接,避免堵塞送锡通道。According to the above technical solution, the clamping wheel used in the present invention clamps the blade to expose only the blade edge of the blade, and fully utilizes the thickness of the clamping wheel to ensure the rigidity of the blade, which not only does not bend and is not easy to occur. Distorted deformation, during the working process, the blade strikes the center line of the positive solder wire, and after the solder wire is penetrated, the edge of the clamping wheel abuts against the solder wire, preventing the blade from piercing the depth of the solder wire to exceed the standard Connect the broken tin holes to avoid blocking the tin channel.
附图说明DRAWINGS
图1是本实用新型提供的破锡刀轮立体示意图;1 is a perspective view of a broken tin wheel provided by the present invention;
图2是本实用新型提供的刀片立体示意图;2 is a perspective view of a blade provided by the present invention;
图3是本实用新型实施例提供的一种刀片示意图;3 is a schematic view of a blade provided by an embodiment of the present invention;
图4是本实用新型实施例提供的一种刀片示意图;4 is a schematic view of a blade provided by an embodiment of the present invention;
图5是本实用新型实施例提供的一种刀片示意图;Figure 5 is a schematic view of a blade provided by an embodiment of the present invention;
图6是本实用新型实施例提供的一种刀片示意图;Figure 6 is a schematic view of a blade provided by an embodiment of the present invention;
本发明的实施方式Embodiments of the invention
为了使本实用新型的目的、技术方案及优点更加清楚明白,以下结合附图及实施例,对本实用新型进行进一步详细说明。应当理解,此处所描述的具体实施例仅仅用以解释本实用新型,并不用于限定本实用新型。In order to make the objects, technical solutions and advantages of the present invention more comprehensible, the present invention will be further described in detail below with reference to the accompanying drawings and embodiments. It is understood that the specific embodiments described herein are merely illustrative of the invention and are not intended to limit the invention.
参照图1和图2所示,本实施例提供一种破锡刀轮,所述破锡刀轮包括刀片10和可将所述刀片10夹紧的夹轮20,所述夹轮20为两片,所述刀片10边缘具有锯齿状刀锋11,所述夹轮20直径小于所述刀片10直径,所述夹轮20与所述刀片10的直径差小于焊锡丝的直径。依借上述技术方案,本实用新型所采用的夹轮20夹紧所述刀片10只露出所述刀片10的刀锋11,充分利用夹轮20的厚度保证了所述刀片10的刚性,不但不会发生折弯也不易发生扭曲变形,工作过程中,所述刀锋11对正焊锡丝的中心线,刺入所述焊锡丝后,所述夹轮20的边缘抵住所述焊锡丝,防止所述刀锋11刺入焊锡丝的深度超标从而使破锡孔连接,避免堵塞送锡通道。Referring to FIG. 1 and FIG. 2, the embodiment provides a broken tin wheel, the blade includes a blade 10 and a pinch wheel 20 for clamping the blade 10, and the pinch wheel 20 is two. The blade 10 has a serrated blade edge 11 having a diameter smaller than the diameter of the blade 10, and the difference between the diameter of the pinch wheel 20 and the blade 10 is smaller than the diameter of the solder wire. According to the above technical solution, the clamping wheel 20 used in the present invention clamps the blade 10 to expose only the blade edge 11 of the blade 10, and fully utilizes the thickness of the clamping wheel 20 to ensure the rigidity of the blade 10, which will not When the bending occurs, the distortion is not easily generated. During the working process, the blade 11 is aligned with the center line of the positive solder wire. After the solder wire is penetrated, the edge of the clamping wheel 20 abuts against the solder wire to prevent the blade from being broken. 11 The depth of the penetration of the solder wire exceeds the standard, so that the broken tin hole is connected to avoid blocking the tin passage.
参照图3所示,本实施例可选用下述刀片,所述刀片10的刀锋11呈等腰三角形位于所述刀片10的边缘。Referring to FIG. 3, the present embodiment may employ a blade having a blade edge 11 having an isosceles triangle at the edge of the blade 10.
参照图4所示,本实施例可选用下述刀片,所述刀片10的刀锋11呈直角三角形位于所述刀片10的边缘,所述直角三角形的一条边的延长线垂直交汇所述刀片10的圆心,所述直角三角形最小锐角向外形成所述刀锋11尖锐部。Referring to FIG. 4, in this embodiment, a blade 11 having a blade 11 having a right-angled triangle at an edge of the blade 10 and an extension of one side of the right triangle vertically intersecting the blade 10 may be used. The center of the circle, the smallest acute angle of the right triangle forms the sharp portion of the blade 11 outward.
参照图5所示,本实施例可选用下述刀片,所述刀片10的刀锋11截面呈由单边斜面所形成的尖锐状。Referring to Fig. 5, in the present embodiment, a blade having a blade 11 having a sharp cross section formed by a single bevel may be used.
参照图6所示,本实施例可选用下述刀片,所述刀片10的刀锋11截面呈由双边斜面所形成的尖锐状等腰三角形。Referring to Fig. 6, the present embodiment may employ a blade having a blade end 11 having a sharp-shaped isosceles triangle formed by a double bevel.
以上所述仅为本实用新型的较佳实施例而已,并不用以限制本实用新型,凡在本实用新型的精神和原则之内所作的任何修改、等同替换和改进等,均应包含在本实用新型的保护范围之内。The above is only the preferred embodiment of the present invention, and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the present invention. The scope of protection of utility models.

Claims (6)

  1. 一种破锡刀轮,其特征在于,所述破锡刀轮包括刀片和可将所述刀片夹紧的夹轮,所述夹轮为两片,所述刀片边缘具有锯齿状刀锋。 A broken tin wheel includes a blade and a pinch wheel that can clamp the blade, the pin wheel is two pieces, and the blade edge has a serrated blade edge.
  2. 如权利要求1所述的破锡刀轮,其特征在于,所述夹轮直径小于所述刀片直径,所述夹轮与所述刀片的直径差小于焊锡丝的直径。A breaker wheel according to claim 1, wherein said pin wheel diameter is smaller than said blade diameter, and said caliper has a diameter difference from said blade that is smaller than a diameter of said solder wire.
  3. 如权利要求2所述的破锡刀轮,其特征在于,所述刀片的刀锋呈等腰三角形位于所述刀片的边缘。A breaker wheel according to claim 2 wherein the blade has an isosceles triangle at the edge of the blade.
  4. 如权利要求2所述的破锡刀轮,其特征在于,所述刀片的刀锋呈直角三角形位于所述刀片的边缘,所述直角三角形的一条边的延长线垂直交汇所述刀片的圆心,所述直角三角形最小锐角向外形成所述刀锋尖锐部。A tin-breaking wheel according to claim 2, wherein the blade has a right-angled triangle at the edge of the blade, and an extension of one side of the right-angled triangle vertically intersects the center of the blade. The smallest acute angle of the right triangle forms the sharp edge of the blade outward.
  5. 如权利要求2所述的破锡刀轮,其特征在于,所述刀片的刀锋截面呈由单边斜面所形成的尖锐状。A breaker wheel according to claim 2, wherein the blade has a sharp cross section formed by a single bevel.
  6. 如权利要求2所述的破锡刀轮,其特征在于,所述刀片的刀锋截面呈由双边斜面所形成的尖锐状等腰三角形。A breaker wheel according to claim 2, wherein the blade has a sharp cross-section of a sharp isosceles triangle formed by a double bevel.
PCT/CN2013/076727 2013-06-04 2013-06-04 Solder-piercing feed wheel WO2014194475A1 (en)