WO2001031691A1 - Method and apparatus for cleaning a semiconductor wafer - Google Patents
Method and apparatus for cleaning a semiconductor wafer Download PDFInfo
- Publication number
- WO2001031691A1 WO2001031691A1 PCT/US2000/025099 US0025099W WO0131691A1 WO 2001031691 A1 WO2001031691 A1 WO 2001031691A1 US 0025099 W US0025099 W US 0025099W WO 0131691 A1 WO0131691 A1 WO 0131691A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- semiconductor wafer
- recited
- wafer
- chemical
- cleaning
- Prior art date
Abstract
Description
Claims