WO1982004061A1 - Extraction par entrainement d'hydrocarbures a partir d'un catalyseur avec gaz de combustion - Google Patents

Extraction par entrainement d'hydrocarbures a partir d'un catalyseur avec gaz de combustion Download PDF

Info

Publication number
WO1982004061A1
WO1982004061A1 PCT/US1981/000646 US8100646W WO8204061A1 WO 1982004061 A1 WO1982004061 A1 WO 1982004061A1 US 8100646 W US8100646 W US 8100646W WO 8204061 A1 WO8204061 A1 WO 8204061A1
Authority
WO
WIPO (PCT)
Prior art keywords
catalyst
feed
process according
range
coke
Prior art date
Application number
PCT/US1981/000646
Other languages
English (en)
Inventor
Oil Inc Ashland
Original Assignee
Mckay William E Jr
Myers George D
Busch Lloyd E
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mckay William E Jr, Myers George D, Busch Lloyd E filed Critical Mckay William E Jr
Priority to EP19810901645 priority Critical patent/EP0078795A1/fr
Priority to PCT/US1981/000646 priority patent/WO1982004061A1/fr
Publication of WO1982004061A1 publication Critical patent/WO1982004061A1/fr

Abstract

Procede de conversion economique d'huiles carbo-metalliques en produits plus legers. Les huiles carbo-metalliques contiennent un materiau ayant un point d'ebullition superieur a 650 F qui est caracterise par un residu de pyrolyse carbone d'au moins environ 1 et une teneur en metaux lourds d'au moins environ 4 parties par million d'equivalents nickel. Ce procede comprend l'ecoulement de l'huile carbo-metallique avec le catalyseur de craquage particulaire au travers d'un reacteur du type a ecoulement progressif (2) ayant une chambre de reaction allongee laquelle est au moins en partie verticale ou inclinee, pendant une duree predeterminee de maintien a la vapeur dans la colonne montante comprise entre 0,5 et 10 secondes environ, a une temperature comprise entre 900 et 1400 F environ et sous une pression absolue d'environ 10 a environ 50 livres par pouce carre, suffisante pour provoquer une conversion par passe de l'ordre de 50% a 90% environ tout en produisant du coke en quantites de 6 a 14% environ en poids calculees sur le produit d'alimentation frais, et le depot du coke sur le catalyseur en quantites de l'ordre de 0,3 a 3% environ en poids. Le catalyseur use charge de coke provenant du courant d'hydrocarbures forme par l'alimentation et les produits de craquage resultant vaporises est separe, les hydrocarbures ayant subit une sorption sont entraines (8) a partir des particules du catalyseur en les mettant en contact dans un ou plusieurs lits fluidises avec des gaz de combustion chauds. Le catalyseur entraine est regenere dans un ou plusieurs lits de regeneration (27) dans une ou plusieurs zones de regeneration (21) en brulant le coke sur le catalyseur use avec de l'oxygene. Les particules du catalyseur sont retenues dans la ou les zones de regeneration en contact avec le gaz de maintien de la combustion pendant un temps de maintien total moyen dans cette ou ces zones de 5 a 30 minutes environ pour reduire le niveau de carbone sur le catalyseur jusqu'a environ 0,25% en poids ou moins. Le catalyseur regenere est
PCT/US1981/000646 1981-05-13 1981-05-13 Extraction par entrainement d'hydrocarbures a partir d'un catalyseur avec gaz de combustion WO1982004061A1 (fr)

Priority Applications (2)

Application Number Priority Date Filing Date Title
EP19810901645 EP0078795A1 (fr) 1981-05-13 1981-05-13 Extraction par entrainement d'hydrocarbures a partir d'un catalyseur avec gaz de combustion
PCT/US1981/000646 WO1982004061A1 (fr) 1981-05-13 1981-05-13 Extraction par entrainement d'hydrocarbures a partir d'un catalyseur avec gaz de combustion

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
WOUS81/00646810513 1981-05-13
PCT/US1981/000646 WO1982004061A1 (fr) 1981-05-13 1981-05-13 Extraction par entrainement d'hydrocarbures a partir d'un catalyseur avec gaz de combustion

Publications (1)

Publication Number Publication Date
WO1982004061A1 true WO1982004061A1 (fr) 1982-11-25

Family

ID=22161225

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/US1981/000646 WO1982004061A1 (fr) 1981-05-13 1981-05-13 Extraction par entrainement d'hydrocarbures a partir d'un catalyseur avec gaz de combustion

Country Status (2)

Country Link
EP (1) EP0078795A1 (fr)
WO (1) WO1982004061A1 (fr)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
EP0184517A1 (fr) * 1984-12-07 1986-06-11 Compagnie De Raffinage Et De Distribution Total France Perfectionnement aux procédés et dispositifs pour le craquage catalytique de charges d'hydrocarbures
FR2624877A1 (fr) * 1987-12-22 1989-06-23 Inst Francais Du Petrole Procede et dispositif pour le craquage catalytique de charges lourdes comportant un second strippage en lit fluide
FR2627187A1 (fr) * 1988-02-15 1989-08-18 Inst Francais Du Petrole Procede de craquage a l'etat fluide d'une charge d'hydrocarbures
US9074147B2 (en) 2010-06-28 2015-07-07 General Electric Company Method for converting carbon and hydrocarbon cracking and apparatus for hydrocarbon cracking

Citations (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US3008896A (en) * 1959-09-21 1961-11-14 Phillips Petroleum Co Catalytic cracking of residual oils
US3303123A (en) * 1964-10-16 1967-02-07 Phillips Petroleum Co Catalytic cracking of residuum oils containing metal contaminants in several stages
US3658693A (en) * 1969-12-11 1972-04-25 Phillips Petroleum Co Catalytic cracking method
US3821103A (en) * 1973-05-30 1974-06-28 Mobil Oil Corp Conversion of sulfur contaminated hydrocarbons
US3844973A (en) * 1972-05-30 1974-10-29 Universal Oil Prod Co Fluidized catalyst regeneration by oxidation in a dense phase bed and a dilute phase transport riser
US3849291A (en) * 1971-10-05 1974-11-19 Mobil Oil Corp High temperature catalytic cracking with low coke producing crystalline zeolite catalysts
US4066533A (en) * 1975-03-24 1978-01-03 Ashland Oil, Inc. Separation of catalyst from effluent of a fluidized catalytic hydrocarbon conversion process
US4274942A (en) * 1979-04-04 1981-06-23 Engelhard Minerals & Chemicals Corporation Control of emissions in FCC regenerator flue gas
US4276150A (en) * 1979-11-05 1981-06-30 Standard Oil Company (Indiana) Fluid catalytic cracking of heavy petroleum fractions

Patent Citations (9)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US3008896A (en) * 1959-09-21 1961-11-14 Phillips Petroleum Co Catalytic cracking of residual oils
US3303123A (en) * 1964-10-16 1967-02-07 Phillips Petroleum Co Catalytic cracking of residuum oils containing metal contaminants in several stages
US3658693A (en) * 1969-12-11 1972-04-25 Phillips Petroleum Co Catalytic cracking method
US3849291A (en) * 1971-10-05 1974-11-19 Mobil Oil Corp High temperature catalytic cracking with low coke producing crystalline zeolite catalysts
US3844973A (en) * 1972-05-30 1974-10-29 Universal Oil Prod Co Fluidized catalyst regeneration by oxidation in a dense phase bed and a dilute phase transport riser
US3821103A (en) * 1973-05-30 1974-06-28 Mobil Oil Corp Conversion of sulfur contaminated hydrocarbons
US4066533A (en) * 1975-03-24 1978-01-03 Ashland Oil, Inc. Separation of catalyst from effluent of a fluidized catalytic hydrocarbon conversion process
US4274942A (en) * 1979-04-04 1981-06-23 Engelhard Minerals & Chemicals Corporation Control of emissions in FCC regenerator flue gas
US4276150A (en) * 1979-11-05 1981-06-30 Standard Oil Company (Indiana) Fluid catalytic cracking of heavy petroleum fractions

Cited By (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
EP0184517A1 (fr) * 1984-12-07 1986-06-11 Compagnie De Raffinage Et De Distribution Total France Perfectionnement aux procédés et dispositifs pour le craquage catalytique de charges d'hydrocarbures
FR2574422A1 (fr) * 1984-12-07 1986-06-13 Raffinage Cie Francaise Perfectionnements aux procedes et dispositifs pour le craquage catalytique a l'etat fluide de charges d'hydrocarbures
FR2624877A1 (fr) * 1987-12-22 1989-06-23 Inst Francais Du Petrole Procede et dispositif pour le craquage catalytique de charges lourdes comportant un second strippage en lit fluide
EP0322276A1 (fr) * 1987-12-22 1989-06-28 Institut Français du Pétrole Procédé et dispositif pour le craquage catalytique de charges lourdes comportant un second strippage en lit fluide
FR2627187A1 (fr) * 1988-02-15 1989-08-18 Inst Francais Du Petrole Procede de craquage a l'etat fluide d'une charge d'hydrocarbures
GB2215734A (en) * 1988-02-15 1989-09-27 Inst Francais Du Petrole Process for fluid catalytic cracking of a hydrocarbon charge
US9074147B2 (en) 2010-06-28 2015-07-07 General Electric Company Method for converting carbon and hydrocarbon cracking and apparatus for hydrocarbon cracking
US9708545B2 (en) 2010-06-28 2017-07-18 General Electric Company Method for converting carbon and hydrocarbon cracking and apparatus for hydrocarbon cracking

Also Published As

Publication number Publication date
EP0078795A1 (fr) 1983-05-18

Similar Documents

Publication Publication Date Title
US4464250A (en) Stripping hydrocarbons from catalyst with combustion gases
US4299687A (en) Carbo-metallic oil conversion with controlled CO:CO2 ratio in regeneration
US4424116A (en) Converting and stripping heavy hydrocarbons in two stages of riser conversion with regenerated catalyst
US4377470A (en) Immobilization of vanadia deposited on catalytic materials during carbo-metallic oil conversion
US4417975A (en) Addition of water to regeneration air
US4406773A (en) Magnetic separation of high activity catalyst from low activity catalyst
US4384948A (en) Single unit RCC
US4347122A (en) Carbo-metallic oil conversion with liquid water
US4495063A (en) Carbometallic oil conversion with ballistic separation
US4332673A (en) High metal carbo-metallic oil conversion
US4454025A (en) Passivating heavy metals in carbo-metallic oil conversion
US4432864A (en) Carbo-metallic oil conversion with liquid water containing H2 S
US4354923A (en) Carbo-metallic oil conversion with liquid water, ballistic separation and controlled CO:CO2 ratio during catalyst regeneration
US4390503A (en) Carbometallic oil conversion with ballistic separation
EP0066725B1 (fr) Procédé pour le craquage d'hydrocarbures de point d'ébullition élevé à l'aide d'un catalyseur très poreux de basse densité
US4341624A (en) Carbo-metallic oil conversion
US4376038A (en) Use of naphtha as riser diluent in carbo-metallic oil conversion
US4432863A (en) Steam reforming of carbo-metallic oils
US4869879A (en) Vented riser for stripping spent catalyst
US4444651A (en) Carbo-metallic oil conversion with controlled CO:CO2 ratio in multistage regeneration
WO1982004063A1 (fr) Reformage a la vapeur d'huiles carbo-metalliques
US4477335A (en) Separation of regenerated catalyst from combustion products
US4374019A (en) Process for cracking high-boiling hydrocarbons using high ratio of catalyst residence time to vapor residence time
US4390415A (en) High metal carbo-metallic oil conversion using low inventory of catalyst
US4419223A (en) Carbo-metallic oil conversion with water

Legal Events

Date Code Title Description
AK Designated states

Designated state(s): DE GB JP NL US

AL Designated countries for regional patents

Designated state(s): FR

REG Reference to national code

Ref country code: DE

Ref legal event code: 8642