US20020047519A1 - Plasma display panel and method for manufacturing the same - Google Patents
Plasma display panel and method for manufacturing the same Download PDFInfo
- Publication number
- US20020047519A1 US20020047519A1 US09/778,879 US77887901A US2002047519A1 US 20020047519 A1 US20020047519 A1 US 20020047519A1 US 77887901 A US77887901 A US 77887901A US 2002047519 A1 US2002047519 A1 US 2002047519A1
- Authority
- US
- United States
- Prior art keywords
- partition
- pattern
- display panel
- plasma display
- panel according
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
A plasma display panel is provided that has a good productivity of partition formation and air exhaustion process and realizes a bright and stable display. A discharge gas is filled in a gap between two substrates. A mesh-patterned partition is arranged on the inner surface of one of the substrates for dividing the gap into plural squares corresponding to a cell arrangement. The partition has low portions for forming a mesh-like air path that travels all gas-filled space enclosed by the partition in a plan view.
Description
- 1. Field of the Invention
- The present invention relates to a plasma display panel (PDP) having a mesh-patterned partition, each square of which encloses one or more cells for constituting a display surface and a method for manufacturing the PDP.
- A PDP is commercialized for a wall-hung TV set, whose screen size has reached 60 inches. PDP is a digital display device comprising binary light emission cells, so it is suitable for a display of digital data and is expected as a multimedia monitor. In order to increase applications of a PDP, a new panel structure is under development, which can provide a brighter and more stable display and can be manufactured in a high productivity.
- 2. Description of the Prior Art
- An AC type PDP for a color display employs a surface discharge format. The surface discharge format has an arrangement of electrodes in which display electrodes that become anodes and cathodes in a display discharge for ensuring a luminance are arranged in parallel on a front or back substrate, and address electrodes are arranged so as to cross a pair of the display electrodes. In the surface discharge format PDP, a partition is necessary for separating a discharge for each column of a matrix display along the longitudinal direction of the display electrode (hereinafter referred to as the row direction). The partition also works as a spacer for defining a discharge space size in the direction of the panel thickness.
- A partition pattern (a shape of the partition in the plan view) is broadly divided into a stripe pattern and a mesh pattern. The stripe pattern divides the discharge space for cells arranged in the row direction (i.e., in each column). In the stripe pattern, the discharge space of cell included in each column is not separated, so that exhausting of inner air and filling of discharge gas are relatively easy in a manufacturing process of a PDP. The mesh pattern divides the discharge space both in the row direction and in the column direction. A typical mesh pattern is a check pattern. A mesh pattern has an advantage in that the discharge is separated for each cell and that a fluorescent material is arranged on a side face of the partition so as to enclose the cell for increasing a light emission area. The mesh pattern, however, has a disadvantage in that a gap generated by subtle unevenness on the upper surface of the partition becomes an air path in the inner air exhaustion, so a resistance of the air exhaustion is large and it takes a long time for the process.
- Conventionally, a partition structure of an overlaying form of the mesh-patterned partition and the stripe-patterned partition (this is called a composite pattern structure) is known. In this structure, since the discharge space is continuous as in the case of the stripe pattern, the air exhaustion resistance is smaller than in the case where the stripe-patterned partition is not overlaid. Furthermore, an improved composite pattern structure is disclosed in Japanese unexamined patent publication No. 4-274141, in which a stripe-patterned partition is provided with a hiatus for each cell, so that a grid-shaped air path (air exhaustion path) is formed for the gas to flow not only in the column direction but also in the row direction.
- The above-explained partition having the composite pattern structure has a mesh-patterned partition whose banding portion in the column direction or the row direction is raised. There was a problem that the partition forming process becomes complicated for forming the above-mentioned structure on the inner surface of one of the substrate pair. Furthermore, if a mesh-patterned partition is disposed at one of the substrates and if a stripe-patterned partition is disposed on the other partition, the fluorescent material should be arranged on both of the substrates for increasing the area in which the fluorescent material is formed. In addition, a registration of the substrate pair in the assembling process is difficult. Thus, the partition having the composite pattern structure is adverse from the viewpoint of the productivity.
- There is a method of forming the air path by cutting a part of the partition. However, this method may manufacturing steps for the cutting process and may reduce the manufacturing yield since the partition can be broken by the cutting process.
- An object of the present invention is to provide a PDP that has a good productivity of partition formation and air exhaustion process and can display more brightly and more stably than a PDP that has a stripe-patterned partition.
- According to the present invention, a mesh-patterned partition is arranged on the inner surface of one of the substrates. The partition has low portions that form a mesh-like air path that travels all gas-filled space enclosed by the partition in a plan view. For example, in a simple check pattern in which a line along the horizontal direction and a line along the vertical direction cross each other, the portion corresponding to the line along the horizontal direction is made low. In this case, the pattern width (the line width) of the portion corresponding to the line along the horizontal direction is made thicker than the pattern width of the portion corresponding to the line along the vertical direction so as to generate a height difference. The shrink quantity in the thick portion is smaller in the width direction but is larger in the height direction than the thin portion.
- FIG. 1 is a diagram showing a cell structure of a PDP according to the present invention.
- FIG. 2 is a plan view showing the arrangement relationship between the display electrode and the partition.
- FIG. 3 is a plan view showing a partition pattern.
- FIG. 4 is a diagram showing a solid structure of the partition.
- FIG. 5 is a schematic diagram showing heat shrink in the partition forming process.
- FIG. 6 is a diagram showing a baking profile in the partition forming process.
- FIGS. 7, 8A and8B show variations of the partition pattern.
- FIGS.9A-12 show variations of the display electrode pattern.
- Hereinafter, the present invention will be explained in detail with reference to embodiments and accompanied drawings.
- FIG. 1 is a diagram showing a cell structure of a PDP according to the present invention. FIG. 2 is a plan view showing the arrangement relationship between the display electrode and the partition. FIG. 1 is a drawing of an inner structure, which shows a pair of substrate structures being separated from each other.
- The
PDP 1 comprises a pair of substrate structures (a structure including a substrate on which cell elements are arranged) 10, 20, and the display surface ES comprises m×n cells. In each cell, the display electrodes X, Y constituting an electrode pair for generating the display discharge are extending in the row direction (the horizontal direction) of the matrix display, and the address electrodes A are extending in the column direction (the vertical direction). - The display electrodes X, Y are arranged on the inner surface of the
glass substrate 11 of thefront substrate structure 10 as a pair for each row. Herein, the “row” means a set of cells whose positions in the column direction are the same, and the number of the cells is equal to the number of columns (m). Each of the display electrodes X and Y includes a transparentconductive film 41 that forms a surface discharge gap (a discharge slit) and a metal film (a bus conductor) 42 that is overlaid on the edge in the column direction. The display electrodes X, Y are covered with adielectric layer 17 having the thickness of approximately 20-40 μm, and the surface of thedielectric layer 17 is coated with aprotection film 18 made of magnesia (MgO). The electrode gap between rows (that is called a reverse slit) is provided with adark color layer 65 that is called a black stripe by applying a paint on the outer surface of theglass substrate 11 or by forming a colored glass layer including fillers such as manganese, iron oxide, chromium and other colorant so as to increase contrast (see FIG. 2). - The address electrodes A are arranged on the inner surface of the
glass substrate 21 of theback substrate structure 20 as one for each column and are covered with adielectric layer 24. On thedielectric layer 24, thepartition 29 is disposed, which has a grid pattern with partially low profile structure that is unique to the present invention. Thepartition 29 is made of a baked material of a low melting point glass and includes a portion for dividing the discharge space into columns (hereinafter referred to as a vertical wall) 291 and a portion for dividing a discharge space into rows (hereinafter referred to as a horizontal wall) 292. The intersection of thevertical wall 291 and thehorizontal wall 292 is a common part of them. Thehorizontal wall 292 is lower than thevertical wall 291 by approximately 10 ì m. The upper surface of thedielectric layer 24 and the side face of thepartition 29 are covered with red, green and blue colors offluorescent material layers - As shown in FIG. 2, the
metal film 42 of each of the display electrodes X, Y is overlaid on thepartition 29 so as to avoid shading and to blind thepartition 29 partially for reducing reflection of external light rays. The transparentconductive film 41 is patterned in such a way that the portion for the surface discharge is substantially separated from the portion overlaid on themetal film 42, for suppressing discharge current so as to enhance the efficiency of light emission. In the case of 42 inch wide VGA type, the portion for the display discharge of the transparentconductive film 41 is separated from thehorizontal wall 292 by a distance more than 30 ì m, so that energy loss is largely reduced compared with the case where the distance is less than 30 ì m. It is desirable that the distance between thehorizontal wall 292 and the transparentconductive film 41 is set so that the discharge current is reduced by more than 5%. - The
PDP 1 having the above-mentioned structure can be manufactured by the following process. - (1) Providing the
glass substrates substrate structures - (2) Overlaying the
substrate structures - (3) Exhausting the inner air and filling the discharge gas through an air hole that is formed in the
back substrate structure 20. - (4) Closing the air hole.
- FIG. 3 is a plan view showing a partition pattern. FIG. 4 is a diagram showing a solid structure of the partition.
- As shown in FIG. 3, the partition pattern is a grid pattern in which each square of the grid pattern encloses a cell C individually. However, it is not a simple check pattern. Namely, the inter-row portion293 (the portion between the cells aligned in the column direction) of the
partition 29 includes twohorizontal walls 292 and a part of thevertical wall 291. The plan view pattern of theinter-row portion 293 is made a ladder pattern, and aspace 33 is formed between the gas-filledspace 32 that corresponds to each of the cells C aligned in the column direction. Since the dielectric constant of the discharge gas is approximately one eighth of that of a low melting point glass that is a common material of the partition, capacitance between the display electrodes of the neighboring rows is reduced, so that a waste of power consumption can be reduced and response of drive control can be improved. In the check pattern, the side face of thevertical wall 291 and the side face of thehorizontal wall 292 respectively are provided with a fluorescent material, so that the light emission area is enlarged and the light emission efficiency can be improved. - In the
PDP 1 of this embodiment, theinter-row portion 293 of thepartition 29 is made approximately 10 μm lower than other portions, thereby forming an air exhaustion path 90 that has a grid shape in the plan view for enabling air exhaustion both in the column direction and in the row direction. The width W20 of theinter-row portion 293 is substantially large, and the air exhaustion conductance is substantially the same as the stripe pattern. Concrete dimension of thepartition 29 is as follows. - row pitch P1: 1080 μm
- column pitch P2: 360 μm
- width W11 of the upper surface of the vertical wall 291: approximately 70 μm
- width W12 of the bottom surface of the vertical wall 291: approximately 140 μm
- height H1 of the vertical wall 291: approximately 140 μm
- width W21 of the upper surface of the horizontal wall 292: approximately 100 μm
- width W22 of the bottom surface of the horizontal wall 292: approximately 200 μm
- height H2 of the horizontal wall 292: approximately 130 μm
- column direction size D11 of the space 32: approximately 680 μm
- row direction size D22 of the space 32: approximately 290 μm
- column direction size D12 of the space 33: approximately 200 μm
- width W20 of the inter-row portion 293: approximately 400 μm
- It is important that the width W20 of the
inter-row portion 293 is substantially larger than the width W11 of thevertical wall 291, so that the difference between the widths makes a height difference between theinter-row portion 293 and other portions. Namely, in a baking process of a material such as a general low melting point glass having a heat shrink property, as shown schematically in FIG. 5, the shrink quantity in the height direction depends on the width of the pattern. The shrink can be generated both in the width direction and in the height direction as a whole in theportion 29A having a small pattern width. In contrast, in theportion 29B having a large pattern width, the shirk in the width direction is suppressed more at the portion closer to the center in width direction, so that the shrink is generated more in the height direction compensating the suppression in the width direction. Therefore, thethick portion 29B becomes lower than thethin portion 29A. In addition, an isotropic shrink occurs in the upper portion of the wall material layer since the shrink can easily occur in any direction, while the shrink in the direction of the substrate surface is suppressed in the bottom portion due to the bond of the substrate. Therefore, the shrink quantity in the height direction becomes larger than the shrink quantity in the direction of the substrate surface. Namely, even if the width of the upper surface is substantially uniform before baking, and if the widths of the bottom surface are different, the height after baking of the material layer having larger width of the bottom surface becomes lower than the material layer having smaller width of the bottom surface. Considering this fact, the pattern width of the partition is defined as the dimension at the position whose distance from the bottom surface is 10% of the height in this specification. It is desirable that the pattern width of the thick portion is set more than 130% of the pattern width of the thin portion so that a difference of height is generated that is sufficient for air exhaustion. In the case of the above-mentioned partition size, twohorizontal walls 292 and the portion between them (a part of the vertical wall 291) are shrunk in the same way in the height direction, and apartition 29 is obtained that has twointer-row portions 293 having low profile as a whole in theinter-row portion 293 of the ladder pattern. - The composition of the low melting point glass that is a material of the
partition 29 is shown in Table 1.TABLE 1 Composition of the low melting point glass Components Content (wt %) PbO 50-60 B2O3 5-10 SiO2 10-20 Al2O3 15-25 CaO −5 - Concerning optical characteristics of the
partition 29, it is desirable that it is semitransparent having the absorptance of visual light at approximately 80% per 30 ì m of film thickness. If it is semitransparent, light rays generated at the vicinity of the top of the partition pass the partition and contribute to improvement of the luminance, while external rays that entered the partition are reflected by the bottom surface of the partition and are absorbed by the partition before reaching the front surface. Therefore, a display having a good contrast can be realized. - The process of forming the
partition 29 is as follows. - (1) Forming the partition material layer having the thickness of approximately 200 μm made of a uniform paste mixture of a low melting point glass powder having the components shown in Table 1 and a vehicle so as to cover the
dielectric layer 24. The partition material layer may be formed by any method such as a screen printing method, a laminating method in which a green sheet is transferred, or other method. - (2) Drying the partition material layer, and then sticking a photosensitive dry film (or a resist material is applied), and forming a cut mask of the grid pattern corresponding to the
partition 29 by using a photolithography including exposure and development. The mask pattern size is set larger that the desired partition size considering the heat shrink quantity. - (3) Grinding the non-masking portion of the partition material layer by a sandblaster until the
dielectric layer 24 is exposed (the partition material layer is patterned). - (4) Performing heating process according to the baking profile shown in FIG. 6 to bake the partition material layer so that the
partition 29 is formed. - FIGS. 7, 8A and8B show variations of the partition pattern.
- The
partition 29 b shown in FIG. 7 includes avertical wall 291 and ahorizontal wall 292 b. Thepartition 29 b corresponds to such that theinter-row portion 293 of thepartition 29 shown in FIG. 3 is replaced with thehorizontal wall 292 b. Thepartition 29 c shown in FIG. 8A includes avertical wall 291 c and ahorizontal wall 292 c. The pattern thereof in a plan view is a mesh pattern in which the positions of cells of the neighboring rows are shifted by a half pitch from each other. In thepartition 29 c, the pattern width of thehorizontal wall 292 c is set larger than the pattern width of thevertical wall 291 c, so that thehorizontal wall 292 c is lower than thevertical wall 291 c, and a mesh-like air exhaustion path 90 c is formed. Thepartition 29 d shown in FIG. 8B includes avertical wall 291 d and ahorizontal wall 292 d, and the pattern thereof in a plan view is a honeycomb mesh pattern. In thepartition 29 d, too, the pattern width of the zigzag bandinghorizontal wall 292 d is set larger than the pattern width of thevertical wall 291 d, so that thehorizontal wall 292 d is lower than thevertical wall 291 d, and a mesh-like air exhaustion path 90 d is formed. In a PDP having thepartitions vertical walls horizontal walls - FIGS.9A-12 show variations of the display electrode pattern.
- Each of the display electrodes Xb and Yb shown in FIG. 9A includes a transparent
conductive film 41 b and ametal film 42 b and corresponds to such display electrodes wherein the pattern of the transparentconductive film 41 of the display electrodes X, Y shown in FIG. 2 is changed. In the display electrodes Xb and Yb, the portion of the transparentconductive film 41 to be a discharge surface is connected to the portion that is overlaid on themetal film 42 b at the position where it is not overlaid on the vertical wall of thepartition 29. Each of the display electrodes Xc and Yc shown in FIG. 9B includes a transparentconductive film 41 c and ametal film 42 c. Themetal film 42 c is arranged at the position where it is not overlaid on the horizontal wall of thepartition 29. In the display electrodes Xd and Yd shown in FIG. 10A, the portion of the transparentconductive film 41 d that forms the surface discharge gap to be the discharge surface is divided into columns to be a T-shape. The portion of the transparentconductive film 41 d that is overlaid on themetal film 42 b is straddling over plural columns. Each of the display electrodes Xe and Ye shown in FIG. 10B includes a T-shaped transparentconductive film 41 e that is divided for each column and ametal film 42 b for supplying electricity to the transparent conductive film. The structures of FIGS. 10A and 10B in which the transparent conductive film is divided are effective for suppressing a discharge current and for reducing a capacitance between electrodes. - In the example shown in FIG. 11 and in the example shown in FIG. 12, a bus conductor is provided for hiding the reverse slit, so that the process of forming the black stripe can be omitted. In FIGS. 11 and 12, the
partition 29 e includes avertical wall 291 and ahorizontal wall 292 e and corresponds to such partition wherein theinter-row portion 293 of thepartition 29 shown in FIG. 3 is replaced with threehorizontal walls 292 e. However, the following electrode structure can be applied both to thepartition 29 shown in FIG. 2 and to thepartition 29 b shown in FIG. 7. - In FIG. 11, each of the display electrodes Xf and Yf includes a transparent
conductive film 41 f and ametal film 42 d and is arranged so that the neighboring electrodes of the neighboring rows are the same kind (e.g., in the order of X, Y, Y, X, X, Y, . . . ). The transparentconductive film 41 f is patterned in the same way as the transparentconductive film 41 b shown in FIG. 9A except for the size of the portion that is overlaid on themetal film 42 d. The display electrodes Xf and Yf have a feature in that themetal film 42 d as a bus conductor has a large width over two neighboringhorizontal walls 292 e. Since an element close to the display surface is drawn at the upper in the figure, a part of themetal film 42 d is covered with the transparentconductive film 41 f. However, actually in the observation from the display surface side, themetal film 42 d can be seen through the transparentconductive film 41 f. Namely, theentire metal film 42 d works as a shading member for hiding the structure thereunder. Therefore, it is not necessary to provide another shading member (a black stripe) to the inter-row portion (the reverse slit), so that the manufacturing steps of a PDP can be reduced. In addition, since the width of themetal film 42 d is enlarged, a line resistance of each of the display electrodes Xf and Yf decreases. Thus, the generation of Joule heat can be reduced, and the voltage drop is also reduced when the discharge current flows. - In FIG. 12, each of the display electrodes Xg and Yg includes a transparent
conductive film 41 g and ametal film 42 e and three display electrodes are arranged for two rows so that a display electrode is shared by two neighboring rows for display (in the order of X, Y, X, Y, . . . ). Themetal film 42 e of the display electrodes Xg and Yg have a large width over three neighboringhorizontal walls 292 e. The example of FIG. 12 has the same advantage as the example of FIG. 11 in that the manufacturing steps can be reduced, and that the line resistance can be reduced. - In the above-mentioned embodiment, the dimension and the material of the
partition 29 are not limited to the examples. The plan-view pattern of thepartitions - According to the present invention, a PDP that has a good productivity of partition formation and air exhaustion process and can display more brightly and more stably than a PDP that has a stripe-patterned partition can be realized.
- While the presently preferred embodiments of the present invention have been shown and described, it will be understood that the present invention is not limited thereto, and that various changes and modifications may be made by those skilled in the art without departing from the scope of the invention as set forth in the appended claims.
Claims (11)
1. A plasma display panel comprising:
a pair of substrates;
a discharge gas being filled in a gap between the substrates; and
a mesh-patterned partition arranged on the inner surface of one of the substrates for dividing the gap into plural squares corresponding to a cell arrangement, wherein the partition is a structure having low portions lowered for forming a mesh-like air path that travels all gas-filled space enclosed by the partition in a plan view.
2. The plasma display panel according to claim 1 , wherein the difference between the heights of the upper surface of the partition is more than 5% of the maximum height.
3. The plasma display panel according to claim 1 , wherein the difference between the heights of the upper surface of the partition is more than 10 μm.
4. The plasma display panel according to claim 1 , wherein a fluorescent material is arranged on the row direction side and the column direction side of the partition in each cell that constitutes the display surface.
5. The plasma display panel according to claim 1 , wherein the plan view pattern of the partition is a check pattern that divides the gap into cells in the row direction and in the column direction of the matrix display and an inter-row portion of the partition that is a boundary wall between rows is lower than other portions.
6. The plasma display panel according to claim 5 , wherein the inter-row portion has a plan view pattern enclosing at least one space for each column.
7. The plasma display panel according to claim 6 , wherein the plan view pattern of the inter-row portion is a ladder pattern.
8. The plasma display panel according to claim 5 , wherein the partition is arranged on the back substrate, an electrode including a transparent conductive film and a metal film straddling over all columns is arranged on the front substrate, and the metal film and the inter-row portion are overlaid in the plan view.
9. The plasma display panel according to claim 1 , wherein the partition is a baked material having a heat shrink property, and the width of the low portions of the partition is wider than that of the other portion of the partition.
10. A method for manufacturing a plasma display panel according to claim 1 , the method comprising the steps of:
forming a layer made of a partition material having a heat shrink property on a substrate;
patterning the layer to be a mesh pattern having a large pattern width portion at the ring-shaped pattern enclosing a cell in the plan view; and
forming the partition by baking the patterned layer.
11. The method according to claim 10 , wherein the patterning step includes the steps of placing a cutting mask corresponding to the mesh pattern on the layer, and cutting non-masked portions of the layer by sandblasting.