Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Национальный Лесотехнический Университет УкраиныfiledCriticalНациональный Лесотехнический Университет Украины
Priority to UAU201008596UpriorityCriticalpatent/UA55928U/en
Publication of UA55928UpublicationCriticalpatent/UA55928U/en
Veneer Processing And Manufacture Of Plywood
(AREA)
Chemical And Physical Treatments For Wood And The Like
(AREA)
Abstract
A method of gluing veneer of high moisture content includes operations of veneer manufacturing, veneer drying, preparation of a glue, application of the glue on veneer, forming and pressing packs of veneer, gluing the veneer packs. Veneer is dried up to certain humidity. During preparation of the glue to phenol formaldehyde resin as a modifying additive phenol resorcin resin is added. Gluing the veneer packs is carried out under certain pressure and temperature.
UAU201008596U2010-07-092010-07-09Method of gluing veneer of high moisture content