UA40445U - СПОСОБ ПОЛУЧЕНИЯ ТЕЛЛУРИДА ГЕРМАНИЯ р-ТИПА - Google Patents

СПОСОБ ПОЛУЧЕНИЯ ТЕЛЛУРИДА ГЕРМАНИЯ р-ТИПА Download PDF

Info

Publication number
UA40445U
UA40445U UAU200812785U UAU200812785U UA40445U UA 40445 U UA40445 U UA 40445U UA U200812785 U UAU200812785 U UA U200812785U UA U200812785 U UAU200812785 U UA U200812785U UA 40445 U UA40445 U UA 40445U
Authority
UA
Ukraine
Prior art keywords
tyre
temperature
ampoule
germanium telluride
obtaining
Prior art date
Application number
UAU200812785U
Other languages
English (en)
Ukrainian (uk)
Inventor
Дмитрий Михайлович Фрейк
Любовь Дмитриевна Юрчишин
Любовь Иосифовна Межиловская
Original Assignee
Прикарпатский Национальный Университет Имени Василия Стефаника
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Прикарпатский Национальный Университет Имени Василия Стефаника filed Critical Прикарпатский Национальный Университет Имени Василия Стефаника
Priority to UAU200812785U priority Critical patent/UA40445U/ru
Publication of UA40445U publication Critical patent/UA40445U/ru

Abstract

Способ получения теллурида германия р-типа состоит в том, что выходные вещества располагают в кварцевой вакуумной ампуле и помещают в печь, температура которой выше температуры плавления выходных компонентов, ампулу с выходными веществами выдерживают при этой температуре. Ампулу охлаждают до комнатной температуры. Полученные слитки дробят и прессуют. В качестве выходного вещества используют высокочистые германий, теллур, серебро, свинец и висмут.
UAU200812785U 2008-10-31 2008-10-31 СПОСОБ ПОЛУЧЕНИЯ ТЕЛЛУРИДА ГЕРМАНИЯ р-ТИПА UA40445U (ru)

Priority Applications (1)

Application Number Priority Date Filing Date Title
UAU200812785U UA40445U (ru) 2008-10-31 2008-10-31 СПОСОБ ПОЛУЧЕНИЯ ТЕЛЛУРИДА ГЕРМАНИЯ р-ТИПА

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
UAU200812785U UA40445U (ru) 2008-10-31 2008-10-31 СПОСОБ ПОЛУЧЕНИЯ ТЕЛЛУРИДА ГЕРМАНИЯ р-ТИПА

Publications (1)

Publication Number Publication Date
UA40445U true UA40445U (ru) 2009-04-10

Family

ID=50619800

Family Applications (1)

Application Number Title Priority Date Filing Date
UAU200812785U UA40445U (ru) 2008-10-31 2008-10-31 СПОСОБ ПОЛУЧЕНИЯ ТЕЛЛУРИДА ГЕРМАНИЯ р-ТИПА

Country Status (1)

Country Link
UA (1) UA40445U (ru)

Similar Documents

Publication Publication Date Title
WO2011112994A3 (en) Thermoelectric figure of merit enhancement by modification of the electronic density of states
WO2010105163A3 (en) High energy-density radioisotope micro power sources
WO2012154200A3 (en) Self-tuning of carrier concentration for high thermoelectric performance
WO2013165514A3 (en) Membrane-supported, thermoelectric compositions
IL210743A0 (en) Crystalline silicon pv cell with selective emitter produced with low temperature precision etch back and passivation process
WO2012138979A3 (en) Thermoelectric materials and methods for synthesis thereof
WO2012165855A3 (en) Method of development for the enhancement of thermoelectric efficiency of thermoelectric material through annealing process
WO2012026775A3 (en) Thermoelectric material, and thermoelectric module and thermoelectric device comprising the thermoelectric material
UA40445U (ru) СПОСОБ ПОЛУЧЕНИЯ ТЕЛЛУРИДА ГЕРМАНИЯ р-ТИПА
UA40444U (ru) СПОСОБ ПОЛУЧЕНИЯ ТЕЛЛУРИДА ОЛОВА р-ТИПА
UA36477U (ru) СПОСоБ получения ТЕРМОэлектрического ТЕЛлУРИДа ГЕРМАНия Р-ТИПа
UA51831U (ru) Способ получения термоэлектрического теллурида свинца
EP2541616A4 (en) METHOD FOR MANUFACTURING SOLAR CELL USING SILICON POWDER
UA36476U (ru) СПОСОБ ПОЛУЧЕНИЯ ТЕРМОЭЛЕКТРИЧЕСКОГО ТЕЛлУРИДа ОЛОВА
UA57333U (ru) СПОСОБ ПОЛУЧЕНИЯ ТЕРМОЭЛЕКТРИЧЕСКОГО PACTBOPA p-PbSnTe
UA39123U (ru) Способ получения теллурида свинца n-типа с улучшенными термоэлектрическими параметрами
UA27517U (en) Method for producing lead telluride-based thermoelectric material
UA36475U (ru) Способ получения термоэлектрического теллурида свинца n-типа
UA63536U (ru) СПОСОБ ПОЛУЧЕНИЯ ЛЕГИРОВАННЫХ СПЛАВОВ PbTe:Bi n-ТИПА
UA102227U (ru) СПОСОБ ПОЛУЧЕНИЯ НАНОКОМПОЗИТА PbTe:ZnO С НЕЗНАЧИТЕЛЬНОЙ ТЕПЛОПРОВОДНОСТЬЮ
UA40443U (ru) СПОСОБ ПОЛУЧЕНИЯ ТЕЛЛУРИДА СВИНЦА n-ТИПА
UA80800U (ru) СПОСОБ ПОЛУЧЕНИЯ СТАБИЛЬНОГО ТЕРМОЭЛЕКТРИЧЕСКОГО n-PbTe:Sb ЭЛЕМЕНТА
UA50778U (ru) СПОСОБ ПОЛУЧЕНИЯ термоэлектрического материала на основе твердых растворов PbTe-Sb2Те3
UA44461U (ru) Способ получения термоэлектрических сплавов на основе теллурида олова, свинца и германия
UA80799U (ru) Способ получения легированного термоэлектрического теллурида свинца