UA112095C2 - THERMAL INSULATION ARBOLITE MIXTURE - Google Patents
THERMAL INSULATION ARBOLITE MIXTUREInfo
- Publication number
- UA112095C2 UA112095C2 UAA201407592A UAA201407592A UA112095C2 UA 112095 C2 UA112095 C2 UA 112095C2 UA A201407592 A UAA201407592 A UA A201407592A UA A201407592 A UAA201407592 A UA A201407592A UA 112095 C2 UA112095 C2 UA 112095C2
- Authority
- UA
- Ukraine
- Prior art keywords
- thermal insulation
- portland cement
- arbolite
- fire
- liquid glass
- Prior art date
Abstract
Винахід належить до будівельної галузі і призначений для виготовлення теплоізоляційних виробів, таких як плити, блоки, монолітні ділянки стін і підлог та ін. Арболітова теплоізоляційна суміш, яка містить костру коноплі і комплексне в'яжуче, відповідно до винаходу як комплексне в'яжуче містить рідке скло і портландцемент при такому співвідношенні компонентів, мас. %: костра коноплі - 14,6-18,1; рідке скло - 65,9-69,9; портландцемент - 12,0-19,5. Винахід дозволяє одночасно підвищити міцність на стиск і згин, знизити коефіцієнт теплопровідності і час витримки до розпалубки.The invention relates to the field of construction and is intended for the manufacture of thermal insulation products such as slabs, blocks, monolithic sections of walls and floors, etc. Arbolite thermal insulation mixture containing hemp fire and complex binder, according to the invention as a complex binder contains liquid glass and Portland cement at this ratio, wt. %: cannabis fire - 14.6-18.1; liquid glass - 65,9-69,9; Portland cement - 12.0-19.5. EFFECT: invention makes it possible to simultaneously increase the compressive and flexural strength, to reduce the thermal conductivity factor and the holding time to detachment.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
UAA201407592A UA112095C2 (en) | 2014-07-07 | 2014-07-07 | THERMAL INSULATION ARBOLITE MIXTURE |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
UAA201407592A UA112095C2 (en) | 2014-07-07 | 2014-07-07 | THERMAL INSULATION ARBOLITE MIXTURE |
Publications (1)
Publication Number | Publication Date |
---|---|
UA112095C2 true UA112095C2 (en) | 2016-07-25 |
Family
ID=56562775
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
UAA201407592A UA112095C2 (en) | 2014-07-07 | 2014-07-07 | THERMAL INSULATION ARBOLITE MIXTURE |
Country Status (1)
Country | Link |
---|---|
UA (1) | UA112095C2 (en) |
-
2014
- 2014-07-07 UA UAA201407592A patent/UA112095C2/en unknown
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EA201391163A1 (en) | DEPUTY CLINKER ON THE BASIS OF THE BLENDED CLAY | |
EA201400102A1 (en) | FIRE-PROTECTIVE CONSTRUCTION SOLUTION | |
EA201791879A1 (en) | COMPOSITE MATERIALS AND CONNECTING ELEMENTS OBTAINED BY CARBONIZATION OF CALCIUM SILICATE AND METHODS OF THEIR RECEIVING AND APPLICATION | |
MY182724A (en) | Concrete materials with modified rheology, methods of making, and uses thereof | |
SG2013096268A (en) | Gypsum-containing construction material compounds | |
BR112014011128A2 (en) | method of manufacturing cement-based material, structure or object | |
UY37648A (en) | CONCRETE, A DRY MIX FOR YOUR PREPARATION, AND A PROCEDURE FOR YOUR PREPARATION | |
GB2538004A (en) | High-alumina refractory aluminosilicate pozzolan in well cementing | |
EA201700287A1 (en) | MIXTURE OF BUILDING MATERIALS | |
EA201891082A1 (en) | SUPPLEMENT FOR BUILDING MATERIALS FROM PLASTER | |
MX363912B (en) | Cement compositions and methods of using the same. | |
UA112095C2 (en) | THERMAL INSULATION ARBOLITE MIXTURE | |
EA202190192A1 (en) | GLASS HOLLOW SPHERICAL PARTICLES | |
PL407916A1 (en) | Cement for applications in low temperatures | |
EA201400864A1 (en) | RAW MIXTURE FOR PRODUCING FOAM CONCRETE | |
EA201500716A1 (en) | CERAMIC MASS FOR THE MANUFACTURING OF A CLINKER BRICK | |
MY172142A (en) | Construction materials and compositions containing same | |
TH169382B (en) | Mortar formulation for structural finishing putty with eggshell structures. | |
UA107436U (en) | CONCRETE MIXTURE FOR PAVEMENT TILES AND Paving | |
GB201720347D0 (en) | Compositions and method to improve the durability of calcium silicate-based cements and concretes | |
UA91933C2 (en) | Additive to cement mixtures | |
TH169382A (en) | Mortar formulation for structural finishing putty with eggshell structures. | |
PL408107A1 (en) | Fireproof concrete mixture | |
EA201700322A1 (en) | RAW MIXTURE FOR THE MANUFACTURE OF HEAT-INSULATING MATERIAL | |
PL415472A1 (en) | Building material with admixture of floatation waste and method for obtaining it |