The process of delignification of cellulose material to produce semi-finished fibrous products includes introduction to the boiling unit of chaff and boiling solution, followed by chaff boiling at given modes. Rape chaff boiling is carried out at a temperature of 175 ° C for 150 minutes, with total consumption of 16% of alkali in Na2O units by weight of abs. dry raw material with boiling solution containing soda ash, sodium hydroxide and an anthraquinone catalyst.
UAU201500935U2015-02-062015-02-06METHOD for DELIGNIFICATION of CELLULOSe MATERIAL
UA100155U
(en)
Dehydration process of avocado (persea americana l) through the lyophilization method for obtaining products in pieces of its pulp and powder of its embryo and uses thereof.