TWM526952U - Thin type energy-saving translucent panel - Google Patents

Thin type energy-saving translucent panel Download PDF

Info

Publication number
TWM526952U
TWM526952U TW105207347U TW105207347U TWM526952U TW M526952 U TWM526952 U TW M526952U TW 105207347 U TW105207347 U TW 105207347U TW 105207347 U TW105207347 U TW 105207347U TW M526952 U TWM526952 U TW M526952U
Authority
TW
Taiwan
Prior art keywords
transmitting plate
energy
saving light
plate according
thin
Prior art date
Application number
TW105207347U
Other languages
Chinese (zh)
Inventor
jia-wei Zhang
Original Assignee
Oriental Green Energy Technology Inc
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Oriental Green Energy Technology Inc filed Critical Oriental Green Energy Technology Inc
Priority to TW105207347U priority Critical patent/TWM526952U/en
Publication of TWM526952U publication Critical patent/TWM526952U/en

Description

薄型節能透光板Thin energy-saving light-transmissive plate

本創作有關於一種薄型節能透光板,尤指一種可薄化膠合玻璃體積之薄型節能透光板。The present invention relates to a thin energy-saving light-transmitting plate, especially a thin energy-saving light-transmitting plate capable of thinning the volume of glued glass.

近年來工業的快速發展造成全球暖化,各地均溫日漸上升,使得空調使用率大幅提高,然而但空調所消耗的能源非常高,大量的發電終究導致進一步的環境汙染,因此,如何在永續發展與環境保護之間取得平衡一直是各國相當熱議之課題。In recent years, the rapid development of industry has caused global warming, and the temperature in all regions has been rising day by day, which has greatly increased the utilization rate of air conditioners. However, the energy consumed by air conditioners is very high, and a large amount of power generation eventually leads to further environmental pollution. Therefore, how to be sustainable A balance between development and environmental protection has always been a hot topic for all countries.

其中一種解決途徑,即是在建築物的採用具備隔熱功效之玻璃,藉以提高熱能傳遞阻抗,部份節能玻璃中設有高分子薄膜,而可反射太陽光線中的紅外線或紫外線,藉此降低室內的熱能,進而降低使用空調的頻率,同時保護人體不受紫外線傷害。習用具可抗紫外線膜體之玻璃結構由於側邊須要施加封邊保護,以避免高分子薄膜在長期的使用下因高溫、濕氣以及與外部空氣接觸種種因素,使膜體產生黃化變色等現象導致降低其吸收光線之效率,及防止變色的玻璃影響建築物之整體外觀。一般的膠合玻璃封邊保護方法,是在一片玻璃上預設一個環狀的膠墊,並將薄膜放在膠墊中央處,再將另一片玻璃蓋合後以結構膠封合兩塊玻璃與膠墊之間的縫隙,然而,此種方是最大的問題在於,膠墊本身需有一定厚度,方能支撐兩塊玻璃的重量而不被壓扁變型,但提高膠墊厚度又將使節能玻璃體積增加,降低了成品規格上的泛用性。是以,先前技術實有改進之必要。One of the solutions is to use a heat-insulating glass in the building to increase the heat transfer resistance. Some energy-saving glass is provided with a polymer film that reflects infrared or ultraviolet light in the sun's rays. The indoor heat energy, which in turn reduces the frequency of air conditioning, while protecting the human body from UV rays. The glass structure of the UV-resistant film body is required to be edge-sealed to protect the side of the polymer film from yellowing, discoloration, etc. due to various factors such as high temperature, moisture and contact with outside air during long-term use. Phenomenon results in reduced efficiency of light absorption and the prevention of discoloration of the glass affecting the overall appearance of the building. The general method for protecting the edge of the glued glass is to preset a ring of rubber on a piece of glass, and place the film in the center of the pad, and then cover the other piece of glass and seal the two pieces of glass with structural glue. The gap between the pads, however, the biggest problem with this type is that the pad itself needs to have a certain thickness to support the weight of the two pieces of glass without being crushed and deformed, but increasing the thickness of the pad will save energy. The increased volume of the glass reduces the versatility of the finished product specification. Therefore, the prior art has been improved.

本創作之目的,在於解決習用節能玻璃的抗紫外線膜體耐候性差而容易產生黃化,以及無法薄型化等問題。The purpose of this creation is to solve the problem that the ultraviolet-resistant film body of the conventional energy-saving glass is poor in weather resistance, is likely to be yellowed, and cannot be thinned.

為達上述目的,本創作提供一種薄型節能透光板,包含有一透光單元、以及一隔絕單元。該透光單元包含有一具黏性的功能薄膜,二分別設置於該功能薄膜兩側的透光基板,以及一環繞在該功能薄膜周圍並位於每一該透光基板之間的容置空間。該隔絕單元包含有一灌注在該容置空間中的第一膠體,以及一由該第一膠體與每一該透光基板的邊緣共同構成的外環面。In order to achieve the above object, the present invention provides a thin energy-saving light-transmitting plate comprising a light-transmitting unit and an insulating unit. The light transmissive unit comprises a viscous functional film, two transparent substrates disposed on opposite sides of the functional film, and an accommodating space surrounding the functional film and located between each of the transparent substrates. The insulating unit includes a first colloid filled in the accommodating space, and an outer annular surface formed by the first colloid and the edge of each of the transparent substrates.

進一步地,該隔絕單元包含有一環繞該外環面設置的第二膠體。Further, the insulation unit includes a second gel disposed around the outer ring surface.

進一步地,該第一膠體係為丁基膠,該第二膠體係為矽力康膠。Further, the first gum system is butyl rubber, and the second gum system is piricon glue.

進一步地,該第一膠體亦可包含有三元乙烯丙烯橡膠(Ethylene propylene diene monomer, EPDM)或吸氣劑。Further, the first colloid may further comprise an Ethylene propylene diene monomer (EPDM) or a getter.

進一步地,該功能薄膜包含有一主膜體,以及二分別設置於該主膜體兩側的副膜體。Further, the functional film comprises a main film body, and two sub-film bodies respectively disposed on both sides of the main film body.

進一步地,該主膜體、每一該副膜體的材質選自聚乙烯醇縮丁醛(PVB)、乙烯醋酸乙烯酯(EVA)及熱塑性聚氨酯(TPU)所構成的群組,且該主膜體更添加有氧化錫摻銻(ATO)、氧化錫摻銦(ITO)、六硼化鑭(LaB 6)或氧化銫鎢 (CsWO 3)或上述兩種以上混合添加,並添加有紫外光吸收劑或光安定劑。該副膜體更添加有紫外線吸收劑或光安定劑。 Further, the material of the main film body and each of the sub-film bodies is selected from the group consisting of polyvinyl butyral (PVB), ethylene vinyl acetate (EVA), and thermoplastic polyurethane (TPU), and the main The film body is further added with tin oxide doped yttrium (ATO), tin oxide indium doped (ITO), lanthanum hexaboride (LaB 6 ) or yttrium tungsten oxide (CsWO 3 ) or a mixture of the above two or more, and added with ultraviolet light. Absorbent or light stabilizer. The submembrane body is further provided with an ultraviolet absorber or a light stabilizer.

進一步地,該容置空間的深度為2mm~15mm之間。Further, the depth of the accommodating space is between 2 mm and 15 mm.

進一步地,每一該透光基板係由玻璃、聚甲基丙烯酸甲酯(PMMA)、聚碳酸酯(PC)或聚乙烯(PE)所構成。Further, each of the light transmissive substrates is composed of glass, polymethyl methacrylate (PMMA), polycarbonate (PC) or polyethylene (PE).

是以,本創作較先前技術具有以下有益功效:Therefore, this creation has the following beneficial effects compared to the prior art:

1.本創作之薄型節能透光板係透過膠框環繞在透光基板與功能薄膜外側,藉此實現減少封邊體積並提高節能玻璃之耐水氣、耐熱等耐候性。1. The thin energy-saving light-transmissive plate of the present invention surrounds the transparent substrate and the functional film through the plastic frame, thereby reducing the sealing margin volume and improving the weather resistance of the energy-saving glass against moisture, heat and the like.

茲就本申請案的技術特徵暨操作方式舉數個較佳實施態樣,並配合圖示說明謹述於后,俾提供審查參閱。再者,本創作中之圖式,為便於說明其比例未必按實際比例繪製,圖式中之比例並不用以限制本創作所欲請求保護之範圍。For a more detailed description of the technical features and operation modes of the present application, and with reference to the illustrations, please refer to the review. In addition, the drawings in this creation are not necessarily drawn to scale in order to facilitate the description, and the proportions in the drawings are not intended to limit the scope of the claimed invention.

關於本創作之技術,請參照第1-1圖、第1-2圖、第2圖及第3圖所示,本創作提供一種薄型節能透光板100,包含有一透光單元10、以及一隔絕單元20。該薄型節能透光板100可用於建築物之窗戶,或是利用自然採光而會使太陽光照入室內之窗玻璃,如採光罩與玻璃帷幕牆,或是交通工具之前檔玻璃、側/後窗、及天窗等,惟上述僅為舉例說明,其應用在此不予限制。Regarding the technology of the present creation, please refer to FIG. 1-1, FIG. 1-2, FIG. 2 and FIG. 3, the present invention provides a thin energy-saving light-transmitting plate 100 comprising a light-transmitting unit 10 and a The unit 20 is isolated. The thin energy-saving light-transmitting plate 100 can be used for windows of buildings, or window glass that uses natural daylight to cause sunlight to enter the room, such as a hood and a glass curtain wall, or a front glass, side/rear window of the vehicle. And the sunroof, etc., but the above is only an example, and its application is not limited herein.

再參照第4圖及第5圖所示,具體而言,該透光單元10包含有一具黏性的功能薄膜12,二分別設置於該功能薄膜12兩側的透光基板11,以及一環繞在該功能薄膜12周圍並位於每一該透光基板11之間的容置空間13。於本實施態樣中,每一該透光基板11係為退火玻璃、強化或硬化玻璃,或是由聚甲基丙烯酸甲酯(PMMA)、聚碳酸酯(PC)或聚乙烯(PE)所構成之塑膠基板。該功能薄膜12包含有一主膜體121,以及二分別設置於該主膜體121兩側的副膜體122,該主膜體121、每一該副膜體122的材質包含但不限於聚乙烯醇縮丁醛(PVB)、乙烯醋酸乙烯酯(EVA)及熱塑性聚氨酯(TPU)所構成的群組,且該主膜體121亦可添加氧化錫摻銻(ATO)、氧化錫摻銦(ITO)、六硼化鑭(LaB 6)或氧化銫鎢(CsWO 3)等隔熱奈米漿料進一步提升紅外線吸熱效率。或是添入苯並三唑(Benzotrizoles)、巴斯夫公司(BASF SE)製售紫外線吸收劑Tinuvin P、Tinuvin 326、Tinuvin 328紫外線吸收劑,藉此賦予其抵抗紫外線之效果。該副膜體122亦添加有苯並三唑(Benzotrizoles)、巴斯夫公司(BASF SE)製售紫外線吸收劑Tinuvin P、Tinuvin 326、Tinuvin 328紫外線吸收劑,以提供該主膜體121全面性的抗紫外線保護。該容置空間13的深度較佳為2mm~15mm之間,以確保後續填膠能完整且確實地封合該容置空間13。 Referring to FIG. 4 and FIG. 5 , in particular, the light transmissive unit 10 includes a viscous functional film 12 , two transparent substrates 11 disposed on opposite sides of the functional film 12 , and a surrounding The accommodating space 13 is disposed around the functional film 12 and between each of the transparent substrates 11 . In this embodiment, each of the transparent substrates 11 is annealed glass, reinforced or hardened glass, or is made of polymethyl methacrylate (PMMA), polycarbonate (PC) or polyethylene (PE). The plastic substrate is constructed. The functional film 12 includes a main film body 121 and two sub-film bodies 122 respectively disposed on two sides of the main film body 121. The main film body 121 and the material of each of the sub-film bodies 122 include but are not limited to polyethylene. a group consisting of butyral butadiene aldehyde (PVB), ethylene vinyl acetate (EVA), and thermoplastic polyurethane (TPU), and the main film body 121 may also be added with tin oxide doped yttrium (ATO), tin oxide doped with indium (ITO). ), the insulating nano slurry such as lanthanum hexaboride (LaB 6 ) or strontium tungsten oxide (CsWO 3 ) further enhances the infrared heat absorption efficiency. Alternatively, Benzotrizoles and BASF SE are used to produce ultraviolet absorbers Tinuvin P, Tinuvin 326, and Tinuvin 328 ultraviolet absorbers, thereby imparting an ultraviolet-resistant effect. The sub-film body 122 is also added with Benzotrizoles, BASF SE, and UV absorbers Tinuvin P, Tinuvin 326, and Tinuvin 328 ultraviolet absorbers to provide comprehensive resistance of the main film body 121. UV protection. The depth of the accommodating space 13 is preferably between 2 mm and 15 mm to ensure that the subsequent filling can completely and surely seal the accommodating space 13.

該隔絕單元20包含有一灌注在該容置空間13中的第一膠體21,以及一由該第一膠體21與每一該透光基板11的邊緣共同構成的外環面22。此外,該隔絕單元20包含有一環繞該外環面22設置的第二膠體23,其中該第一膠體21係為丁基膠,或是混摻入三元乙烯丙烯橡膠(Ethylene propylene diene monomer, EPDM)或以鋯為主體之非蒸散型吸氣劑(getter),進一步提升耐候性並降低透水率以提高其防水、阻氣之效果,該第二膠體23係可為矽力康膠等結構膠,使整體更加穩固密合。基此,本創作薄型節能透光板100透過兩側的透光基板11、副膜體122,環繞外側的第一膠體21、第二膠體23等結構,可完善保護具有隔熱及抗紫外線功能之該主膜體121,並達成薄型化之目的。The insulating unit 20 includes a first colloid 21 filled in the accommodating space 13 and an outer annular surface 22 formed by the first colloid 21 and the edge of each of the transparent substrates 11. In addition, the isolation unit 20 includes a second colloid 23 disposed around the outer annular surface 22, wherein the first colloid 21 is a butyl rubber or is blended with an ethylene propylene diene monomer (EPDM). Or a non-evaporable getter with zirconium as the main body, further improving the weather resistance and reducing the water permeability to improve the effect of waterproofing and gas barrier. The second colloid 23 can be a structural adhesive such as 矽力康胶To make the whole more stable and close. Therefore, the thin-type energy-saving light-transmitting plate 100 of the present invention can pass through the transparent substrate 11 and the sub-film body 122 on both sides, and surrounds the outer first colloid 21 and the second colloid 23, thereby improving the protection against heat and ultraviolet rays. The main film body 121 is formed to have a reduced thickness.

以下進一步說明本創作薄型節能透光板100的製造方法。參照第3圖所示,首先,實施步驟S1.提供一具黏性的功能薄膜12,以及二分別夾設在該功能薄膜12兩側的透光基板11,此一步驟中,實際上可將該功能薄膜12預設為較每一該透光基板11面積更大的片體,將其鋪上其中一該透光基板11後,再蓋上另一該透光基板11,並將多餘的該功能薄膜12裁除。接續,實施步驟S2.加熱該功能薄膜12及每一該二透光基板11,使該功能薄膜12與每一該二透光基板11黏合,此步驟中可透過高壓爐(圖中未示)等設備加熱,加熱的溫度範圍約為攝氏115度~150度。接續,實施步驟S3.環繞刮除該功能薄膜12的邊緣,使每一該透光基板11間形成一容置空間13,本步驟中具體可利用如第4圖所示之一圓鋸片30深入每一該透光基板11之間的縫隙,並將該功能薄膜12部份割除。最後,參照第6圖所示,實施步驟S4.灌注一第一膠體21於該容置空間13,該第一膠體21與每一該透光基板11的邊緣共同構成一外環面22,本步驟中亦可將該容置空間13灌滿該第一膠體21並使膠液溢出,並將多餘的膠液刮除即可。進一步地,參照第7圖所示,所述之製造方法於步驟S4之後更包含有步驟S5. 設置一第二膠體23使其覆蓋該外環面22,使該薄型節能透光板100整體結構更為結實、穩固。此外,該第二膠體23亦可透過膠帶(圖未示)捲繞該外環面22所形成,使該隔離單元密封該功能薄膜12及每一該透光基板11之邊隙。藉此提高該薄型節能透光板100之耐水氣、耐熱等耐候性特質。The method of manufacturing the thin-type energy-saving light-transmitting plate 100 of the present invention will be further described below. Referring to FIG. 3, first, step S1 is performed to provide a viscous functional film 12, and two transparent substrates 11 respectively sandwiched on both sides of the functional film 12. In this step, The functional film 12 is preset to have a larger area than each of the transparent substrates 11 , and after laminating one of the transparent substrates 11 , the other transparent substrate 11 is covered, and the excess is replaced. The functional film 12 is cut. In the step S2, the functional film 12 and each of the two transparent substrates 11 are heated, and the functional film 12 is bonded to each of the two transparent substrates 11. In this step, the high-pressure furnace (not shown) can be passed through. When the equipment is heated, the heating temperature ranges from about 115 degrees Celsius to 150 degrees Celsius. In the step S3, the edge of the functional film 12 is scraped off, and an accommodating space 13 is formed between each of the transparent substrates 11. In this step, a circular saw blade 30 as shown in FIG. 4 can be specifically used. A gap between each of the transparent substrates 11 and a portion of the functional film 12 are cut off. Finally, referring to FIG. 6 , step S4 is performed to inject a first colloid 21 into the accommodating space 13 , and the first colloid 21 and the edge of each of the transparent substrate 11 together form an outer annular surface 22 . In the step, the accommodating space 13 can also fill the first colloid 21 and overflow the glue, and the excess glue can be scraped off. Further, referring to FIG. 7, the manufacturing method further includes step S5 after step S4. A second colloid 23 is disposed to cover the outer annular surface 22, so that the overall structure of the thin energy-saving light-transmitting plate 100 is Stronger and more stable. In addition, the second colloid 23 can also be formed by winding the outer ring surface 22 through a tape (not shown), so that the isolation unit seals the gap between the functional film 12 and each of the transparent substrates 11. Thereby, the weather resistance of the thin energy-saving light-transmitting sheet 100 against moisture, heat, and the like is improved.

綜上所述,本創作之薄型節能透光板100係透過環繞在透光基板11與功能薄膜12外側之膠框封合,藉此實現減少封邊體積並提高節能玻璃之耐水氣、耐熱等耐候性。In summary, the thin energy-saving light-transmitting plate 100 of the present invention is sealed by a plastic frame surrounding the transparent substrate 11 and the outer surface of the functional film 12, thereby reducing the volume of the edge-sealing and improving the moisture resistance and heat resistance of the energy-saving glass. Weather resistance.

100‧‧‧薄型節能透光板
10‧‧‧透光單元
11‧‧‧透光基板
12‧‧‧功能薄膜
121‧‧‧主膜體
122‧‧‧副膜體
13‧‧‧容置空間
20‧‧‧隔絕單元
21‧‧‧第一膠體
22‧‧‧外環面
23‧‧‧第二膠體
30‧‧‧圓鋸片
100‧‧‧Thin energy-saving light-transmissive plate
10‧‧‧Lighting unit
11‧‧‧Transparent substrate
12‧‧‧ functional film
121‧‧‧Main membrane body
122‧‧‧Submembrane body
13‧‧‧ accommodating space
20‧‧‧Isolation unit
21‧‧‧First colloid
22‧‧‧ outer annulus
23‧‧‧Second colloid
30‧‧‧Circular saw blade

第1-1圖:為本創作薄型節能透光板之立體圖。 第1-2圖:為本創作第1-1圖在A-A位置之剖視圖。 第2圖:為本創作透光基板與功能薄膜之立體分解圖。 第3圖:為本創作透光基板與功能薄膜之立體組合圖。 第4圖:為本創作設置容置空間之操作示意圖。 第5圖:為本創作透光基板與鑿設後功能薄膜之平面圖。 第6圖:為本創作設置第一膠體之操作示意圖。 第7圖:為本創作設置第二膠體之操作示意圖。Figure 1-1: A perspective view of a thin, energy-saving light-transmissive plate. Figure 1-2: A cross-sectional view of the A-A position of Figure 1-1 of this creation. Fig. 2 is an exploded perspective view of the transparent substrate and the functional film. Figure 3: The three-dimensional combination of the transparent substrate and the functional film. Figure 4: Schematic diagram of the operation of setting up the accommodating space for this creation. Figure 5: A plan view of the light-transmissive substrate and the functional film after the chiseling. Figure 6: Schematic diagram of the operation of setting the first colloid for this creation. Figure 7: Schematic diagram of the operation of setting the second colloid for this creation.

100‧‧‧薄型節能透光板 100‧‧‧Thin energy-saving light-transmissive plate

11‧‧‧透光基板 11‧‧‧Transparent substrate

12‧‧‧功能薄膜 12‧‧‧ functional film

121‧‧‧主膜體 121‧‧‧Main membrane body

122‧‧‧副膜體 122‧‧‧Submembrane body

20‧‧‧隔絕單元 20‧‧‧Isolation unit

21‧‧‧第一膠體 21‧‧‧First colloid

22‧‧‧外環面 22‧‧‧ outer annulus

23‧‧‧第二膠體 23‧‧‧Second colloid

Claims (8)

一種薄型節能透光板,包含有: 一透光單元,包含有一具黏性的功能薄膜,二分別設置於該功能薄膜兩側的透光基板,以及一環繞在該功能薄膜周圍並位於每一該透光基板之間的容置空間;以及 一隔絕單元,包含有一灌注在該容置空間中的第一膠體,以及一由該第一膠體與每一該透光基板的邊緣共同構成的外環面。A thin energy-saving light-transmitting plate comprises: a light-transmissive unit comprising a viscous functional film, two transparent substrates disposed on opposite sides of the functional film, and a surrounding around the functional film and located at each An accommodating space between the transparent substrates; and an insulating unit comprising a first colloid filled in the accommodating space, and an outer surface formed by the first colloid and the edge of each of the transparent substrates Torus. 如申請專利範圍第1項所述之薄型節能透光板,其中該隔絕單元包含有一環繞該外環面設置的第二膠體。The thin type energy-saving light-transmitting plate according to claim 1, wherein the insulation unit comprises a second gel disposed around the outer ring surface. 如申請專利範圍第2項所述之薄型節能透光板,其中該第一膠體係為丁基膠,該第二膠體係為矽力康膠。The thin type energy-saving light-transmitting plate according to claim 2, wherein the first glue system is butyl rubber, and the second glue system is piricon glue. 如申請專利範圍第3項所述之薄型節能透光板,其中該第一膠體包含有三元乙烯丙烯橡膠(Ethylene propylene diene monomer, EPDM)或吸氣劑。The thin type energy-saving light-transmitting plate according to claim 3, wherein the first colloid comprises an ethylene triene monomer (EPDM) or a getter. 如申請專利範圍第1項所述之薄型節能透光板,其中該功能薄膜包含有一主膜體,以及二分別設置於該主膜體兩側的副膜體。The thin type energy-saving light-transmitting plate according to claim 1, wherein the functional film comprises a main film body, and two sub-film bodies respectively disposed on two sides of the main film body. 如申請專利範圍第5項所述之薄型節能透光板,其中該主膜體、每一該副膜體的材質選自聚乙烯醇縮丁醛(PVB)、乙烯醋酸乙烯酯(EVA)及熱塑性聚氨酯(TPU)所構成的群組,且該主膜體更添加有氧化錫摻銻(ATO)、氧化錫摻銦(ITO)、六硼化鑭(LaB 6)或氧化銫鎢 (CsWO 3) 其一者或兩種以上的混合物。 The thin energy-saving light-transmitting plate according to claim 5, wherein the main film body and the material of each of the sub-film bodies are selected from the group consisting of polyvinyl butyral (PVB), ethylene vinyl acetate (EVA), and a group consisting of thermoplastic polyurethane (TPU), and the main film body is further added with tin oxide doped yttrium (ATO), tin oxide indium doped (ITO), lanthanum hexaboride (LaB 6 ) or yttrium tungsten oxide (CsWO 3 ) One or a mixture of two or more. 如申請專利範圍第1項所述之薄型節能透光板,其中該容置空間的深度為2mm~15mm之間。The thin energy-saving light-transmitting plate according to claim 1, wherein the depth of the accommodating space is between 2 mm and 15 mm. 如申請專利範圍第1項所述之薄型節能透光板,其中每一該透光基板係由玻璃、聚甲基丙烯酸甲酯(PMMA)、聚碳酸酯(PC)或聚乙烯(PE)所構成。The thin energy-saving light-transmitting plate according to claim 1, wherein each of the light-transmitting substrates is made of glass, polymethyl methacrylate (PMMA), polycarbonate (PC) or polyethylene (PE). Composition.
TW105207347U 2016-05-19 2016-05-19 Thin type energy-saving translucent panel TWM526952U (en)